• Title/Summary/Keyword: Natural adhesive

Search Result 160, Processing Time 0.032 seconds

Effect of Fiber Orientation on Failure Strength Properties of Natural Fiber Reinforced Composites including Adhesive Bonded Joint (접착제 접합된 자연섬유강화 복합재료의 파괴강도 특성에 미치는 섬유 방향의 영향)

  • Yoon, Ho-Chel
    • Journal of Welding and Joining
    • /
    • v.24 no.5
    • /
    • pp.43-48
    • /
    • 2006
  • This paper is concerned with a fracture strength study of composite adhesive lap joints. The tests were carried out on specimen joints manufactured hybrid stacked composites such as the polyester and bamboo natural fiber layer. The main objective of the work was to test the fracture strength using hybrid stacked composites with a polyester and bamboo natural fiber layer. Tensile and peel strength of hybrid stacked composites are tested before appling adhesive bonding. From results, Natural fiber reinforced composites have lower tensile strength than the original polyester. and The load directional orientation and small amount and low thickness of bamboo natural fiber layer have a good effect on the tensile and peel strength of natural fiber reinforced composites. The failure strength of these materials applied adhesive bonding is also affected by fiber orientation and thickness of bamboo natural fiber layer. There for, Fiber orientation of bamboo natural fiber layer have a great effect on the tensile-shear strength of natural fiber reinforced composites including adhesive bonded joints.

Effect of Spew Fillet on Failure Strength Properties of Natural Fiber Reinforced Composites Including Adhesive Bonded Joints (접착제 접합된 자연섬유강화 복합재료의 파괴강도 특성에 미치는 접착제 필릿의 영향)

  • Yoon Ho-Chel;Choi Jun-Yong;Kim Yong-Jig;Lim Jae-Kyoo
    • Journal of Welding and Joining
    • /
    • v.23 no.6
    • /
    • pp.67-71
    • /
    • 2005
  • This paper is concerned with a study on fracture strength of composites in an adhesive single lap joint. The tests were carried out on joint specimens made with hybrid stacked composites consisting of the polyester and bamboo natural fiber layer. The main objective of this work was to evaluate the fracture properties adjacent to adhesive bonded joint of natural fiber reinforced composite specimens. From the results, natural fiber reinforced composites have lower tensile strength than the original polyester. But tensile-shear strength of natural fiber reinforced composites with bamboo layer far from adhesive bond is as high as that of the original polyester adhesive bonded joints. Spew filet at the end of the overlap reduced the stress concentration at the bonded area. Spew fillet and position of bamboo natural fiber layer have a peat effect on the tensile-shear strength of natural fiber reinforced composites including adhesive bonded joints.

Natural Adhesives from Agricultural By-products: A Review

  • Kim, Min-Hyeok;Kim, Hye-Been;Cheong, Kyu-Min;Seo, Yu-Ri;Lim, Ki-Taek
    • Proceedings of the Korean Society for Agricultural Machinery Conference
    • /
    • 2017.04a
    • /
    • pp.111-111
    • /
    • 2017
  • There still exist adhesives that have toxic compounds or consist of those materials in both our life and lots of industries. For instance, formaldehyde adhesive had been still used for woodworking and some medical adhesives had been considered as toxicity problems. In this situation, natural adhesives from raw materials have been suggested as an one of considerable interests. Natural adhesives in recent have been reported fabrication methods via biological materials such as proteins, celluloses, and starches. By-products derived from agricultural something have them richly and each has additional special properties. Using these properties to make natural adhesives, unique adhesives would be attained. In particular, rice-based adhesive is such a good example. Rice-based by-product adhesives have interestingly some pros pertaining to high adhesive strength, excellent water resistance and could dramatically be reduced a formaldehyde a harmful component of plywood. Hence, rice-based adhesive like glues could be applied to lots of industries including agricultural and biological technology. This review paper highlighted some recent development on natural adhesives as a promising biomaterial for agricultural and biological technology fields. The design of agricultural by-product-based natural adhesives were described to demonstrate the application of agricultural and biological technology

  • PDF

Effect of Fiber Orientation on Failure Strength Properties of Natural Fiber Reinforced Composites including Adhesive Bonded Joints (접착제 접합된 자연섬유강화 복합재료의 파괴 강도특성에 미치는 섬유방향의 영향)

  • Im, Jae-Gyu;Yun, Ho-Cheol;Lee, Sang-Yong;Renliang, Wang
    • Proceedings of the KWS Conference
    • /
    • 2005.11a
    • /
    • pp.94-96
    • /
    • 2005
  • This paper is concerned with a fracture strength study of composite adhesive lap joints. The tensile and peel tests were carried out on specimen manufactured hybrid stacked composites such as the polyester and bamboo natural fiber layer. The main objective of the work was to test the failure strength of adhesive bonded joints using hybrid stacked composites with a polyester and bamboo natural fiber layer adjacent to the fiber orientation. From results, the load directional orientation, small amount and low thickness of bamboo natural fiber layer have a good effect on the tensile and peel strength of natural fiber reinforced composites. and these characters are have a great influence on fracture strength and failure shape of adhesive bonded joints using hybrid stacked composites in the difference of fiber orientation.

  • PDF

Influence of Heat-Treatment on the Adhesive Strength between a Micro-Sized Bonded Component and a Silicon Substrate under Bend and Shear Loading Conditions

  • Ishiyama, Chiemi
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.32 no.2
    • /
    • pp.122-130
    • /
    • 2012
  • Adhesive bend and shear tests of micro-sized bonded component have been performed to clarify the relationship between effects of heat-treatment on the adhesive strength and the bonded specimen shape using Weibull analysis. Multiple micro-sized SU-8 columns with four different diameters were fabricated on a Si substrate under the same fabrication condition. Heat-treatment can improve both of the adhesive bend and shear strength. The improvement rate of the adhesive shear strength is much larger than that of the adhesive bend strength, because the residual stress, which must change by heat-treatment, should effect more strongly on the shear loading. In case of bend type test, the adhesive bend strength in the smaller diameters (50 and $75\;{\mu}m$) widely vary, because the critical size of the natural defect (micro-crack) should vary more widely in the smaller diameters. In contrast, in case of shear type test, the adhesive shear strengths in each diameter of the columns little vary. This suggests that the size of the natural defects may not strongly influence on the adhesive shear strength. All the result suggests that both of the adhesive bend and shear strengths should be complicatedly affected by heat-treatment and the bonded columnar diameter.

Study on the filling material for the painting wall layer of the temple wall painting using a natural adhesive (천연 접착제를 활용한 사찰벽화 화벽층의 충전 재료연구)

  • Kim, Soon-Kwan;Jeong, Hye-Young
    • 보존과학연구
    • /
    • s.29
    • /
    • pp.255-278
    • /
    • 2008
  • Considering the physical quality of the wall body in this study we tried to select a replenishing that is proper for filling the cracked part of the painting wall layer and apply the natural adhesives that have traditionally been used, investigating whether it is possible to substitute those for the chemical adhesive which is used at present time. The result of this study showed the red algae adhesive was, in a weathering environment, as safe as the synthetic resin originated from the polyvinyl acetate which is used generally on the present spot, and it was concluded that although the starch adhesive displayed its superiority in enhancing the strength of the earth mortar and its work disposition, it seemed proper for it to be used as a filling adhesive for the first or midterm layer because it showed a surface hardening phenomenon. And also the glue and fish glue were judged they were not qualified as a filling adhesive due to mold occurring in a environment of high moisture that is a biological problem, showing at same time a weak physical feature in a weathering environment. Therefore it would be possible to use the red algae adhesive or starch one substituting them for the original one sold on the present market, if among natural adhesives the weak points of the them were to be corrected.

  • PDF

Effect of Spew fillet on Failure Strength Evaluation in Adhesive Bonded Joints involving Natural Fiber Reinforced Composites (접착제 접합된 자연섬유강화 복합재료의 파괴강도 특성에 미치는 접착제 필릿의 영향)

  • Kim, Yeon-Jik;Yun, Ho-Cheol;Im, Jae-Gyu
    • Proceedings of the KWS Conference
    • /
    • 2005.06a
    • /
    • pp.262-264
    • /
    • 2005
  • This paper is concerned with a fracture strength study of composite adhesive lap joints. The tests were carried out on specimen joints manufactured hybrid stacked joints such as the polyester and bamboo natural fiber layer. The main objective of the work was to test the fracture strength using hybrid fiber composites with a polyester and bamboo natural fiber layer adjacent to the spew fillet of adhesive bonded joints and hybrid stacked joints. The results are presented using tensile-shear strength graph and finite element analysis. The failure mechanisms are discussed in order to explain that spew fillet at the end of the overlap reduces greatly the adhesive shear and effects the tensile-shear strength in hybrid stacked joints.

  • PDF

A STUDY OF THE SHEAR BOND STRENGTH OF METAL BRACKETS AND CERAMIC BRACKETS AND THE CONDITION AFTER DEBONDING (Metal bracket과 ceramic bracket의 전단 결합 강도와 debonding 상태에 관한 연구)

  • Yoon, Jung-Jin;Ryu, Young-Kyu
    • The korean journal of orthodontics
    • /
    • v.22 no.2 s.37
    • /
    • pp.327-343
    • /
    • 1992
  • Metal brackets and ceramic brackets were bonded to natural teeth, porcelain crowns and gold crowns After stored in artificial saliva solution for 72 hours at $37^{\circ}C$, the shear bond strengths were measured by Instron and compared with them, the bonding sites and bracket bases were examined by scanning electron microscope and light optical stereomicroscope. The results were as follows: 1. The shear bond strengths of the group which metal brackets were bonded to natural teeth and the groups which ceramic brackets were bonded to natural teeth and porcelain crowns were comparable to each other, the shear bond strength of the group which metal brackets were bonded to gold crowns was significantly low. 2. The bond failed predominantly at the bracket base/adhesive interface with the bulk of adhesive remaining on enamel in the group which metal brackets were bonded to natural teeth. 3. The bond failed consistently at the crown/adhesive interface with all of adhesive remaining on the bracket babes in the group which metal brackets were bonded to gold crowns. 4. The bond failed at the enamel or crown/adhesive interface with the bulk of adhesive remaining on the bracket bases in the groups which cramic brackets were bonded to natural teeth and porcelain crowns. 5. The shear bond strengths of the groups which ceramic brackets were bonded to porcelain crowns were not affected by etching time.

  • PDF

Soybean-based Green Adhesive for Environment-friendly Furniture Material

  • Jeon, Ji-Soo;Lee, Jeong-Hun;Kim, Su-Min
    • Journal of the Korea Furniture Society
    • /
    • v.22 no.3
    • /
    • pp.174-182
    • /
    • 2011
  • Over the last decade, Sick Building Syndrome has become a significant social issue in Korea and many methods have been considered to maintain comfortable indoor air quality. To reduce toxic substances emitted from wood composite products, the source control is an efficient method through the reduction of formaldehyde content by using natural material-based adhesives for composite wood products production. Among alternative materials, soybean protein is considered an appropriate natural material to replace formaldehyde-based resin and many efforts have been made to produce new products, such as soap, shampoo, ink, resin, adhesive and textile through changing the chemical or physical properties of soybean. To process soybeans into these useful products, the beans are dehulled and the oil is removed by crushing at very high pressure or by solvent extraction. For use soybean as an adhesive, it is processed at temperatures below $70^{\circ}C$ to preserve the alkaline solubility of the proteins. In addition, soybean-based adhesive is undergone treatment process to improve mechanical properties using urea, urease inhibitor N-(n-butyl) thiophosphoric triamide and sodium dodecyl sulfate. The modified soybean-based adhesive exhibited sufficient mechanical properties to use as an adhesive for composite wood products. This paper is a review article to discuss the possibilities of soybean-based adhesive for environment-friendly furniture materials.

  • PDF

Mechanical Properties Analysis of Epoxy and Polyurethane Adhesive for Accurate Structural Analysis of LNG Cargo Hold (LNG 화물창 정밀 구조해석을 위한 에폭시와 폴리우레탄 접착제 기계적 물성치 분석)

  • Jeong, Yong-Cheol;Jeong, Yeon-Jae;Kim, Jeong-Dae;Park, Seong-Bo;Kim, Yong-Tai;Oh, Hoon-Gyu;Lee, Jae-Myung
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.58 no.2
    • /
    • pp.66-72
    • /
    • 2021
  • As the demand for natural gas that satisfies environmental regulations increases, the quantities of natural gas cargo that carrier can load is also increasing. Natural gas is transported in a liquefied state at -163 ℃ to increase loading efficiency. Among several LNG CCS types, MARK-III types are generally adopted in terms of loading efficiency. The secondary barrier adhesives of the MARK-III, nevertheless, is subjected to tensile stress due to thermal contraction and tension in the environment. In terms of these reasons, local analysis of the adhesive to evaluate the stress state must be carried out. According to previous studies, local analysis is unavailable since material properties for secondary barrier adhesives have not been reported. Thus, in this study, the cryogenic tensile test and coefficient of thermal expansion of epoxy and polyurethane (PU15, PU45), which are most widely used at cryogenic temperatures, were experimentally analyzed. At cryogenic temperature, the mechanical behavior of the polyurethane adhesive was better than epoxy of the adhesive. the joint of FSB and epoxy adhesive of the secondary barrier has the maximum coefficient of thermal expansion difference at 25 ℃ and minimum at -150 ℃, respectively.