Synthesis of Gold Nanoparticles by Chemical Reduction Method for Direct Ink Writing

  • Cho, Young-Sang;Son, Soo-Jung;Kim, Young-Kuk;Chung, Kook-Chae;Choi, Chul-Jin
    • 한국분말재료학회지
    • /
    • 제17권5호
    • /
    • pp.390-398
    • /
    • 2010
  • Aqueous gold nanoparticle dispersion was synthesized by chemical reduction method using diethanolamine as reducing agent and polyethyleneimine as dispersion stabilizer. The synthesis conditions for the stable dispersion of the gold nanoparticle suspension were determined by changing the amount of the reducing agent and dispersant during the wet chemical synthesis procedures. The face centered cubic lattice structure of the gold nanoparticles was confirmed by using X-ray diffraction and the morphologies of the nanoparticles were observed by transmission electron microscope. The synthesized gold nanoparticle dispersion was concentrated by evaporating the dispersion medium at room temperature followed by the addition of ethyleneglycol as humectant for the increase of the elastic properties to obtain gold nanoparticle inks for direct ink writing process. The line patterns were obtained with the gold nanoparticle inks during the writing procedures and the morphologies of the fine patterns were observed by scanning electron microscope.

전도성 잉크의 레이저 열경화 공정 시 온도에 따른 비저항 연구 (Study of Specific Resistance of Conductive Ink According to Temperature During Laser Sintering Process)

  • 이대건;박용한;박지용;김동근;문윤재;문승재;황준영;강희석
    • 대한기계학회논문집B
    • /
    • 제37권2호
    • /
    • pp.119-124
    • /
    • 2013
  • 본 연구에서는 전도성 잉크의 레이저 열경화 공정시 은 나노입자 잉크의 레이저 열경화 공정 온도를 수치해석하였다. 유리기판 위에 잉크젯 프린팅을 이용하여 인쇄한 은 나노 입자 잉크를 532 nm 파장의 CW 레이저를 각기 다른 세기로 60 초 동안 조사하여 가열하였다. 온도계산을 위해서, 열생성항에 들어가는 반사율을 구하였고, 레이저 조사 중 실시간 은 나노입자 잉크의 비저항을 측정하였다. 온도 계산은 2차원 열전도 방정식에 Wiedemann-Franz law 를 적용하였다. 그 결과, 레이저 조사로 인해 인쇄된 잉크의 온도가 상승할수록 비저항이 떨어지는 결과를 확인하였다.

Ultrafine ITO Nanoparticle for Ink Jet Printing

  • Hong, Sung-Jei;Kim, Yong-Hoon;Han, Jeong-In
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권1호
    • /
    • pp.467-470
    • /
    • 2007
  • Ultrafine Indium tin oxide (ITO) nanoparticle was successfully fabricated by low temperature synthetic method (LTSM). Mean size of ITO nanoparticle is 5 nm, and uniformly dispersed with (222) orientated cubic structure. Using the nanoparticle, ITO thin film with good optical and electrical properties was fabricated by inkjet printing.

  • PDF

Influence an Oxide Layer Thickness on Resistivity of Cu Conductive Film and Ink-jet Printing of Cu Nanoparticle Ink

  • Jeong, Sun-Ho;Woo, Kyoo-Hee;Kim, Dong-Jo;Lim, Soon-Kwon;Kim, Jang-Sub;Moon, Joo-Ho
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권1호
    • /
    • pp.724-726
    • /
    • 2007
  • We have developed the synthesis method to reduce the surface oxide layer in Cu nanoparticle, which is based on controlling the molecular weight of capping polymer. In addition, we demonstrated how the variation of oxide layer thickness influences the resistivity of conductive Cu film.

  • PDF

잉크젯에 의한 은나노 잉크의 패턴닝 및 소결 (Patterning and Sintering of Silver Nano Ink by the Ink-Jet Printing Technology)

  • 전명표;박명성;명성재;남중희;김병익
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.329-329
    • /
    • 2008
  • Silver nanoparticles were synthesized by polyol process and its particle size observed with TEM is about 20nm. Silver nanoparticle ink with metal content of 30wt% was prepared using solvent of ethanol and has low viscosity of 5cps (10rpm). This ink was printed by as ink-jet printer on Al2O3 and Silicone substrate. The resistivity and morphology of the printed film was investigated as a function of sintering termperature.

  • PDF

수계 Cu 나노입자 잉크에서 Poly(styrene-co-maleic acid) 접착 증진제가 잉크 레올로지와 인쇄패턴의 접착력에 미치는 영향 (Effects of Poly(Styrene-Co-Maleic acid) as Adhesion Promoter on Rheology of Aqueous Cu Nanoparticle Ink and Adhesion of Printed Cu Pattern on Polyimid Film)

  • 조예진;서영희;정선호;최영민;김의덕;오석헌;류병환
    • 한국재료학회지
    • /
    • 제25권12호
    • /
    • pp.719-726
    • /
    • 2015
  • For a decade, solution-processed functional materials and various printing technologies have attracted increasingly the significant interest in realizing low-cost flexible electronics. In this study, Cu nanoparticles are synthesized via the chemical reduction of Cu ions under inert atmosphere. To prevent interparticle agglomeration and surface oxidation, oleic acid is incorporated as a surface capping molecule and hydrazine is used as a reducing agent. To endow water-compatibility, the surface of synthesized Cu nanoparticles is modified by a mixture of carboxyl-terminated anionic polyelectrolyte and polyoxylethylene oleylamine ether. For reducing the surface tension and the evaporation rate of aqueous Cu nanoparticle inks, the solvent composition of Cu nanoparticle ink is designed as DI water:2-methoxy ethanol:glycerol:ethylene glycol = 50:20:5:25 wt%. The effects of poly(styrene-co-maleic acid) as an adhesion promoter(AP) on rheology of aqueous Cu nanoparticle inks and adhesion of Cu pattern printed on polyimid films are investigated. The 40 wt% aqueous Cu nanoparticle inks with 0.5 wt% of Poly(styrene-co-maleic acid) show the "Newtonian flow" and has a low viscosity under $10mPa{\cdots}S$, which is applicable to inkjet printing. The Cu patterns with a linewidth of $50{\sim}60{\mu}m$ are successfully fabricated. With the addition of Poly(styrene-co-maleic acid), the adhesion of printed Cu patterns on polyimid films is superior to those of patterns prepared from Poly(styrene-co-maleic acid)-free inks. The resistivities of Cu films are measured to be $10{\sim}15{\mu}{\Omega}{\cdot}cm$ at annealing temperature of $300^{\circ}C$.