• Title/Summary/Keyword: Monolithic crown

Search Result 44, Processing Time 0.025 seconds

Monolithic zirconia crowns: effect of thickness reduction on fatigue behavior and failure load

  • Prott, Lea Sophia;Spitznagel, Frank Akito;Bonfante, Estevam Augusto;Malassa, Meike Anne;Gierthmuehlen, Petra Christine
    • The Journal of Advanced Prosthodontics
    • /
    • v.13 no.5
    • /
    • pp.269-280
    • /
    • 2021
  • PURPOSE. The objective of this study was to evaluate the effect of thickness reduction and fatigue on the failure load of monolithic zirconia crowns. MATERIALS AND METHODS. 140 CAD-CAM fabricated crowns (3Y-TZP, inCorisTZI, Dentsply-Sirona) with different ceramic thicknesses (2.0, 1.5, 1.0, 0.8, 0.5 mm, respectively, named G2, G1.5, G1, G0.8, and G0.5) were investigated. Dies of a mandibular first molar were made of composite resin. The zirconia crowns were luted with a resin composite cement (RelyX Unicem 2 Automix, 3M ESPE). Half of the specimens (n = 14 per group) were mouth-motion-fatigued (1.2 million cycles, 1.6 Hz, 200 N/ 5 - 55℃, groups named G2-F, G1.5-F, G1-F, G0.8-F, and G0.5-F). Single-load to failure was performed using a universal testing-machine. Fracture modes were analyzed. Data were statistically analyzed using a Weibull 2-parameter distribution (90% CI) to determine the characteristic strength and Weibull modulus differences among the groups. RESULTS. Three crowns (21%) of G0.8 and five crowns (36%) of G0.5 showed cracks after fatigue. Characteristic strength was the highest for G2, followed by G1.5. Intermediate values were observed for G1 and G1-F, followed by significantly lower values for G0.8, G0.8-F, and G0.5, and the lowest for G0.5-F. Weibull modulus was the lowest for G0.8, intermediate for G0.8-F and G0.5, and significantly higher for the remaining groups. Fatigue only affected G0.5-F. CONCLUSION. Reduced crown thickness lead to reduced characteristic strength, even under failure loads that exceed physiological chewing forces. Fatigue significantly reduced the failure load of 0.5 mm monolithic 3Y-TZP crowns.

Capillary Electrochromatography with Liquid Crystal Crown Ether Modified Hybrid Silica Monolith for Analysis of Imidacloprid and Carbendazim in Tomatoes

  • Wang, Mingming;Feng, Rui;Shen, Jing;Chen, Hao;Zeng, Zhaorui
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.7
    • /
    • pp.2224-2228
    • /
    • 2012
  • This study describes the ability of capillary electrochromatography (CEC) for the determination of imidacloprid and carbendazim in tomato samples. A novel liquid crystal crown ether modified hybrid silica monolithic column was synthesized, characterized and developed as separation column for the first time. Baseline separation of imidacloprid and carbendazim could be achieved using a mobile phase containing 90% (v/v) 20 mmol/L phosphate buffer (pH 7.0) and 10% (v/v) acetonitrile. The matrix matched calibration curves were linear with correlation coefficient $r^2$ > 0.9998 in the range of 0.20-10.00 mg/L. The limits of detection for imidacloprid and carbendazim were 0.061 and 0.15 mg/kg, respectively, which were below the maximum residue limits established by the European Union as well as Codex Alimentarius. Average recoveries for imidacloprid and carbendazim varied from 101.6-108.0% with relative standard deviations lower than 6.3%. This method was applied to the analysis of tomatoes collected from local markets.

A simple technique for impression taking of teeth and functionally generated paths

  • Yamamoto, Takatsugu;Sato, Yohei;Watanabe, Hidehiko;Punj, Amit;Abe, Minoru;Momoi, Yasuko;Ohkubo, Chikahiro
    • Restorative Dentistry and Endodontics
    • /
    • v.43 no.1
    • /
    • pp.9.1-9.6
    • /
    • 2018
  • The objective of this case report is to introduce a simple technique for simultaneously taking a closed-mouth impression and functionally generated path (FGP) for a full coverage crown restoration. A monolithic zirconia crown was the restoration of choice. An alginate impression of the abutment tooth was taken to fabricate a custom-made closed-mouth impression tray covering the abutment tooth and the adjacent teeth. The tray had an FGP table and an abutment tray in cameo and intaglio surfaces, respectively. The impression was taken with silicone impression material after adjusting the abutment tray and inscribing the FGP using self-curing acrylic resins. Plaster casts were made from the impression, and a zirconia crown was fabricated. The crown was cemented to the abutment tooth with minimal adjustments. This simple technique resulted in a well-fitting crown that accounted for mandibular movements. Using the custom closed-mouth impression tray incorporating an FGP table simultaneously aids in fabricating an accurately fitting restoration that incorporates harmonious mandibular movements using a single impression capture.

Six-year clinical performance of lithium disilicate glass-ceramic CAD-CAM versus metal-ceramic crowns

  • Ahmed Aziz;Omar El-Mowafy
    • The Journal of Advanced Prosthodontics
    • /
    • v.15 no.1
    • /
    • pp.44-54
    • /
    • 2023
  • PURPOSE. To assess the clinical performance of monolithic CAD-CAM lithium disilicate glass-ceramic (LDGC) crowns and metal-ceramic (MC) crowns provided by predoctoral students. This study also assessed the effects of patient and provider-related factors on their clinical performance as well as patient preference for these types of crowns. MATERIALS AND METHODS. Twenty-five patients who received 50 crowns (25 LDGC CAD-CAM and 25 MC) provided by predoctoral students were retrospectively examined. LDGC CAD-CAM crowns were milled in-house using the CEREC Bluecam system and cemented with either RelyX Unicem or Calibra Esthetic resin cements. MC crowns were cemented with RelyX Unicem cement. Clinical assessment of the crowns and the supporting periodontal structures were performed following the modified California Dental Association (CDA) criteria. Patients' preference was recorded using a visual analog scale (VAS). The results were statistically analyzed using log-rank test, Pearson Chi-squared test and Kaplan-Meier survival analysis. RESULTS. Twelve complications were observed in the MC crown group (9-esthetic, 2-technical and 1-biological). In comparison, 2 complications in the LDGC CAD-CAM crown group were observed (1-technical and 1-esthetic). The 6-year cumulative survival rates for MC crowns and LDGC CAD-CAM were 90.8% and 96%, respectively, whereas the success rates were 83.4% and 96%, respectively. Overall, patients preferred the esthetic outcomes of LDGC CAD-CAM crowns over MC crowns. CONCLUSION. The high survival and success rates, low number of complications, and the high level of patients' acceptance of monolithic LDGC CAD-CAM crowns lend them well as predictable and viable alternatives to the "gold standard" MC crowns.

Comparison of the marginal fit of milled yttrium stabilized zirconium dioxide crowns obtained by scanning silicone impressions and by scanning stone replicas

  • Yus, Estefania Aranda;Cantarell, Josep Maria Anglada;Alonso, Antonio Minarro
    • The Journal of Advanced Prosthodontics
    • /
    • v.10 no.3
    • /
    • pp.236-244
    • /
    • 2018
  • PURPOSE. To determine the discrepancy in monolithic zirconium dioxide crowns made with computer-aided design and computer-aided manufacturing (CAD/CAM) systems by comparing scans of silicone impressions and of master casts. MATERIALS AND METHODS. From a Cr-Co master die of a first upper left molar, 30 silicone impressions were taken. The 30 silicone impressions were scanned with the laboratory scanner, thus obtaining 30 milled monolithic yttrium stabilized zirconium dioxide (YSZD) crowns (the silicone group). They were poured and the working models were scanned, obtaining 30 milled monolithic yttrium stabilized zirconium dioxide (YSZD) crowns (the plaster group). Three predetermined points were analyzed in each side of the crown (Mesial, Distal, Vestibular and Palatal), and the marginal fit was evaluated with SEM (${\times}600$). The response variable is the discrepancy from the master model. A repeated measures ANOVA with two within subject factors was performed to study significance of main factors and interaction. RESULTS. Mean marginal discrepancy was $22.42{\pm}35.65{\mu}m$ in the silicone group and $8.94{\pm}14.69{\mu}m$ in the plaster group. The statistical analysis showed significant differences between the two groups and also among the four aspects. Interaction was also significant (P=.02). CONCLUSION. The mean marginal fit values of the two groups were within the clinically acceptable values. Significant differences were found between the groups according to the aspects studied. Various factors influenced the accuracy of digitizing, such as the design, the geometry, and the preparation guidance, as well as the texture, roughness and the color of the scanned material.

Comparison of the fit accuracy of zirconia-based prostheses generated by two CAD/CAM systems

  • Ha, Seok-Joon;Cho, Jin-Hyun
    • The Journal of Advanced Prosthodontics
    • /
    • v.8 no.6
    • /
    • pp.439-448
    • /
    • 2016
  • PURPOSE. The purposes of this study are to evaluate the internal and marginal adaptation of two widely used CAD/CAM systems and to study the effect of porcelain press veneering process on the prosthesis adaptation. MATERIALS AND METHODS. Molar of a lower jaw typodont resin model was prepared by adjusting a 1.0 mm circumferential chamfer, an occlusal reduction of 2.0 mm, and a $5^{\circ}$ convergence angle and was duplicated as an abrasion-resistant master die. The monolithic crowns and copings were fabricated with two different CAD/CAM system-Ceramil and Zirkonzahn systems. Two kinds of non-destructive analysis methods are used in this study. First, weight technique was used to determine the overall fitting accuracy. And, to evaluate internal and marginal fit of specific part, replica technique procedures were performed. RESULTS. The silicone weight for the cement space of monolithic crowns and copings manufactured with Ceramil system was significantly higher than that from Zirkonzahn system. This gap might cause the differences in the silicone weight because the prostheses were manufactured according to the recommendation of each system. Marginal discrepancies of copings made with Ceramil system were between 106 and $117{\mu}m$ and those from Zirkonzahn system were between 111 and $115{\mu}m$. Marginal discrepancies of copings made with Ceramil system were between 101 and $131{\mu}m$ and those from Zirkonzahn system were between 116 and $131{\mu}m$. CONCLUSION. Marginal discrepancy was relatively lower in Ceramil system and internal gap was smaller in Zirkonzahn system. There were significant differences in the internal gap of monolithic crown and coping among the 2 CAD/CAM systems. Marginal discrepancy produced from the 2 CAD/CAM systems were within a reported clinically acceptable range of marginal discrepancy.

The effect of reduced thickness in different regions on the fracture resistance of monolithic zirconia crowns (다양한 부위에서의 감소된 두께가 지르코니아 크라운의 파절 저항에 미치는 영향)

  • Abukabbos, Layla;Park, Je Uk;Lee, Wonsup
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.60 no.2
    • /
    • pp.135-142
    • /
    • 2022
  • Purpose. This study aims to evaluate the combined effect of reduced thickness in different regions on the fracture resistance of monolithic zirconia crowns. Materials and methods. Seven nickel-chromium dies were generated from a 3D model of mandibular first molar using the digital scanner with the following geometries: 1.5 mm occlusal reduction, 1.0 mm deep chamfer. Based on the abutment model, Zirconia blocks (Luxen Zirconia) were selected to fabricate Sixty-three zirconia crowns with occlusal thicknesses of 0.3 mm, 0.5 mm, and 1.5 mm, and different axial thicknesses of 0.3 mm, 0.5 mm, and 1.0 mm. All crowns were cemented by resin cement. Next, the crowns were subjected to load-to-fracture test until fracture using an electronic universal testing machine. In addition, fracture patterns were observed with a scanning electron microscope (SEM). Two-way ANOVA and the Tuckey HSD test for post hoc analysis were used for statistical analysis (P < .05). Results. The mean values of fracture resistancerecorded was higher than the average biting force in the posterior region. The two-way ANOVA showed that the occlusal and axial thickness affected the fracture resistance significantly (P < .05). However, the effect of axial thickness on fracture resistance did not show a statistical difference when thicker than 0.5 mm. The observed failure modes were partial or complete fracture depending on the severity of crack propagation. Conclusion. Within the limitations of the present study, the CAD-CAM monolithic zirconia crown with extremely reduced thickness showed adequate fracture resistance to withstand occlusal load in molar regions. In addition, both occlusal and axial thickness affected the fracture resistance of the zirconia crown and showed different results as combined.

Implant-supported fixed prostheses with high-performance polymer (PEKK) abutments in partial edentulous patients: A case report (부분 무치악 환자에서 고기능성 폴리머(PEKK) 지대주를 이용한 임플란트 고정성 보철물 수복 증례)

  • Ha, Seung-Ryong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.59 no.1
    • /
    • pp.71-78
    • /
    • 2021
  • Implant treatment, which was first attempted in fully edentulous patients, is now widely used in partially edentulous, and a single tooth missing patients. Moreover, implant treatment has become an essential treatment modality in modern dentistry. The material of fabricating implant prostheses has also become more diverse than before, one of which is the use of high-performance polymers. The frequency of using high-performance polymers, which have been used in the medical field, is also increased in the dental field compared to the past. In the first case, a PEKK abutment and a PFG crown (cement-screw-retaining type) were fabricated in the lower left second premolar, and in the second case, a PEKK abutment and a monolithic zirconia crown (cement-screw-retaining type) were fabricated in the missing upper left first molar, and in the third case two PEKK abutments and a splinted PFM crowns (cement-screw-retaining type) were fabricated and connected to the upper right first and second molar implants. Through these procedures the patients obtained esthetically and functionally satisfactory results after 4 years of follow-up.

Full mouth rehabilitation with vertical dimension increase in patient with severly worn dentition (과도한 치아 마모를 보이는 환자에서 수직고경 증가를 동반한 전악 구강 회복 증례)

  • Jo, Wi-Sang;Kim, Seong-A;Kim, Sung-Yong;Bang, Joo-Hyuk
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.59 no.1
    • /
    • pp.107-115
    • /
    • 2021
  • Excessive pathological attrition over the entire dentition can cause decreased masticatory function, and pathological problems of the temporomandibular joint and the muscular nervous system. In this case, 71 year-old male patient with severe attrition and fracture across the entire tooth was treated by full mouth rehabilitation for regaining space of restoration. In order to determine the appropriate vertical dimension of the patient's occlusion, facial appearance, aesthetics, restoration space were evaluated, and provisional restoration of the raised vertical dimension was made. After 4 months of evaluation, the entire restoration of monolithic zirconia crown using CAD-CAM was completed. Through the above process, satisfactory aesthetic and functional results were obtained.

Effect of abutment types and resin cements on the esthetics of implant-supported restorations

  • Asena Ceken;Hamiyet Kilinc;Sedanur Turgut
    • The Journal of Advanced Prosthodontics
    • /
    • v.15 no.3
    • /
    • pp.114-125
    • /
    • 2023
  • PURPOSE. The aim of the study was to evaluate the optical properties of new generation (3Y-TZP) monolithic zirconia (MZ) with different abutment types and resin cement shades. MATERIALS AND METHODS. A1/LT MZ specimens were prepared (10 × 12 × 1 mm, N = 30) and divided into 3 groups according to cement shades as transparent (Tr), yellow (Y) and opaque (O). Abutment specimens were obtained from 4 different materials including zirconia (Group Z), hybrid (Group H), titanium (Group T) and anodized yellow titanium (Group AT). MZ and abutment specimens were then cemented. L*, a*, and b* parameters were obtained from MZ, MZ + abutment, and MZ + abutment + cement. ∆E001* (between MZ and MZ + abutment), ∆E002* (between MZ and MZ + abutment + cement) and ∆E003* (between MZ + abutment and MZ + abutment + cement) values were calculated. Statistical analyses included 2-way ANOVA, Bonferroni, and Paired Sample t-Tests (P < .05). RESULTS. Abutment types and resin cements had significant effect on L*, a*, b*, ∆E001*, ∆E002*, and ∆E003* values (P < .001). Without cementation, whereas zirconia abutment resulted in the least discoloration (∆E001* = 0.68), titanium abutment caused the most discoloration (∆E001* = 4.99). The least ∆E002* = 0.68 value was seen using zirconia abutment after cementation with yellow shaded cement. Opaque shaded cement caused the most color change (∆E003* = 5.24). Cement application increased the L* values in all groups. CONCLUSION. The least color change with/without cement was observed in crown configurations created with zirconia abutments. Zirconia and hybrid abutments produced significantly lower ∆E002* and ∆E003* values in combination with yellow shaded cement. The usage of opaque shaded cement in titanium/anodized titanium groups may enable the clinically unacceptable ∆E00* value to reach the acceptable level.