Sol-Gel법에 의한$ZrO_2$ Ceramic Fiber 제조 ($ZrO_2$ Ceramic Fiber Fabrication by Sol-Gel Processing)

  • 김선욱;김성숭
    • 한국세라믹학회지
    • /
    • 제27권6호
    • /
    • pp.824-828
    • /
    • 1990
  • Zirconia gel fibers were fabricated by sol-gel processing using zirconium alkoxides and 2, 4-pentanedione. Their phase transformation and microstructural evolution were studied after heat treatments up to 150$0^{\circ}C$. Tetragonal ZrO2 began to form at 50$0^{\circ}C$ and followed by monoclinic, tetragonal phase during subsequent heat treatments at 1000, 150$0^{\circ}C$ for 1hour respectively. During cooling from 150$0^{\circ}C$, cracks were created, propagated along grain boundaries due to the volume change from tetragonal to monoclinic transformation.

  • PDF

Ni3Al-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B 합금의 고온산화막분석 (Characterization of Oxide Scales Formed on Ni3Al-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B)

  • 김기영;이동복
    • 한국재료학회지
    • /
    • 제12권3호
    • /
    • pp.220-224
    • /
    • 2002
  • The oxide scales formed on $Ni_3Al$-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B after oxidation at 900, 1000 and 110$0^{\circ}C$ in air were studied using XRD, SEM, EPMA and TEM. The oxide scales consisted primarily of $NiO,\; NiAl_2O_4,\;{\alpha}-Al_2O_3,\; monoclinic-ZrO_2,\; and \;tetragonal-ZrO_2$. The outer layer of the oxide scale was rich in Ni-oxides, whereas the internal oxide stringers were rich in Al-oxides and $ZrO_2$. Within the above oxide scales, Cr and Mo tended to exist as dissolved ions.

저온 준안정상 $ZrO_2$의 안정화 (Stabilization of Low-Temperature Metastable Phase of $ZrO_2$)

  • 오영제;정형진;이희수
    • 한국세라믹학회지
    • /
    • 제27권5호
    • /
    • pp.613-618
    • /
    • 1990
  • The pure and 6mol% MgO-doped ZrO2 powders were prepared by hot petroleum drying method. The power characterization of homogeneous fine powder was indentified by the method of thermal analysis, BET and electron microscope. The transformation, content of t-ZrO2, crystallite size and apparent strain were measured by X-ray diffraction technique. The prepared powders were transformed in order of amorphouslongrightarrowmetastable cubic ZrO2longrightarrowmetastable tetragonal ZrO2longrightarrowstable monoclinic ZrO2 by a adequate heat treatment. The stabilization of metastable phase can be discussed in terms of energetial concept ; the difference of surface energy and internal strain in particle.

  • PDF

Zr-2.5Nb 합금의 부식거동에 대한 부식환경 효과

  • 주기남;권상철;김영석
    • 한국원자력학회:학술대회논문집
    • /
    • 한국원자력학회 1996년도 추계학술발표회논문집(2)
    • /
    • pp.533-538
    • /
    • 1996
  • 40$0^{\circ}C$ $H_2O$, D$_2$O 및 $O_2$ 분위기에서 Zr-2.5wt% Nb 합금의 부식거동을 비교.분석하였다. Zr-2.5wt% Nb 합금은 열처리에 따른 조직에 따라 각각의 부식매질에 대해 부식거동이 큰 차이를 보이고 있으나, 형성된 oxide는 열처리 및 부식매질에 관계없이 monoclinic ZrO$_2$ 만이 관찰되었다. 급냉조직인 martensitic $\alpha$'-Zr 상과 소둔처리 조직의 준안정상인 $\beta$-Zr 상의 경우. 부식분위기에 매우 민감하여, D$_2$O, H $_2$O, $O_2$ 순으로 큰 부식속도를 보였다. 반면, 안전성들인 $\alpha$-Zr과 $\beta$-Nb 상의 경우, 부식 분위기에 따른 별다른 부식거동 차이를 보이지 않았다. 이들 실험 결과를 바탕으로 월성형 원자로 압력관의 부식특성을 분석하였다.

  • PDF

Preparation and Characterization of NiO/CeO2-ZrO2/WO3 Catalyst for Ethylene Dimerization: Effect of CeO2 Doping and WO3 Modifying on Catalytic Activity

  • Sohn, Jong-Rack;Han, Jong-Soo;Kim, Hae-Won;Pae, Young-Il
    • Bulletin of the Korean Chemical Society
    • /
    • 제26권5호
    • /
    • pp.755-762
    • /
    • 2005
  • A series of catalysts, NiO/$CeO_2-ZrO_2/WO_3$, for ethylene dimerization was prepared by the precipitation and impregnation methods. For NiO/$CeO_2-ZrO_2/WO_3$ sample, no diffraction line of nickel oxide was observed up to 40 wt%, indicating good dispersion of nickel oxide on the surface of catalyst. The hexagonal and monoclinic phases of $WO_3$ up to the calcination temperature of 500 ${^{\circ}C}$ were observed, whereas the hexagonal phase of WO3 completely was transformed into monoclinic phase of $WO_3$ at 600 ${^{\circ}C}$ and above. The role of $CeO_2$ in the catalysts was to form a thermally stable solid solution with zirconia and consequently to give high surface area and acidity. The catalytic activities for ethylene dimerization were correlated with the acidity of catalysts measured by the ammonia chemisorption method. 25-NiO/5-$CeO_2-ZrO_2/15-WO_3$ containing 25 wt% NiO, 15 wt% $WO_3$ and 5 mol% $CeO_2$, and calcined at 400 ${^{\circ}C}$ exhibited a maximum catalytic activity due to the effects of $WO_3$ modifying and $CeO_2$ doping.

$ZrO_2$를 이차상으로한 복합체의 기계적 특성 (A Study on the Mechanical Properties of $ZrO_2$ Based Composite)

  • 신동우;김종희
    • 한국세라믹학회지
    • /
    • 제22권5호
    • /
    • pp.76-84
    • /
    • 1985
  • Mechanical property enhancing mechanisms of $Al_2O_3-ZrO_2$ two phase ceramic composites were studied for several compositions of different $ZrO_2$/$Al_2O_3$ ratio. Microstructural analysis of $Al_2O_3-ZrO_3$(pure) composites indicated that pre-existing microcrack due to larger $ZrO_2$ particle at grain boundary extended along alumina grain boundaries within process zone. Microcracks also nucleated when very small $ZrO_2$ particles at the grain boundaries transformed to monoclinic phase at near of main crack tip. These types of microcracks could contribute to the toughening achieved by creating additional crack surface area during crack propagation. Microstructural analyses also showed that the average grain size and abnormal grain size of $Al_2O_3$ were decreased with increasing $ZrO_2$ vol% in $Al_2O_3$ matrix. As a result it could be concluded as follows In TEX>$Al_2O_3-ZrO_3$(pure) system 1. Microcrack nucleation (stress-induced microcracking) and extension was effective mechanism for absorpiton of fracture energy 2, More narrow distribution and smaller grain size of $Al_2O_3$ due to $ZrO_2$particles mainly contributed to main-tatin the strength and hardness.

  • PDF

Synthesis of Zirconium Oxides on silicon by Radio-Frequency Magnetron Sputtering Deposition

  • Ma, Chunyu;Zhang, Qingyu
    • 한국진공학회지
    • /
    • 제12권S1호
    • /
    • pp.83-87
    • /
    • 2003
  • Zirconium oxide films have been synthesized by radio-frequency magnetron sputtering deposition on n-Si(001) substrate with metal zirconium target at variant $O_2$ partial pressures. The influences of $O_2$ partial pressures of the morphology, deposition rate, microstructure, and the dielectric constant of $ZrO_2$ have been discussed. The results show that deposition rate of $ZrO_2$ films decreases, the roughness, and the thickness of the native $SiO_2$ interlayer increases with the increase of $O_2$ partial pressure. $ZrO_2$ films synthesized at low $O_2$ partial pressure are amorphous and monoclinic polycrystalline in nanometer scale at low $O_2$ partial pressure. The relative dielectrics of $ZrO_2$ films are in the range of 12 to 25.

금속 알콕사이드법에 의한 구형의 단분산 $ZrO_2$ 미립자의 제조 (Preparation of Spherical Monodispersed $ZrO_2$ Fine Powders by Metal Alkoxide Method)

  • 김병익;민경소;최상흘
    • 한국세라믹학회지
    • /
    • 제27권8호
    • /
    • pp.1064-1070
    • /
    • 1990
  • ZrO2 fine powders were prepared by hydrolysis, adding 0.1, 0.2, 0.3, 0.4, 0.5, 0.6mol/1H2O/ethanol to 0.1 mol/l Zr(OC3H7)4/ethanol. When hydrolized by adding 0.1mol/l Zr(OC3H7)4/ethanol to 0.1, 0.2mol/l H2O/ethanol., spherical monodispersed ZrO2 fine powders were obtained. And in this condition average sizes were about 0.5, 0.3${\mu}{\textrm}{m}$, respectively. The more H2O/ethanol concentration increased, the more the particle size decreased and the particles were agglomerated strongly. Prepared powders were amorphous and hydrates. The calcined powders with 43$0^{\circ}C$ and 100$0^{\circ}C$ were showed tetragonal and monoclinic phase, respectively.

  • PDF

Heat Treatment Effects on the Phase Evolutions of Partially Stabilized Grade Zirconia Plasma Sprayed Coatings

  • Park, Han-Shin;Kim, Hyung-Jun;Lee, Chang-Hee
    • 한국표면공학회지
    • /
    • 제34권5호
    • /
    • pp.486-493
    • /
    • 2001
  • Partially stabilized zirconia (PSZ) is an attractive material for thermal barrier coating. Zirconia exists in three crystallographic phases: cubic, tetragonal and monoclinic. Especially, the phase transformation of tetragonal phase to monoclinic phase accompanies significant volume expansion, so this transition generally results in cracking and contributes to the failure of the TBC system. Both the plasma sprayed ZrO$_2$-8Y$_2$O$_3$ (YSZ) coat and the ZrO$_2$,-25CeO$_2$,-2.5Y$_2$O$_3$ (CYSZ) coat are isothermally heat -treated at 130$0^{\circ}C$ and 150$0^{\circ}C$ for 100hr and cooled at different cooling rates. The monoclinic phase is not discovered in all the CYSZ annealed at 130$0^{\circ}C$ and 150$0^{\circ}C$. In the 150$0^{\circ}C$ heat-treated specimens, the YSZ contains some monoclinic phase while none exists in the 130$0^{\circ}C$ heat-treated YSZ coat. For the YSZ, the different phase transformation behaviors at the two temperatures are due to the stabilizer concentration of high temperature phases and grain growth. For the YSZ with 150$0^{\circ}C$-100hr annealing, the amount of monoclinic phase increased with the slower cooling rate. The extra oxygen vacancy, thermal stress, and c to t'phase transformation might suppress the t to m martensitic phase transformation.

  • PDF

Fabrication of Crystalline $ZrO_2$ Nanotubes by ALD

  • 김현철;;유현준;김명준;양윤정;이선희;신현정
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.241.1-241.1
    • /
    • 2011
  • Numerous possible applications for $ZrO_2$ nanotubes exist such as for catalyst support structures, for sensing or for applications as a solid state electrolyte. Especially, because of a large specific surface area, high efficiency for solid oxide fuel cell (SOFC) application at low temperature can be expected for nanotublar structures in even small size. A zirconium precursor, Tetrakis (ethylmethylamino) zirconium, TEMAZr and $H_2O$ oxidant were used to deposit$ZrO_2$ thin films on an anodized aluminum oxide (AAO) templates having sub-100nm cylindrical pores by atomic layer deposition (ALD) in the temperature range of 150~250$^{\circ}C$. The crystalline structures of as-prepared and post-annealed $ZrO_2$ nanotubes were characterized by x-ray diffraction and high-resolution transmission electron microscopy. The as-prepared samples at $150^{\circ}C$ and $200^{\circ}C$ were showed amorphous, whereas a mixed phase of tetragonal, monoclinic and amorphous polymorph was observed at $250^{\circ}C$. In the bulk, zirconia remains monoclinic phase up to $1,175^{\circ}C$, however, $ZrO_2$ nanotubes were showed tetragonal phase upon post thermal treatments merely at $400^{\circ}C$. This trend may be indicative of high-curvature surfaces of nanotubes and thereby the presence of intrinsic compressive strain. The amount of amorphous structures in the mixed phase as well as as-grown $ZrO_2$ nanotubes were also gradually decreased by subsequent heat treatment.

  • PDF