Rice hull was reduced to ash by carbonization grades to illcuidate alkalinity increase and extract of inorganic nutrients in the rice hull charcoal. Alkaline reaction of water extraction was neutral at less carbonized charcoal, but much carbonized ash from 65% weight loss reached over 10 of pH value, also origin shape of rice hull was maintained until near 65% carbonized grade. Therefore, physical properties sustained good condition for seedling bed. The more charcoal carbonized to ash, the pH value and concentration of inorganic nutrient in their extracts were increased gradually. Nitric acid concentrations for neutralizing extract from charcoal were stronger in proportion to the carbonized grade but 0.1 N nitric acid solution was very reasonable to neutralize the 65% carbonized charcoal for mixing with heavy texture acidy soil(pH 5.3) of uncultivated deep horizon to transplant the tobacco seedlings. Volume ratio mixing for seedling bed is adequate at five of ash to one of acid solution. Neutralization with nitric acid solution also accelerated extraction of the inorganic nutrient in rice hull ash. Tobacco seedlings grown on bed mixed with neutralized rice hull charcoal and soil had shown better results on the agronomic measurement than alkaline ash bed, and phosphorus and cations were uptaken more amounts.
Korean Journal of Construction Engineering and Management
/
v.1
no.2
s.2
/
pp.63-70
/
2000
Since inorganic pigment, among admixtures used for cement composites, can raise the esthetic value of a building due to its effect of coloring, it can be assumed that the quantity consumed is expected to increase in connection with the recent trend of emphasizing the beautiful sights of the city. We carried out a flow test by changing the mix proportion of the cement mortar mixed with an inorganic pigment, water-cement ratio and pigment mixing ratio in order to present the basic materials for utilizing colored cement mortars. In construction by exploring the effect of inorganic pigments on the workability of cement mortar. In case of red pigment mortar and yellow pigment mortar, the workability was found to be rapidly decreased. To secure proper workability, it is necessary to increase the amount of mixing water, or to use superplasticizer. In case of green pigment mortar, however, it recorded $-2.4{\~}6.9{\%}$, showing that there was almost no change in flow. In case of black pigment mortar, it was also confirmed that there is no need to consider workability.
Proceedings of the Korea Concrete Institute Conference
/
2008.11a
/
pp.697-700
/
2008
Recently, high strength, flowability, and durability of concrete were required according to increase of large scale and high rise structure. However, cracks occurred easily on the high performance concrete. In this reason, using expansion agent for reducing shrinkage cracks were increased, but it did not consider on durability of high performance concrete. Accordingly, this study1 investigated the resistance of shrinkage and damage form salt by mixing CSA expansion agent on the blast-furnace slag cement and mixed cement for the low heat of hydration by three components. The cases that 8% of expansion agent was mixed and the proportion was OPC were expanded till 43.7 times compared with control concrete. For the resistance to the damage of salt, it was improved when mixing ratio was incresed and the maximum size of coarse aggregate growed bigger. In this study, the resistance to the damage of salt of the cases that 8% of expansion agent was mixed was improved about 16% compared with control concrete.
Journal of the Korean Recycled Construction Resources Institute
/
v.4
no.1
/
pp.68-75
/
2016
The present study evaluated the mechanical properties of open graded asphalt for semi-rigid pavements in order to determine the mixing proportion experimentally. A total twelve types of basic mixing proportions were set up and mechanical tests such as marshall stability, porosity, permeability, and cantabro loss were conducted based on Korean standards. From the tests results, it was found that the marshall stability in case of straight and modified asphalt increase up to the contents with 5.0% and 5.5% respectively. The porosity and permeability of asphalt tended to decrease as the asphalt contents increase, the coefficient of correlation between both were estimated 86%. The increase contents with asphalt range from 3.5% to 6.0% tended to decrease the cantabro loss and the modified asphalt enhanced the resistance of cantabro loss with range from 18.8% to 33.1% than straight asphalt under same asphalt contents. In comparison with test results and quality standards, it was concluded that the modified asphalt content of 4.5% is effective to adopt for open graded asphalt.
Song, Jung-Min;Bu, Jun-Oh;Kim, Won-Hyung;Kang, Chang-Hee;Ko, Hee-Jung;Chambers, S.
Journal of Korean Society for Atmospheric Environment
/
v.33
no.2
/
pp.174-183
/
2017
The background level and timely variation characteristics of atmospheric $^{222}Rn$ concentrations have been evaluated by the real time monitoring at Gosan site of Jeju Island, Korea, during 2008~2015. The average concentration of atmospheric radon was $2,480mBq\;m^{-3}$ for the study period. The cyclic seasonality of radon was characterized such as winter maximum and summer minimum, consistent with the reduction in terrestrial fetch going to summer. On monthly variations of radon, the mean concentration in October was the highest as $3,041mBq\;m^{-3}$, almost twice as that in July ($1,481mBq\;m^{-3}$). The diurnal radon concentrations increased throughout the nighttime approaching to the maximum ($2,819mBq\;m^{-3}$) at around 7 a.m., and then gradually decreased throughout the daytime by the minimum ($2,069mBq\;m^{-3}$) at around 3 p.m. The diurnal radon cycle in winter showed comparatively small amplitude due to little variability in atmospheric mixing depth, conversely, large amplitude was observed in summer due to relatively a big change in atmospheric mixing depth. The cluster back-trajectories of air masses showed that the high radon events occurred by the predominant continental fetch over through Asia continent, and the radon concentrations from China continent were about 1.9 times higher on the whole than those from the North Pacific Ocean. The concentrations of $PM_{10}$ also increased in proportion to the high radon concentrations, showing a good linear correlation between $PM_{10}$ and radon concentrations.
Journal of the Korean Society for Aeronautical & Space Sciences
/
v.34
no.7
/
pp.28-34
/
2006
In general engineering problems, the purpose of an optimization is to get optimal design variables. It is the same problem to fix the total amount of the design variables and to judge the optimal mixing proportions of the design variables. That is to say, we can recompose the engineering problems in the concepts of the mixture amount experiments. The goal of mixture amount method is to get the response surfaces of varying both the mixing proportion of component and the total amount of the mixture. The solution of the aircraft fuselage optimization problem is obtained by the mixture amount method and genetic algorithm. In this study, it is shown that the mixture amount method can be utilized for the aircraft structural optimization problem. Also, this method in this study can be applied for the optimization problems over 12 design variables which is impossible for D-optimal design.
This is a study about how the increase of strength is changed when ground improvement material is mixed with either coastal clay or sandy soil. The ground improvement material was made from mixing a certain proportion of the slag which is by-products generated by smelting the iron ore and the paper fly ash which is formed by bumping up the paper. The ground improvement material was added to coastal soil and sandy soil each. And then according to ratio of water contents, number of curing days and ratio of mixture, specimen for uniaxial compression test was made. The change of uniaxial compression strength and the generated substances was analyzed while the specimen is being cured for 28days. The result of analysis shows that the strength of coastal clay was increased about eleven times more than that of sandy soil. This means that ettringite reaction by ground improvement material becomes more distinctive in the coastal clay than in the sandy soil.
The Application of Steel Fiber Shotcrete in tunneling construction has become part of tunneling practice at least since the 1970s because of its high bending and tensile properties. Over the past 3 decades, researcher from all over the world have been significantly developing the associated technologies for improved performance of SFRS. But still it has some major drawbacks in terms of durability, damage of pumping hose, wastage due to rebound concrete, corrosion and it costs high. To overcome this situation researcher has to look for some alternative material. Therefore, this part study deals with the three types of fiber in order to find good alternative for steel fiber. Polyamide and Polypropylene fiber were used in this study with 0.6, 0.5% mixing ratio. To evaluate its fresh and harden properties air content, slump, compressive, split tensile and bending strength were measured. After comparing the results of all three types of fiber reinforced concrete with its different mixing proportion this study propose that polyamide fiber with addition ratio of 0.6 % for field use.
In this study, we examined the physical properties of cement mortar by replacing a part of the amount of fine aggregate in moist mud flat. I analyzed the possibilities of using bricks. Flow measurement results show that the flow value increases as the mixing ratio of cement and fine aggregate increases and the flow value decreased as the replacement ratio of moist mud flats decreased. Chloride contents were also found to decrease with decreasing substitution rate of moist mud flats. As a result of the compressive strength measurement, the compressive strength increased in inverse proportion as the displacement ratio of moist mud flats decreased in most mixing ratio. As a result of tensile strength measurement, the tendency was similar to compressive strength and the intensity increased as the replacement ratio of moist mud flats decreased.
In the many kind of construct-material, the concrete which has the high-strength and a durability is sufficient to use with structure-material. but the color of concrete is very monotony, so generally concrete isn't used the out surface. although color concrete is a method of expressing surface, the combination of pigment and cement cause many physical problem such as efflorescence phenomenon, strength degradation and so on. In this study, It attempt to develop the black mortar using the industrial granulated blast furnace slag and to evaluate basic physical properties compare with general color concrete to solve the color concrete problem. The result of experiment showed that the flow dropped mixing of pigment. but flow increased in proportion to the mixing rate in occasion of mortar that mix granulated blast furnace sla and black mortar which was made granulated blast furnace slag has more visible black color than any mortar.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.