• Title/Summary/Keyword: Mixed-size particles

Search Result 217, Processing Time 0.027 seconds

Effect of Hollow Sphere Size on Heat Shield Properties of hollow TiO2/polyacrylate Composites (중공구의 크기에 의한 hollow TiO2/polyacrylate 복합체의 열차단 특성)

  • Kim, Jong Seok
    • Applied Chemistry for Engineering
    • /
    • v.32 no.6
    • /
    • pp.690-694
    • /
    • 2021
  • Carbon spheres (CS) were fabricated using glucose as a precursor in the hydrothermal method. Hollow TiO2 (H-TiO2) spheres with 200 nm, 500 nm, and 1,200 nm were synthesized by CS/TiO2 core-shell particles via a sol-gel and calcination method. H-TiO2 spheres with nano and micron sizes were characterized using FE-SEM, HR-TEM, and X-ray diffraction. The CIE color coordinate, solar reflectance, and heat shield temperatures of H-TiO2/polyacrylate (PA) composite film were investigated using a UV-Vis-NIR spectrometer and homemade heat insulation temperature measuring device. H-TiO2/PA composites exhibit excellent thermal insulation since the hollow structure filled with dry air has low thermal conductivity and near infrared light reflecting performance. The thermal insulation increased with increasing the hollow sphere (HS) size on H-TiO2/PA composites. The PA composite film mixed with H-TiO2 filled with 1200 nm HS reduced the heat shield temperature by 26 ℃ compared to that of the transparent glass counterpart.

Synthesis of Cubic and Rod Shapes CaCO3 by Hydrothermal Method (수열합성법을 이용한 큐빅과 로드형의 탄산칼슘 합성)

  • Kang, Kuk-Hyoun;Jeon, Sang-Chul;Hyun, Mi-Ho;Lee, Dong-Kyu
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.6
    • /
    • pp.255-261
    • /
    • 2016
  • $CaCO_3$ was applied in various industries including rubber, plastics, paint, paper, food additives, and acid neutralizer, etc., owing to its excellent physical and chemical characteristics as well as various appearances of crystals and many reserves. In particular, research on controlling the structure and shape of $CaCO_3$ has attracted considerable attention recently, because the whiteness and physical characteristics of $CaCO_3$ depend on the size and shapes of the particles. In this study, $CaCO_3$ was synthesized using $CaCl_2$ and $(NH4)_2CO_3$, which has multi-shapes and structures, using a self-assembly method with a hydrothermal method. The structure and morphology of the $CaCO_3$ could be controlled by adjusting the pH and precursor concentration. In particular, the pH adjustment appeared to be a critical factor for the morphology and crystal form. In addition, the calcite and cubic shape were obtained at pH 7, while the mixed calcite, aragonite structure, and rod shapes appeared at pH 7 and over. Through an analysis of the particle formation process, the formation of the calcium carbonate particles was confirmed. The physicochemical properties of the synthesized $CaCO_3$ were analyzed by SEM, XRD, EDS, FTIR, and TG/DTA.

A study on the application of waste concrete powder as a material for construction (건설용 재료로써 폐콘크리트 미분말의 활용성 연구)

  • Kim, Yong-Jic;Choi, Yun-Wang;Kim, Sang-Chel;Kim, Young-Jin
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.4
    • /
    • pp.88-94
    • /
    • 2012
  • This study is conducted to utilize waste concrete powder made as a by-product manufacturing high quality recycled aggregate. The blaine fineness of the used waste concrete powder was 928 and $1,360cm^2/g$. As the main characteristic of waste concrete powder, it showed an angular type similar to cement, but hydrated products were attached on the surface of particles. In addition, the size of the particles of waste concrete powder was larger than OPC and in terms of chemical components it had higher $SiO_2$ contents. The viscosity of the paste that mixed waste concrete power decreased by 62% at the most, compared to the paste that only used OPC, and the final set time was delayed about two hours. As composition rates of waste concrete powder increased, the flow value decreased by 30% at the most according to the comparison with mortar that only used OPC, and sorptivity coefficients increased by 70%. The compressive strength of mortar decreased by 73% at the most as composition rates of waste concrete powder increased. According to the test results, it is desirable to use waste concrete powder by combining OPC appropriately(below 15%).

  • PDF

Diagnosis of Coloration Status and Scientific Analysis for Pigments to Used Large Buddhist Painting(Gwaebultaeng) in Tongdosa Temple (통도사 괘불탱의 채색상태 및 사용 안료의 과학적 분석)

  • Lee, Jang Jon;Ahn, Ji Yoon;Yoo, Young Mi;Lee, Kyeong Min;Han, Min Su
    • Journal of Conservation Science
    • /
    • v.33 no.6
    • /
    • pp.431-442
    • /
    • 2017
  • The purpose of this study is to reveal that coloring status and the degree of damage and the kinds of pigments used in large buddhist painting (Gwaebultaeng) of Tongdosa temple using a scientific analysis methods. It was observed that the physical damage patterns of the Gwaebultaeng were folding, lifting, fading, and peeling. Lead red, cinnabar and organic pigments were used as red pigments. Malachite and atacamite were used as green pigments, azulite and lazulite were blue pigments, lead white and talc were white pigment. It is estimated that overlapping organic pigments on the lead white were used as the yellow pigment and carbon was the black pigment. Through the analysis of the particle status of the pigments, it was confirmed that different types of raw materials were used for the green pigment, and the crystal form was easily distinguishable. Also, the dark blue color and the light blue color differed from each other depending on the size and shape of the raw material particles. Yellow and purple colors were organic pigments which did not have a graininess. The yellow and purple colors were organic pigments free from the graininess, and the pigments of dark red pigments was found to be mixed with the orange color pigments and carbon particles.

Sintering Mixtures in the Stage of Establishing Chemical Equilibrium

  • Savitskii, A.P.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 1999.04a
    • /
    • pp.5-5
    • /
    • 1999
  • The Principal deficiency of the existing notion about the sintering-mixtures consists in the fact that almost no attention is focused on the Phenomenon of alloy formation during sintering, its connection with dimensional changes of powder bodies, and no correct ideas on the driving force for the sintering process in the stage of establishing chemical equilibrium in a system are available as well. Another disadvantage of the classical sintering theory is an erroneous conception on the dissolution mechanism of solid in liquid. The two-particle model widely used in the literature to describe the sintering phenomenon in solid state disregards the nature of the neighbouring surrounding particles, the presence of pores between them, and the rise of so called arch effect. In this presentation, new basic scientific principles of the driving forces for the sintering process of a two-component powder body, of a diffusion mechanism of the interaction between solid and liquid phases, of stresses and deformation arising in the diffusion zone have been developed. The major driving force for sintering the mixture from components capable of forming solid solutions and intermetallic compounds is attributed to the alloy formation rather than the reduction of the free surface area until the chemical equilibrium is achieved in a system. The lecture considers a multiparticle model of the mixed powder-body and the nature of its volume changes during solid-state and liquid-phase sintering. It explains the discovered S-and V-type concentration dependencies of the change in the compact volume during solid-state sintering. It is supposed in the literature that the dissolution of solid in liquid is realised due to the removal of atoms from the surface of the solid phase into the melt and then their diffusicn transfer from the solid-liquid interface into the bulk of liquid. It has been shown in our experimental studies that the mechanism of the interaction between two components, one of them being liquid, consist in diffusion of the solvent atoms from the liquid into the solid phase until the concentration of solid solutions or an intermetallic compound in the surface layer enables them to pass into the liquid by means of melting. The lecture discusses peculimities of liquid phase formation in systems with intermediate compounds and the role of the liquid phase in bringing about the exothermic effect. At the frist stage of liquid phase sintering the diffusion of atoms from the melt into the solid causes the powder body to grow. At the second stage the diminution of particles in size as a result of their dissolution in the liquid draws their centres closer to each other and makes the compact to shrink Analytical equations were derived to describe quantitatively the porosity and volume changes of compacts as a result of alloy formation during liquid phase sinteIing. Selection criteria for an additive, its concentration and the temperature regime of sintering to control the density the structure of sintered alloys are given.

  • PDF

Production and Mechanical Properties of Mg-Zn-Ce Amorphous Alloys by Dispersion of Ultrafine hcp-Mg Paticles (hcp-Mg 입자분산형 Mg-Zn-Ce계 비정질합금의 제조와 기계적 성질)

  • Kim, Seong-Gyu;Park, Heung-Il;Kim, U-Yeol;Jo, Seong-Myeong;Kim, Yeong-Hwan;Inoue, A.;Masumoto, T.
    • Korean Journal of Materials Research
    • /
    • v.4 no.8
    • /
    • pp.847-854
    • /
    • 1994
  • An amorphous single phase and coexistent amorphous and hcp-Mg phases in Mg-Zn-Ce system were found to form in the composition ranges of 20 to 40% Zn, 0 to 10% Ce and 5 to 20% Zn, 0 to 5% Ce, respectively. A $Mg_{85}Zn_{12}Ce_{3}$ amorphous alloy containing nanoscale hcp-Mg particles was found to form either by melt spinning or by heat treatment of melt -spun ribbon. The particle size of the hcp-Mg phase can be controlled in the range of 4 to 20 nm. The mixed phase alloy prepared thus has a good bending ductility and exhibits high ultimate tensile strength($\sigma_{B}$) ranging from 670 to 930 MPa and fracture elongation($\varepsilon_{f}$) of 5.2 to 2.0%. The highest specific strength($\sigma_{B}$/density =$\sigma_{s}$)$3.6 \times 10^5N \cdot m/kg$. It should be noted that the highest values of flB, US and ?1 are considerably higher than those (690MPa,$2.5 \times 10^5N \cdot m/kg$and 2.5%) for amorphous Mg-Zn-Ce alloys. The increase of the mechanical strengths by the formation of the mixed phase structure is presumably due to a dispersion hardening of the hcp supersaturated solution which has the hardness higher than that of the amorphous phase with the same composition.

  • PDF

Analysis of Bed Material Changes by Flushing Flow from Daecheong Dam (대청댐에서 증가방류에 의한 하상토의 변화 분석)

  • Jang, Chang-Lae;Woo, Hyo-Seop
    • Journal of Korea Water Resources Association
    • /
    • v.42 no.10
    • /
    • pp.845-855
    • /
    • 2009
  • In this study, changing characteristics of bed materials downstream of Daecheong Dam by flushing flow was investigated. Flushing flow affected the downstream environment in such a way that the mean diameter of bed material was increased and the standard deviation was decreased. The vertical sorting of bed materials composed of mixed sediment in the sediment box was observed. The surface layer was composed of gravels, and uniform sand material was buried below it. Relative fractions (Di/D50) of the bed material trapped in the box was nearly 1.0 for the bed material coarser than D$_{50}$ at Hyundo gauging station, and was between two values on the bed surface before and after the flushing flow at Bugang gauging station. Ratio of driving force to resisting force for each fraction ($\tau_i^*$) with the faction size maintained constant for the bed material coarser than D$_{50}$ at Hyundo station. At Bugang station, however, it was rapidly decreased. It means that pavement of the surface layer of bed material at Bugang station was developed, with the sediment particles moving downstream uniformly by flushing flow.

Development of Recycled Paper Properties using In-Situ Process (In-Situ 공정(工程)을 이용한 재활용(再活用) 펄프의 물성특성(物性特性) 향상 연구(硏究))

  • Lee, Jong-Kyu;Yoo, Kwang-Suk;Nam, Seong-Yong;Ah, Ji-Whan
    • Resources Recycling
    • /
    • v.19 no.3
    • /
    • pp.62-70
    • /
    • 2010
  • As the demand for paper continues to grow and the importance of recycled paper, white ledgar(WL) and old newspaper pulp(ONP), continuously increase. In addition, usage of recycled paper is essential in terms of forest conservation and environmental protection issues. However, optical and mechanical properties of recycled paper have some drawbacks than regular paper's properties that is indispensable. In order to complement these problems of recycled paper, precipitated calcium carbonate (PCC) was synthesized by the In-situ process with a recycled pulp. Depending on the size of PCC is divided into 2 types, $0.01{\mu}m{\sim}0.09{\mu}m$ colloid type ultra-fine particle and $0.1{\mu}m{\sim}0.9{\mu}m$ cubic type particles. In this study, we analyze how the different shape and size of precipitated calcium carbonate affects in the optical and mechanical properties of the recycled paper used as a filler. Furthermore, we mixed with chemical pulp for overcome reduce of mechanical properties, without using other chemicals, when we use PCC as a filler. The results has the possibility to meet in GR excellent recycling certification mark, standard was proposed.

Study on the Flame Retardation and Thermal Resistance for CPE Rubber Material Added Etching By-product of Aluminum (알루미늄 엣칭부산물을 첨가한 CPE 고무재료의 난연성 및 내열성 연구)

  • Kim, Kyung Hwan;Lee, Chang Seop
    • Journal of the Korean Chemical Society
    • /
    • v.45 no.4
    • /
    • pp.341-350
    • /
    • 2001
  • Aluminum Hydroxide was employed as a thermal retardent and flame retardent for Chloropolyethylene (CPE) rubbery materials which is the construction material of automotive oil cooler hose. and then cure characteristics, physical properties, thermal resistance and flame retardation of compounded rubber were investigated, and optimum mixing conditions of rubber and flame retarding agent were deduced from the experimental results. CPE rubber material which has excellent properties of chemical corrosion resistance and cold resistance and inexpensive in price was used to prepare rubber specimen. The by-product of ething, produced from the process of surface treatment of aluminum was processed to aluminum hydroxide via crushing and purification, which is characterized by XRD, PSA, SEM and ICP-AES techniques in terms of phase, size, distribution, morphology and components of particles and then mixed to CPE rubber materials in the range of 0~80 phr. Hardness, tensile strength, elongation and thermal properties of compounded rubber specimens were tested. The optimum mixing ratio of rubber to additives to give maximum effect on thermal resistance and flame retardation, within the range of tolerable specification for rubber materials, was determined to be 40 phr. The flame retardation of CPE rubber materials was found to be increased by 5 times at this mixing ratio.

  • PDF

A Study on the Correlation between Strength and Compaction of Porous Concrete Using Bottom Ash Aggregate (바텀애시 골재를 사용한 다공성 콘크리트의 강도와 컴펙션의 상관관계 연구)

  • In-Hwan, Yang;Seung-Tae, Jeong;Ji-Hun, Park
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.4
    • /
    • pp.359-366
    • /
    • 2022
  • In this paper, the effect of compression levels on the strengths of porous concrete using bottom ash aggregates was analyzed. Coal bottom ash (CBA) was used as aggregate in porous concrete in this study. The aggregate size types used in the CBA concrete mixtures were catagorized into two different ones. One included only a single aggregate particle size and the other included hybrid aggregate particles mixed at a ratio of 8:2 volume proportion. The water-binder ratio was fixed at 0.30, and the compression levels were applied at 0.5, 1.5, and 3.0 MPa valu es to fabricate a porou s concrete specimen. The total porosity, compressive, splitting tensile, and flexural tensile strengths were tested and analyzed. When the compression level increased, the total porosity decreased, meanwhile the compressive, split tensile, and flexural tensile strengths increased. The total porosity of concrete using hybrid aggregate was lower and the strength was larger than those of concrete using single-type aggregate. Finally, the correlation between the total porosity, compressive, split tensile, and flexural tensile strengths of porous concrete were presented. The total porosity and strength characteristics showed an inversely proportional correlation.