• Title/Summary/Keyword: Mix Viscosity

Search Result 110, Processing Time 0.02 seconds

Influence of plastic viscosity of mix on Self-Compacting Concrete with river and crushed sand

  • Rama, J.S. Kalyana;Sivakumar, M.V.N.;Kubair, K. Sai;Vasan, A.
    • Computers and Concrete
    • /
    • v.23 no.1
    • /
    • pp.37-47
    • /
    • 2019
  • In view of the increasing utility of concrete as a construction material, the major challenge is to improve the quality of construction. Nowadays the common problem faced by many of the concrete plants is the shortage of river sand as fine aggregate material. This led to the utilization of locally available materials from quarries as fine aggregate. With the percentage of fines present in Crushed Rock Fines (CRF)or crushed sand is more compared to river sand, it shows a better performance in terms of fresh properties. The present study deals with the formulation of SCC mix design based on the chosen plastic viscosity of the mix and the measured plastic viscosity of cement pastes incorporating supplementary cementitious materials with CRF and river sand as a fine aggregate. Four different combinations including two binary and one ternary mix are adopted for the current study. Influence of plastic viscosity of the mix on the fresh and hardened properties are investigated for SCC mixes with varying water to cement ratios. It is observed that for an increasing plastic viscosity of the mix, slump flow, T500 and J-ring spread increased but V-funnel and L-box decreased. Compressive, split tensile and flexural strengths decreased with the increase in plastic viscosity.

Plastic viscosity based mix design of self-compacting concrete with crushed rock fines

  • Kalyana Rama, JS;Sivakumar, MVN;Vasan, A;Kubair, Sai;Ramachandra Murthy, A
    • Computers and Concrete
    • /
    • v.20 no.4
    • /
    • pp.461-468
    • /
    • 2017
  • With the increasing demand in the production of concrete, there is a need for adopting a feasible, economical and sustainable technique to fulfill practical requirements. Self-Compacting Concrete (SCC) is one such technique which addresses the concrete industry in providing eco-friendly and cost effective concrete. The objective of the present study is to develop a mix design for SCC with Crushed Rock Fines (CRF) as fine aggregate based on the plastic viscosity of the mix and validate the same for its fresh and hardened properties. Effect of plastic viscosity on the fresh and hardened properties of SCC is also addressed in the present study. SCC mixes are made with binary and ternary blends of Fly Ash (FA) and Ground Granulated Blast Slag (GGBS) with varying percentages as a partial replacement to Ordinary Portland Cement (OPC). The proposed mix design is validated successfully with the experimental investigations. The results obtained, indicated that the fresh properties are best achieved for SCC mix with ternary blend followed by binary blend with GGBS, Fly Ash and mix with pure OPC. It is also observed that the replacement of sand with 100% CRF resulted in a workable and cohesive mix.

A study on the mix desing for stabilizing liquid of sluryy wall (Slury Wall용 안정액의 배합설계에 관한 연구)

  • ;;;Motoshige Ariyama
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.04a
    • /
    • pp.457-462
    • /
    • 1999
  • The purpose of this study is to design the requirements for the materials of stabilizing slurry and to determine the optimum slruuy mix design used in the underground wall of Inchon LNG #213 and 214 tank. After the materials and mix conditions of stabilizing slurry investigated and tested, we propose materials and optimum mix design according to testing items including funnel viscosity, we propose materials and optimum mix design according to testing items including funnel viscosity, fluid loss, cake thickness and specific gravity. As this results, we select optimum mix design that the upper limit ratio of bentonite is 2.0%, polymer is 0.1% considering the funnel viscosity and dispersion agent is 0.05% considering the fluid loss. Also we select all materials which are composed of GTC4 as bentonite, KSTP as polymer and Bentocryl as dispersion agent. All test results are satisfied our specifications for stabilizing slurry.

  • PDF

Performance Analysis of Low-viscosity type Superplasticizer (저점도형 감수제의 성능 분석)

  • Han, Dongyeop
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.10a
    • /
    • pp.35-36
    • /
    • 2016
  • Recently, with the increasing demand of high performance of concrete, the mix design of concrete mixture has became low water-to-binder ratio with high binder content. To compensate these trend of mix design, high range water reducer, or superplascizier has been invented to achieve high flowable concrete. Although this superplasticizer provides favorable workability based on its dispersing action on the components of concrete mixture, it has an limitation of decreasing viscosity of the mixture, and thus it is difficult to secure sufficient workability for high performance concrete mixtures with high binder content. To improve the workability of concrete with high viscosity, recently, low-viscosity type superplasticizer was introduced, and in this research, a fundamental properties of low-viscosity type superplasticizer is evaluated.

  • PDF

A Study on the Optimum Mix Proportion of the Stabilizing Liquid Used for Excavation of the Deep and Massive Slurry Wall

  • Kwon Yeong-Ho
    • KCI Concrete Journal
    • /
    • v.14 no.4
    • /
    • pp.151-159
    • /
    • 2002
  • This study investigates experimentally the optimum mix proportion and design factors of the stabilizing liquid used for excavation of the massive and deep slurry wall in LNG in-ground tank before pouring concrete. Considering those site conditions, the stabilizing liquid used for excavation of slurry wall has to be satisfied with some requirements including specific gravity, fluid loss, cake thickness, funnel viscosity and sand content in order to construct the safe and qualified slurry wall. For this purpose, we select materials including bentonite, polymer and dispersion agent. After performing many tests for materials and mix design process, we propose the optimum mix proportion that the upper limit ratio of bentonite is $2.0\%$, polymer is $0.1\%$ considering the funnel viscosity and dispersion agent is $0.05\%$considering the fluid loss of the stabilizing liquid. Also, we select all materials which are consisted of GTC4 as bentonite, KSTP as polymer and Bentocryl 86 as dispersion agent. Based on the results of this study, the optimum mix proportion of the stabilizing liquid is applicable to excavate the deep and massive slurry wall in LNG in-ground tank successfully.

  • PDF

A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag (고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구)

  • 김재훈;윤상천;지남용
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.29-36
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of molar and fineness modulus of ,and on the properties of fresh mortar. The effect of water-binder ratio, sand-binder ration, content; of ggbs (by mass of total cementitious materials), and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the following conclusion; can be drawn: (1) The mixing time needed (or high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

  • PDF

Evaluation of Fundamental Properties of Warm-mix Recycled Asphalt Concretes (준고온 재생 아스팔트 콘크리트의 기본특성 평가)

  • Kim, Nam-Ho;Kim, Jin-C.;Hong, Jun-P.;Kim, Kwang-W
    • International Journal of Highway Engineering
    • /
    • v.12 no.4
    • /
    • pp.111-120
    • /
    • 2010
  • This study evaluated strength properties of recycled asphalt concretes using warm-mix technology. Granite with maximum size of 13mm and penetration grade of 80-100 virgin binder were used for mixing in recycled mixtures. Mix design was performed using 20% and 30% RAP(coarse : fine= 6 : 4) contents. GPC, penetration, absolute viscosity and kinematic viscosity were measured for determining ratio of two warm-mix additives (Evotherm and Sasobit). Low-density polyethylene(LD) used as asphalt modifier for improving stiffness of recycled WMA mixtures in this study. Therefore, a total of 11 mixtures were prepared in this study; 8 warm-mix recycled mixtures(2 RAP contents${\times}$2 warm-mix additives${\times}$2 modifiers), 2 hot-mix recycled mixtures and 1 HMA virgin mixture(control). Deformation strength, indirect tensile strength, moisture sensitivity, permanent deformation by wheel tracking tests were measured out for evaluating fundamental properties of recycled asphalt concretes using warm-mix technology.

Properties of SBS-modified Warm-mix Asphalt Binders (SBS 개질 준고온 아스팔트 바인더의 특성)

  • Kim, Sung Un;Lee, Sung Jin;Youn, Yeo;Kim, Kwang Woo
    • International Journal of Highway Engineering
    • /
    • v.16 no.2
    • /
    • pp.19-24
    • /
    • 2014
  • PURPOSES : The study objective was to evaluate rheology and physical properties of SBS-modified warm-mix asphalt (WMA) binders in comparison with hot-mix asphalt (HMA) binders. METHODS : Four different SBS polymers were used to prepare polymer-modified asphalt (PMA) binders, and three different warm-mix additives (WAD) were used to prepare a total of 12 WMA PMA binders. The kinematic viscosity was measured at 115, $135^{\circ}C$. The PG was determined using DSR and BBR. The pass/fail (P/F) temperatures for high and low PG grading were evaluated for HMA PMA and WMA PMA binders. RESULTS : PG 76-22 binders could be prepared by modifying the base binder (PG 64-22) using 4.5 wt% of SBS. The kinematic viscosity (KV) of SBS PMA was increased by 3 times higher than that of base asphalt. The SBS PMA with WAD showed 10% lower KV than that of the normal SBS PMA at $115^{\circ}C$ The high P/F temperatures showed almost no difference between HMA PMA and WMA PMA binders. The high P/F temperature showed very high correlations with KV ($R^2$ > 0.97). The result of SBS modification caused increase of low P/F temperature by $2.7^{\circ}C$ on average. CONCLUSIONS : Since the PMA with WAD showed 10% lower KV than normal (HMA) PMA at $115^{\circ}C$, reducing PMA mixture temperature down to a WMA level was possible in this study. The higher KV binders showed the higher P/F temperature. There was almost no change in high P/F temperature due to the use of WAD. The SBS PMA, showing an increased low P/F temperature, might show somewhat poorer performance at low-temperature, even though the lower PG grade was staying at the same level, i.e., $-22^{\circ}C$.

A Study on the Factors Affecting the High Fluid Mortar Containing Ground Granulated Blast-furnace Slag (고로슬래그 미분말을 함유한 고유동 모르터의 유동성상에 미치는 영향 요인에 관한 연구)

  • Kim, Jae-Hun;Yoon, Sang-Chun;Jee, Nam-Yong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.2 no.4
    • /
    • pp.145-152
    • /
    • 2002
  • High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of mortar and fineness modulus of sand on the properties of fresh mortar. The effect of water-binder ratio. sand-binder ration. contents of ggbs (by mass of total cementitious materials). and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the fellowing conclusions can be drawn: (1) The mixing time needed for high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

Effect Analysis of Mix Designing Factors on Workability and Rheological Parameters of Self-Compacting Concrete (배합요인이 자기충전 콘크리트의 워커빌리티 및 레올로지 파라미터에 미치는 영향 분석)

  • Yoon, Seob;Han, Min-Cheol
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.3
    • /
    • pp.235-242
    • /
    • 2018
  • The objective of the paper is to investigate the effect of mix designing factors on the workability and rheological parameters of self compacting concrete in order to facilitate the difficulties of quality control of high sensitivity of SCC. Mix proportions of SCC were prepared with various conditions of coarse, and fine aggregate, and unit water content, and the SCC mixtures were tested on workability, rheological properties to provide basic data for quantitative evaluation. Test results indicated that the yield stress of SCC decreased with increasing the coarse aggregate volume ratio, and increased with increasing the amount of VMA. However, unit water content, fine aggregate type, and air content didn't affect the yield stress value. The plastic viscosity according to the mixing factors showed a similar tendency to the yield stress. In addition, there was no correlation between yield stress and workability (flow, T50, V-lot). However, there was closely correlation among plastic viscosity and T50 and V-lot. Especially, T50 and V-lot time decreased with decreasing plastic viscosity.