Texture and Microstructure in AA3004 after Continuous Confined Strip Shearing (CCSS 변형된 AA 3004 판재의 집합조직과 미세조직)

  • 김훈동;정영훈;황병복;최호준;허무영
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2002.05a
    • /
    • pp.181-183
    • /
    • 2002
  • A new deformation process termed "continuouis confined sup shearing" (CCSS) has been developed for shear deformation of metallic sheets. The tools of CCSS were designed to provide a constant shear deformation of the order of 0.5 per pass while preserving the original sheet shape. In order to clarify the evolution of texture and microstructure during CCSS, strips of the aluminum alloy AA3004 were deformed by CCSS in up to three passes. FEM results indicated that CCSS provides a quite uniform shear deformation at thickness layers close to the strip center, although the deformation is not homogeneous in the die channel, in particular at the surface layers. The rolling texture of the initial sheet decreased during CCSS, and preferred orientations along two fibers developed. However, with an increasing number of CCSS passes the deformation texture did not develop futher. The evolution of annealing textures depended on the number of CCSS passes. A strong {112}<110> component in the deformation texture led to the formation of a strong {111}<112) orientation in the annealing texture. Observations by TEM and EBSD revealed the formation of very fine grains of ∼1.0$\mu\textrm{m}$ after CCSS.

  • PDF

Evolution of Microstructure and Mechanical Properties of Porous Al Alloy Under Various Heat Treatment (열처리에 따른 다공성 알루미늄 합금 재료의 미세구조와 기계적 성질 변화)

  • 류관무;권영재;김준규;조원승;조남희;황진명;유연철
    • Transactions of Materials Processing
    • /
    • v.12 no.6
    • /
    • pp.588-596
    • /
    • 2003
  • The relationships between evolution of microstructure and mechanical properties of porous Al-3Si-2Mg-2Cu alloy after the foaming and various heat treating were investigated. The foamed alloy having various densities were manufactured by powder compact foaming and heat treated. Then compression test was performed with deformation rate of 0.5/s. The ultimate compression strength was not changed after solution heat treatment but the flow curve after ultimate strength showed very smooth and uniform plateau region. This change of flow curve means that the deformation mechanism is altered from brittle fracture to ductile deformation and the energy absorption property of Al foam is dramatically improved. The improvement of energy absorption without any detriment of mechanical properties is due to that the very brittle precipitation like Al-Cu and Al-Mg was uniformly dissolved in Al matrix after solution heat treatment. And various mechanical properties of Al alloy porous material were improved by 40% with aging of $200^{\circ}C$ and 50min. These improvements are ascribe to the various fine precipitates like $\Omega$ and $\theta$'.

Effect of Heat Treatment on the Microstructural Evolution of Pt-aluminide Coated Ni-based Superalloy (Pt-Aluminide로 코팅된 초내열합금의 열처리에 따른 미세조직변화)

  • Joo, D.;Park, S.H.;Jung, Y.G.;Lee, K.H.;Kim, C.S.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.19 no.2
    • /
    • pp.103-108
    • /
    • 2006
  • Microstructural evolution of Pt-aluminide coated Ni-based superalloy has been investigated with ductilization heat treatment. The Pt coat was prepared on the superalloy and then aluminide coating was conducted using a pack cementation process. Samples were heat-treated at $1050^{\circ}C$ for 2 hrs and the microstructure and element analysis were preformed. A various precipitated compounds were observed within the coating layer and the diffusion region in the Pt-aluminide coating and heat treatment, indicating that the bi-phase compounds of $PtAl_2$ and NiAl were performed during the Pt-aluminide coating, whereas $M_{23}C_6$, MC, $Ni_3Al$ and ${\sigma}$ phases were precipitated in the inter-diffusion region. The bi-phase compounds of $PtAl_2$ and NiAl were transformed into the single phase compound of $PtAl_2$ with the heat treatment, increasing the amount of carbide and ${\sigma}$ phase.

Identification of crystal variants in shape-memory alloys using molecular dynamics simulations

  • Wu, Jo-Fan;Yang, Chia-Wei;Tsou, Nien-Ti;Chen, Chuin-Shan
    • Coupled systems mechanics
    • /
    • v.6 no.1
    • /
    • pp.41-54
    • /
    • 2017
  • Shape-memory alloys (SMA) have interesting behaviors and important mechanical properties due to the solid-solid phase transformation. These phenomena are dominated by the evolution of microstructures. In recent years, the microstructures in SMAs have been studied extensively and modeled using molecular dynamics (MD) simulations. However, it remains difficult to identify the crystal variants in the simulation results, which consist of large numbers of atoms. In the present work, a method is developed to identify the austenite phase and the monoclinic martensite crystal variants in MD results. The transformation matrix of each lattice is calculated to determine the corresponding crystal variant. Evolution of the volume fraction of the crystal variants and the microstructure in Ni-Ti SMAs under thermal and mechanical boundary conditions are examined. The method is validated by comparing MD-simulated interface normals with theoretical solutions. In addition, the results show that, in certain cases, the interatomic potential used in the current study leads to inconsistent monoclinic lattices compared with crystallographic theory. Thus, a specific modification is applied and the applicability of the potential is discussed.

Effect of Lubrication on the Evolution of Texture and Microstructure in AA5052 Sheet during Shape Rolling (알루미늄 AA5052 판재의 이형압연 시 집합조직 및 미세조직 발달에 미치는 윤활의 영향)

  • Park, Eun-Soo;Kang, Hyung-Gu;Huh, Moo-Young;Kim, Hwi-Jun;Bae, Jung-Chan
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.6
    • /
    • pp.363-371
    • /
    • 2009
  • The effect of lubrication on the evolution of strain states during shape rolling in AA5052 sheet was studied by the finite element method (FEM) simulation. The strain states calculated by FEM were verified by texture analysis. Shape rolling with and without lubrication produces shape-rolled samples in fairly similar outer shapes, since the distribution of normal strain components is nearly independent of the lubrication condition. In contrast, the distribution of shear strain components strongly depends on the lubrication condition. Shape rolling without lubrication gives rise to the development of strong shear strain gradients leading to the formation of highly inhomogenous textures and microstructures. The {011}//ND fiber develops during rolling with the operation of plane strain plus ${\dot{\varepsilon}}_{22}$.

Microstructure Evolution and Mechanical Properties of Wire-Brushed Surface and Roll-Bonded Interface of Aluminum Sheets (와이어 브러싱한 알루미늄 판재 표면 및 압연접합 계면의 미세조직 및 기계적 성질)

  • Kim, Su-Hyeon;Kim, Hyoung-Wook;Kang, Joo-Hee;Euh, Kwangjun
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.5
    • /
    • pp.380-387
    • /
    • 2011
  • Wire brushing, which is a typical surface preparation method for roll bonding, has recently been highlighted as a potentially effective method for surface nanocrystallization. In the present study, the microstructure evolution and hardness of the wire-brushed surface and roll-bonded interface of a 1050 aluminum sheet were investigated. Wire brushing formed protruded layers with a nanocrystalline structure and extremely high surface hardness. After roll bonding, the protruded layers remained as hard layers at the interface. Due to their hardness and brittleness the interface hard layers, can affect the interface bonding properties and also play an important role determining the mechanical properties of multi-layered clad sheets.

Hardness and Microstructure evolution of SUS630 Stainless steel Fabricated by Directed Energy Deposition (Direct energy deposition 공정으로 제조된 SUS630 스테인리스강 적층조형체의 경도 및 미세조직 연구)

  • Back, Seong Eun;Noh, Kyung-Ho;Park, Jin Yong;Cho, Yong Ju;Kim, Jeoung Han
    • Journal of Powder Materials
    • /
    • v.25 no.3
    • /
    • pp.220-225
    • /
    • 2018
  • The microstructure and mechanical characteristics of SUS630 specimens fabricated using the direct energy deposition (DED) process are investigated. In DED, several process parameters such as laser scan speed, chamber gas flow, powder carrier gas flow, and powder feed rate are kept fixed; the laser power is changed as 150 W, 180 W, and 210 W. As the laser power increases, the surface becomes smooth, the thickness uniformity improves, and the size and number of pores decreases. With the increase in laser power, the hardness deviation decreases and the average hardness increases. The microstructure of the material is columnar; pores are formed preferentially along the columnar interface. The lath-martensite phase governs the overall microstructure. The volumetric fraction of the retained austenite phase is measured to increase with the increase of laser input power.

Effects of ion irradiation on microstructure and properties of zirconium alloys-A review

  • Yan, Chunguang;Wang, Rongshan;Wang, Yanli;Wang, Xitao;Bai, Guanghai
    • Nuclear Engineering and Technology
    • /
    • v.47 no.3
    • /
    • pp.323-331
    • /
    • 2015
  • Zirconium alloys are widely used in nuclear reactors as structural materials. During the operation, they are exposed to fast neutrons. Ion irradiation is used to simulate the damage introduced by neutron irradiation. In this article, we briefly review the neutron irradiation damage of zirconium alloys, then summarize the effect of ion irradiation on microstructural evolution, mechanical and corrosion properties, and their relationships. The microstructure components consist of dislocation loops, second phase precipitates, and gas bubbles. The microstructure parameters are also included such as domain size and microstrain determined by X-ray diffraction and the S-parameter determined by positron annihilation. Understanding the relationships of microstructure and properties is necessary for developing new advanced materials with higher irradiation tolerance.

Microstructure and Tensile Properties of Spray Cast Cu-Sn-Ni-Si Alloy (가스분무주조 Cu-Sn-Ni-Si 합금의 미세조직 및 상온 인장성질)

  • Kang, Hee-Soo;Lee, Eon-Sik;Lee, Gyu-Chang;Baik, Kyeong-Ho
    • Journal of Powder Materials
    • /
    • v.17 no.6
    • /
    • pp.470-476
    • /
    • 2010
  • In this study, Cu-10Sn and Cu-10Sn-2Ni-0.2Si alloys have been manufactured by spray casting in order to achieve a fine scale microstructure and high tensile strength, and investigated in terms of microstructural evolution, aging characteristics and tensile properties. Spray cast alloys had a much lower microhardness than continuous cast billet because of an improved homogenization and an extended Sn solid solubility. Spray cast Cu-Sn-Ni-Si alloy was characterized by an equiaxed grain microstructure with a small-sized (Ni, Si)-rich precipitates. Cold rolling of Cu-Sn-Ni-Si alloy increased a tensile strength to 1220 MPa, but subsequent ageing treatment reduced a ultimate tensile strength to 780 MPa with an elongation of 18%.

The Effects of TiC Content on Microstructure of Modified A6013-3wt.%Si Alloy Powder Compact (TiC 첨가량에 따른 개량된 A6013-3wt.%Si 합금 분말성형체의 미세조직 변화)

  • Yoo, Hyo-Sang;Kim, Yong-Ho;Son, Hyeon-Taek
    • Journal of Powder Materials
    • /
    • v.29 no.1
    • /
    • pp.28-33
    • /
    • 2022
  • Aluminum-based powders have attracted attention as key materials for 3D printing owing to their low density, high specific strength, high corrosion resistance, and formability. This study describes the effects of TiC addition on the microstructure of the A6013 alloy. The alloy powder was successfully prepared by gas atomization and further densified using an extrusion process. We have carried out energy dispersive X-ray spectrometry (EDS) and electron backscatter diffraction (EBSD) using scanning electron microscopy (SEM) in order to investigate the effect of TiC addition on the microstructure and texture evolution of the A6013 alloy. The atomized A6013-xTiC alloy powder is fine and spherical, with an initial powder size distribution of approximately 73 ㎛ which decreases to 12.5, 13.9, 10.8, and 10.0 ㎛ with increments in the amount of TiC.