• 제목/요약/키워드: Micro strength

검색결과 1,214건 처리시간 0.025초

저온 분사를 이용한 Cu계 비정질 코팅층의 제조 및 특성 연구 (Fabrication and Characterization of Cu-based Amorphous Coatings by Cold Spray Process)

  • 정동진;박동용;이진규;김형준;이기안
    • 대한금속재료학회지
    • /
    • 제46권5호
    • /
    • pp.321-327
    • /
    • 2008
  • Cu based amorphous ($Cu_{54}Zr_{22}Ti_{18}Ni_6$) coating was produced by cold spraying as a new fabrication process. The microstructure and macroscopic properties of amorphous coating layer was investigated and compared with those of cold sprayed pure Cu coating. Amorphous powders were prepared by gas atomization and Al 6061 was used as the substrate plate. X-ray diffraction results showed that Cu based amorphous powder could be successfully deposited by cold spraying without any crystallization. The Cu based amorphous coating layer ($300{\sim}400{\mu}m$ thickness) contained 4.87% porosity. The hardness of Cu based amorphous coating represented $412.8H_v$, which was correspond to 68% of the hardness of injection casted bulk amorphous material. The wear resistance of Cu based amorphous coating was found to be three times higher than that of pure Cu coating. The 3-point bending test results showed that the adhesion strength of Cu based amorphous coating layer was higher than that pure Cu coating. It was also observed that hard Cu base amorphous particle could easily deform soft substrate by particle collisions and thus generated strong adhesion between coating and substrate. However, the amorphous coating layer unexpectedly represented lower corrosion resistance than pure Cu coating, which might be resulted from the higher content of porosity in the cold sprayed amorphous coating.

Study on shear fracture behavior of soft filling in concrete specimens: Experimental tests and numerical simulation

  • Lei, Zhou;Vahab, Sarfarazi;Hadi, Haeri;Amir Aslan, Naderi;Mohammad Fatehi, Marji;Fei, Wu
    • Structural Engineering and Mechanics
    • /
    • 제85권3호
    • /
    • pp.337-351
    • /
    • 2023
  • In this paper, the shear behavior of soft filling in rectangular-hollow concrete specimens was simulated using the 2D particle flow code (PFC2D). The laboratory-measured properties were used to calibrate some PFC2D micro-properties for modeling the behavior of geo-materials. The dimensions of prepared and modeled samples were 100 mm×100 mm. Some disc type narrow bands were removed from the central part of the model and different lengths of bridge areas (i.e., the distance between internal tips of two joints) with lengths of 30 mm, 50 mm, and 70 mm were produced. Then, the middle of the rectangular hollow was filled with cement material. Three filling sizes with dimensions of 5 mm×5 mm, 10 mm×5 mm, and 15 mm×5 mm were provided for different modeled samples. The parallel bond model was used to calibrate and re-produce these modeled specimens. Therefore, totally, 9 different types of samples were designed for the shear tests in PFC2D. The shear load was gradually applied to the model under a constant loading condition of 3 MPa (σc/3). The loading was continued till shear failure occur in the modeled concrete specimens. It has been shown that both tensile and shear cracks may occur in the fillings. The shear cracks mainly initiated from the crack (joint) tips and coalesced with another one. The shear displacements and shear strengths were both increased as the filling dimensions increased (for the case of a bridge area with a particular fixed length).

Effect of the circle tunnel on induced force distribution around underground rectangular gallery using theoretical approach, experimental test and particle flow code simulation

  • Vahab, Sarfarazi;Reza, Bahrami;Shadman Mohammadi, Bolbanabad;Fariborz, Matinpoor
    • Structural Engineering and Mechanics
    • /
    • 제84권5호
    • /
    • pp.633-649
    • /
    • 2022
  • In this study, the effect of circle tunnel on the force distribution around underground rectangular gallery was investigated using theoretical approach, experimental test and Particle flow code simulation (PFC). Gypsum model with dimension of 1500×1500 mm was built. Tensile strength of material was 1 MPa. Dimension of central gallery was 100 mm×200 mm and diameter of adjacent tunnel in its right side was 20 mm, 40 mm and 60 mm. Horizontal distance between tunnel wall and gallery edge were 25, 50, 75, 100 and 125 mm. using beam theory, the effect of tunnel diameter and distance between tunnel and gallery on the induced force around gallery was analyzed. In the laboratory test, the rate of loading displacement was set to 0.05 millimeter per minute. Also sensitivity analysis has been done. Using PFC2D, interaction between tunnel and gallery was simulated and its results were compared with experimental and theoretical analysis. The results show that the tensile force concentration has maximum value in center of the rectangular space. The tensile force concentration at the right side of the axisymmetric line of gallery has more than its value in the left side of the galleries axisymmetric line. The tensile force concentration was decreased by increasing the distance between tunnel and rectangular space. In whole of the configurations, the angles of micro cracks fluctuated between 75 and 105 degrees, which mean that the variations of tunnel situation have not any influence on the fracture angle.

Repair of sports bone injury based on multifunctional nanomaterial particles

  • Dongbai Guo
    • Structural Engineering and Mechanics
    • /
    • 제86권4호
    • /
    • pp.487-501
    • /
    • 2023
  • Nanoparticles have lower size and larger specific surface area, good stability and less toxic and side effects. In recent years, with the development of nanotechnology, its application range has become wider and wider, especially in the field of biomedicine, which has received more and more attention. Bone defect repair materials with high strength, high elasticity and high tissue affinity can be prepared by nanotechnology. The purpose of this paper was to study how to analyze and study the composite materials for sports bone injury based on multifunctional nanomaterials, and described the electrospinning method. In this paper, nano-sized zirconia (ZrO2) filled micro-sized hydroxyapatite (HAP) composites were prepared according to the mechanical properties of bone substitute materials in the process of human rehabilitation. Through material tensile and compression experiments, the performance parameters of ZrO2/HAP composites with different mass fraction ratios were analyzed, the influence of filling ZrO2 particles on the mechanical properties of HAP matrix materials was clarified, and the effect of ZrO2 mass fraction on the mechanical properties of matrix materials was analyzed. From the analysis of the compressive elastic modulus, when the mass fraction of ZrO2 was 15%, the compressive elastic modulus of the material was 1222 MPa, and when 45% was 1672 MPa. From the analysis of compression ratio stiffness, when the mass fraction of ZrO2 was 15%, the compression ratio stiffness was 658.07 MPa·cm3/g, and when it was 45%, the compression ratio stiffness is 943.51MPa·cm3/g. It can be seen that by increasing the mass fraction of ZrO2, the stiffness of the composite material can be effectively increased, and the ability of the material to resist deformation would be increased. Typically, the more stressed the bone substitute material, the greater the stiffness of the compression ratio. Different mass fractions of ZrO2/HAP filling materials can be selected to meet the mechanical performance requirements of sports bone injury, and it can also provide a reference for the selection of bone substitute materials for different patients.

MEMS 공정에서의 자기 조립 단분자층 기술 응용 (Applications of Self-assembled Monolayer Technologies in MEMS Fabrication)

  • 이우진;이승민;강승균
    • 마이크로전자및패키징학회지
    • /
    • 제30권2호
    • /
    • pp.13-20
    • /
    • 2023
  • 마이크로 전자기계 시스템 공정에서 표면 처리는 공정 방법의 일환이자 디바이스에 자체적인 기능을 부여하는 역할을 한다. 특히 자기 조립 단분자층은 마이크로 전자기계 시스템 공정에서 표면 개질 및 기능화를 수행하는 표면처리 방법으로 침지 시간과 용액 농도에 따라 강도를 정밀하게 조절할 수 있는 유기 단분자막이다. 고분자 기판이나 금속/세라믹 부품에 자발적으로 흡착되어 형성되는 자기 조립 단분자층은 표면 특성의 개질 뿐만 아니라 나노스케일 단위의 높은 정밀도로 하여금 양산용 리소그래피 기술 및 초민감 유기/생체분자 센서에도 응용되고 있다. 본 논문에서는 마찰 특성의 조절부터 생체 분자의 탐침 기능까지 자기 조립 단분자층 기술이 발전되어 응용되고 있는 다양한 분야들에 대해 소개한다.

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF

치질접착에서 접착강도와 변연누출 (BOND STRENGTH AND MICROLEAKAGE IN RESIN BONDING TO TOOTH STRUCTURE)

  • 김진희;박정원;박진훈;김성교
    • Restorative Dentistry and Endodontics
    • /
    • 제24권4호
    • /
    • pp.570-577
    • /
    • 1999
  • 치질에 대한 접착수복은 건전한 치질을 보존하면서 유지력을 증가시킬 뿐 아니라 치질과 수복물 계면에서의 미세누출을 방지할 수 있다는 측면에서 임상에서 그 사용빈도가 높아지고 있다. 그러나 복합레진충전후 중합과정에서의 수축현상이 여전히 해결되지 않는 문제로 남아 있으며 이로 인한 변연누출은 술후 지각과민, 변연변색이나 이차우식과 아울러 치수병변의 유발인자로 작용할 수 있다. 치질과 레진수복물간의 접착강도를 강화시킴으로써 변연부위의 누출현상을 극복할 수 있다는 인식 하에 많은 종류의 상아질 접착제에 대한 접착강도 검사와 미세누출 검사가 행해졌으나 접착강도와 변연누출간의 관계에 대한 직접적인 연구는 미흡한 상태이다. 본 연구에서는 우치를 이용한 동일시편에서 접착강도와 미세누출의 정도를 측정 후 상호관계를 알아보고자 하였다. 소의 하악 전치를 이용하여 법랑질 또는 상아질 시편을 각 군마다 30개씩 준비하였다. 32% 인산으로 15초 처리 및 20초 수세 후 치질처리 방법에 따라 법랑질/완전 건조시킨 군, 법랑질/습윤상태의 군, 상아질/완전 건조시킨 군, 상아질/습윤상태의 군으로 나누었다. 각 군의 시편을 One-Step$^{TM}$ adhesive를 적용 후 Charisma 복합레진으로 충전하였다. 그 후 2% methylene blue에 1주일 간 침잠시킨 후 24시간 흐르는 물에 수세한 뒤 인장접착 강도를 측정하였다. 인장 접착 강도 측정 후 컴퓨터 프로그램 상에서 색소의 침투 면적을 계산하였으며 그 결과는 다음과 같이 나타났다. 1. 법랑질 및 상아질 군 공히, 접착강도와 미세누출을 비교시 유의한 음의 상관관계를 나타내어 접착강도가 높을수록 미세변연누출은 적게 나타내는 경향을 나타내었다 (r=-0.50, p<0.05). 2 법랑질 군 및 상아질 군 공히, 습윤상태의 시편이 완전히 건조된 시편에 비해 높은 집착강도를 나타내었다 (p<0.05). 3. 상아질에서는 습윤상태의 군이 건조시킨 군 사이에 유의하게 적은 미세변연 누출을 나타낸 반면(p<0.05), 법랑질에서는 습윤상태의 군과 건조시킨 군 사이에 미세변연 누출에 있어 유의한 차이가 나타나지 않았다 (p>0.05).

  • PDF

마찰용접된 국산내열 강 (SUH3-SUS303 )의 시효열처리가 고온피로강도 및 파괴거동에 미치는 영향에 관한 연구 (The Effect of Aging Treatment on the High Temperature Fatigue Fracture Behavior of Friction Welded Domestic Heat Resisting Steels (SUH3-SUS 303))

  • 이규용;오세규
    • 수산해양기술연구
    • /
    • 제17권2호
    • /
    • pp.93-103
    • /
    • 1981
  • Si-Cr계 내열강 SUH3와 Cr-Ni계 stainless강 SUS 303 및 이들이 마찰용접재 SUH3-SUS303을 $1,060^{\circ}C$에서 용체화처리하고 다시 $700^{\circ}C$에서 10, 100시간 시효열처리한 각 시험편의 고온 피로강도에 대한 시효열처리의 효과를 알기 위하여 $700^{\circ}C$에서 고온 회전굽힘 피로시험을 하고 파약거동을 미시적으로 관찰하여 다음과 같은 결과를 얻었다. 1) SUH3재와 SUS303재의 최적마찰용접조건은 회전수 2420rpm, 마찰가압력 $8kg/mm^2$, 전 upset량 7mm(마찰가압시간 3sec, upset시간 2sec)이었다. 2) $700^{\circ}C$ 고온에서 장시간 이루어지는 고온피로시험에 있어, 용체화처리재의 S-N 곡선 경사부의 기울기가 가장 급하게 나타났다. 3) SUH3-SUS303 마찰용접재는 $1,060^{\circ}C$에서 1시간용체화 처리하고, $700^{\circ}C$에서 시효처리하는 경우 최적시효시간은 10시간이었다. 4) 10시간 시료재의 고온피로한도는 모재보다 SUH3은 75.4%, SUS303은 28.5% 높았으며, 용접재 SUH3-SUS303은 44.2% 정도 높았다. 100시간 시효재는 모재보다 SUH3은 64.91% SUS303은 30.4% 높았으며, SUH3-SUS303은 30.4% 높았으며, SUH3-SUS303은 36.6% 높았다. 5) 마찰용접재의 상온 및 고온의 피로파단은 모두 SUS303의 모재측에 발생하였으며, 용접면에서의 파단은 전혀 없었다. 6) SUS303재와 마찰용접재 SUH3-SUS303재의 크랙은 입내파양형이었으나 SUH3은 입계크랙의 전파로 파양한다.

  • PDF

Ziegler-Natta와 메탈로센 촉매로 합성된 폴리올레핀 2원 블렌드의 상 형태학 (Morphological Properties of Binary Blends of Polyolefins Synthesized by Metallocene and Ziegler-Natta Catalysts)

  • 곽한진;김학림;최순자
    • 공업화학
    • /
    • 제10권6호
    • /
    • pp.944-948
    • /
    • 1999
  • 메탈로센 촉매로 만든 폴리에틸렌(MCPE)과 Ziegler-Natta 촉매로 만들어진 4가지의 폴리올레핀으로 구성된 2원 블렌드의 상 형태학을 통하여 미세 분자 구조의 변화가 이들 블렌드의 상 형태학과 계면 거동에 미치는 영향을 연구하였다; 연구한 네 쌍의 블렌드는 고밀도 폴리에틸렌(HDPE)-MCPE, 폴리프로필렌(PP)-MCPE, poly(propylene-co-ethylene) (CoPP)-MCPE, poly(propylene-co-ethylene-co-1-buthylene) (TerPP)-MCPE이며 모두 상 분리된 시스템이다. HDPE-MCPE는 HDPE 성분이 증가할수록 HDPE 결정이 MCPE 연속상에서 고르게 성장하는 동질상(homogeneous phase)을 나타내는 반면에, 나머지 세 쌍의 블렌드는 복잡한 이종의 상(heterogeneous phase) 형태학을 보였다. PP-MCPE는 PP와 MCPE의 상과 계면이 완전히 분리된 상 형태학을 보였고, MCPE가 50% 함유된 조성에서 상전이가 일어났다. CoPP-MCPE와 TerPP-MCPE는 이들 코폴리머에 함유한 에틸렌기로 인해 두 계면 사이의 혼화성이 증가하는 현상을 보였으며 MCPE가 40%인 블렌드에서 상전이가 일어났다. 특히 TerPP-MCPE 블렌드는 TerPP의 코폴리머가 MCPE와 같은 화학구조를 보이는 1-부텐과 에틸렌기를 가지고 있어 다른 두 블렌드인 PP-MCPE, CoPP-MCPE 보다 두 상간의 계면이 서로 부분적으로 섞이는 양상을 보였다. 상 형태학에서 본 미세 분자구조에 의한 부분적 상용성은 기계적 특성이나 유변학적 성질과도 밀접한 관계를 나타냈다. 그러므로 본 연구에 사용한 네 가지 블렌드는 두 상이 완전히 분리되어 열역학적으로 비 혼화성을 나타내지만 다음과 같은 특성을 제시할 수 있다. 즉 계면의 세기는 HDPE-MCPE>TerPP-MCPE>CoPP-MCPE>PP-MCPE 순이며, 이는 미세 분자 구조측면에서 공통의 화학 구성물이 계면 접착력(interfacial adhesion)의 증가를 가져오는 중요한 요인으로 작용하기 때문으로 여겨진다.

  • PDF

산부식 전처리에 따른 2단계 자가부식 접착제의 연마 법랑질에 대한 미세인장결합강도 (The micro-tensile bond strength of two-step self-etch adhesive to ground enamel with and without prior acid-etching)

  • 김유리;김지환;심준성;김광만;이근우
    • 대한치과보철학회지
    • /
    • 제46권2호
    • /
    • pp.148-156
    • /
    • 2008
  • 자가부식 접착제는 사용하기 쉽고, 술식 민감성이 적은 장점이 있으나 특히 산도가 약한 자가부식 접착제의 법랑질에 대한 결합력은 논란이 되고 있다. 본 연구에서는 2단계 자가부식 접착제인 Clearfil SE Bond (Kuraray, Okayama, Japan)의 연마 법랑질에 대한 미세인장 결합강도를 측정하여 3단계 산부식수세 접착제인 Scotchbond Multi-Purpose (3M ESPE, St. Paul, MN, USA) 및 1단계 자가부식 접착제인 iBond (Heraeus Kulzer Gmbh, Hanau, Germany)의 결합강도와 비교하고자 하였고, 2단계 자가부식 접착제에 산부식 전처리를 시행하는 것이 법랑질에 대한 결합강도를 높일 수 있는지 알아 보고자 하였다. 실험군은 2단계 자가부식 접착제인 Clearfil SE Bond만 사용한 비산부식 군과 35% 인산 (Scotchbond Etchant, 3M ESPE)으로 산부식 후 Clearfil SE Bond를 사용한 산부식 군, 그리고 1단계 자가부식 접착제인 iBond를 사용한 군으로 나누었다. 대조군은 3단계 산부식수세 접착제인 Scotchbond Multi-Purpose를 사용한 군으로 정하였다. Bovine 전치의 순면을 십자가형으로 4등분하여 각 군으로 무작위로 배분하였다. 각 치아의 순면을 800-grit 실리콘 카바이드 지로 연마한 후 삭제된 법랑질면에 제조사의 설명서에 따라 각 군의 접착제를 적용하고 Light-Core (Bisco)로 적층 충전하였다. 시편은 $37i{\acute{E}}$, 증류수에 일주일 동안 보관한 후 low speed precicion diamond saw (TOPMENT Metsaw-LS, R&B, Daejeon, Korea)를 이용하여 약 $0.8{\times}0.8mm$ 단면이 되도록 시편을 절단하여 미세시편을 제작하였다. 일주일마다 증류수를 교환하면서 한 달, 세 달 동안 $37i{\acute{E}}$, 증류수에 미세시 편을 보관한 후 각각의 미세인장결합강도를 측정하였다. 미세인장결합강도 (MPa)는 파절 시에 가해진 힘 (N)을 접착면적 ($mm^2$)으로 나누어 계산하였다. 접착계면에서의 파절 양상은 실물현미경 (Microscope-B nocular, Nikon)을 이용하여 분류하였다. 미세인장결합강도에 대한 통계분석은 one-way ANOVA를 이용하여 유의수준 5%에서 검정하였고, 사후감정은 Least Significant Difference 방법을 이용하였다. 중합 후 1개월 뒤 측정된 각각의 접착제의 평균 미세인장결합강도는 유의수준 5%에서 모든 접착제 간에 유의한 차이가 없었다. 3개월 뒤 측정된 각각의 접착제의 평균 미세인장결합강도는 유의수준 5%에서 iBond 와 Clearfil SE Bond 비산부식 군과 Scotchbond Multi- Purpose 간에는 각각 유의한 차이가 없었다. 본 연구에서는 2단계 자가부식 접착제인 Clearfil SE Bond의 연마 법랑질에 대한 미세인장결합강도가 3단계 산부식수세 접착제인 Scotchbond Multi-Purpose 와 비교하여 유의한 차이가 없었으며 (P>0.05), 3개월 후의 결과에서 Clearfil SE Bond 비산부식 군의 미세인장결합강도가 Clearfil SE Bond 산부식 군보다 유의하게 낮았다 (P<0.05). 즉 35% 인산으로 산부식 전처리를 시행한결과 Clearfil SE Bond 의 법랑질에 대한 결합강도가 증가하였다.