• Title/Summary/Keyword: Micro joining

Search Result 243, Processing Time 0.026 seconds

Strategy and progress to establish a micro-assembly technology archive considering the mechanisms of joining- and manipulating- processes

  • Takahashi, Kunio
    • Proceedings of the KWS Conference
    • /
    • 2005.06a
    • /
    • pp.367-369
    • /
    • 2005
  • For the purpose of the optimization or the break through of production processes, it is essential to understand or theoretically interpret dominant mechanisms of the processes, and further more, archive them. and utilize them combining some of them which are needed. Especially in the technology for micro- or nano-scaled objects, adhesion phenomenon is no more negligible, because the adhesion force is proportional to the size of objects meanwhile gravity force is proportional to the third power of it. Author has been working about the mechanisms for micro-assembly processes, which include joining processes and manipulation processes. In the present paper, the strategy and the progress to establish the micro-assembly technology archive are introduced. Some of the mechanisms are introduced with related basic approaches to the adhesion phenomena. Also it will be expressed that our data base project for the surface and interfacial energies is strongly related to these basic approaches.

  • PDF

Effect of Fine Alumina Filler Addition on the Thermal Conductivity of Non-conductive Paste (NCP) for Multi Flip Chip Bonding (멀티 플립칩 본딩용 비전도성 접착제(NCP)의 열전도도에 미치는 미세 알루미나 필러의 첨가 영향)

  • Jung, Da-Hoon;Lim, Da-Eun;Lee, So-Jeong;Ko, Yong-Ho;Kim, Jun-Ki
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.24 no.2
    • /
    • pp.11-15
    • /
    • 2017
  • As the heat dissipation problem is increased in 3D multi flip chip packages, an improvement of thermal conductivity in bonding interfaces is required. In this study, the effect of alumina filler addition was investigated in non-conductive paste(NCP). The fine alumina filler having average particles size of 400 nm for the fine pitch interconnection was used. As the alumina filler content was increased from 0 to 60 wt%, the thermal conductivity of the cured product was increased up to 0.654 W/mK at 60 wt%. It was higher value than 0.501 W/mK which was reported for the same amount of silica. It was also found out that the addition of fine sized alumina filler resulted in the smaller decrease in thermal conductivity than the larger sized particles. The viscosity of NCP with alumina addition was increased sharply at the level of 40 wt%. It was due to the increase of the interaction between the filler particles according to the finer particle size. In order to achieve the appropriate viscosity and excellent thermal conductivity with fine alumina fillers, the highly efficient dispersion process was considered to be important.

Laser Transmission Welding of Flexible Substrates and Evaluation of the Mechanical Properties (플렉서블 기판의 레이저 투과 용접 및 기계적 특성 평가)

  • Ko, Myeong-Jun;Sohn, Minjeong;Kim, Min-Su;Na, Jeehoo;Ju, Byeong-Kwon;Park, Young-Bae;Lee, Tae-Ik
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.2
    • /
    • pp.113-119
    • /
    • 2022
  • In order to improve the mechanical reliability of next-generation electronic devices including flexible, wearable devices, a high level of mechanical reliability is required at various flexible joints. Organic adhesive materials such as epoxy for bonding existing polymer substrates inevitably have an increase in the thickness of the joint and involve problems of thermodynamic damage due to repeated deformation and high temperature hardening. Therefore, it is required to develop a low-temperature bonding process to minimize the thickness of the joint and prevent thermal damage for flexible bonding. This study developed flexible laser transmission welding (f-LTW) that allows bonding of flexible substrates with flexibility, robustness, and low thermal damage. Carbon nanotube (CNT) is thin-film coated on a flexible substrate to reduce the thickness of the joint, and a local melt bonding process on the surface of a polymer substrate by heating a CNT dispersion beam laser has been developed. The laser process conditions were constructed to minimize the thermal damage of the substrate and the mechanism of forming a CNT junction with the polymer substrate. In addition, lap shear adhesion test, peel test, and repeated bending experiment were conducted to evaluate the strength and flexibility of the flexible bonding joint.

A study of joint properties of Sn-Cu-(X)Al(Si) middle-temperature solder for automotive electronics modules (자동차 전장부품을 위한 Sn-0.5Cu-(X)Al(Si) 중온 솔더의 접합특성 연구)

  • Yu, Dong-Yurl;Ko, Yong-Ho;Bang, Junghwan;Lee, Chang-Woo
    • Journal of Welding and Joining
    • /
    • v.33 no.3
    • /
    • pp.19-24
    • /
    • 2015
  • Joint properties of electric control unit (ECU) module using Sn-Cu-(X)Al(Si) lead-free solder alloy were investigated for automotive electronics module. In this study, Sn-0.5Cu-0.01Al(Si) and Sn-0.5Cu-0.03Al(Si) (wt.%) lead-free alloys were fabricated as bar type by doped various weight percentages (0.01 and 0.03 wt.%) of Al(Si) alloy to Sn-0.5Cu. After fabrications of lead-free alloys, the ball-type solder alloys with a diameter of 450 um were made by rolling and punching. The melting temperatures of 0.01Al(Si) and 0.03Al(Si) were 230.2 and $230.8^{\circ}C$, respectively. To evaluation of properties of solder joint, test printed circuit board (PCB) finished with organic solderability perseveration (OSP) on Cu pad. The ball-type solders were attached to test PCB with flux and reflowed for formation of solder joint. The maximum temperature of reflow was $260^{\circ}C$ for 50s above melting temperature. And then, we measured spreadability and shear strength of two Al(Si) solder materials compared to Sn-0.7Cu solder material used in industry. And also, microstructures in solder and intermetallic compounds (IMCs) were observed. Moreover, thickness and grain size of $Cu_6Sn_5$ IMC were measured and then compared with Sn-0.7Cu. With increasing the amounts of Al(Si), the $Cu_6Sn_5$ thickness was decreased. These results show the addition of Al(Si) could suppress IMC growth and improve the reliability of solder joint.

Development of SiC Composite Solder with Low CTE as Filling Material for Molten Metal TSV Filling (용융 금속 TSV 충전을 위한 저열팽창계수 SiC 복합 충전 솔더의 개발)

  • Ko, Young-Ki;Ko, Yong-Ho;Bang, Jung-Hwan;Lee, Chang-Woo
    • Journal of Welding and Joining
    • /
    • v.32 no.3
    • /
    • pp.68-73
    • /
    • 2014
  • Among through silicon via (TSV) technologies, for replacing Cu filling method, the method of molten solder filling has been proposed to reduce filling cost and filling time. However, because Sn alloy which has a high coefficient of thermal expansion (CTE) than Cu, CTE mismatch between Si and molten solder induced higher thermal stress than Cu filling method. This thermal stress can deteriorate reliability of TSV by forming defects like void, crack and so on. Therefore, we fabricated SiC composite filling material which had a low CTE for reducing thermal stress in TSV. To add SiC nano particles to molten solder, ball-typed SiC clusters, which were formed with Sn powders and SiC nano particles by ball mill process, put into molten Sn and then, nano particle-dispersed SiC composite filling material was produced. In the case of 1 wt.% of SiC particle, the CTE showed a lowest value which was a $14.8ppm/^{\circ}C$ and this value was lower than CTE of Cu. Up to 1 wt.% of SiC particle, Young's modulus increased as wt.% of SiC particle increased. And also, we observed cross-sectioned TSV which was filled with 1 wt.% of SiC particle and we confirmed a possibility of SiC composite material as a TSV filling material.