• Title/Summary/Keyword: Micro Cement

검색결과 320건 처리시간 0.023초

급결 마이크로 시멘트의 성능평가를 통한 차수층 활용성에 관한 연구 (A Study on the Application of the Water Impermeable by the Evaluation of the Performance of Rapid Micro Cement.)

  • 조일규;유재형;오상근
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2018년도 춘계 학술논문 발표대회
    • /
    • pp.345-346
    • /
    • 2018
  • In this study, various materials such as epoxy material, urethane material, cement material, and acrylic material are used to solve the water leakage occurring in underground structures. However, in the reality that the durability is insufficient and the effect is insufficient, it is aimed to improve the repairing effect by using cement and acrylics n combination. As a first study, we tried to verify the performance of rapid micro cement and cement paste and to improve the performance by checking the product properties. Three types of micro cement are evaluated. Three types of micro cement are used: fiber inclusion, fiber unfolding, and cement paste. When the material is selected for micro cement, it is applied to the field to understand the maintenance effect and durability.

  • PDF

보통포틀랜드 시멘트와 초미립자 시멘트의 혼화재료 혼입시 특성 (The Specification of OPC and Micro Cement using the Admixture)

  • 김득모;이화영;박원춘;문경주;소승영;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.905-908
    • /
    • 2008
  • 보통 포틀랜드 시멘트(Ordinary Portland Cement 이하 OPC)에 혼화재료를 사용하는 기존의 콘크리트는 초기 고강도를 발현하는데에 많은 어려움을 지니고 있다. 이에 본 연구에서는 그 방안으로 초미립자 시멘트(Micro Cement 이하 MC)의 사용에 대해 연구하고자 실험을 진행하였다. 실험 결과 MC는 OPC보다 플로우에서 취약함을 보였으나 초기강도에서 우수한 강도특성을 보였고 28일 강도에서도 OPC를 상회하는 것을 알 수 있었다. GBFS(granulated Blast Furnace Slag이하 GBFS라 함)의 경우 플로우는 감소하며, 초기강도는 증가하는 것으로 나타났다. MC의 경우 플라이애시 혼입시 강도발현에 있어 도움이 되지 않는 것으로 나타났다.

  • PDF

석분의 효과적인 이용에 관한 연구 (Effective Use of Aggregate Fines)

  • 백신원
    • 한국안전학회지
    • /
    • 제16권1호
    • /
    • pp.65-72
    • /
    • 2001
  • Portland cement concrete is made with coarse aggregate, fine aggregate, portland cement, water and, in some cases, selected chemical admixture such as air-entraining agents, water reducer, superplasticizer, and so on, and mineral admixture such as fly ash, silica fume, slags, etc. Typically, in the concrete, the coarse aggregate and fine aggregate will occupy approximately 80 percent of the total volume of the finished mixture. Therefore, the coarse and fine aggregates affect to the properties of the portland cement concrete. As the deposits of natural sands have slowly been depleted, it has become necessary and economical to produce crushed sand(manufactured fine aggregate). It is reported that crushed sand differs from natural sands in gradation, particle shape and texture, and that the content of micro fines in the crushed sand affect to the quality of the portland cement concrete. Therefore, the purpose of this paper is to investigate the characteristics of fresh and hardened concrete with higher micro fines. This study provides a firm data to apply crushed sand with higher micro fines.

  • PDF

Laboratory tests for studying the performance of grouted micro-fine cement

  • Aflaki, Esmael;Moodi, Faramarz
    • Computers and Concrete
    • /
    • 제20권2호
    • /
    • pp.145-154
    • /
    • 2017
  • In geological engineering, grouting with Portland cement is a common technique for ground improvement, during which micro-fine cement is applied as a slurry, such that it intrudes into soil voids and decreases soil porosity. To determine the utility and behavior of cements with different Blaine values (index of cement particle fineness) for stabilization of fine sand, non-destructive and destructive tests were employed, such as laser-ray determination of grain size distribution, and sedimentation, permeability, and compressive strength tests. The results of the experimental study demonstrated a suitable mix design for the upper and lower regions of the cement-grading curve that are important for grouting and stabilization. Increasing the fineness of the cement decreased the permeability and increased the compressive strength of grouted sand samples considerably after two weeks. Moreover, relative to finer (higher Blaine value) or coarser (lower Blaine value) cements, cement with a Blaine value of $5,100cm^2/g$ was optimal for void reduction in a grouted soil mass. Overall, study results indicate that cement with an optimum Blaine value can be used to satisfy the designed geotechnical criteria.

미분의 효과적인 이용에 관한 연구 (Effective Use of Micro Fines)

  • 백신원
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.73-78
    • /
    • 2001
  • Portland cement concrete is made with coarse aggregate, fine aggregate, portland cement, water and, in some cases, selected chemical admixtures such as air-entraining agents, water reducer, superplasticizer, and so on, and mineral admixtures such as fly ash, silica fume, slags, etc. Typically, in the concrete, the coarse aggregate and fine aggregate will occupy approximately 80 percent of the total volume of the final mix. Therefore, the coarse and fine aggregates affect to the properties of the portland cement concrete. As the natural sands are drained, it is necessary and economical to utilize crushed sands(manufactured fine aggregate). It is reported that crushed sands differ from natural sands in gradation, particle shape and texture, and the micro fines in the crushed sands affect to the quality of the portland cement concrete. Therefore, the purpose of this paper is to investigate the characteristics of fresh and hardened concrete with high content of micro fines. This study provides firm data for the use of crushed sands with higher micro fines.

  • PDF

경량콘크리트를 사용한 충전용 재료의 공학적 특성 (Engineering Characteristics of Filling Materials using Lightweight Foamed Concrete)

  • 도종남;강형남;서두원;천병식
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2009년도 세계 도시지반공학 심포지엄
    • /
    • pp.519-523
    • /
    • 2009
  • In this study, the base mixing ratio was determinated to estimate the optimal mixing ratio of material with a change of mixing ratio of micro cement, sand, foaming agent, plasticizer by testing the unconfined compressive strength test. The unconfined compressive strength test was performed to grasp a engineering characteristics of with a change of micro cement, bubble. The results of test, the unconfined compressive strength increased with a micro cement's increase and bubble's decrease. In the future, it will be secured that is reliable datas from laboratory of various condition and in-situ tests to develop optimal lightweight foamed concrete.

  • PDF

감수제의 사용이 micro-POFA 혼입 시멘트 페이스트의 초기 수화 특성에 미치는 영향에 관한 실험적 연구 (Experimental Study on the Influence of Superplasticizer on the Early Hydration Properties of Cement Paste Containing Micro-POFA)

  • 위광우;이한승;임승민
    • 한국건축시공학회지
    • /
    • 제21권4호
    • /
    • pp.269-279
    • /
    • 2021
  • Palm Oil Fuel Ash(POFA)는 콘크리트의 물리적 특성 및 내구성을 향상시키기 위해 일정량 시멘트를 치환하여 사용된다. 그러나 높은 강열감량과 각진 입자 형상으로 인해 POFA를 사용한 콘크리트의 워커빌리티가 감소한다. 본 연구에서는 micro-POFA를 혼입한 시멘트 페이스트의 초기 물리적, 수화 특성에 감수제 종류 및 사용량이 미치는 영향을 mini-slump 실험, 초기 압축 강도, TGA, XRD, SEM을 이용하여 검토하였다. micro-POFA 치환율이 증가함에 따라 시멘트 페이스트의 유동성은 감소하였으며, 감수제의 사용량이 증가할수록 시멘트 페이스트의 유동성은 증가하였다. 또한, 감수제의 사용은 시멘트 페이스트의 초기 압축 강도를 저하시켰으며, 사용량이 증가할수록 압축 강도 저하가 뚜렷하게 나타났다. 미세분석을 통해 감수제가 C-S-H 형성을 억제하고 상대적으로 Ca(OH)2의 생성량을 증가시켰기 때문이라고 사료된다.

하수슬러지 소각재와 무기바인더를 이용한 응용 블록 개발 II (Development of Application Block Using Geobond and Ash from Sewage Sludge Incinerator II)

  • 이현주
    • 대한환경공학회지
    • /
    • 제37권7호
    • /
    • pp.412-417
    • /
    • 2015
  • 본 연구는 하수처리장에서 발생하는 하수슬러지 소각재와 Geobond를 이용한 응용 블록의 개발을 위하여 수행하였다. 실험은 무소성 공정으로 진행하였으며, Sewage Sludge Ash (SSA)를 Geobond(무기바인더)와 특수시멘트인 초조강 시멘트 마이크로 시멘트, 모래 등의 바인더를 혼합한 각각의 페이스트 시편을 성형 후 건조 및 양생과정을 거친 시편을 단기 압축강도를 측정한 후 28일 장기 양생한 결과 압축 강도가 64.6 MPa로 발현하였다. 이는 KS기준치 22.54 MPa ($229.7kg/cm^2$)을 훨씬 상회하는 고강도의 압축강도를 나타내었다. 하수슬러지 소각재(SSA) 첨가율은 각 바인더 별 약 10~40%까지 혼합 가능한 것으로 나타났다. 따라서 SSA를 무기바인더인 Geobond와 특수시멘트(HESPC, MC)의 대체 물질로의 사용이 가능함을 입증하였다.

폴리머 시멘트 콘크리트를 이용한 LB-DECK의 미소균열 제어 (Micro-Cracks Control of LB-DECK Using Polymer Cement Concrete)

  • 노병철;최종윤;조규대;최종권
    • 콘크리트학회논문집
    • /
    • 제24권2호
    • /
    • pp.103-109
    • /
    • 2012
  • 프리캐스트 콘크리트 패널에서의 0.1 mm 이하의 미세균열은 구조적 문제점은 없으나, 미관은 물론 장기적으로 내구성을 저하시키는 요인이 될 수 있으므로, 이의 보수를 위한 추가비용이 발생할 수 있다. 이 논문에서는 이러한 미세균열의 발생을 개선하고자 폴리머 시멘트 콘크리트를 적용하여 휨인장강도를 증진시킴으로써 초기 균열하중을 증대시킴으로써, 초기 시공하중에 의한 미세균열 발생을 최소화 하였다. 그 결과 폴리머-시멘트비 5%를 적용하였을 경우의 균열저항모멘트가 증가함에 따라 초기 시공하중에 의한 균열 발생을 제어할 수 있었다.