• Title/Summary/Keyword: MgO-$TiO_2$ content

Search Result 76, Processing Time 0.029 seconds

Enhanced Crystallization Behaviour and Microwave Dielectric Properties of 0.9CaMgSi2O6-0.1MgSiO3 Glass-Ceramics Doped with TiO2

  • Jo, Hyun Jin;Sun, Gui Nam;Kim, Eung Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.2
    • /
    • pp.139-144
    • /
    • 2016
  • The dependence of the microwave dielectric properties of the glass-ceramic composite $0.9CaMgSi_2O_6-0.1MgSiO_3$ on the crystallization behaviour was investigated as functions of the $TiO_2$ content and heat-treatment temperature. The crystallization behaviour of the specimens was evaluated via a combination of the Rietveld and reference-intensity ratio methods. For specimens with a $TiO_2$ content of up to 1 wt.%, a monoclinic diopside phase was formed, whereas a secondary $TiO_2$ phase was formed with further increases in the $TiO_2$ content. The quality factor (Qf) of the specimens was strongly dependent on the degree of crystallization. The highest Qf value was obtained with a $TiO_2$ content of 0.5 wt.%, which was improved by increasing the heat-treatment temperature. The dielectric constant (K) was affected by the size of the crystallites and the $TiO_2$ content. The temperature coefficient of the resonant frequency (TCF) was nearly constant for all of the specimens, regardless of the $TiO_2$ content or heattreatment temperature.

Effect of $TiO_2$ Addition on the Secondary Electron Emission and Discharge Properties of MgO Protective Layer (산화마그네슘 보호막의 이차전자방출과 방전특성에 미치는 산화티타늄첨가의 효과)

  • Kim, Young-Hyun;Kim, Rak-Hwan;Kim, Hee-Jae;Park, Jong-Wan
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.04a
    • /
    • pp.148-151
    • /
    • 2000
  • $Mg_{2-2x}Ti_xO_2$ films were prepared by e-beam evaporation method to be used as possible substitutes for the conventional MgO protective layer. The oxygen content in the films and in turn, the ratio of metal to oxygen gradually increased with increasing the $TiO_2$ content in the starting materials. The pure MgO films exhibited the crystallinity with strong (111) orientation. The $Mg_{2-2x}Ti_xO_2$ films, however, had the crystallinity with (311) preferred orientation. When the $[TiO_2/(MgO+TiO_2)]$ ratios of 0.1 and 0.15 were used, the deposited films exhibited the secondary electron emission yields improved by 50% compared to that of the conventional MgO protective layer, which resulted in reduction in discharge voltage by 12%.

  • PDF

Influence of the MgO-TiO2 Co-Additive Content on the Phase Formation, Microstructure and Fracture Toughness of MgO-TiO2-Reinforced Dental Porcelain Nanocomposites

  • Waiwong, Ranida;Ananta, Supon;Pisitanusorn, Attavit
    • Journal of the Korean Ceramic Society
    • /
    • v.54 no.2
    • /
    • pp.141-149
    • /
    • 2017
  • The influence of the co-additive concentration (0 - 45 wt% with an interval of 5 wt%) of MgO-$TiO_2$ on the phase formation, microstructure and fracture toughness of MgO-$TiO_2$-reinforced dental porcelain nanocomposites derived from a one-step sintering technique were examined using a combination of X-ray diffraction, scanning electron microscopy and Vickers indentation. It was found that MgO-$TiO_2$-reinforced dental porcelain nanocomposites exhibited significantly higher fracture toughness values than those observed in single-additive (MgO or $TiO_2$)-reinforced dental porcelain composites at any given sintering temperature. The amount of MgO-$TiO_2$ as a co-additive was found to be one of the key factors controlling the phase formation, microstructure and fracture toughness of these nanocomposites. It is likely that 30 wt% of MgO-$TiO_2$ as a co-additive is the optimal amount for $MgTi_2O_5$ and $Mg_2SiO_4$ crystalline phase formation to obtain the maximum relative density (96.80%) and fracture toughness ($2.60{\pm}0.07MPa{\cdot}m^{1/2}$) at a sintering temperature of $1000^{\circ}C$.

A Study on the Synthesis and Properties of Additives Coated BaTiO3 (첨가제가 Coating된 BaTiO3의 합성 및 특성에 관한 연구)

  • Park, Jae-Sung;Kim, Young-Tae;Hur, Kang-Heon;Han, Young-Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.2
    • /
    • pp.189-199
    • /
    • 2009
  • The Powder characteristics and sintering behavior of $SiO_2$ coated $BaTiO_3$ were studied. $BaTiO_3$ powders were synthesized by the liquid mix method developed by Pechini, and silica coating was prepared by alkoxide hydrolysis method with TEOS and ethanol. The particle size of the $BaTiO_3$ powders was 35 nm and the thickness of the $SiO_2$ coating layer was 5 nm. As the $SiO_2$ content increased, the $SiO_2$ layers improved the powder dispersion by increasing electrostatic repulsion between the $BaTiO_3$ particles. Effects of MgO coating on microstructure and dielectric properties of $BaTiO_3$ have been studied compared with mechanically MgO mixed $BaTiO_3$. MgO coated $BaTiO_3$ particles were prepared by a homogeneous precipitation method using $MgCl_2\cdot 6H_2O$ and urea. MgO coated $BaTiO_3$ exhibited homogeneous microstructure compared with mixed samples. XRD analysis revealed that Mg substitution for the Ti site in the MgO mixed sample was much greater than in the coated one. Electrical properties of MgO mixed and coated $BaTiO_3$ were affected by the diffusion behavior of Mg in $BaTiO_3$ lattice.

Influence of BaTiO3 Content and Firing Temperature on the Dielectric Properties of Pb(Mg1/3Nb2/3)O3 Ceramics (Pb(Mg1/3Nb2/3)O3계의 유전성에 미치는 BaTiO3첨가량 및 열처리 온도의 영향 (PMN-BaTiO3계 세라믹스의 합성 및 유전성))

  • 윤기현;강동헌
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.2
    • /
    • pp.249-257
    • /
    • 1989
  • Dielectric properties and the stability of the perovskite phase in the Pb(Mg1/3Nb2/3)O3 system have been investigated as a function of amount of BaTiO3 and firing temperature. In the specimens fired at 120$0^{\circ}C$, the pyrochlore phase was eliminated by the addition of 10-15m/o BaTiO3 and also the dielectric constant increased. However, the dielectric constant decreased with further addition of BaTiO3 even though no pyrochlore phase was found to be present. The reducing tendency of the pyrochlore phase decreased with lowering the firing temperature in the system of Pb(Mg1/3Nb2/3)O3 with BaTiO3. Dielectric properties in PMN ceramics were affected by the character of the BaTiO3 rather than the pyrochlore phase.

  • PDF

Dielectric and strain properties of Pb(Mg$_{1/3}$Nb$_{2/3}$)O$_{3}$-PbTiO$_{3}$ Ceramic with Respect to the Variation of SrTiO$_{3}$ Substitution (SrTiO$_{3}$ 고용에 따른 Pb(Mg$_{1/3}$Nb$_{2/3}$)O$_{3}$-PbTiO$_{3}$계 세라믹스의 유전 및 전왜특)

  • 지승한;이해영;이덕출;이진걸;이연학
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.45 no.2
    • /
    • pp.235-241
    • /
    • 1996
  • In this paper dielectric and electrostrictive strain properties of (1-y-x)Pb(Mg$_{1/3}$Nb$_{2/3}$)O$_{3}$-PbTiO$_{3}$$-yPbTiO_{3}-xSrTiO_{3}[(1-y-x)PMN-yPT-xST]$ ceramics fabricated by using columbite precursor method have been investigated with the substitution of SrTiO$_{3}$(ST). Dielectric constant of the specimens increased with the increase of ST content up to 5[m/o] and decreased with further substitution of ST. And the pyrochlore phase decreased with the increase of ST content up to 5[m/o] in XRD analysis. The elimination of the pyrochlore phase improved dielectric constants. The electrostrictive strains generated by AC electric field have the highest value at 5[m/o] SrTiO$_{3}$ addition and the hysteresis of strain ranged from 12 to 20[%]. The electrostrictive strain at various temperature investigated in the temperature range of $-50[^{\circ}C]~74[^{\circ}C].$ In higher temperature than phase transition region, it showed paraelectric property which shows very small hystersis.

  • PDF

A study on the improvement of TiN diffusion barrier properties using Cu(Mg) alloy (Cu(Mg) alloy 금속배선에 의한 TiN 확산방지막의 특성개선)

  • 박상기;조범석;조흥렬;양희정;이원희;이재갑
    • Journal of the Korean Vacuum Society
    • /
    • v.10 no.2
    • /
    • pp.234-240
    • /
    • 2001
  • The diffusion barrier properties of TiN by using Cu(Mg) alloy film have been investigated. Cu(Mg) alloy film was deposited on air-exposed TiN film. Upon annealing, interfacial MgO of 100 $\AA$ has been formed due to the reaction of Mg with oxygen existed on the surface of TiN. Combined MgO/TiN structure prevented the interdiffusion of Cu and Si up to $800^{\circ}C$. To improve the adhesion of Cu(Mg) alloy film to the TiN, TiN layer was treated by $O_2$ plasma, followed by vacuum annealing at $300^{\circ}C$. It was found that increased oxygen on the surface of TiN film by plasma treatment enhanced segregation of Mg toward the interface, resulting in the formation of dense MgO layer. Improved adhesion characteristics have been formed through this treatment. However, increased power of $O_2$ plasma led to the formation of TiO$_2$ and decreased the Mg content to be segregated to the interface, resulting in the decrease in adhesion property. In addition, the deposition of 50 ${\AA}$ Si on the TiN enhanced the adhesion of Cu(Mg) alloy to TiN without deteriorating the TiN diffusion barrier characteristics.

  • PDF

Dielectric and Strain Properties of PMN-PT Ceramics Doped with $\textrm{SrTiO}^3$ and excess MgO ($\textrm{SrTiO}^3$ 와 과잉 MgO가 첨가된 $\textrm{Pb(Mg_{1/3}Nb_{2/3})O}_3$ - $\textrm{PbTiO}^3$ 계 세라믹스의 유전 및 변위 특성)

  • 이상훈
    • Journal of the Korean Institute of Telematics and Electronics T
    • /
    • v.36T no.3
    • /
    • pp.7-12
    • /
    • 1999
  • In this paper, dielectric and strain properties of (1-f-y)PMN-yPT-xST ceramics investigated with the amount of $\textrm{SrTiO}^3$(ST). The $\textrm{SrTiO}^3$ content is ranged within 1~6㏖%. Another compositions with excess MgO also investigated. As the amount of ST is increased, dielectric constant has a maximum value at 5㏖% composition. The Curie temperature is decreased linearly with increasing the amount of ST. Coercive field and ramnant polarization has a maximum value at l㏖% composition. As for the effects of excess MgO, the dielectric constant has been increased by the addition of excess MgO up to 3㏖% to a 0.8PMN-0.12PT-0.04ST specimen. But the strain has been decreased by the addition of excess MgO.

  • PDF

Deoxidation of Off-grade Ti scrap by Molten Mg in YCl3-MgCl2 Molten Salt (YCl3-MgCl2 혼합 용융염 중 용융 Mg에 의한 Off-grade Ti 스크랩의 탈산)

  • Jung, Jae-Heon;Lee, So-Yeong;Park, Sung-Hun;Sohn, Ho-Sang
    • Resources Recycling
    • /
    • v.30 no.2
    • /
    • pp.46-52
    • /
    • 2021
  • Off-grade Ti generated from smelting and mechanical processing has a high oxygen content. In this work, off-grade Ti was deoxidized using Mg and a chloride mixture as the reductant and flux, respectively. The experiments were conducted in the α-Ti temperature range (1,023~1,123 K) and the effects of the reaction time, reaction temperature, quantitiy of Mg and chloride ratio on deoxidation were investigated. Notably, when YCl3 is used as the flux to react with MgO, it is possible to reduce the activity of MgO. Therefore Ti can be deoxidized using Mg. In this study, the O content was decreased from 0.5 wt% to 0.1004 wt% at 1073 K, for 6 hours, with Mg=3.6 g and $X_{YCl_3}=0.22$.