마그네슘 판재의 고온 물성치 실험 (Experiments for Material Properties of Magnesium Metal Sheet at Elevated Temperatures)

  • 최의근;이상욱
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.378-381
    • /
    • 2009
  • In this study, the repetitive loading-unloading tensile tests with AZ31B magnesium sheet metal have been conducted under various elevated temperatures to check out how the Young's moduli of the sheets evolve during the plastic deformation. The loading-unloading tests have been carried out at every 1% of strain increment. With the tested results, some damage parameters of magnesium sheets based on the Lemaitre's continuum damage theory could be calculated at room temperature, $100^{\circ}C$, $150^{\circ}C$, $200^{\circ}C$ and $250^{\circ}C$. It has been shown that the critical damage parameters obtained in all temperature conditions are within the range of 0.12 to 0.18.

  • PDF

Numerical Simulation of Interactions between Corrosion Pits on Stainless Steel under Loading Conditions

  • Wang, Haitao;Han, En-Hou
    • Corrosion Science and Technology
    • /
    • 제16권2호
    • /
    • pp.64-68
    • /
    • 2017
  • The interactions between corrosion pits on stainless steel under loading conditions are studied by using a cellular automata model coupled with finite element method at a mesoscopic scale. The cellular automata model focuses on a metal/film/electrolyte system, including anodic dissolution, passivation, diffusion of hydrogen ions and salt film hydrolysis. The Chopard block algorithm is used to improve the diffusion simulation efficiency. The finite element method is used to calculate the stress concentration on the pit surface during pit growth, and the effect of local stress and strain on anodic current is obtained by using the Gutman model, which is used as the boundary conditions of the cellular automata model. The transient current characteristics of the interactions between corrosion pits under different simulation factors including the breakdown of the passive film at the pit mouth and the diffusion of hydrogen ions are analyzed. The analysis of the pit stability product shows that the simulation results are close to the experimental conclusions.

Cadmium and zinc removal from water by polyelectrolyte enhanced ultrafiltration

  • Ennigrou, Dorra Jellouli;Ali, Mourad Ben Sik;Dhahbi, Mahmoud;Mokhtar, Ferid
    • Membrane and Water Treatment
    • /
    • 제5권3호
    • /
    • pp.183-195
    • /
    • 2014
  • The efficiency of two metal ions (cadmium, zinc) removal from aqueous solutions by ultrafiltration (UF) and Polymer Enhanced Ultrafiltration (PEUF) processes were investigated in this work. The UF and PEUF studies were carried out using an ultrafiltration tangential cell system equipped with 5.000 MWCO regenerated cellulose. A water-soluble polymer: the polyacrylic acid (PAA) was used as complexant for PEUF experiments. The effects of transmembrane pressure, pH, metal ions and loading ratio on permeate fluxes and metal ions removals were evaluated. In UF process, permeate fluxes increase linearly with increasing pH for different transmembrane pressure, which may be the consequence of the formation of soluble metal hydroxyl complexes in the aqueous phase. In PEUF process, above pH 5.0, the Cd(II) retention reaches a plateau at 90% and Zn(II) at 80% for L = 5. Also, cadmium retention at different L is greater than zinc retention at pH varying from 5.0 to 9.0. In a mixture solution, cadmium retention is higher than zinc for different loading ratio, this is due to interactions between carboxylic groups of PAA and metal ions and more important with cadmium ions.

Chemical Assessment of Heavy Metal Contamination in Soil

  • Yang, Jae-E.;Choi, Moon-Heon
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 1997년도 총회 및 춘계 학술발표회 논문집
    • /
    • pp.8-11
    • /
    • 1997
  • Current methods of evaluating soil contamination by heavy metals rely on analyzing samples for total contents of metals or quantities recovered in various chemical extracting solutions. Results from these approaches provide only an index for evaluation because these methodologies yield values not directly related to bioavailability of soil-borne metals. In addition, even though concentrations of metals may be less than those required to cause toxic effects to biota, they may cause substantial effects on soil chemical parameters that determine soil quality and sustainable productivity. The objective of this research was to characterize effects of Cu or Cd additions on soil solution chemistry of soil quality indices, such as pH, EC, nutrient cation distribution and quantity/intensity relations (buffer capacity). Metals were added at rates ranging from 0 to 400 mg/kg of soil. Soil solution was sequentially extracted from saturated pastes using vacuum. Concentrations of Cu or Cd remaining in soil solutions were very low as compared to those added to the soils, warranting that most of the added metals were recovered as nonavailable (strongly adsorbed) fractions. Adsorption of the added metals released cations into soil solution causing increases of soluble cation contents and thus ionic strength of soil solution. At metal additions of 200~400 mg/kg, EC of soil solution increased to as much as 2~4 dS/m; salinity levels considered high enough to cause detrimental effects on plant production. More divalent cations (Ca+Mg) than monovalent cations (K+Na) were exchanged by Cu or Cd adsorption. The loss of exchangeable nutrient cations decreased long-term nutrient supplying capacity or each soil. At 100 mg/kg or metal loading, the buffering capacity was decreased by 60%. pH of soil solution decreased linearly with increasing metal loading rates, with a decrement of up to 1.3 units at 400 mg Cu/kg addition. Influences of Cu on each of these soil quality parameters were consistently greater than those of Cd. These effects were of a detrimental nature and large enough in most cases to significantly impact soil productivity. It is clear that new protocols are needed for evaluating potential effects of heavy metal loading of soils.

  • PDF

다층 FCA 용착금속의 수소취성 저항성 및 확산성 수소 방출 거동 (Hydrogen Embrittlement Resistance and Diffusible Hydrogen Desorption Behavior of Multipass FCA Weld Metals)

  • 유재석;곽현;이명진;김용덕;강남현
    • Journal of Welding and Joining
    • /
    • 제31권6호
    • /
    • pp.112-118
    • /
    • 2013
  • In this study, constant loading test (CLT) was performed to evaluate the hydrogen embrittlement resistance for multipass FCA weld metals of 600MPa tensile strength grade. The microstructures of weld metal-2 having the smallest carbon equivalent (Ceq=0.37) consisted of grain boundary ferrite and widmanstatten ferrite in the acicular ferrite matrix. The weld metal-1 having the largest Ceq=0.47, showed the microstructures of grain boundary ferrite, widmanstatten ferrite and the large amount of bainite (vol.%=19%) in the acicular ferrite matrix. The weld metal-3 having the Ceq=0.41, which was composed of grain boundary ferrite, widmanstatten ferrite, and the small amount of bainite (vol.%=9%) in the acicular ferrite matrix. Hydrogen desorption spectrometry (TDS) used to analyze the amount of diffusible hydrogen and trapping site for the hydrogen pre-charged specimens electrochemically for 24 hours. With increasing the current density of hydrogen pre-charging, the released amount of diffusible hydrogen was increased. Furthermore, as increasing carbon equivalent of weld metals, the released diffusible hydrogen was increased. The main trapping sites of diffusible hydrogen for the weld metal having a low carbon equivalent (Ceq=0.37) were grain boundaries and those of weld metals having a relatively high carbon equivalent (Ceq: 0.41~0.47) were grain boundaries and dislocation. The fracture time for the hydrogen pre-charged specimens in the constant loading test was decreased as the carbon equivalent increased from 0.37 to 0.47. This result is mainly due to the increment of bainite that is vulnerable to hydrogen embrittlement.

Hybrid-Ceramic Crown과 금속 도재관의 파절강도 비교 (COMPARISON OF FRACTURE STRENGTH BETWEEN HYBRID-CERAMIC CROWN AND METAL-CERAMIC CROWN)

  • 구철회;양홍서
    • 대한치과보철학회지
    • /
    • 제39권1호
    • /
    • pp.14-24
    • /
    • 2001
  • The purpose of this study was to compare the fracture strengths and the fracture patterns of several hybrid-ceramic crowns and metal-ceramic crown. Ten crowns were constructed for each group according to the manufacturer's instruction. Removable template of silicone rubber impression material was used for standardization of each crowns. Each crown was cemented on a metal die with hybrid glass ionomer cement. All crowns cemented were stored in distilled water, $36^{\circ}C$ for 24 hours prior to loading in an universal testing machine. The load was directed at 130 degrees the long axis of metal die. The fracture strengths were measured and the fracture patterns were observed. The following results were obtained from this study 1. The mean fracture strengths of $Artglass^{(R)}$, $Sculpture^{(R)}$ and $Targis^{(R)}$ were $57.5{\pm}9.5Kgf,\;62.7{\pm}12.2Kgf$ and $60.2{\pm}10.1Kgf$ respectively. There was no significant difference among each hybrid ceramic crown group. 2. The toad required to fracture hybrid-ceramic crowns was significantly smaller than metal-ceramic crowns($131.7{\pm}22.0Kgf$). 3. In the metal-ceramic crowns, labial porcelain detached partially from porcelain-metal junction of proximal side by load. 4. Hybrid-ceramic crowns showed a simple fracture pattern that fracture line began at the loading area and extended through proximal surface, perpendicular to the margin. The crown was separated into two parts of labial side and lingual side. Above results revealed that three kinds of the hybrid-ceramic crowns used in this study must have careful application in clinical use since the strength of hybrid-ceramic crown was lower(about 1/2) than that of metal-ceramic crown.

  • PDF

Impact performance study of filled thin-walled tubes with PM-35 steel core

  • Kunlong Tian;Chao Zhao;Yi Zhou;Xingu Zhong;Xiong Peng;Qunyu Yang
    • Structural Engineering and Mechanics
    • /
    • 제91권1호
    • /
    • pp.75-86
    • /
    • 2024
  • In this paper, the porous metal PM-35 is proposed as the filler material of filled thin-walled tubes (FTTs), and a series of experimental study is conducted to investigate the dynamic behavior and energy absorption performance of PM-35 filled thin-walled tubes under impact loading. Firstly, cylinder solid specimens of PM-35 steel are tested to investigate the impact mechanical behavior by using the Split Hopkinson pressure bar set (SHP); Secondly, the filled thin-walled tube specimens with different geometric parameters are designed and tested to investigate the feasibility of PM-35 steel applied in FTTs by the orthogonal test. According to the results of this research, it is concluded that PM-35 steel is with the excellent characteristics of high energy absorption capacity and low yield strength, which make it a potential filler material for FTTs. The micron-sizes pore structure of PM-35 is the main reason for the macroscopic mechanical behavior of PM-35 steel under impact loading, which makes the material to exhibit greater deformation when subjected to external forces and obviously improve the toughness of the material. In addition, PM-35 steel core-filled thin-wall tube has excellent energy absorption ability under high-speed impact, which shows great application potential in the anti-collision structure facilities of high-speed railway and maglev train. The parameter V0 is most sensitive to the energy absorption of FTT specimens under impact loading, and the sensitivity order of different variations to the energy absorption is loading speed V0>D/t>D/L. The loading efficiency of the FTT is affected by its different geometry, which is mainly determined by the sleeve material and the filling material, which are not sensitive to changes in loading speed V0, D/t and D/L parameters.

초음파와 AE기법을 이용한 금속복합재료의 피로손상진전 평가 (A Study on Fatigue Damage Accumulation of MMC using Ultrasonic Wave and Acoustic Emission)

  • 이진경;이준현
    • Composites Research
    • /
    • 제13권4호
    • /
    • pp.1-10
    • /
    • 2000
  • SiC가 강화된 금속복합재료는 기존의 금속재료에 비하여 비탄성계수와 비강도가 높기 때문에 자동차 및 항공산업에 많은 응용이 기대되고 있다. 금속복합재료의 파손기구는 적용된 하중에 의한 미시적 손상의 축적에 의해 많은 영향을 받기 때문에 금속복합재료의 광범위한 응용을 위해서는 금속복합재료가 반복 하중을 받을 때 미시적 파손기구를 이해하는 것이 대단히 중요하다. 따라서 본 연구에서는 SiCp/A356 금속복합재료의 미시적 손상 축적을 모니터링 하기 위하여 초음파와 음향방출기법을 적용하였다. 반복하중의 증가에 따라 초음파의 속도와 감쇠의 변화는 각 미시적 손상기구에 따라 3영역으로 나눌 수 있었다. 또한 각 영역에서 발생하는 AE 신호의 특징은 초음파의 속도 및 감쇠 변화와 비교, 분석되었다.

  • PDF

상악중절치에서 전부도재관의 finish line형태에 따른 파절강도와 응력 분포에 관한 연구 (THE FRACTURE RESISTANCE AND STRESS DISTRIBUTION OF ALL CERAMIC CROWNS WITH TWO TYPES OF FINISH LINE ON MAXILLARY CENTRAL INCISOR)

  • 기태석;김계순;이진한;김유리;동진근
    • 대한치과보철학회지
    • /
    • 제41권4호
    • /
    • pp.405-420
    • /
    • 2003
  • Purpose : The purpose of this study was to compare the fracture resistance of the IPS Empress ceramic crown with 1.0mm width rounded shoulder, which is usually recommended in all ceramic crown. and 0.5mm width chamfer finish lines on the maxillary central incisor. Material and method : After 15 metal dies were made for each group, the IPS Empress all ceramic crowns were fabricated and cemented with resin cement(Bistite resin cement, Tokuyama Soda Co. LTD., Japan) on the metal die. The cemented crowns were mounted on the positioning jig and the universal testing machine(Zwick Z020, Zwick Co. Germany)was used to measure the fracture strength with loading on the incisal edge. And also, three-dimensional finite element stress analysis was used to measure the stress distribution with the various types of the finish lines(1.0mm width rounded shoulder, 0.5mm width chamfer), the loading site(incisal edge, incisal $\frac{1}{3}$) and the type of loading(concentration loading, distribution loading). Results and conclusion : 1. In the fracture resistance experiment according to the finish line, the mean fracture strength of rounded shoulder(876N) and the mean fracture strength of chamfer(882N) did not skew any significant difference between each other(p>0.05). 2. The stress distribution of all ceramic crown in three dimensional finite element analysis showed concentration aspect at loading point and cervical area or labial surface. 3. In metal die, there were no differences in stress distribution between finish lines, but in natural teeth model, chamfer finish line showed higher stress than rounded shoulder finish line. 4. When force was loaded on the incisal edge the stress was concentrated on the incisal edge and the cervical area of labial surface. When force was loaded on the incisal $\frac{1}{3}$, the stress concentrated on the cervical area of labial surface and the cingulum area. 5. Generally, natural teeth model showed higher and various stress than the metal die.

FINITE ELEMENT ANALYSIS AND MEASUREMENT ON THE RELEASE OF RESIDUAL STRESS AND NON-LINEAR BEHAVIOR IN WELDMENT BY MECHANICAL LOADING(I) -FINITE ELEMENT ANALYSIS-

  • Jang, Kyoung-Bok;Kim, Jung-Hyun;Cho, Sang-Myoung
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.378-383
    • /
    • 2002
  • In previous study, the decrease and recovery of total stiffness in welded structure was discussed on the basis of experimental examination through tensile loading and unloading test of welded specimen. The recovery of structure stiffness was caused by the release of welding residual stress through mechanical loading. In this study, analysis model that is indispensable for the effective application of MSR method was established on the basis of test and measurement result. Thermal elasto-plastic analysis for welding process was performed by non-coupled analysis. Analysis results of welding process were transfer to elasto-plastic model for tensile loading & unloading by restart technique. In elasto-plastic analysis model for mechanical loading & unloading, hardening appearance of weld metal was considered by rezoning technique and tying technique was used for JIG condition of test machine.