The aim of this paper is to determine temperature and stress distributions in a ceramic based on Partially Stabilized Zirconia coated steel piston crown by using plasma spraying for improving performance of a marine diesel engine. Effects of coating constituent and thickness on temperature and stress distributions were investigated including comparisons with results from an uncoated piston by means of finite element method namely ANSYS. Temperature developed at the coated surface is significantly higher than that of the uncoated piston. The maximum stress components occur between bond coat and adjacent ceramic layer. Provided that coating thickness is constant as 0.5 mm, when numbers of layers increase, magnitude of the normal stress decrease about 34.1% on the base metal surface according to uncoated piston, but the base metal surface temperature of the steel piston increase about 13.1%.
The purpose of this study is to compare and analyze the shade changes(${\Delta}E^*$) about $In-Ceram^{(R)}$, $IPS-Empress^{(R)}$, $OPC^{(R)}$ by using of the spectrophotometer arising from inital status and before and after cementation of the resin cement mounted on the metal core. We used a couple of statistics such as 'One- Way ANOVA' and 'Multiple Range Test.' We could be able to verify significantly what is being discussed here up to 95%. The results drawn from our research are as follows : 1. At the time of our experiments regarding the initial shapes of all-ceramic and mounting status of all-ceramic on the metal crown(${\Delta}E^*1$), and a comparison of mounting of all ceramic on the metal crown with all-ceramic cemented on the metal core(${\Delta}E^*2$), at the time of shade change of initial shapes and after we cemented on the metal core. (1) no significant difference among all-ceramics was found. (2) no particular difference was found regarding the $In-Ceram^{(R)}$. (3) a significant difference between the ${\Delta}E^*1$ and ${\Delta}E^*2$ regarding the $IPS-Empress^{(R)}$ was found(P<0.05). (4) a significant difference between the ${\Delta}E^*1$ and ${\Delta}E^*2$ regarding the $OPC^{(R)}$ was found(P<0.05). 2. When we compared the shade changes(${\Delta}E^*$) resulted from before and after the cementation on each of the parts involved of some all-ceramic, we could be able to find shade change increase form incisal third, middle third. and cervical third in that order in $In-Ceram^{(R)}$(spinell), IPS $Empress^{(R)}$, and $OPC^{(R)}$ all. In addition. we could be able to find a significant difference between cervical third and incisal third, middle third. (P<0.05) From what we have just seen, we might conclude that there is a significant shade change difference before and after the cementation with respect to $IPS-Empress^{(R)}$ and $OPC^{(R)}$. In addition, we could also be able to find more shade change difference at the cervical third rather than incisal third and middle third depending on the parts involved.
본 연구는 심미보철 치료에서 사용되는 금속도재관 제작시 Ni-Cr alloy 하부 구조물에 상부도재를 축성하고 소성하는 과정이 완성된 보철물의 적합도에 미치는 영향을 조사함으로써 임상적 허용을 재확인하기 위함이다. 1차로 lost wax technique으로 제작된 NCC (Ni-Cr alloy core)의 변연 및 내면 적합도를 측정하였고, 2차로 NCC에 상부도재 축성, 소성하여 금속도재관을 최종 완성하여 2차로 측정한 뒤비교한 결과는 다음과 같다. 금속도재관 제작 시 Ni-Cr alloy로 제작된 코어 위에 상부도재를 축성하고 소성하는 과정이 금속 도재관의 적합도를 악화시키는 결과를 보였으며, 부위 별 구분 없이 두 그룹에서 측정된 모든 값의 평균을 비교한 결과 NCC 그룹에서는 $67.1{\pm}23.3{\mu}m$, NMC 그룹에서는 $74.4{\pm}21.9{\mu}m$로 나타났으며 통계적으로 유의한 차이를 보였다(p<0.05). 이와 같은 결과를 토대로 Ni-Cr alloy로 금속도재관 제작 시 상부도재를 축성하는 과정에서 적합도를 악화시킨다는 결론을 얻었으나, 본 실험에서 측정된 결과 값은 임상적 허용 수치($120{\mu}m$)를 넘지 않아 적합도의 기준으로 평가하였을 때 임상적으로 허용 가능할 것으로 생각된다.
The purpose of this study was to evaluate the effect of surface treatment of fractured metal-ceramic crown on bond strength of porcelain repair resin. The specimens were divided into two groups for metal specimens add five groups for porcelain specimens by surface treatment methods. the metal specimens were treated by 2 methods. : micro-sandblasting with $50{\mu}m$ aluminum oxide and grinding with diamond bur. The porcelain specimens were treated by 5 methods : micro-sandblasting with $50{\mu}m$ aluminum oxide, grinding with diamond bur, etching with porcelain etching agent, combination of micro-sandblasting and etching procedure, and combination of grinding and etching procedure. After surface treatment, each specimen was bonded with composite resin and the bond strength was measured and the surface texture was observed by scanning electromicroscope(SEM). The results were as follows : 1. There was significant difference in shear bond strength between metal specimen and prorcelain specimen. 2. Bood strength of metal specimens treated with diamond bur was higher than that treated with $50{\mu}m$ aluminum oxide sandblasting. 3. Bond strength of porcelain specimen treated with diamond bur was higher than that treated with $50{\mu}m$ aluminum oxide sandblasting and porcelain etching agent. 4. There was no significant difference in shear bond strength between the group treated with diamond bur and combined treatment groups respectively. 5. The large undercuts were observed in group treated with diamond bur by SEM.
Cha Young-Joo;Yang Jae-Ho;Lee Sun-Hyung;Han Jung-Suk
대한치과보철학회지
/
제39권6호
/
pp.599-610
/
2001
Due to an increasing interest in esthetics and concerns about toxic and allergic reactions to certain alloys, patients and dentists have been looking for metal-free tooth-colored restorations. Recent improvement in technology of new all-ceramic materials and composite materials has broadened the options for esthetic single crown restorations. The aim of this investigation was to study the fracture strength of the metal-free posterior single crowns fabricated using two recently introduced systems, Empress 2 ceramic and Targis-Vectris. Forty premolar-shaped stainless steel dies with the 1mm-wide circumferential shoulder were prepared. Ten cylindrical crowns having a diameter of 8.0mm and total height of 7.5mm were fabricated for each crown system respectively(PFM, Empress staining technique, Empress 2 layering technique, and Targis- Vectris). The crowns were filled with cement and placed on the stainless steel dies with firm finger pressure. The crowns were then stored in distilled water at room temperature for 24 hours before testing. The crowns were tested for fracture strength in an Instron universal testing machine (Instron 6022). With a crosshead speed of 1mm/min the center of the occlusal surface of the crown was loaded using a 4-mm-diameter stainless steel ball until fracture occurred. The fracture surfaces of the crowns were gold coated and examined using scanning electron microscopy(Jeol JSM-840 Joel Ltd., Akishima, Tokyo, Japan). Within the parameters of this study the following conclusions were drawn: 1. The mean fracture strength for PFM crowns was 5829(${\pm}906$)N; for Empress staining technique the fracture strength was 1697(${\pm}604$)N; for Empress 2 Layering technique the fracture strength was 1781N(${\pm}400$)N, and the fracture strength for Targis- Vectris was 3093(${\pm}475$)N. 2. The fracture strength of the PFM crowns was significantly higher than that of the Empress 2 and the Targis-Vectris crowns (P<0.05). 3. The fracture strength of the Targis-Vectris crowns was significantly higher than that of the Empress 2 crowns (P<0.05). 4. No statistical difference was found when Empress staining technique was compared with Empress 2 layering technique. 5. The SEM image of fracture surface of Empress 2 crown showed a very dense microstructure of the lithium disilicate crystals and the SEM image of fracture surface of Targis-Vectris crown showed indentations of Vectris and some fibers tom off from Vectris.
The microstructure and hardness of a porcelain fused Au-Pt-Cu-In alloy was investigated using optical microscopy, secondary electron microscopy, electron probe microanalyzer, transmission electron microscope, and vickers hardness. The hardness of the heat-treated Au-Pt-Cu-In quartenary alloy reached a maximum value in 30 min at 550$^{\circ}C$ in the range of 150 to 950$^{\circ}C$. In the aged Au-Pt-Cu-0.5In alloy at 550$^{\circ}C$, the hardness of the alloy rapidly increased until 30min with increasing aging time and after that it was remained nearly constant value. Based on above results, glazing and final aging of the porcelain fused Au-Pt-Cu-0.5In alloy were performed at 920 and 550$^{\circ}C$, respectively. The hardness of Au-Pt-Cu-0.5In alloy glazed at 920$^{\circ}C$ was 90 Hv and that of the alloy aged for 30 min at 550$^{\circ}C$ increased to 160 Hv. This indicates that a ceramic-metal crown with high strength can be manufactured using the glazing at 920$^{\circ}C$ and followed final aging at 550$^{\circ}C$ for 30 min.
Purpose: This study was to observe characteristic of metal oxidation and bonding strength according to composition of Ni-Cr alloy for porcelain fused to metal crown. The three kinds of Ni-Cr alloy with different composition ratio of parent metal were observed general properties and chemical properties of each alloy surface and measured the shear bonding strength between ceramic and each alloys. The aim of study was to suggest the material for design of parent metal's composition ratio to development of alloy for porcelain fused to metal crown. Methods: The three kinds of alloy as test specimen was Ni(59wt%)-Cr(24wt%), Ni(67wt.%)-Cr(16wt.%) alloy and Ni(71wt%)-Cr(12wt%)alloy. The oxide on surface was observed by EDX. And the shear test was performed by MTS. Results: The surface property and oxide characteristic analysis of oxide layer, weight percentage of Element O within $Ni_{59}Cr_{24}$ alloy measured 23.03wt%, $Ni_{67}Cr_{16}$ alloy measured 21.13wt% and $Ni_{71}Cr_{12}$ alloy was measured 48.55wt%. And the maximum shear bonding strength was measured 58.02Mpa between $Ni_{59}Cr_{24}$ alloy and vintage halo(H2 group). Conclusion: The surface property and oxide characteristic three kind of Ni-Cr alloy was similar. and shear bonding strength showed the highest bonding strength in H2 specimens.
he purpose of this study was to compare the fracture resistance of the IPS Empress ceramic crown with 1.0mm width rounded shoulder, which is usually recommended in all ceramic crown, and 0.5mm width chamfer finish lines on the maxillary first premolar. 30 sound maxillary first premolars were selected and then storaged in 5% NaOCl and saline. 15 teeth were performed preparation for each group(1.0mm rounded shoulder, 0.5mm chamfer). After 30 stone dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement(Bistite resin cement, Tokuyama Soda Co. LTD., Japan) on the natural teeth. The cemented crowns were mounted on the positioning jig and the universal testing machine(Zwick Z020, Zwick Co., Germany)was used to measure the fracture strength, with stress loading on the occlusal surface between buccal and lingual cusp. And also, three-dimensional finite element model was used to measure the stress distribution with two types of the finish lines(1.0mm rounded shoulder, 0.5mm chamfer) and two loading conditions(both buccal and lingual cusp inclination, lingual cusp inclination only). The result of the this study were as follows. In the fracture resistance experiment according to the finish line, the mean fracture strength of rounded shoulder(842N) showed higher value than that of the chamfer(590N) (p<0.05). In the three dimensional finite element analysis of all ceramic crown, metal die and natural teeth model did not show any differences in stress distribution between finish lines. Generally, when force was loaded on the occlusal inclination of buccal and lingual cusp, the stress was concentrated on the loading point and the central groove of occlusal surface. When force was loaded only on the occlusal inclination of lingual cusp, the stress was concentrated on the lingual finish line and loading point.
최근, 치과 산업에서 레이저를 열원으로 합금을 제조하는 선택적 레이저 용융법(Selective laser melting, SLM)이 소개되고 있다. 하지만 SLM으로 제작된 금속-세라믹 수복물에 대한 연구가 부족한 실정이다. 따라서 본 연구의 목적은 SLM 그리고 CAST(casting)에 의해 제조된 Co-Cr 합금의 금속-세라믹(metal-ceramic) 결합 강도(bond strength)를 평가하는 것이다. SLM 그리고 CAST 방법을 사용하여 Co-Cr 시편을 제조하고 세라믹을 소결하여 시료를 제작하였다. 연구의 실험은 표본 준비 및 분석을 통해 2020년 1월부터 6월까지 수행되었다. 금속-세라믹 결합 강도는 만능 시험기에 의해 측정되었다. 부착 세라믹의 면적분(The area fraction of adherence ceramic, AFAC)은 SEM/EDS로 시편의 Si 함량을 측정하였다. 금속-세라믹 결합 강도 및 AFAC 결과는 t-test를 사용하여 분석하였다(α = .05). SLM 그리고 CAST Co-Cr 합금 사이의 결합 강도에 대해서는 유의한 차이가 발견되지 않았다(P>.05). SLM은 CAST 그룹보다 많은 세라믹 부착성(ceramic adherence)을 나타냈다(P<.001). 세라믹과 합금의 결합 강도는 제조 방법엥 영향을 받지 않았다. 그러나 SLM은 더 우수한 세라믹 부착성을 보였다. 이는 향후 임플란트 상부 보철물 제작에도 SLM으로 제작한 합금이 사용 가능한 것을 시사한다. CAST 방식의 단점을 극복하고 시간과 비용을 절약할 수 있을 것으로 기대된다.
The purpose of this study was compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower second premolar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement. The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1284 N). Crowns of 1.5mm depth and $8^{\circ}$ inclination had the lowest strength (951 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.