  • The interest of the fatigue life of rubber components such as engine mounts is increasing according to the extension of warranty period of the automotive components. Automotive engine mounts get damaged due to thermal and mechanical loadings. This paper discusses a fatigue life prediction of the 3-dimensional dumbbell specimens for natural rubber compound considering the effects of maximum strain and heat aging temperature. Displacement controlled fatigue life tests were performed using specimens with different levels of maximum strain and various hardness. The basic mechanical properties test and the fatigue test of aged rubber specimen under normal and elevated temperature were executed. A procedure to predicted the fatigue life of vulcanized natural rubber material based on the maximum strain method was proposed, and then this curve was in good agreement with fatigue test data less than 200% error range.

Ni-Cr-Mo과 SM45C의 마찰용접특성(摩擦熔接特性)에 관한 연구(硏究) (A Study on the Properties in Friction Weldability of Ni-Cr-Mo and SM45C)

  • 임형택;민택기
    • 한국공작기계학회논문집
    • /
    • 제16권6호
    • /
    • pp.29-36
    • /
    • 2007
  • The present study examined the mechanical properties of the friction welding of Ni-Cr-Mo to SM45C. Friction welding was conducted at welding conditions of 2,000 rpm, friction pressure of 100MPa, friction time of 0.8, 1.0, 1.2, 1.4, 1.6, 1.8, 2.0 seconds, upset pressure of 150MPa, and upset time of 3.0 seconds. When the friction time was 1.6 seconds, the maximum tensile strength of the friction weld happened to be 1,020MPa, which is 120% of the base material's tensile strength(850MPa). At the same condition, the maximum shear strength was 438MPa, which is equivalent to 103% of the base material's shear strength(425MPa). At the same condition, the maximum vickers hardness was Hv490 at Ni-Cr-Mo nearby weld interface, which is higher Hv40 than condition of the friction time 0.8 seconds, and the maximum vickers hardness was Hv305 from weld interface of SM45C, which is higher Hv12 than condition of the friction time 0.8 seconds. The results of microstructure analysis show that the structures of two base materials have fined and rearranged along a column due to heating and axial force during friction, which has affected in raising hardness and tensile strength.

계장화 압입시험법을 이용한 차량용 컴프레서 저널 경도 평가 (Hardness Estimation of Compressor Journal for a Use of Instrumented Indentation Techniques)

  • 곽성종;진지원;김태성;노기한;강기원
    • 한국생산제조학회지
    • /
    • 제21권3호
    • /
    • pp.376-381
    • /
    • 2012
  • This paper deals with application of instrumented indentation technique for quality inspection methodology for automobile component. For this, the instrumented indentation tests were performed the normal and cracked compressor journal, which is made from spheroidal graphite cast iron and utilized in air-conditioning system. And the Brinell hardness was estimated using the unloading slope and maximum indentation force. With the aid of Normal distribution, this Brinell hardness was statistically compared and analyzed with hardness measured by indentation hardness tests. Also, application possibility of reliability-based quality inspection criteria for compressor journal was evaluated through the probabilistic analysis for the Brinell hardness estimated by instrumented indentation technique.

변형시효처리한 탄소강의 소성역 해석에 관한 연구 (A Study on the Analysis of Plastic Zone in Carbon Steel after Strain Aginig)

  • 손세원;이진수;장정원
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 추계학술대회 논문집
    • /
    • pp.933-937
    • /
    • 1996
  • In this paper, the behavior of plastic zone in the notch tip was studied under Loye's Micro Vickers Hardness Measurement Method. The direction forming maximum plastic zone was estimated by finite element analysis. In the experiments, cold rolling sheet SGCD3, SK5 and hot rolling sheet SS41, S4SC was used to study the influence of carbon contents on plastic zone. The standard hardness test specimen and the notch hardness test specimen was made and loaded cyclically. The specimen was aged to stabilize the hardness. After aging treatment, the notch specimen was made and simple tension load of 50% yield strength was applied. The hardness test at the notch tip until the hardness data of standard hardness specimen was checked was performed.

  • PDF

식품의 물성이 제작근의 활성도 및 저작 양태에 미치는 영향 (A STUDY ON THE EFFECTS OF TEXTURE OF FOOD ON CHEWING MOVEMENTS AND EMG OF MASTICATORY MUSCLE)

  • 조리라;김광남;장익태;허성주
    • 대한치과보철학회지
    • /
    • 제36권3호
    • /
    • pp.427-452
    • /
    • 1998
  • To elucidate the effects of food texture such as hardness, cohesiveness, adhesiveness on mastication procedure, the electromyographic activity (EMG) of the masticatory muscles and the chewing movements were analyzed in eighteen young subjects during ordinary chewing. Seven different foods were selected by sensory texture profiling and mechanical test with texturometer; egg white, sausage, pizza cheese, yang-geng, biscuit, peanut and almond. The indexes of jaw movements used were the chewing number, chewing time, maximum opening, average opening, closing velocity and opening velocity. The EMG indexes analyzed were maximum and average integrated amplitude of the anterior temporal and masseter muscles. The results obtained were as follows. 1. The chewing time and chewing number, mandibular displacement and mandibular movement velocity were not changed by the hardness, cohesiveness and adhesiveness of the food (p>0.05). 2. The harder food materials showed a higher amplitude of the anterior temporal muscle integrated EMGs than the softer ones (p<0.05). 3. The maximum and average integrated EMGs of the masseter muscle increased with the increase of hardness of the food (p<0.05). 4. The integrated EMGs of preferred side and non-preferred side masticatory muscles increased with the increase of hardness of the food (p<0.05). 5. The adhesiveness and cohesiveness of the food were not the determining factor to the integrated EMGs of masticatory muscles (p<0.05).

  • PDF

Effects of feed intake and water hardness on fluralaner pharmacokinetics in layer chickens

  • Sari, Ataman Bilge;Gunes, Yigit;Anlas, Ceren;Alkan, Fulya Ustun;Guncum, Enes;Ustuner, Oya;Bakirel, Tulay
    • Journal of Veterinary Science
    • /
    • 제23권5호
    • /
    • pp.64.1-64.9
    • /
    • 2022
  • Background: Fluralaner is a novel drug belonging to the isoxazoline class that acts on external parasites of domestic animals. It is used systemically via drinking water, especially against red poultry mite in layer chickens. Fluralaner is frequently used in layers infected with D. gallinae. However, no study to date has investigated the effects of feed intake and water hardness. Objectives: This study aimed to investigate the effects of variable water hardness and feed intake on the pharmacokinetic profile of fluralaner. Methods: Layer chickens were divided into four groups (n = 8): fed + purified water (Group 1), feed restricted + purified water (Group 2), feed restricted + hard water (Group 3), and feed restricted + soft water (Group 4). After administering a single dose of the drug with drinking water, the blood samples were collected for 21 days. Fluralaner concentrations in plasma samples were determined by liquid chromatography/tandem mass spectrometry. The maximum plasma concentration (Cmax), time to reach maximum plasma concentration (tmax), area under the concentration-time curve values (AUC0-21d), half-life (t1/2), and other pharmacokinetic parameters were calculated. Results: Although the highest maximum plasma concentration (Cmax) was determined in Group 1 (fed + purified water), no statistically significant difference was found in the Cmax, tmax, t1/2, MRT0-inf_obs, Vz/Fobs, and Cl/F_obs parameters between the experimental groups. Conclusions: It was concluded that the feed intake or water hardness did not change the pharmacokinetic profile of fluralaner in layer chickens. Therefore, fluralaner could be used before or after feeding with the varying water hardness in poultry industry.

Mechanical and metallurgical properties of diffusion bonded AA2024 Al and AZ31B Mg

  • Mahendran, G.;Balasubramanian, V.;Senthilvelan, T.
    • Advances in materials Research
    • /
    • 제1권2호
    • /
    • pp.147-160
    • /
    • 2012
  • In the present study, diffusion bonding was carried out between AZ31B magnesium and AA2024 aluminium in the temperature range of $405^{\circ}C$ to $475^{\circ}C$ for 15 min to 85 min and 5MPa to 20 MPa uniaxial loads was applied. Interface quality of the joints was assessed by microhardness and shear testing. Also, the bonding interfaces were analyzed by means of optical microscopy, scanning electron microscopy, energy dispersive spectrometer and XRD. The maximum bonding and shear strength was obtained at $440^{\circ}C$, 12 MPa and 70 min. The maximum hardness values were obtained from the area next to the interface in magnesium side of the joint. The hardness values were found to decrease with increasing distance from the interface in magnesium side while it remained constant in aluminium side. It was seen that the diffusion transition zone near the interface consists of various phases of $MgAl_2O_4$, $Mg_2SiO_4$ and $Al_2SiO_5$.

PZT-PYW 세라믹스의 조성변화가 경도 및 인성에 미치는 영향 (Effect of Composition on the Hardness and Toughness in PZT-PYW Ceramics)

  • 류소연;임대순;윤석진;김현재
    • 한국세라믹학회지
    • /
    • 제31권3호
    • /
    • pp.305-311
    • /
    • 1994
  • In this paper, a change of fracture toughness and hardness in PZT-PYW ceramics system before and after poling treatment was measured to investigate the effect of composition on the mechanical properties in PZT-PYW ceramics. The hardness of the PZT-PYW ceramics increased with increasing mole fraction of PYW. The fracture toughness achieved maximum values for x=0.03. Both of the hardness and the fracture toughness also increased with poling treatment. The variation of both hardness and fracture toughness with increasing PYW mole fracture was explained by the change in microstructures such as grain size and second phase. The difference in hardness and fracture toughness in the electrically poled and unpoled specimens was also explained on the bases of internal stress.

  • PDF

Surface hardness measurement of NiP-plated AA7050

  • Moon, Sungmo;Kim, Juseok
    • 한국표면공학회지
    • /
    • 제54권4호
    • /
    • pp.171-177
    • /
    • 2021
  • This paper is concerned with the surface hardness measurement of NiP-coated AA7050 using different loads from 10 to 100 g. The surface hardness was observed to increase from 180 to 600 Hv with increasing NiP layer thickness, depending on the load applied for indentation. When NiP coating thickness is thinner than 2 ㎛, the surface hardness of NiP-coated AA7050 was mainly determined by AA7050 substrate, while it was significantly increased by NiP coating layer when NiP coating thickness is thicker than 2 ㎛. Hardness of AA7050 substrate itself was not dependent on the applied load but the hardness of NiP-coated AA7050 was largely influenced by the load applied for indentation. The largest difference of hardness between 10 g and 100g of applied loads, was obtained at the NiP thickness of about 8 ㎛ above which the measured hardness at 10 g reached a maximum value of about 600 Hv. It was also observed that indentation-induced plastic deformation next to the indented zone occurs when NiP layer is 5.64 times thicker than the depth of impression formed by indentation.

PTA법에 의한 스텔라이트 12합금 육성층의 미세조직 및 경도에 미치는 시효처리의 영향 (The effect of aging on the Microstructure and Hardness of Stellite 12 alloy overlayer by PTA process)

  • 정병호;김무길;이성열
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제26권1호
    • /
    • pp.68-75
    • /
    • 2002
  • Stellite 12 alloy-powders were overlaid on 410 stainless steel valve seat by plasma transferred arc(PTA)process. Variation of microstructure and hardness of overlaid deposit with aging time at $750^{\circ}C$ was investigated. The deposit showed hypoeutectic microstructure, which was consisting of primary cobalt dendrite and networked $M_{7}C_{3}$type eutectic carbides. After aging new M_{23}C_{6}$ carbide was formed by the partial decomposition of $M_7C_3$ type eutectic carbides and finely dispersed $M_{23}C_6$ type carbides were also precipitated in the matrix. Hardness of the deposit was increased with increase of aging time at $750^{\circ}C$ and showed maximum value at 35hours. After showing maximum value, it was fallen down again at 70hours because of overaging. The increase of hardness in aging is ascribed to the formation of new stable $M_{23}C_6$ type carbide by the partial decomposition of $M_7C_3$ type eutectic carbides and also precipitation of finely dispersed $M_{23}C_6$ carbides in matrix.