• 제목/요약/키워드: Material Erosion

검색결과 327건 처리시간 0.03초

탄화규소의 R-curve, 침식 및 마모 특성 (R-curve, erosion and wear of silicon carbide ceramics)

  • 채준혁;조성재;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제27회 춘계학술대회
    • /
    • pp.139-145
    • /
    • 1998
  • This paper addresses the R-curve properties, wear resistance, and erosion resistance of the two silicon carbide ceramics with different microstructures, i.e. , fine grained SiC and in situ-toughened SiC(IST SIC). Fine grained SiC exhibits a relatively flat R-curve behavior whereas the IST SiC exhibits a increasing R-curve behavior. The increasing R-curve behavior in IST SiC is attributed to relatively weak grain boundaries. The rate of material removal during wear tests and erosion tests was higher for IST SiC than that for fine grained SiC. This is attributed to the weaker grain boundaries in IST SiC than that in fine grained SiC. It is implied that fracture toughness in short crack regime should be taken into consideration in the interpretation of the microscopical material removal process. We show that the higher the strength of grain boundaries is, the higher wear and erosion resistances are.

  • PDF

선박 프로펠러의 케비테이션 침식 저항 향상을 위한 Ni-P 무전해 도금층 형성 및 열처리를 통한 미세조직 제어 (Electroless Ni-P Plating and Heat Treatments of the Coating Layer for Enhancement of the Cavitation Erosion Resistance of Vessel Propellers)

  • 김영재;손인준;이승훈
    • 한국재료학회지
    • /
    • 제27권8호
    • /
    • pp.409-415
    • /
    • 2017
  • For enhanced cavitation erosion resistance of vessel propellers, an electroless Ni-P plating method was introduced to form a coating layer with high hardness on the surface of Cu alloy (CAC703C) used as vessel propeller material. An electroless Ni-P plating reaction generated by Fe atoms in the Cu alloy occurred, forming a uniform amorphous layer with P content of ~10 wt%. The amorphous layer transformed to (Ni3P+Ni) two phase structure after heat treatment. Cavitation erosion tests following the ASTM G-32 standard were carried out to relate the microstructural changes by heat treatment and the cavitation erosion resistance in distilled water and 3.5 wt% NaCl solutions. It was possible to obtain excellent cavitation erosion resistance through careful microstructural control of the coating layer, demonstrating that this electroless Ni-P plating process is a viable coating process for the enhancement of the cavitation erosion resistance of vessel propellers.

해상용 원심펌프 임펠러의 침식억제법으로 음극방식 및 재료개발에 관한 기초연구 1 (Fundamental Study on Cathodic Protection and Material Development as Erosion-Control Methods of Oceanic Centrifugal Pump(1))

  • 이진열;임우조
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제19권2호
    • /
    • pp.56-66
    • /
    • 1995
  • Recently, with theraped advancement in th oceanology such an ocean-going vessel and oceanic structures, there is a need to study the cavitation erosion-corrosion control of pump impeller, the partial element of ocean machinery, for more effective operation. Especially, the cathodic protection (impressed current method & Al-sacrificial anode method) was applied to sea water, and Cu-alloy material mixed Zn & Al was used as a control method of cavitation erosion-corrosion. In this study, used the piezoelectric vibrator with 20KHz, 24.mu.m to cavity generation apparatus, and investigated the weight loss, weight loss rate, electrode potential & current density etc. under this condition. According to test result, thos describes how to indentify an influence of the cathodic protection and Al & Zn addition in material development for the control of cavitation erosion-corrosion, and those will serve as fundamental data on the cavitation erosion-corrosion control of oceanic centrifugal pump.

  • PDF

AgWC/AgCdO 접점의 소모특성에 미치는 개리속도의 영향 (The Effect of Opening Velocity on the Arc Erosion of AgWC/AgCdO Contacts)

  • 연영명;박흥태;이상엽;조상순;오일성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.517-520
    • /
    • 2003
  • The purpose of this paper is to investigate the effect of arc current and contact velocity on the erosion of silver contact to be used in low voltage circuit breakers. The arc current range from $2kA_{rms}$ to $20kA_{rms}$. A test system allows the control of the opening velocity profiles with contact velocities up to 10m/s and also enables the synchronization of the contact opening with a point on the arc current waveform. Contact erosion is evaluated by measuring the mass change of the cathode and anode. The results show that increase the opening velocity from 2m/s to 6m/s leads to an decrease in the contact erosion. The material transfer from one electrode to another is shown to depend on the transfer charge and the opening velocity of the contacts.

  • PDF

VORTEX SHEAR VELOCITY AND ITS EROSION IN THE SCOUR HOLE

  • Lee, Hong-Sik;Kim, Jin-Hong;Lee, Sam-Hee
    • Water Engineering Research
    • /
    • 제1권4호
    • /
    • pp.259-266
    • /
    • 2000
  • Scour hole is formed due to the high shear stress of the jet flow at the outlet of a hydraulic structure and vortex erosion occurs in the scour hole. It is important to determine the amount of vortex erosion occurs in the scour hole. It is important to determine the amount of vortex erosion for the design of bed protection. If the vortex erosion continues and reaches to the hydraulic structure, it causes the deformation of the structure itself. To obtain the amount of the vortex erosion, it is necessary to determine the shear velocity of the line vortex in the scour hole was derived by the theory of energy conservation and found to be related to the upstream overflow velocity. The amount of vortex erosion from the scour hole was obtained using entrainment equation for given value of shear velocity. For a design purpose, if the flow velocity at the end of an apron and the properties of bed material are given, the amount of vortex erosion was obtained.

  • PDF

원통다관형 열교환기의 침식-부식 특성에 관한 연구 (I) (Study on the Characteristics of Erosion-Corrosion for Heat Exchanger of Shell and Tube Type(I))

  • 임우조;정해규
    • 수산해양기술연구
    • /
    • 제35권2호
    • /
    • pp.196-200
    • /
    • 1999
  • In the case that erosion and corrosion occurs in machinery and structure at the same time, the synergy effect by erosion-corrosion affects fatal effect to durability of machinery and structure. Therefore, in machinery and structure which use corrosion liquid, the study of the synergy effect of erosion-corrosion which affects metal material is requested. In this paper. the flow corrosion experiment about the effect of temperature change and liquid velocity change in sea water was carried out to study the characteristics of erosion-corrosion for tube material Cu heat exchanger The main results obtained are as follows. (1) Damage appearance of tube outside by erosion-corrosion becomes dull because electrode potentials of Cu tube is higher than electrode potential of STPG38 shell. (2) In the cooling system by sea water, the weight loss rate of Cu at tube outside liquid temperature of $70^{\circ}C$ is higher than that of temperature of $20^{\circ}C$. (3) In cooling system by sea water, the weight loss rate of Cu at liquid velocity of 5.1m/s is higher than that of velocity of 1.47m/s. But as the testing time passed, the weight loss rate of Cu at velocity of 5.1m/s is almost steady and becomes dull at velocity of 1.47m/s.

  • PDF

탄화규소의 T-curve, 마모 및 침식 (T-curve, wear and Erosion of Silicon Carbide)

  • 채준혁;조성재;윤경진;김석삼
    • Tribology and Lubricants
    • /
    • 제14권4호
    • /
    • pp.114-120
    • /
    • 1998
  • The T-curve, wear and erosion behaviors of two different silicon carbides, i.e., the fine grained SiC and the in situ-toughened SiC(IST-SiC). Both materials exhibited an increasing T-curve behavior, although the T-curve of IST-SiC was steeper than that of fine grained SiC. The fracture toughness of IST-SiC was larger than that of fine grained SiC at long crack regime, whereas an opposite tendency occurred at short crack regime. The rate of material removal during wear and erosion tests was higher in IST-SiC compared to fine grained SiC. The difference between the material removal rates of two materials was discussed in the light of their R-curve behaviors.

Tribological Behavior of Silicon Carbide Ceramics - A Review

  • Sharma, Sandan Kumar;Kumar, B. Venkata Manoj;Kim, Young-Wook
    • 한국세라믹학회지
    • /
    • 제53권6호
    • /
    • pp.581-596
    • /
    • 2016
  • A comprehensive review on sliding and solid particle erosion wear characteristics of silicon carbide (SiC) ceramics and SiC composites is provided. Sliding or erosion wear behavior of ceramics is dependent on various material characteristics as well as test parameters. Effects of microstructural and mechanical properties of SiC ceramics are particularly focused to understand tribological performance of SiC ceramics. Results obtained between varieties of pairs of SiC ceramics indicate complexity in understanding dominant mechanisms of material removal. Wear mechanisms during sliding are mainly divided in two groups as mechanical and tribochemical. In solid particle erosion conditions, wear mechanisms of SiC ceramics are explained by elastic-plastic deformation controlled micro-fracture on the surface followed by radial-lateral crack propagation beneath the plastic zone.