Tribological Behavior of Silicon Carbide Ceramics - A Review  

Sharma, Sandan Kumar (Department of Metallurgical and Materials Engineering, Indian Institute of Technology (IIT) Roorkee)
Kumar, B. Venkata Manoj (Department of Metallurgical and Materials Engineering, Indian Institute of Technology (IIT) Roorkee)
Kim, Young-Wook (Functional Ceramics Laboratory, Department of Materials Science and Engineering, the University of Seoul)
Publication Information
Abstract
A comprehensive review on sliding and solid particle erosion wear characteristics of silicon carbide (SiC) ceramics and SiC composites is provided. Sliding or erosion wear behavior of ceramics is dependent on various material characteristics as well as test parameters. Effects of microstructural and mechanical properties of SiC ceramics are particularly focused to understand tribological performance of SiC ceramics. Results obtained between varieties of pairs of SiC ceramics indicate complexity in understanding dominant mechanisms of material removal. Wear mechanisms during sliding are mainly divided in two groups as mechanical and tribochemical. In solid particle erosion conditions, wear mechanisms of SiC ceramics are explained by elastic-plastic deformation controlled micro-fracture on the surface followed by radial-lateral crack propagation beneath the plastic zone.
Keywords
Silicon carbide; Sliding wear; Erosion wear; Microstructure; Wear mechanisms;
Citations & Related Records
연도 인용수 순위
  • Reference
1 S. Gochnour, J. D. Bright, D. K. Shett, "Solid Particle Erosion of SiC-$Al_2OC$ Ceramics," J. Mater. Sci., 25 3229-35 (1990).   DOI
2 S. Wada and N. Watanabe, "Solid Particle Erosion of Brittle Materials. III. The Interaction with Material Properties of Target and That of Impingement Particle on Erosive Wear Mechanism," J. Ceram. Soc. Jpn., 95 [6] 573-78 (1987).
3 J. J. Kim and S. K. Park, "Solid-Particle Erosion of Hot-Pressed Silicon Carbide and SiC-$TiB_2$ Composite," J. Mater. Sci. Lett., 16 821-23 (1997).   DOI
4 B. Q. Wang and A. V. Levy, "Erosion Behavior of SiC Fiber-SiC Matrix Composites," Wear, 138 125-36 (1990).   DOI
5 I. Finnie, J. Wolak, and Y. H. Kabil, "Erosion of Metals by Solid Particles," J. Mater., 2 [3] 682-700 (1967).
6 G. Amirthana, A. Udaya Kumar, V.V. Bhanu Prasad, and M. Balasubramanian, "Solid Particle Erosion Studies on Biomorphic Si/SiC Ceramic Composites," Wear, 268 145-52 (2010).   DOI
7 A. R. de A. Lopez, J. M. Fernandez, F. M. V. Feria, T. S . Orlova, K. C. Goretta, F. G. Mora, Nan Chen, and J. L. Routbort, "Erosion and Strength Degradation of Biomorphic SiC," J. Eur. Ceram. Soc., 24 861-70 (2004).   DOI
8 B. J. Hockey, S. M. Wiederhorn, and H. Johnson, "Erosion of Brittle Materials by Solid Particle Impact," pp. 379-402 in Fracture Mechanics of Ceramics Vol. 3, Ed. by R. C. Bradt, D. P. H. Hasselman, and F. F. Lange, Plenum Press, New York, 1978.
9 B. J. Hockey and B. R. Lawn, "Electron Microscopy of Microcracking about Indentations in Aluminium Oxide and Silicon Carbide," J. Mater. Sci., 10 [8] 1275-84 (1975).   DOI
10 S. M. Wiederhorn and B. J. Hockey, "Effect of Material Parameters on the Erosion Resistance of Brittle Materials," J. Mater. Sci., 18 [3] 766-80 (1983).   DOI
11 B. R. Lawn, B. J. Hockey, and S. M. Wiederhorn, "Atomically Sharp Cracks in Brittle Solids: An Electron Microscopy Study," J. Mater. Sci., 15 1207-23 (1980).   DOI
12 D. C. Evans and J. K. Lancaster, "The Wear of Polymers," pp. 85-139 in Treatise on Materials Science and Technology: Wear, Vol. 13, Academic Press, New York and London, 1979.
13 Z. H. Huang, J. L. Sun, J. X. Wang, and Y. R. Hong, "${\alpha}-Sialon-Al_2O_3-SiC$ Composite Refractories," Key Eng. Mater., 224 275-80 (2012).
14 D. B. Marshall, B. R. Lawn, and A. G. Evans, "Elastic/Plastic Indentation Damage in Ceramics: The Lateral Crack System," J. Am. Ceram. Soc., 65 [11] 561-66 (1982).   DOI
15 A. G. Evans, M. E. Gulden, and M. Rosenblatt. "Impact Damage in Brittle Materials in the Elastic-Plastic Response Regime," Proc. of the Royal Society of London, 361 343-65 (1978).
16 D. Wang and Z. Mao, "Microscopic Observations of Wear of Heat-Resistant Ceramics," Wear, 167 [1] 87-9 (1993).   DOI
17 M. M. Chaudhri and S. M. Walley, "Damage to Glass Surfaces by the Impact of Small Glass and Steel Spheres," Phil. Mag. A, 37 [2] 153-65 (1978).   DOI
18 C. G. Knight, M. V. Swain, and M. M. Chaudhri, "Impact of Small Steel Spheres on Glass Surfaces," J. Mater. Sci., 12 [8] 1573-86 (1977).   DOI
19 B. R. Lawn and D. B. Marshall, "Indentation Fracture and Strength Degradation in Ceramics," pp. 205-29 in Fracture Mechanics of Ceramics, Vol. 3, Ed. by R. C. Bradt, D. P. H. Hasselman, and F. F. Lange, Plenum Press, New York, 1978.
20 M. M. Chaudhri, and P. A. Brophy, "Single Particle Impact Damage of Fused Silica." J. Mater. Sci., 15 [2] 345-52 (1980).   DOI
21 M. S. Suh, T. Hinoki, and A. Kohyama, "Erosive Wear Mechanism of New SiC/SiC Composites by Solid Particles," Tribol. Lett., 41 503-13 (2011).   DOI
22 Z. Zhu, V. Muratov, and T. E. Fischer, "Tribochemical Polishing of Silicon Carbide in Oxidant Solution," Wear, 225-229 848-56 (1999).   DOI
23 L. C. Erickson, A. Blomberg, S. Hogmark, and J. Bratthall, "Tribological Characterization of Alumina and Silicon Carbide under Lubricated Sliding," Tribology Int., 26 [2] 83-92 (1993).   DOI
24 H. Tomizawa and T. E. Fischer, "Friction and Wear of Silicon Nitride and Silicon Carbide in Water: Hydrodynamic Lubrication at Low Sliding Speed Obtained by Tribochemical Wear," ASLE Trans., 30 [1] 41-6 (1987).   DOI
25 J. K. Lancaster, "A Review of the Influence of Environmental Humidity and Water on Friction, Lubrication and Wear," Tribology Int., 23 [6] 371-89 (1990).   DOI
26 S. Sasaki, "The Effects of Water on Friction and Wear of Ceramics," J. Jpn. Soc. Lubr. Eng., 10 10-26 (1988).
27 R. Wasche and D. Klaffke, "Ceramic Particulate Composites in the System SiC-TiC-$TiB_2$ Sliding against SiC and $Al_2O_3$ Under Water," Tribology Int., 32 197-206 (1999).   DOI
28 E. Medvedovski, "Ballistic Performance of Armour Ceramics: Part 1. Influence of Design and Structure," Ceram. Int., 36 2103-15 (2010).   DOI
29 A. G. Evans and T. R. Wilshaw, "Dynamic Solid Particle Damage in Brittle Materials, An Appraisal," J. Mater. Sci. 12 97-116 (1977).   DOI
30 J. G. Chacon-Nava, F. H. Stott, S. D. de la Torre, and A. Martinez-Villafane, "Erosion of $Al_2O_3$ and SiC at Low Impact Velocities," Mater. Lett., 55 269-73 (2002).   DOI
31 J. L. Routbort and R. O. Scattergood, "Anomalous Solid-Particle Erosion Rate of Hot Pressed Silicon Carbide," J. Am. Ceram. Soc., 63 593-95 (1980).   DOI
32 S. M. Wiederhorn and B. J. Hockey, "Effect of Material Parameters on the Erosion Resistance of Brittle Materials," J. Mater. Sci., 18 766-80 (1983).   DOI
33 J. L. Routbort and H. Matzke, "On the Correlation Between Erosion and Fracture Parameters in SiC Ceramics," J. Mater. Sci., 18 1491-96 (1983).   DOI
34 D. Jianxin, L. Lili, and D. Mingwei, "Erosion Wear Behaviours of SiC/(W,Ti)C Laminated Ceramic Nozzles in Dry Sand Blasting Processes," Mater. Sci. Eng. A, 444 120-29 (2007).   DOI
35 A. F. Colclough and J. A. Yeomans, "Hard Particle Erosion of Silicon Carbide and Silicon Carbide-Titanium Diboride from Room Temperature to 1000$^{\circ}C$," Wear, 209 229-36 (1997).   DOI
36 I. M. Hutchings, "Tribology: Friction and Wear of Engineering Materials; pp. 352, Edward Arnold, London, 1992.
37 J. F. Bell, and P. S. Rogers, "Laboratory Scale Erosion Testing of a Wear Resistant Glass-Ceramic," Mater. Sci. Tech., 3 807-13 (1987).   DOI
38 P. Gautier and K. Kato, "Wear Mechanisms of Silicon Nitride Partially Stabilized Zirconia and Alumina in Unlubricated Sliding against Steel," Wear, 162-164 305-13 (1993).   DOI
39 D. K. Shetty, I. G. Wright, and A. H. Clauer, "Coal Slurry Erosion of Reaction-Bonded SiC," Wear, 79 275-79 (1982).   DOI
40 J. F. Li, J. Q. Huang, S. H. Tan, Z. M. Cheng, and C. X. Ding, "Tribological Properties of Silicon Carbide under Water-Lubricated Sliding," Wear, 218 167-71 (1998).   DOI
41 A. Kovalcikova, P. Kurek, J. Balko, J. Dusza, P. Sajgalik, and M. Mihalikova, "Effect of the Counterpart Material on Wear Characteristics of Silicon Carbide Ceramics," Int. J. Refract. Met Hard Mater., 44 12-8 (2014).   DOI
42 G. Amirthan and M. Balasubramanian, "Reciprocating Sliding Wear Studies on Si/SiC Ceramic Composites," Wear, 271 1039-49 (2011).   DOI
43 V. M. Candelario, O. B. Lopez, F. Guiberteau, R. Morenob, and A. L. Ortiz, "Sliding- Wear Resistance of Liquid-Phase-Sintered SiC Containing Graphite Nanodispersoids," J. Eur. Ceram. Soc., 34 2597-602 (2014).   DOI
44 J. Takadoum, Z. Zsiga, and C. Roques-Carmes, "Wear Mechanism of Silicon Carbide: New Observations," Wear, 174 239-42 (1994).   DOI
45 L. Micele, G. Palombarini, S. Guicciardi, and L. Silvestroni, "Tribological Behaviour and Wear Resistance of a SiC-$MoSi_2$ Composite Dry Sliding against $Al_2O_3$," Wear, 269 368-75 (2010).   DOI
46 R. Wasche, D. Klaffke, and T. Troczynski, "Tribological Performance of SiC and $TiB_2$ against SiC and $Al_2O_3$ at Low Sliding Speeds," Wear, 256 695-704 (2004).   DOI
47 K. Kato, "Tribology of Ceramics," Wear, 136 117-33 (1990).   DOI
48 S. Hotta and Y. Mizutani, "Effect of Water and Organic Solvents on the Friction of SiC," pp. 1-4 in Proceedings, 32nd JSLE, Japanese Society of Lubrication Engineers Conference, Tokyo, Japan (1988).
49 X. F. Chen, X. G. Xu, X. B. Hu, J. Li, S. Z. Jiang, L. N. Ning, Y. M. Wang, and M. H. Jiang, "Anisotropy of Chemical Mechanical Polishing in Silicon Carbide Substrates," Mater. Sci. Eng. B, 142 28-30 (2007).   DOI
50 D. Sciti and A. Bellosi, "Effects of Additives on Densification, Microstructure and Properties of Liquid-Phase Sintered Silicon Carbide" J. Mater. Sci., 35 3849-55 (2000).   DOI
51 G. Rixecker, I. Wiedmann, A. Rosinus, and F. Aldinger, "High-Temperature Effect in the Fracture Mechanical Behaviour of Silicon Carbide Liquid-Phase Sintered with $AlN-Y_2O_3$ Additives," J. Eur. Ceram. Soc., 21 1013-19 (2001).   DOI
52 R. R. Lee and W. C. Wei, "Fabrication, Microstructure, and Properties of SiC-AlN Ceramic Alloys," Ceram. Eng. Sci. Proc., 11 [7-8] 1094-121 (1990).   DOI
53 S. G. Lee, Y.-W. Kim, and M. Mitomo, "Relationship between Microstructure and Fracture Toughness of Toughened Silicon Carbide Ceramics," J. Am. Ceram. Soc., 84 1347-53 (2001).
54 H. J. Choi, J. G. Lee, and Y.-W. Kim, "Oxidation Behavior of Liquid-Phase Sintered Silicon Carbide with Aluminum Nitride and Rare-Earth Oxides ($Re_2O_3$, where Re =Y, Er, Yb)," J. Am. Ceram. Soc., 85 [9] 2281-86 (2002).   DOI
55 W. M. Rainforth, "The Wear Behavior of Oxide Ceramics-A Review," J. Mater. Sci., 39 [2] 6705-21 (2004).   DOI
56 H. Y. Liu and M. E. Fine, "Modeling of Grain-Size Dependent Microfracture-Controlled Sliding Wear in Polycrystalline Alumina," J. Am. Ceram. Soc., 76 [9] 2393-96 (1993).   DOI
57 S. J. Cho, H. Moon, B. J. Hockey, and S. M. Hsu, "The Transition from Mild to Severe Wear in Alumina During Sliding," Acta Metall., 40 [1] 185-92 (1992).   DOI
58 X. Dong and S. Jahanmir, "Wear Transition Diagram for Silicon Nitride," Wear, 165 169-80 (1993).   DOI
59 X. Wang, N. P. Padture, H. Tanaka, and A. L. Ortiz, "Wear-Resistant Ultra-Fine-Grained Ceramics," Acta Mater., 53 [2] 271-77 (2005).   DOI
60 B. Frisch, W. R. Thiele, R. Drumm, and B. Muennich, "On the Oxidation Mechanism of Silicon Carbide in the 300$^{\circ}C$ to 1300$^{\circ}C$ Temperature Range," Ceram. Forum Int., 65 [8-9] 277-84 (1988).
61 S. C. Singhal, "Thermodynamical Analysis of the High-Temperature Stability of Silicon Nitride and Silicon Carbide," Ceram. Int., 2 [3] 123-30 (1976).   DOI
62 P. C. Kong and E. Pfender, "Formation of Ultrafine ${\beta}$-Silicon Crabide Powders in an Agron Thermal Plasma Jet," Langmuir, 3 [2] 259-65 (1987).   DOI
63 S. J. Cho, B. J. Hockey, B. R. Lawn, and S. J. Bennison, ''Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina,'' J. Am. Ceram. Soc., 72 [7] 1249-52 (1989).   DOI
64 S. J. Cho, C. D. Um, and S. S. Kim, ''Wear and Wear Transition Mechanism in Silicon Carbide during Sliding,'' J. Am. Ceram. Soc., 78 [4] 1076-78 (1995).   DOI
65 P. F. Becher, "Microstructural Design of Toughened Ceramics," J. Am. Ceram. Soc., 74 255-269 (1991).   DOI
66 Y. Zhou, K. Hirao, Y. Yamauchi, and S. Kanzaki, "Tailoring the Mechanical Properties of Silicon Carbide Ceramics by Modification of the Intergranular Phase Chemistry and Microstructure," J. Eur. Ceram. Soc., 22 2689-96 (2002).   DOI
67 D. Chen, X. F. Zhang, and R. O. Ritchie, "Effects of Grain-Boundary Structure on the Strength, Toughness, and Cyclic-Fatigue Properties of a Monolithic Silicon Carbide," J. Am. Ceram. Soc., 83 2079-81 (2000).
68 R. Yuan, J. J. Kruzic, X. F. Zhang, L. C. De Jonghe, and R. O. Ritchie, "Ambient to High Temperature Fracture Toughness and Cyclic Fatigue Behavior in Al Containing Silicon Carbide Ceramics," Acta Mater., 51 6477-91 (2003).   DOI
69 V. S. R. Murthy, H. Kobayashi, N. Tamari, S. Tsurekawa, T. Watanabe, and K. Kato, "Effect of Doping Elements on the Friction and Wear Properties of SiC in Unlubricated Sliding Condition," Wear, 257 89-96 (2004).   DOI
70 J. D. O. Barceinas-Sanchez and W. M. Rainforth, ''On the Role of Plastic Deformation during the Mild Wear of Alumina,'' Acta Mater., 46 [18] 6475-83 (1998).   DOI
71 R. K. Iier, The Chemistry of Silica; pp. 40-60, Wiley Inc., New York, 1979.
72 E. Ciudad, O. B. Lopez, A. L. Ortiz, and F. Guiberteau, "Microstructural Effects on the Sliding-Wear Resistance of Pressureless Liquid-Phase-Sintered SiC Under Diesel Fuel," J. Eur. Ceram. Soc., 33 [4] 879-85 (2013).   DOI
73 Y. Zhou, K. Hirao, Y. Yamauchi, and S. Kanzaki, "Tribological Properties of Silicon Carbide and Silicon Carbide-Graphite Composite Ceramics in Sliding Contact," J. Am. Ceram. Soc., 86 [6] 991-1002 (2003).   DOI
74 S. K. Sharma, B. V. M. Kumar, and Y.-W. Kim, "Effect of WC Addition on Sliding Wear Behavior of SiC Ceramics," Ceram. Int., 41 3427-37 (2015).   DOI
75 X. Guo, H. Yang, L. Zhang, and X. Zhu, "Sintering Behavior, Microstructure and Mechanical Properties of Silicon Carbide Ceramics Containing Different Nano-TiN Additive," Ceram. Int., 36 161-65 (2010).   DOI
76 H. J. Yeom, Y.-W. Kim, and K. J. Kim, "Electrical, Thermal and Mechanical Properties of Silicon Carbide-Silicon Nitride Composites Sintered with Yttria and Scandia," J. Eur. Ceram. Soc., 35 77-86 (2015).   DOI
77 J. Llorente, B. R. Manso, P. Miranzo, and M. Belmonte, "Tribological Performance under Dry Sliding Conditions of Graphene/Silicon Carbide Composites," J. Eur. Ceram. Soc., 36 429-35 (2016).   DOI
78 Y.-W. Kim, J. H. Lee, and D. Y. Kim, "Effect of Sintering Additive Composition on Grain Boundary Structure in Liquid-Phase-Sintered Silicon Carbide," Mater. Sci. Forum, 558-559 897-902 (2007).
79 H. J. Choi, Y. -W. Kim, M. Mitomo, T. Nishimura, J. H. Lee, and D. Y. Kim, "Intergranular Glassy Phase Free SiC Ceramics Retains Strength at 1500$^{\circ}C$," Scripta Mater., 50 1203-7 (2004).   DOI
80 Y. -W. Kim, S. H. Lee, T. Nishumura, and M. Mitomo, "Heat-Resistant Silicon Carbide with Aluminum Nitride and Scandium Oxide," Acta Mater., 53 4701-8 (2005).   DOI
81 B. V. M. Kumar, M. H. Roh, Y.-W. Kim, W. Kim, S. W. Park, and W. S. Seo, "Effect of Additive Composition on Microstructure and Mechanical Properties of SiC Ceramics Sintered with Small Amount of $RE_2O_3$ (RE: Sc, Lu, Y) and AlN," J. Mater. Sci., 44 5939-5943 (2009).   DOI
82 A. Tewari, B. Basu, and R. K. Bordia, "Model for Fretting Wear of Brittle Ceramics," Acta Mater., 57 2080-87 (2009).   DOI
83 X. Yang, X. Liu, L. Wang, H. Zhang, X. Yao, and Z. Huang, "R-Curve Analysis of Solid-Phase-Sintered and Liquid-Phase-Sintered Silicon Carbide Ceramics by Indentation Fracture and Indentation-Strength-in-Bending Methods," Ceram. Int., 42 4011-18 (2016).   DOI
84 D. B. Marshall, B. R. Lawn, and A. G. Evans, "Elastic/Plastic Indentation Damage in Ceramics: the Lateral Crack System," J. Am. Ceram. Soc., 65 [11] 561-66 (1982)   DOI
85 B. R. Lawn, N. P. Padture, F. Guiberteau, and H. Cai, "A Model for Microcrack Initiation and Propagation Beneath Hertzian Contacts in Polycrystalline Ceramics," Acta Metall. Mater., 42 [5] 1683-93 (1994).   DOI
86 S. Gupta, S. K. Sharma, B. V. M. Kumar, and Y.-W. Kim, "Tribological Characteristics of SiC Ceramics Sintered with a Small Amount of Yttria," Ceram. Int., 41 14780-89 (2015).   DOI
87 O. B. Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padture, "Effect of the Nature of the Intergranular Phase on Sliding-Wear Resistance of Liquid-Phase-Sintered ${\alpha}-SiC $," Scripta Mater., 57 [6] 505-8 (2007).   DOI
88 E. Ciudad, O. B. Lopez, F. Rodriguez-Rojas, A. L. Ortiz, and F. Guiberteau, "Effect of Intergranular Phase Chemistry on the Sliding-Wear Resistance of Pressureless Liquid-Phase-Sintered ${\alpha}-SiC $," J. Eur. Ceram. Soc., 32 [2] 511-16 (2012).   DOI
89 A. L. Ortiz, O. B. Lopez, M. Z. Quadir, and F. Guiberteau, "A Route for the Pressureless Liquid-Phase Sintering of SiC with Low Additive Content for Improved Sliding-Wear Resistance," J. Eur. Ceram. Soc., 32 [4] 965-73 (2012).   DOI
90 Y.-W. Kim, Y. S. Chun, T. Nishumura, M. Mitomo, and Y. H. Lee, "High Temperature Strength of Silicon Carbide Ceramics Sintered with Rare-Earth Oxide and Aluminum Nitride," Acta Mater., 55 727-36 (2007).   DOI
91 N. P. Padture, "In Situ-Toughened Silicon Carbide," J. Am. Ceram. Soc., 77 519-23 (1994).   DOI
92 G. Rixecker, K. Biswas, A. Rosinus, S. Sharma, I. Wiedmann, and F. Aldinger, "Fracture Properties of SiC Ceramics with Oxynitride Additives," J. Eur. Ceram. Soc., 22 2669-75 (2002).   DOI
93 K. Strecker and M. J. Hoffmann, "Effect of AlN-Content on the Microstructure and Fracture Toughness of Hot-Pressed a Heat-Treated LPS-SiC Ceramics," J. Eur. Ceram. Soc., 25 801-7 (2005).   DOI
94 M. Herrmann, G. Standke, S. Hohn, G. Himpel, and T. Gestrich, "High-Temperature Corrosion of Silicon Carbide Ceramics by Coal Ashes," Ceram. Int., 40 1471-79 (2014).   DOI
95 L. Jordi, C. Iliev, and T. E. Fischer, "Lubrication of Silicon Nitride and Silicon Carbide by Water: Running in, Wear and Operation of Sliding Bearings," Tribol. Lett., 17 [3] 367-76 (2004).   DOI
96 R. S. Gates and S. M. Hsu, "Tribochemistry between Water and $Si_3N_4$ and SiC: Induction Time Analysis," Tribol. Lett., 17 [3] 399-407 (2004).   DOI
97 S. M. Hsu and M. C. Shen, "Ceramic Wear Maps," Wear, 200 [1-2] 154-75 (1996).   DOI
98 K. Kato and K. Adachi, "Wear of Advanced Ceramics," Wear, 253 [11-12] 1097-104 (2002).   DOI
99 A. Udayakumar, M. Balasubramanian, H. B. Gopala, P. Sampathkumaran, S. Seetharamu, R. Babu, D. Sathiyamoorthy, and G. R. Reddy, "Influence of the Type of Interface on the Tribological Characteristics of ICVI Generated $SiC_f/SiC $ Composites," Wear, 271 859-65 (2011).   DOI
100 U. Dulias and K. H. Z. Gahr, "Investigation of $Al_2O_3$- and SSiC-Ceramic Under Lubricated, Reciprocating Sliding Contact and Cavitation Erosion," Mater Sci. Eng. Technol., 36 [3-4] 140-47 (2005).
101 S. K. Sharma, B. V. M. Kumar, K. Y. Lim, Y.-W. Kim, and S. K. Nath, "Erosion Behavior of SiC-WC Composites," Ceram. Int., 40 6829-39 (2014).   DOI
102 J. J. Kim and S.K. Park, "Solid Particle Erosion of SiC and SiC-$TiB_2$ Composite Hot-Pressed with $Y_2O_3$," Wear, 222 [2] 114-19 (1998).   DOI
103 X. Li, H. Ding, Z. Huang, M. Fang, B. Liu, Y. Liu, X. Wu, and S. Chen, "Solid Particle Erosion-Wear Behavior of SiC-$Si_3N_4$ Composite Ceramic at Elevated Temperature," Ceram. Int., 40 16201-7 (2014).   DOI
104 B. Wang and A.V. Levy, "Erosion Behavior of SiC Fiber-SiC Matrix Composites," Wear, 138 125-36 (1990).   DOI
105 J. L. Routbort, R. O. Scattergood, and A. P. L. Turner, "The Erosion of Reaction-Bonded SiC," Wear, 59 363-75 (1980).   DOI
106 K. Y. Lim, Y.-W. Kim, and K. J. Kim, "Mechanical Properties of Electrically Conductive Silicon Carbide Ceramics," Ceram. Int., 40 10577-82 (2014).   DOI
107 S. Grasso, T. Saunders, H. Porwal, and M. Reece, "Ultra-High Temperature Spark Plasma Sintering of ${\alpha}-SiC$," Ceram. Int., 41 225-30 (2015).   DOI
108 S. Lafon-Placette, K. Delbe, J. Denape, and M. Ferrato, "Tribological Characterization of Silicon Carbide and Carbon Materials," J. Eur. Ceram. Soc., 35 1147-59 (2015).   DOI
109 D. F. Wang, J. H. She, and Z. Y. Ma, "Effect of Microstructure on Erosive Wear Behavior of SiC Ceramics," Wear, 180 35-41 (1995).   DOI
110 J. L. Routbort and A. P. L. Turner, "The Erosion Rate of Reaction-Bonded SiC Containing Various Amounts of Free Silicon," Wear, 84 381-85 (1983).   DOI
111 B. Basu and M. Kalin, "Tribology of Ceramics and Composites," pp. 70-100 in Wear Mechanisms, John Wiley & Sons, Inc., New Jersey, 2011.
112 N. P. Padture, "In Situ-Toughened Silicon Carbide," J. Am. Ceram. Soc., 77 519-23 (1994).   DOI
113 P. T. B. Shaffer, "A Review of the Structure of Silicon Carbide," Acta Cryst., B, 25 477-88 (1969).   DOI
114 H. P. Iwata, U. Lindefelt, S. Oberg, and P.R. Briddon, "Stacking Faults in Silicon Crabides," Phys. B, 340-342 165-70 (2003).   DOI
115 Y. M. Tairov and V. F. Tsvetkov, "Investigation of Growth Processes of Ingots of Silicon Carbide Single Crystals," J. Crys. Growth, 43 [2] 209-12 (1978).   DOI
116 A. J. Van Bommel, J. E. Crombeen, and A. V. Tooren, "Leed and Auger Electron Observations of the SiC (0001) Surface," Surf. Sci., 48 463-72 (1975).   DOI
117 A. Taylor and D. S. Laidler, "The Formation and Crystal Structure of Silicon Carbide," Br. J. Appl. Phys., 1 [7] 174-81 (1950).   DOI
118 W. Wesch, "Silicon Carbide: Synthesis and Processing," Nucl. Instrum. Meth. B, 116 305-21 (1996).   DOI
119 D. Chen, X. F. Zhang, and R. O. Ritchie, Effects of Grain-Boundary Structure on the Strength, Toughness, and Cyclic-Fatigue Properties of a Monolithic Silicon Carbide," J. Am. Ceram. Soc., 83 2079-81 (2000).
120 S. M. Hsu and M. Sheng, "Wear Prediction of Ceramics," Wear, 256 867-78 (2004).   DOI
121 X. Dong, S. Jahanmir, and L. K. Ives, "Wear Transition Diagram for Silicon Carbide," Tribo. Int., 28 559-72 (1995).   DOI
122 D. C. Cranmer, "Friction and Wear Properties of Monolithic Silicon-Based Ceramics," J. Mater. Sci., 20 2029-37 (1985).   DOI
123 K. H. Z. Gahr, R. Blattner, D. H. Hwang, and K. Pohlmann, "Micro- and Macro-Tribological Properties of SiC Ceramics in Sliding Contact," Wear, 250 299-310 (2001).   DOI
124 V. S. R. Murthy, H. Kobayashi, S. Tsurekawa, N. Tamari, T. Watanabe, and K. Kato, "Influence of Humidity and Hoping Elements on the Friction and Wear of SiC in Unlubricated Sliding," Tribo. Int., 37 353-64 (2004).   DOI
125 Y. -W. Kim, K. Y. Lim, and W. S. Seo, "Microstructure and Thermal Conductivity of Silicon Carbide with Yttria and Scandia," J. Am. Ceram. Soc., 97 923-28 (2014).   DOI
126 Y. Wang and S. M. Hsu, "Wear and Wear Transition Mechanisms of Ceramics," Wear 195 112-22 (1996).   DOI
127 T. Hase, "Boron Transport and Change of Lattice Parameter during Sintering of ${\beta}$-SiC," J. Am. Ceram. Soc., 63 [5-6] 349-50 (1980).   DOI
128 G. Roewer, U. Herzog, K. Trommer, E. Muller, and S. Fruhauf, "Silicon Carbide-A Survey of Synthetic Approaches, Properties and Applications," Struct. Bond., 101 59-135 (2002).   DOI
129 B. V. M. Kumar, Y.-W. Kim, D. S. Lim, and W. S. Seo, "Influence of Small Amount of Sintering Additives on Unlubricated Sliding Wear Properties of SiC Ceramics," Ceram. Int., 37 [8] 3599-608 (2011).   DOI
130 V. A. Izhevskyi, L. A. Genova, J. C. Bressiani, and A. H. A. Bressiani, "Silicon Carbide. Structure, Properties and Processing," Ceramica, 46 4-13 (2000).   DOI
131 K. Negita, "Effective Sintering Aids for Silicon Carbide Ceramics: Reactivities of Silicon Carbide with Various Additives," J. Am. Ceram. Soc., 69 [12] C308-10 (1986).
132 D. Sciti, S. Guicciardi, and A. Bellosi, "Effect of Annealing Treatment on Microstructure and Mechanical Properties of Liquid-Phase Sintered Silicon Carbide," J. Eur. Ceram. Soc., 21 621-32 (2001).   DOI
133 D. I. Cheong, J. Kim, and S. J. Kang, "Effect of Isothermal Annealing on the Microstructure and Mechanical Properties of SiC Ceramics Hot-Pressed with $Y_2O_3$ and $Al_2O_3$ Additions," J. Eur. Ceram. Soc., 22 1321-27 (2002).   DOI
134 O. B. Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padture, "Microstructural Design of Sliding-Wear-Resistant Liquid-Phase-Sintered SiC: An Overview," J. Eur. Ceram. Soc., 27 3351-57 (2007).   DOI
135 X. F. Zhang, G. Y. Lee, D. Chen, R. O. Ritchie, and L. C. D. Jonghe, "Abrasive Wear Behavior of Heat-Treated ABC-Silicon Carbide," J. Am. Ceram. Soc., 86 1370-78 (2003).   DOI
136 P. Andersson and A. Blomberg, "Instability in the Tribochemical Wear of Silicon Carbide in Unlubricated Sliding Contacts," Wear, 174 1-7 (1994).   DOI
137 O. O. Adewoye and T. F. Page, "Frictional Deformation and Fracture in Polycrystalline SiC and $Si_3N_4$," Wear, 70 37-5 (1981).   DOI
138 S. J. Cho, C. D. Um, and S. S. Kim, "Wear and Wear Transition in Silicon Carbide Ceramics During Sliding," J. Am. Ceram. Soc., 79 1247-51 (1996).   DOI
139 O. B. Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padture, "Sliding-Wear-Resistant Liquid-Phase-Sintered SiC Processed Using ${\alpha}-SiC $ Starting Powders," J. Am. Ceram. Soc., 90 [2] 541-45 (2007).   DOI
140 O. B. Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padture, "Effect of Microstructure on Sliding-Wear Properties of Liquid-Phase-Sintered ${\alpha}-SiC $," J. Am. Ceram. Soc., 88 [8] 2159-2163 (2005).   DOI
141 O. B. Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padture, "Improved Sliding-Wear Resistance in In-situ Toughened Silicon Carbide," J. Am. Ceram. Soc., 88 [12] 3531-34 (2005).   DOI