Magnetic and Microwave Absorbing Properties of M-type Ba-ferrite($BaFe_{12-2X}Ti_XCo_XO_{19}$)with Planar Magnetic Anisortropy (면내 자기이방성을 갖는 M-type Ba-ferrite($BaFe_{12-2X}Ti_XCo_XO_{19}$)의 자기적특성 및 전파흡수특성)

  • 조한신;김성수
    • Resources Recycling
    • /
    • v.7 no.4
    • /
    • pp.22-26
    • /
    • 1998
  • The purpose of this experimenL is to investigate the magnetic anisotropy and microwave absorbing properties in M-type Bat territe (${BaFe}_{12-2X}{A}_{X}{Me}_{X}{O}_{19}$), where $Fe_{3+}$ is substituted by $Ti_{4+}$ in A site and $Co_{2+}$ in Me site. The saturation magnetization (Ms) is linearly decreased with the substitution rate(x) and the coerciviLy (He) is rapidly decreased in accordance with the reduction in t the magnetocrystalline anisotropy For the specimen with x=0.8 and thickness of 2 mm, the reflection loss calculated from the n material constants is less than -10 dB (90% absorption) in the frequency range of 10~16 GHz. The absorption loss is pre이.ctcd t to be more than 20 dElern in the frequency range of 12-16 GHz. The results demonstrate that the Ti-Co substituted M-type Ba-ferrite can be effectively used as a microwave absorber at high frequency range.

  • PDF

Strain induced/enhanced ferromagnetism in $Mn_3Ge_2$thinfilms

  • Dung, Dang Duc;Feng, Wuwei;Thiet, Duong Van;Sin, Yu-Ri-Mi;Jo, Seong-Rae
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.135-135
    • /
    • 2010
  • In Mn-Ge equilibrium phase diagram, many Mn-Ge intermetallic phases can be formed with difference structures and magnetic properties. The MnGe has the cubic structure and antiferromagnetic(AFM) with Neel temperature of 197 K. The calculation predicted that the $MnGe_2$ with $Al_2Cu$-type is hard to separate between the paramagnetic(PM) states and the AFM states because this compound displays PM and AFM configuration swith similar energy. Mn-doped Ge showed the FM with Currie temperature of 285 K for bulk samples and 116 K for thin films. In addition, the $Mn_5Ge_3$ compound has hexagonal structure and FM with Curie temperature around 296K. The $Mn_{11}Ge_8$ compound has the orthorhombic structure and Tc is low at 274 K and spin flopping transition is near to 140 K. While the bulk $Mn_3Ge_2$ exhibited tetragonal structure ($a=5.745{\AA}$;$c=13.89{\AA}$) with the FM near to 300K and AFM below 150K. However, amorphous $Mn_3Ge_2$ ($a-Mn_3Ge_2$) was reported to show spin glass behavior with spin-glass transition temperature (Tg) of 53 K. In addition, the transition of crystalline $Mn_3Ge_2$ shifts under high pressure. At the atmospheric pressure, $Mn_3Ge_2$ undergoes the magnetic phase transition from AFM to FM at 158 K. The pressure dependence of the phase transition in $Mn_3Ge_2$ has been determined up to 1 GPa. The transition was found to occur at 1 GPa and 155 K with dT/dP=-0.3K/0.1 GPa. Here report that Ferromagnetic $Mn_3Ge_2$ thin films were successfully grown on GaAs(001) and GaSb(001) substrates using molecular beam epitaxy. Our result revealed that the substrate facilitates to modify magnetic and electrical properties due to tensile/compressive strain effect. The spin-flopping transition around 145 K remained for samples grown on GaSb(001) while it completely disappeared for samples grown on GaAs(001). The antiferromagnetism below 145K changed to ferromagnetism and remained upto 327K. The saturation magnetization was found to be 1.32 and $0.23\;{\mu}B/Mn$ at 5 K for samples grown on GaAs(001) and GaSb(001), respectively.

  • PDF

Electromagetic Wave Absorbing Properties of $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$(X=Cu, Mg, Mn)-Rubber Composite ($Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$(X=Cu, Mg, Mn)-Rubber Composite의 전파흡수특성에 관한 연구)

  • Im, Hui-Dae;Yun, Guk-Tae;Lee, Chan-Gyu
    • Korean Journal of Materials Research
    • /
    • v.9 no.12
    • /
    • pp.1234-1239
    • /
    • 1999
  • Electromagnetic wave asorbing properties of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$, where X was replaced by substitution elements Cu, Mg, Mn, have been studied. The structure, shape, size and magnetic properties of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$ were analyzed by XRD, SEM, VSM. The relative complex permittivity, permeability, and electromagnetic wave absorbing properties were measured by Network Analyzer. The structure, shape, size and magnetization value of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$ were found to be similar in spite of substitution elements. The coercive force and hysteresis-loss showed maximum value when Mg was substituted for X. The dielectric loss(${\varepsilon}_r"/{\varepsilon}_r'$) was found to be maximum value when Mn was substituted for X. Also the magnetic loss(${\mu}_r"/{\mu}_r'$} was found to be maximum with Cu substitution. The electromagnetica wave absorbing property of the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$-Rubber composite with 4mm thickness was excellent as over - 40dB at 9GHz, and the $Ni_{0.5}-Zn_{0.4}-X_{0.1}{\cdot}Fe_2O_4$-Rubber composite with 8mm thickness was over-40dB at 2GHz. Those composites also showed superior microwave absorbing properties.

  • PDF

Colossal Magnetoresistance and Mossbauer Studies of La-Ca-Mn-O Compound Doped with $^{57}Fe$ ($^{57}Fe$를 미량 치환한 La-Ca-Mn-O의 초거대자기저항과 Mossbauer분광학연구)

  • 박승일;김성철
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.6
    • /
    • pp.335-340
    • /
    • 1998
  • Colossal magnetoresistance $La_{0.67}Ca_{0.33}Mn_{0.99}^{57}Fe_{0.01}O_3$ material has been produced by a metal-salt routed sol-gel process method. Magnetic properties of $La_{0.67}Ca_{0.33}Mn_{0.99}^{57}Fe_{0.01}O_3$ have been studied with x-ray diffraction, Rutherford back-scattering spectroscopy(RBS), vibrating sample magnetometer, and Mossbauer spectroscopy. Crystalline $La_{0.67}Ca_{0.33}Mn_{0.99}^{57}Fe_{0.01}O_3$ was perovskite cubic structure with a lattice parameter $a_0=3.868$\AA$$. And there was no appreciable change in the value of the lattice parameter when a small amount (x=0.01) of iron was added. However, Mossbauer and VSM data indicate the Curie temperature of the $La_{0.67}Ca_{0.33}Mn_{0.99}^{57}Fe_{0.01}O_3$ decreased from 282 to 270 k and also the saturation magnetization from 84 to 81 emu/g at 77 K. Mossbauer spectra of $La_{0.67}Ca_{0.33}Mn_{0.99}^{57}Fe_{0.01}O_3$ have been taken at various temperatures ranging form 4.2 K to room temperature. Analysis of $^{57}Fe$ Mossbauer data in terms of the local configurations of Mn atoms has permitted the influence of the magnetic hyperfine interactions to be monitored. The isomer shifts show that the charge state of all Fe ions are ferric. The magnetoresistance of $La_{0.67}Ca_{0.33}Mn_{0.99}^{57}Fe_{0.01}O_3$ was about 33 % at semiconductor-metal transition temperature $T_{SC-M}=250K$.

  • PDF

Growth and Magnetic Properties of $Y_{3-x}La_xFe_5O_{12}(0.0{\le}X{\le}1.0)$ Powders and Thin Films by a Sol-Gel Method (Sol-Gel 법에 의한 $Y_{3-x}La_xFe_5O_{12}(0.0{\le}X{\le}1.0)$ 분말과 박막의 합성 및 자기적 특성에 관한 연구)

  • 엄영랑;김철성;임연수;이재광
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.6
    • /
    • pp.350-356
    • /
    • 1998
  • $Y_{3-x}La_xFe_5O_{12}$ (x=0.0, 0.25, 0.5, 0.75, 1.0) powders and thin films were fabricated by a sol-gel method and their magnetic properties and crystal structure were investigated by using X-ray diffraction (XRD), atomic force microscopy (AFM), scanning electron microscopy (SEM), vibrating sample magnetometer (VSM), and Mossbauer spectroscopy. XRD and Mossbauer spectroscopy measurements show that garnet powders annealed at 900 $^{\circ}C$ for 8 hours were single-phased and that thin films fired at 800 $^{\circ}C$ for 2 hours were crystallized without any preferred direction. X-ray diffraction patterns of $Y_{3-x}La_xFe_5O_{12}$ powders annealed at 1000 $^{\circ}C$ had only peaks of the garnet structure in case of x$\leq$0.75 but those of $Y_2LaFe_5O_{12}$ powders consisted of peaks from garnets and $LaFeO_3$. Mossbauer sepectra of garnet powders grown by the sol-gel method had a similar shape of those of powders grown by a conventional ceramic method. Grain sizes of garnet powders were 200~300 nm and the averaged surface roughness was 3.17 nm. Results of VSM measurements show the powders and thin films had soft magnetic properties and that the garnet powders had the largest saturation magnetization, 30 emu/g, and the lowest coercivity, 52 Oe.

  • PDF

Magnetism of Pd(111) Thin Films: A First-principles Calculation (Pd(111) 박막의 자성: 제일원리계산)

  • Hong, Soon Cheol
    • Journal of the Korean Magnetics Society
    • /
    • v.26 no.1
    • /
    • pp.1-6
    • /
    • 2016
  • Pd has the highest magnetic susceptibility among single element metals and often shows ferromagnetism under some special environments. In this paper, we report magnetism of 5- and 9-monolayers (ML) calculated by using full-potential linearized augmented plane wave method. Exchange-correlation interaction is taken into account in local density approximation (LDA) and generalized gradient approximation (GGA) and calculational results in LDA and GGA are compared with each other. It is found that calculations by LDA are more reliable compared to those by GGA because LDA prediction of paramagnetism of bulk Pd is consistent with experiments, whereas GGA predicts wrongly ferromagnetim of bulk Pd. Calculational results in LDA on a 5-ML Pd(111) thin film shows a ferromagnetic ground state unlike a paramagnetic ground state of bulk Pd. The center Pd layer of the 5-ML Pd(111) thin film has the largest magnetic moment ($0.273{\mu}_B$) among the layers and |m| = 1 orbital states play a dominant role in stabilizing the ferromagnetism of the 5-ML Pd(111) thin film. A 9-ML Pd(111) thin film in a ferromagnetic state has almost the same total energy as in a paramagnetic state. Since the magnetization of the 9-ML Pd(111) thin film is stable, the ferromagnetic state may be meta-stable.

Effect on the Formation of Fe3O4 with Ferrous Sulfate/Ferric Sulfate Molar Ratio and Precipitants (Fe3O4 생성에 미치는 황산제일철/황산제이철 몰비와 침전제의 영향)

  • Eom, Tae-Hyoung;Kim, Sam-Joong;An, Suk-Jin;Oh, Kyoung-Hwan;Suhr, Dong-Soo
    • Journal of the Korean Magnetics Society
    • /
    • v.21 no.5
    • /
    • pp.157-162
    • /
    • 2011
  • The effect of ferrous/ferric molar ratio and precipitants on the formation of nano size magnetite particle was investigated by coprecipitation method. Ferrous sulfate and ferric sulfate were used as iron sources and sodium hydroxide and ammonium hydroxide was used as a precipitant. Single phase magnetite was synthesized with all of experiment conditions (ferrous/ferric molar ratios and precipitants). Particle size was smaller, and particle size distribution was narrower when NaOH was used than $NH_4OH$ was used. The crystallinity and particle size was increased and narrower particle size distribution with increasing molar ratio ferrous/ferric sulfate with the same precipitant. Super paramagnetism could be obtained at all of experiment conditions. The highest saturation magnetization (72 emu/g) was obtained when the ferrous/ferric molar ratio was 2.5 and precipitant was used $NH_4OH$.

Magnetic and Microwave Absorbing Properties of M-type Hexagonal Ferrites Substituted by Ru-Co(BaFe12-2xRuxCoxO19) (Ru-Co가 치환된 M-형 육방정 페라이트(BaFe12-2xRuxCoxO19)의 자기적 성질 및 전파흡수 특성)

  • Cho, Han-Shin;Kim, Sung-Soo
    • Journal of the Korean Magnetics Society
    • /
    • v.18 no.4
    • /
    • pp.136-141
    • /
    • 2008
  • In this study, the magnetic(static and high-frequency) and microwave absorbing properties have been investigated in Ru-Co substituted M-hexaferrites($BaFe_{12-2x}Ru_xCo_xO_{19}$). The powders and sintered specimens were prepared by conventional ceramic processing technique. With the calcined powders, the composite specimens were prepared using the silicone rubber as a matrix material. The substitution ratio of Ru-Co to obtain in-plane magnetic anisotropy, thus having the minimum coercivity, is much smaller (about x=0.3) than the previously reported Ti-Co substituted specimen. Owing to this low substitution, the specimen has a large value of saturation magnetization($M_s$=65 emu/g). Ferromagnetic resonance behavior and microwave absorbing frequency band is strongly influnced by the coercvity which can be controlled by Ru-Co substitution ratio. It is found that the M-hexaferrites with planar magnetic anisotropy by doping Ru-Co in both sintered and composite form have superior microwave absorbing properties in GHz frequency range.

Structure and Magnetic Properties on Synthesis Route of Co2Z-type Barium Hexaferrite (Co2Z-type Barium Hexaferrite의 합성방법에 따른 결정구조 및 자기적 특성)

  • Baek, In Seung;Nam, In Tak
    • Journal of the Korean Magnetics Society
    • /
    • v.24 no.1
    • /
    • pp.1-10
    • /
    • 2014
  • $Co_2Z$-type barium ferrites ($Ba_3Co_2Fe_{24}O_{41}$) were synthesized using variation method. First, M-type, $Co_2Y$-type and $Co_2Z$-type synthesized by hydrothermal method. Second, M- and Y-type precursors for synthesis of $Co_2Z$ hexaferrite by hydrothermal and ball milling method. the morphology, structure and magnetic properties of the barium ferrite particles were characterized using XRD, FESEM, VSM, impedance. As a result, Single phase of M-type and $Co_2Y$-type were obtained. Manufactured powders of M+Y ball milling, M+Y hydrothermal were similar to single phase of $Co_2Z$-type hexaferrite, all powders were obtained theoretical magnetization (50 emu/g). The largest initial permeability were obtained $Co_2Z$ hexaferrite synthesized by reagent precusor, With increasing calcination temperature was lowered the initial permeability. In another synthesis didn't almost that little change could be found.

Archaeomagnetic Study of Historic Sites in Chungcheong Region Regional Difference of Geomagnetic Field and Issues on Reliability of Data (충청지역 유적에 대한 고고지자기학적 연구 지자기의 지역적인 차이와 데이터의 신뢰도 문제를 중심으로)

  • Sung, Hyong Mi
    • Korean Journal of Heritage: History & Science
    • /
    • v.41 no.1
    • /
    • pp.21-33
    • /
    • 2008
  • In this study, the researcher examined archaeomagnetic secular variation of Chungcheong Region through measured data of archaeomagnet obtained from 34 relics, which discovered in the baked earth from varied historic sites within the region. Furthermore, the researcher closely reviewed regional differences of geomagnetic field in the domestic territory. Reviewing the comparison between the measured data of archaeomagnet in Chungcheong Region and the archaeomagnetic secular variation of Japan, which has difference in distance, it reveals a noticeable change in declination by tilting more than 10 degree toward East in the year of about A.D. 300, although the feature of whole variation is quite similar. In other period of times, it was confirmed that the regional differences of geomagnetic field in which the magnetic dip became deeper to some degree, and the declination was tilted westward a little bit. Such patterns do not differ significantly from the pattern of entire archaeomagnetic secular variation of our country, and even in the direct comparison to the data of Chungcheong Region, the distinct regional difference in both periods before and after Christian era was not confirmed. The fact may become clearer that, when the volume of the measured data of archaeomagnet increases further, and when more data connected with varied time period are filled, the problem such as deviation of the measurement period of archaeomagnet caused by the regional difference of geomagnetic field would not be worrisome issue, especially in Korean territory, judging from the measured data of archaeomagnet of historic relics in Chungcheong Region. Besides, as great efforts are being exerted in order to get the most reliable measured data as much as possible in taking both samples and measurement, it is thought that there would be no problem not only in the issue of deviation of the measurement period involving with the measured data of archeomagnet, but also in the aspect of reliability of data.