• 제목/요약/키워드: Magnesium alloy

검색결과 561건 처리시간 0.036초

Corrosion protection behavior of AZ31 magnesium alloy with cathodic electrophoretic coating pretreated by cerium based conversion coatings at various pH

  • Fazal, Basit Raza;Phuong, Nguyen Van;Moon, Sungmo
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2015년도 추계학술대회 논문집
    • /
    • pp.268-268
    • /
    • 2015
  • The corrosion protection behavior of AZ31 magnesium alloy (Mg alloy) with cathodic electrophoretic coating (E-coating) pretreated by cerium-based conversion coatings at various pH was investigated in this study. Cerium-based conversion coatings (CeCCs) were deposited on AZ31 Mg alloy by immersion treatment in the nitrate-based cerium salt solution. The morphology and composition of the CeCCs were analyzed using scanning electron microscopy and energy dispersive X-ray spectroscopy. The corrosion properties of the AZ31 Mg alloy pretreated with cerium coating and subsequently E-coated were studied during salt-spray testing. The surface morphologies of the E-coated Mg alloy were examined in detail after different testing times using digital photography. It was found that the protective properties of the E-coating on AZ31 Mg alloy generated are heavily dependent upon the CeCC factors such as treatment time, coating thickness and pH of the solution.

  • PDF

Mg-Nd-Y-Zr-Zn 주조합금의 인장특성에 미치는 시효처리의 영향 (Effect of Aging Treatment on the Tensile Properties of Mg-Nd-Y-Zr-Zn Casting Alloys)

  • 김현식;예대희;강민철;김인배
    • 한국재료학회지
    • /
    • 제18권5호
    • /
    • pp.266-271
    • /
    • 2008
  • Magnesium alloys are alloyed with rare earth elements (Re, Ca, Sr) due to the limited use of magnesium in high-temperature conditions. In this study, the influences of Zr and Zn on the aging behavior of a Mg-Nd-Y alloy were investigated. magnesium alloys containing R.E elements require aging treatments Specifically, Nd, Y and Zr are commonly used for high-temperature magnesium alloys. Various aging treatments were conducted at temperatures of 200, 250 and $300^{\circ}C$ for 0.5, 1, 3, 6, and 10 hours in order to examine the microstructural changes and mechanical properties at a high temperature ($150^{\circ}C$). Hardness and high-temperature ($150^{\circ}C$) tensile tests were carried out under various aging conditions in order to investigate the effects of an aging treatment on the mechanical properties of a Mg-3.05Nd-2.06Y-1.13Zr-0.34Zn alloy. The maximum hardness was 67Hv; this was achieved after aging at $250^{\circ}C$ for 3 hours. The maximum tensile, yield strength and elongation at $150^{\circ}C$ were 237MPa, 145MPa and 13.6%, respectively, at $250^{\circ}C$ for 3 hours. The strengths of the Mg-3.05Nd-2.06Y-1.13Zr-0.34Zn alloy increased as the aging time increased to 3 hours at $250^{\circ}C$ This is attributed to the precipitation of a Nd-rich phase, a Zr-rich phase and $Mg_3Y_2Zn_3$.

Ca 첨가에 따른 Mg-4Al-2Sn-xCa 다이캐스팅 합금의 기계적특성 연구 (Effect of Ca additions on Mechanical Properties of Mg-4Al-2Sn-xCa Die-Casting Alloys)

  • 김영민;이영철;박용호
    • 한국주조공학회지
    • /
    • 제31권5호
    • /
    • pp.293-301
    • /
    • 2011
  • Representative magnesium alloys applied to the die-casting are AZ91, AM60, etc., and the application of these alloys is restricted to components operating at moderate temperatures, due to grain boundary siding of ${\beta}$-phase($Mg_{17}Al_{12}$) at temperatures above $120^{\circ}C$. Heat-resistant magnesium alloys such as AE42, AE44 have been developed, but that have been too burdensome to produce because of the expensive rare earth materials. Research work for the development of low-priced heat-resistant magnesium alloy is actively in progress and positive results are being reported. This study aims to investigate the effect of Ca additions on mechanical properties of Mg-4Al-2Sn heat resistant magnesium alloys. Mg-4Al-2Sn alloys with Ca (0wt.%, 0.3wt.%, 0.7wt.%, 1wt.%) have been produced through the die-casting process for the development of low-priced heat-resistant magnesium alloy, and high temperature tensile tests are performed using the specimens. The results showed that mechanical properties of Mg-4Al-2Sn-xCa increased with the addition of Ca up to 0.7wt.% Ca and further addition of Ca deteriorated the mechanical properties of the alloys. A significant amount of porosity was observed at the sample with 1wt%. Ca and the longer freezing range of the alloy was believed to cause the formation of porosity.

인크리멘탈 성형을 이용한 마그네슘 합금 판재의 성형변수에 관한 연구 (A parametric Study in Incremental Forming of Magnesium Alloy Sheet)

  • 박진기;유봉선;김영석
    • 소성∙가공
    • /
    • 제17권6호
    • /
    • pp.412-419
    • /
    • 2008
  • Using lightweight materials in vehicle manufacturing in order to reduce energy consumption is one of the most effective approach to decrease pollutant emissions. As a lightweight material, magnesium is increasingly employed in automotive parts. However, because of its hexagonal closed-packed(HCP) crystal structure, in which only the basal plane can move, the magnesium alloy sheets show low ductility and formability at room temperature. Thus the press forming of magnesium alloy sheets has been performed at elevated temperature within range of $200^{\circ}C{\sim}250^{\circ}C$. Here we try the possibility of sheet metal forming at room temperature by adopting incremental forming technique with rotating tool, which is so called as rotational-incremental sheet forming(RISF). In this rotational-incremental sheet forming the spindle tool rotates on the surface of the sheet metal and moves incrementally with small pitch to fit the sheet metal on the desired shape. There are various variables defining the formability of sheet metals in the incremental forming such as speed of spindle, pitch size, lubricants, etc. In this study, we clarified the effects of spindle speed and pitch size upon formability of magnesium alloy sheets at room temperature. In case of 0.2, 0.3 and 0.4mm of pitch size with hemispherical rotating tool of 6.0mm radius, the maximum temperature at contact area between rotating tool and sheet metal were $119.2^{\circ}C,\;130.8^{\circ}C,\;and\;177.3^{\circ}C$. Also in case of 300, 500, and 700rpm of spindle speed, the maximum temperature at the contact area were $109.7^{\circ}C,\;130.8^{\circ}C\;and\;189.8^{\circ}C$.

Surface Treatment of Automotive Cast Parts of Magnesium Alloy

  • Sim, Yangjin;Kim, Jongmyung
    • Corrosion Science and Technology
    • /
    • 제2권2호
    • /
    • pp.102-108
    • /
    • 2003
  • The surface treatments. Chrome/Manganese and Modified Chrome Pickle, that are treated to improve the anti-corrosion property which is needed to increased the probability of prototype product enabled the sand cast Magnesium test specimens to have better corrosion resistance than non-treated one. Sand cast Magnesium specimens which was treated only with chemical conversion coating had same corrosion resistance with the Steel specimens plated by Zinc, and the another one that had the finishing treatment(painting) worked on the chemical surface treatment had the corrosion resistance property to meet to FPO-3 requirement. We also investigated the multiple finishing system(chemical surface treatment + 3 coating) to test the severe condition that magnesium should to endure.

고온변형 중의 AZ80 마그네슘합금의 집합조직 형성거동에 영향을 미치는 변형속도의 영향 (The Effect of Strain Rate on Texure Formation Behaviors in AZ80 Magnesium Alloy)

  • 배상대
    • 열처리공학회지
    • /
    • 제33권6호
    • /
    • pp.296-302
    • /
    • 2020
  • Magnesium alloys have been rapidly attracting as lightweight structural material in various industry fields because of having high specific strength and low density. It is well known that the crystallographic texture plays an important role in improvement of poor room temperature ductility of magnesium alloys. In this study, high-temperature plane strain compression deformation was conducted on extruded AZ80 magnesium alloy at 723K by varying the strain rates ranging from 5.0×10-3s-1 to 5.0×10-2s-1 in order to investigate the behaviors of texture formation. It was found that texture formation behaviors in three kinds of specimens were affected by continuous and discontiuous deformation mechanism.

Mg AZ31B 판재의 기계적 특성과 성형성 분석 (A Study on the Mechanical Properties and Formability of Mg AZ31B Sheet)

  • 이규현;윤태욱;강창룡
    • 소성∙가공
    • /
    • 제23권8호
    • /
    • pp.495-500
    • /
    • 2014
  • Magnesium alloys are currently expected to be widely used for weight reduction of cars and as high efficient materials in the automotive and electronics industries. Although the specific strength of magnesium is excellent, it cannot be easily formed at room temperature due to its HCP structure. However in order to improve the formability of magnesium, it is necessary to investigate its formability in the warm temperature range. In the current study, the aim was to add to the magnesium property database so that the mass production of a magnesium car body can be accomplished. Warm tensile tests were conducted and the forming limit diagram was determined to confirm formability characteristics of magnesium AZ31B alloy sheet. In addition the bending formability and the magnesium damping capacity were evaluated for AZ31B and compared to SPRC440E which is a sheet steel used for car bodies.

Anodizing과 Burning 공정 혼합으로 표면처리 된 마그네슘합금(AZ31) 안경테 표면의 특성 연구 (The study of characterization about magnesium alloy eye-glasses case by anodizing and mixed method (anodizing+burning))

  • 유재용;임진환;유재인;김진희;박창훈;김기홍
    • 한국진공학회지
    • /
    • 제16권3호
    • /
    • pp.231-234
    • /
    • 2007
  • 마그네슘 합금을 Anodizing과 Burning anodizing만으로만 표면 처리했을 때는 표면에 기공이 많이 발생 되었지만, anodizing 처리 후, burning 공정을 추가 하였을 때는 기공이 현저히 줄어들었다. 즉 burning 공정이 추가 되므로 인해 anodizing 공정의 단점인 기공의 봉공처리가 가능함을 알았다. 또한 막 두께도 anodizing 만 처리 했을 때 보다 더 균일하게 성장함을 보았다.

AZ31B 마그네슘 합금판재의 온간 성형한계도 및 스프링백 특성 시험 (Experiments for Forming Limit Diagram and Springback Characteristics of AZ31B Magnesium Alloy Sheet at Elevated Temperature)

  • 최선철;이한수;김형종;이경택;김헌영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.289-293
    • /
    • 2007
  • The effect of temperature on the forming limit diagram was investigated for AZ31B magnesium alloy sheet through the limit dome height test in the range from room temperature to $300^{\circ}C$. The formability of AZ31B sheet was improved significantly according to the increasing temperature. Also we studied the springback characteristics through the 2D draw bending test with different blank holding forces at elevated temperatures. Springback quantity was considerably reduced as temperature went up. The blank holding force in the range used, however, had little influence on springback. Experimental results obtained in this study may provide a material database for AZ31B sheet.

  • PDF

Ni 삽입재를 사용한 마그네슘 AZ31 합금의 TLP접합 특성평가 (Characterization of TLP Bonded of Magnesium AZ31 Alloy using a Nickel Interlayer)

  • 진영준
    • 한국자동차공학회논문집
    • /
    • 제21권4호
    • /
    • pp.113-119
    • /
    • 2013
  • The transient liquid phase (TLP) bonding was used to fabricate autogenous joints in a magnesium alloy AZ31 with the aid of a pure Ni interlayer. A $13{\mu}m$ thick pure Ni foil was used in order to form a Mg-Ni eutectic liquid at the joint interface. The interface of reaction and composition profiles were investigated as a function of bonding time using a pressure of 0.16 MPa and a bonding temperature of $515^{\circ}C$. The quality of the joints produced was examined by metallurgical characterization and the joint microstructure developed across the diffusion bonds was related to changes in mechanical properties as a function of the bonding time.