Microstructural Analysis on Oxide Film of Al6061 Exposed to Atmospheric Conditions (대기 노출된 Al6061 알루미늄 합금 산화막에 대한 미세조직 분석)

  • Jo, Junyeong;Kwon, Daeyeop;Choi, Wonjun;Bahn, Chi Bum
    • Journal of the Korean institute of surface engineering
    • /
    • v.55 no.5
    • /
    • pp.273-283
    • /
    • 2022
  • Al6061 aluminum alloy specimens were exposed to atmospheric conditions for maximum 24 months. 24-month exposure specimen showed some more frequent and larger size of corrosion products and pitting on the surface compared with the 12-month exposure specimens. The XRD examination revealed the dominant surface oxide phases of Al2O3 and Al(OH)3. The oxide thickness at uniform oxidation (or non-pitting) region was not much changed over exposure time. The 1.2 ㎛ deep oxygen penetration area was found in the 12-months exposed specimen near the thin uniform aluminum oxide film. The line-EDS was conducted through the penetration regions and non-penetrated grain boundary. There were signs of O and Si concentration through the penetration region, whereas non-penetration region showed no concentration of O or Si. It was confirmed that pitting is a more severe degradation mode in Al6061 (max. >4 ㎛ deep) compared with the uniform oxidation (max. ~200 nm deep) up to 24-months exposure.

Relation of Calcium Activity in Milk and Milk Production of Holstein Cows in Hot Season

  • Tanaka, Masahito;Suzuki, Tomoyuki;Kotb, Saber;Kamiya, Yuko
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.24 no.10
    • /
    • pp.1372-1376
    • /
    • 2011
  • The content of Ca in milk exceeds the typical saturation level of Ca salts, which is necessary for neonate growth. This calcium is distributed between the casein micelles in the colloidal and aqueous phases. Information on the properties of calcium activity in the aqueous phase is limited compared with that on the properties of bound or sequestrated calcium. The objectives of this study were to evaluate the changes in calcium activity in fresh milk using an ion-selective electrode and to assess the relationship between calcium activity and milk production in hot season. Milk samples collected from 10 cows at the National Agricultural Research Center for Kyushu Okinawa Region in June to October (Min-Max: 7.2-$35.2^{\circ}C$, 24.3-100% RH) were analyzed on total calcium concentrations and calcium activity. We observed that the rectal temperature of the cows increased according to elevation of ambient temperature but that the pH of the collected milk ($6.61{\pm}0.01$ (Mean${\pm}$SEM)) was not significantly influenced by rectal and ambient temperature. Total calcium concentrations and calcium activity in fresh milk decreased in July (Min-Max: 21.1-$33.5^{\circ}C$, 48.9-100.0% RH) compared with the values after August (Min-Max: 18.1-$35.0^{\circ}C$, 26.5-96.2% RH) (p<0.05); however, there was no significant correlation between the two parameters. The ratio of calcium activity to total calcium concentration decreased after August compared with the values in June and July (p<0.05). The calcium activity in fresh milk was positively correlated with milk yield (r = 0.45, p<0.01) and negatively correlated with milk lactose content (r = -0.53, p<0.01). These results suggest that the calcium activity in milk could be affected by ambient temperature and might be associated with milking production in hot season.

Enhanced Piezoelectric Properties of (1-x)[0.675BiFeO3-0.325BaTiO3]-xLiTaO3 Ternary System by Air-Quenching

  • Akram, Fazli;Malik, Rizwan Ahmed;Lee, Soonil;Pasha, Riffat Asim;Kim, Myong Ho
    • Korean Journal of Materials Research
    • /
    • v.28 no.9
    • /
    • pp.489-494
    • /
    • 2018
  • Lead free $(1-x)(0.675BiFeO_3-0.325BaTiO_3)-xLiTaO_3$ (BFBTLT, x = 0, 0.01, 0.02, and 0.03, with 0.6 mol% $MnO_2$ and 0.4 mol% CuO) were prepared by a solid state reaction method, followed by air quenching and their crystalline phase, morphology, dielectric, ferroelectric and piezoelectric properties were explored. An X-ray diffraction study indicates that lithium (Li) and tantalum (Ta) were fully incorporated in the BFBT materials with the absence of any secondary phases. Dense ceramic samples (> 92 %) with a wide range of grain sizes from $3.70{\mu}m$ to $1.82{\mu}m$ were obtained in the selected compositions ($0{\leq}x{\leq}0.03$) of BFBTLT system. The maximum temperatures ($T_{max}$) were mostly higher than $420^{\circ}C$ in the studied composition range. The maximum values of maximum polarization ($P_{max}{\approx}31.01{\mu}C/cm^2$), remnant polarization ($P_{rem}{\approx}22.82{\mu}C/cm^2$) and static piezoelectric constant ($d_{33}{\approx}145pC/N$) were obtained at BFBT-0.01LT composition with 0.6 mol% $MnO_2$ and 0.4 mol% CuO. This study demonstrates that the high $T_{max}$ and $d_{33}$ for BFBTLT ceramics are favorable for industrial applications.

Magnetic Properties of NdFeB Powders Prepared by Mechanical Alloying (기계적합금법으로 제조한 NdFeB계 분말의 자기적 성질)

  • Kim, Taek-Soo;Hwang, Yeon;Lee, Hyo-Sook
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.4
    • /
    • pp.210-215
    • /
    • 1998
  • $Nd_{15}Fe_{77}B_8$ and $Nd_{16}Fe_{76}B_8$ powders were prepared by mechanical alloying in Ar atmosphere, and their phases and magnetic properties were investigated with as a function of the annealing temperature. It was found that the mechanical alloyed $Nd_{16}Fe_{76}B_8$ powder for 450 hours was amorphous phase with a part of $\alpha$-Fe crystallites. The obtained powders at 700 $^{\circ}C$ for 30 minute resulted in two phase of $Nd_2Fe_{14}B$ and $NdB_6$ by the solid-state reaction. The mechanical alloyed $Nd_{16}Fe_{76}B_8$ powder for 450 hour and annealed at 700 $^{\circ}C$ for 30 minute was showed $_iH_c\;of\;9.91\;kOe,\; B_{max}\;of\;12.93\;kG,\;Br\;of\;7.6\;kG\;and\;(BH)_{max}\;10.1\;MGOe$.

  • PDF

Tribological Properties of Raction-Bonded SiC-Graphite Composites (반응소결 SiC-graphite 복합체의 마찰마모특성)

  • 백용혁;신종윤;곽효섭;박용갑
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.5
    • /
    • pp.479-484
    • /
    • 1996
  • The tribological properties of ceramics are very important in the application to engineering ceramic parts such as mechanical seal slurry valve disc and so on. In this study the effect of graphite addition on the mechanical and tribological properties of RBSC/graphite composites were investigated. The composites were prepared by adding graphite powder to the mixture of SiC powder metallic siliconcarbon black and alumina. Bending strength water absorption friction coefficient the amount of worn out material at a certain time and maximum surface roughness(Rmax) of the prepared composites were measured and crystalline phases were examined with XRD. The composite containing 5 vol% graphite powder showed improved bending strength due to high green density and decreased friction coefficient and wear resistance. The friction coefficient and the wear resistance of the composite were increased by adding graphite powder up to 10 vol% They decreased however as increasing the amount of graphite powder more that 10vol% There was no linear relationship between the tribological properties and bending strength of the composites.

  • PDF

A Study on Video Encoder Design having Pipe-line Structure (파이프라인 구조를 갖는 비디오 부호화기 설계에 관한 연구)

  • 이인섭;이선근;박규대;박형근;김환용
    • Proceedings of the IEEK Conference
    • /
    • 2001.06e
    • /
    • pp.169-172
    • /
    • 2001
  • In this paper, it used a different pipeline method from conventional method which is encoding the video signal of analog with digital. It designed with pipeline structure of 4 phases as the pixel clock ratio of the whole operation of the encoder, and secured the stable operational timing of the each sub-blocks, it was visible the effect which reduces a gate possibility as designing by the ROM table or the shift and adder method which is not used a multiplication flag method of case existing of multiplication of the fixed coefficient. The designed encoder shared with the each sub-block and it designed the FPGA using MAX+PLUS2 with VHDL.

  • PDF

Bonding and Elastic Properties in Ti2AC (A = Ga or Tl)

  • Kang, Dae-Bok
    • Journal of the Korean Chemical Society
    • /
    • v.57 no.1
    • /
    • pp.35-39
    • /
    • 2013
  • The chemical bonding and elastic properties of $Ti_2AC$ (A = Ga, Tl) have been investigated by means of extended H$\ddot{u}$ckel tight-binding band structure calculations. The bulk modulus of $Ti_2AC$ decreases as Ga is replaced with Tl at the A sites. This can be understood by considering the relative strength of Ti-A bonds resulting from the different atomic size of 3A-group elements. The analysis of the projected density of states (PDOS) and the crystal orbital overlap population (COOP) for the respective phases shows that Ti-Ga bonds in $Ti_2GaC$ are stronger than Ti-Tl bonds in $Ti_2TlC$.

Synthesis and Properties of Di-azomesogenic Liquid Crystal Compounds with Terminal Substituents (말단에 치환기를 갖는 이-아조메소젠 액정화합물의 합성 및 성질)

  • Park, Jong-Ryul;Gu, Su-Jin;Yoon, Doo-Soo;Bang, Moon-Soo;Choi, Jae-Kon
    • Applied Chemistry for Engineering
    • /
    • v.26 no.6
    • /
    • pp.698-705
    • /
    • 2015
  • Two series of symmetric dimesogenic compounds containing a butylene or 1-methylbutylene spacer as a flexible group were synthesized. The mesogenic groups of synthesized compounds consist of an azobenzene group with a terminal substituent. Chemical structures as well as, thermal, mesomorphic, and photochemical properties of the synthesized compounds were investigated using FT-IR, $^1H-NMR$, differential scanning calorimetry (DSC), polarizing optical microscopy (POM), and UV-visible spectrometry. P-H, P-F, and $P-OC_6H_{13}$ showed monotropic liquid crystal phases, whereas the others showed enantiotropic liquid crystal phases. Compounds with butylene group as a flexible spacer exhibited wider mesophase temperature ranges and higher thermal transition temperatures than compounds containing a 1-methylbutylene group. Compounds with a high absolute value of the Hammett substituent constant exhibited high thermal transition temperatures and improved stability in the liquid crystal phase. Furthermore, in the absence or presence of UV light illumination, terminal substituents of the azomesogenic group were important factors in deciding the maximum absorbance wavelength (${\lambda}_{max}$) and the rate of photoisomerization (K).

Micro-EDM Feasibility and Material Properties of Hybrid Ti2AlC Ceramic Bulk Materials (하이브리드 Ti2AlC 세라믹 소결체의 재료특성 및 Micro-EDM 유용성 연구)

  • Jeong, Guk-Hyun;Kim, Kwang-Ho;Kang, Myung-Chang
    • Journal of Powder Materials
    • /
    • v.21 no.4
    • /
    • pp.301-306
    • /
    • 2014
  • Titanium alloys are extensively used in high-temperature applications due to their excellent high strength and corrosion resistance properties. However, titanium alloys are problematic because they tend to be extremely difficult-to-cut material. In this paper, the powder synthesis, spark plasma sintering (SPS), bulk material characteristics and machinability test of hybrid $Ti_2AlC$ ceramic bulk materials were systematically examined. The bulk samples mainly consisted of $Ti_2AlC$ materials with density close to theoretical value were synthesized by a SPS method. Random orientation and good crystallization of the $Ti_2AlC$ was observed at $1100^{\circ}C$ for 10 min under SPS sintering conditions. Scanning electron microscopy results indicated a homogeneous distribution and nano-laminated structure of $Ti_2AlC$ MAX phase. The hardness and electrical conductivity of $Ti_2AlC$ were higher than that of Ti 6242 alloy at sintering temperature of $1000^{\circ}C{\sim}1100^{\circ}C$. Consequently, the machinability of the hybrid $Ti_2AlC$ bulk materials is better than that of the Ti 6242 alloy for micro-EDM process of micro-hole shape workpiece.

The Effect of Magnetic Field Treatment on Enhanced Exchange Coupling of $Nd_{2}Fe_{14}B/Fe_{3}B$ Magnet (자장중 열처리에 의한 $Nd_{2}Fe_{14}B/Fe_{3}B$ 초미세립 복합자성상의 자기특성 향상)

  • 박언병;양충진
    • Journal of the Korean Magnetics Society
    • /
    • v.6 no.2
    • /
    • pp.80-85
    • /
    • 1996
  • An externally applied magnetic field during annealing the $Nd_{2}Fe_{14}B/Fe_{3}B$ based spring magnet was found to enhance the exchange coupling between the hard and soft magnetic grains. More than 30 % increase in remanence values for melt-spun $Nd_{4}Fe_{73.5}Co_{3}(Hf_{1-x}-Ga_{x})B_{18.5}$(x=0, 0.5, 1.0) alloys was resulted from uniform distribution of $Fe_{3}B$, $\alpha$-Fe as well as $(Nd_{2}Fe_{14}B)$, and also from reduced grain size of those phases by 20 %. The result also showed that there is an optimum grain size exhibiting a high coercivity value which will be discussed in terms of previously simulated exchange coupling parameter.

  • PDF