• Title/Summary/Keyword: Low temperature treatment

Search Result 1,963, Processing Time 0.03 seconds

Synthesis of zeolite A from coal fly ash by alkali fusion followed by hydrothermal treatment (알칼리 용융 및 수열 합성에 의한 석탄회로부터 제올라이트 A의 합성)

  • Jeong, Ji-Baek;Choi, Ko-Yeol
    • Journal of the Korean Applied Science and Technology
    • /
    • v.32 no.2
    • /
    • pp.240-247
    • /
    • 2015
  • Zeolite A was prepared from coal fly ash upon NaOH fusion treatment, followed by hydrothermal treatment. The effects of treatment conditions such as NaOH/ash ratio, fusion temperature, the amount of sodium aluminate added, hydrothermal treatment temperature and time on the type and the crystallinity of zeolites were investigated. The optimal NaOH/ash weight ratio and fusion temperature to produce high crystalline zeolite A were 1.2 and $550^{\circ}C$, respectively. The dissolution of $Si^{4+}$ and $Al^{3+}$ from the fused fly ash was not affected by stirring time. The type of synthetic zeolites was found to be dependent on the amount of sodium aluminate added. The low amount of sodium aluminate favored zeolite X, while a single phase zeolite A was produced by increasing the amount sodium aluminate. Zeolite A was transformed into hydroxysodalite with increasing hydrothermal treatment time and temperature. A high crystalline zeolite A could be obtained by decreasing the temperature increasing time up to the reaction temperature.

Effects of different heating conditions on protein composition in each muscle type of yellowtail (Seriola quinqueradiata)

  • Furuta, Ayumi;Hamakawa, Yumi;Ishibashi, Chinami;Mabuchi, Ryota;Tanimoto, Shota
    • Fisheries and Aquatic Sciences
    • /
    • v.25 no.1
    • /
    • pp.31-39
    • /
    • 2022
  • To clarify the factors influencing the physical properties of fish after heat treatments, we investigated changes in the properties of proteins in the dorsal ordinary and dark muscle of yellowtail (Seriola quinqueradiata) heated under different conditions commonly used for the purposes of food hygiene. High-temperature/short-time heating (85℃ for 90 s and 75℃ for 60 s) affected the protein solubility more than low-temperature/long-time heating (63℃ for 30 min). Sodium dodecyl sulphate-polyacrylamide gel electrophoresis and differential scanning calorimetry showed that low-temperature/long-time heating reduced the degree of actin denaturation in fish compared with that by other heating conditions. In addition, collagen solubility was enhanced with low-temperature/long-time heating. Therefore, these results suggest that differences in the degree of actin and collagen denaturation are responsible for the enhanced meat tenderness and diminished meat shrinkage, resulting from low-temperature/long-time heating.

Hydrophilic Modification of Polypropylene Hollow Fiber Membrane by Dip Coating, UV Irradiation and Plasma Treatment

  • Kim Hyun-Il;Kim Jin Ho;Kim Sung Soo
    • Korean Membrane Journal
    • /
    • v.7 no.1
    • /
    • pp.19-27
    • /
    • 2005
  • PP hollow fiber membrane was hydrophilized by EVOH dip coating followed by low temperature plasma treatment and UV irradiation. EVOH coating attained high water flux without any prewetting but its stability did not guaranteed at high water permeation rate. At high water permeation rate, water flux declined gradually due to swelling and delamination of the EVOH coating layer causing pore blocking effect. However, plasma treatment reduces the swelling, which suppress delamination of the EVOH coating layer from PP support result in relieving the flux decline. Also, UV irradiation helped the crosslinking of the EVOH coating layer to enhance the performance at low water permeation rate. FT-IR and ESCA analyses reveal that EVOH dip coating performed homogeneously through not only membrane surface but also matrix. Thermogram of EVOH film modified plasma treatment and W irradiation show that crosslinking density of EVOH layer increased. Chemical modification by plasma treatment and UV irradiation stabilized the hydrophilic coating layer to increase the critical flux of the submerged membrane.

Germination Characteristics in Seeds of Broussonetia kazinoki Siebold ex Siebold & Zucc (Moraceae) Native to East Asia (동아시아 특산식물 애기닥나무 Broussonetia kazinoki Siebold ex Siebold & Zucc (Moreaceae) 종자의 발아특성)

  • Kim, Gun Mo;Chung, Jae Min;Jung, Ji Young;Choi, Hyeok Jae;Lee, Seung Youn
    • Korean Journal of Plant Resources
    • /
    • v.35 no.1
    • /
    • pp.36-43
    • /
    • 2022
  • This research was conducted to develop a seed propagation protocol for the use of Broussonetia kazinoki Siebold ex Siebold & Zucc, which native to East Asia. Light and temperature conditions, GA3 treatment, and low-temperature stratification were performed to evaluate the germination characteristics. The germination percentage at 4, 15/6, 20/10 and 25/15℃ was 0, 42. 5, 44. 4 and 91.7%, respectively. Thus, the optimal germination temperature of the B. kazinoki seeds was 25/15℃. Although germination was delayed by relatively low temperature conditions, GA3 treatment allowed for increased germination rates even under the low temperature conditions. Cold stratification reduced time to germination. Relatively low germination percentages at 20/10℃ and 15/6℃ indicated that the seeds had been under the state of conditional dormancy. Through this study, B. kazinoki seeds have conditional dormancy because they can be germinated through GA3 treatment even under relatively low temperature conditions and it is judged that it will support the commercial propagation practice in the future.

Effect of Color Developing by Water Treatment on Cotton Fabrics Dyed with Persimmon Extract (감물염색 면직물의 물에 의한 발색 효과)

  • Kim, Ok soo;Jang, Jeong dae
    • Fashion & Textile Research Journal
    • /
    • v.19 no.5
    • /
    • pp.646-652
    • /
    • 2017
  • In order to clarify an availability of water treatment for persimmon extract dyeing, effect of color developing by water treatment process on cotton fabrics dyed with persimmon extract was investigated. Dyed fabrics were dipped still water and circulation water in various temperature. Concerning water color developing, still water color developing and circulation water color developing have been examined, and the temperature of water has been apprehended to prepare an effective basis of water color development. The surface color based on circulation water color development displays low values of $a^{\ast}$ and $b^{\ast}$, and the range of the c value(Munsell chroma) is narrow and has the value of 2 to 3, thus displays the coloration of a dark tone. The effect of temperature in water color development was insignificant, due to the small difference in temperature from $20^{\circ}C$ to $40^{\circ}C$. At $80^{\circ}C$, remarkable color development manifested, which is evidence of the high influence of temperature. The effects of circulation were clear at low temperatures, and the effects of temperature highly manifested at high temperatures. Circulation water color development display great color development at all temperatures to allow industrial color development with the absence of sunlight, thereby having an effect of energy reduction and developing color in dark tones, however this also is a strength of persimmon extract concerning color diversification, and is judged to have great value of industrial and practical application.

The Effects of Processing Parameters on Surface Hardening Layer Characteristics of Low Temperature Plasma Nitriding of 316L Austenitic Stainless Steel (316L 오스테나이트계 스테인리스강의 저온 플라즈마질화처리시 공정변수가 표면경화층 특성에 미치는 영향)

  • Lee, Insup
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.4
    • /
    • pp.194-202
    • /
    • 2019
  • A systematic investigation was made on the influence of processing parameters such as gas composition and treatment temperature on the surface characteristics of hardened layers of low temperature plasma nitrided 316L Austenitic Stainless Steel. Various nitriding processes were conducted by changing temperature ($370^{\circ}C$ to $430^{\circ}C$) and changing $N_2$ percentage (10% to 25%) for 15 hours in the glow discharge environment of a gas mixture of $N_2$ and $H_2$ in a plasma nitriding system. In this process a constant pressure of 4 Torr was maintained. Increasing nitriding temperature from $370^{\circ}C$ to $430^{\circ}C$, increases the thickness of S phase layer and the surface hardness, and also makes an improvement in corrosion resistance, irrespective of nitrogen percent. On the other hand, increasing nitrogen percent from 10% to 25% at $430^{\circ}C$ decreases corrosion resistance although it increases the surface hardness and the thickness of S phase layer. Therefore, optimized condition was selected as nitriding temperature of $430^{\circ}C$ with 10% nitrogen, as at this condition, the treated sample showed better corrosion resistance. Moreover to further increase the thickness of S phase layer and surface hardness without compromising the corrosion behavior, further research was conducted by fixing the $N_2$ content at 10% with introducing various amount of $CH_4$ content from 0% to 5% in the nitriding atmosphere. The best treatment condition was determined as 10% $N_2$ and 5% $CH_4$ content at $430^{\circ}C$, where the thickness of S phase layer of about $17{\mu}m$ and a surface hardness of $980HV_{0.1}$ were obtained (before treatment $250HV_{0.1}$ hardness). This specimen also showed much higher pitting potential, i.e. better corrosion resistance, than specimens treated at different process conditions and the untreated one.

Effect of Low Temperature Heat Treatment on the Physical and Chemical Properties of Carbon Anode Materials and the Performance of Secondary Batteries (저온 열처리가 탄소 음극재의 물리·화학적 특성 및 이차전지 성능에 미치는 영향)

  • Whang, Tae Kyung;Kim, Ji Hong;Im, Ji Sun;Kang, Seok Chang
    • Applied Chemistry for Engineering
    • /
    • v.32 no.1
    • /
    • pp.83-90
    • /
    • 2021
  • In this study, effects of the physical and chemical properties of low temperature heated carbon on electrochemical behavior as a secondary battery anode material were investigated. A heat treatment at 600 ℃ was performed for coking of petroleum based pitch, and the manufactured coke was heat treated with different heat temperatures at 700~1,500 ℃ to prepare low temperature heated anode materials. The physical and chemical properties of carbon anode materials were studied through nitrogen adsorption and desorption, X-ray diffraction (XRD), Raman spectroscopy, elemental analysis. Also the anode properties of low temperature heated carbon were considered through electrochemical properties such as capacity, initial Coulomb efficiency (ICE), rate capability, and cycle performance. The crystal structure of low temperature (≤ 1500 ℃) heated carbon was improved by increasing the crystal size and true density, while the specific surface area decreased. Electrochemical properties of the anode material were changed with respect to the physical and chemical properties of low temperature heated carbon. The capacity and cycle performance were most affected by H/C atomic ratio. Also, the ICE was influenced by the specific surface area, whereas the rate performance was most affected by true density.

Effect of Prior Deformation on the Martensitic Transformation Temperature(Ms) and Reversed Martensitic Transformation Temperature(As) in Fe-Ni Alloy (Fe-Ni합금(合金)의 마르텐사이트변태온도(變態溫度)(Ms)와 역변태온도(逆變態溫度)(As)에 미치는 소성가공(塑性加工)의 영향(影響))

  • Shon, In-Jin;Nam, Kee-Seok
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.3 no.4
    • /
    • pp.41-52
    • /
    • 1990
  • This research has been performed in order to investigate the effect of prior deformation on the Ms temperature and reversed As of Fe-Ni alloy. The Ms temperature rose with increment of strain to 30% but lowered over 50%. It can be analysed that martensitic transformation was promoted by partial dislocation in low strain, but suppressed by dislocation cell structures in high strain. The As temperature was substantially increased with higher deformation to 20% but slowly above 50%. It may be caused that as the transition bands formed by deformation constrained shear strain, therefore austenitic transformation was hindered.

  • PDF

The Effects of Ni Content on Mechanical and Oxidation Resistance Properties of B2-NiAl Intermetallic Compounds (B2-NiAl 금속간 화합물의 기계적 성질 및 내산화성에 미치는 Ni함량의 영향)

  • Oh, Chang-Sup;Han, Chang-Suk
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.26 no.1
    • /
    • pp.1-6
    • /
    • 2013
  • The B2-ordered NiAl has attracted much attention as one of the candidates as a next generation high temperature material, because it has a high melting temperature, a low specific gravity and an excellent high temperature oxidation resistance. However, the application of NiAl to structural materials needs the improvement of its brittleness at room temperature. The study was carried out on the relation between several properties of NiAl and some variation of Ni content within NiAl phase, which means deviations from the stoichiometric composition. The main results were as follows; (i) Good ductility was obtained at the testing temperature more than 1073 K irrespective of Ni content. (ii) Increasing Ni content offered preferable tensile properties. (iii) Every NiAl with varying Ni contents showed the superior oxidation resistance.

Influence of Heat Treatment on Brazing Characteristics between Cemented Carbides and Steel (초경합금과 강의 Brazing특성에 미치는 열처리의 영향)

  • Kim Ha Young;Nakamura Mitsuru;Lee Sang Hak
    • Proceedings of the KWS Conference
    • /
    • v.43
    • /
    • pp.43-45
    • /
    • 2004
  • Brazing between cemented carbides and steel for tool investigated by copper alloy brazing filler. Copper alloy filler was high liquidus temperature($990^{\circ}C$), therefor the shank(steel) occurred softening. Because brazing sample was necessary to heat treatment after brazing process. This experiment, influence of austenite time and purge temperature on heat treatment were investigated. As a result, these treatments obtained to high deflective strength In case of austenite time was short and purge temperature was low. Especially, nitride precipitated brazing layers was strongly influenced by the deflective strength.

  • PDF