• 제목/요약/키워드: Low heat cement

검색결과 212건 처리시간 0.037초

온도균열 저감공법을 복합사용한 매스콘크리트의 현장적용 (Field Application of the Mass Concrete Utilizing Combined Method for Temperature Crack Reduction)

  • 한상윤;이충섭;백대현;장덕배;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2010년도 춘계 학술논문 발표대회 1부
    • /
    • pp.37-39
    • /
    • 2010
  • In this study, with new office construction site of S Construction company as subject, to solve all the problems according to reduced hydration heat and temperature crack of mass concrete used mat foundation and placing time difference, low heat combination of coarse particle cement and fly-ash and setting time difference applied AE water reducing agent, and to prevent the early frost damage caused by low outdoor temperature, a heat insulation method using double bubble sheet was conducted. As a result, it was found that hydration heat and setting time difference was reduced by applying a low heat combination and setting time difference construction method, and that the high insulation capability of the double bubble sheet was able to not only prevent the early frost damage but also reduce temperature difference between the central part and the upper part of mass concrete.

  • PDF

수직 밀폐형 자중 열교환기용 뒤채움재의 열전도 및 점도특성 연구 (Experimental Study on Thermal Conductivity and Viscosity of Grouts for Backfilling Ground Heat Exchanger)

  • 최항석;이철호;길후정;최효범;우상백
    • 신재생에너지
    • /
    • 제3권4호
    • /
    • pp.38-46
    • /
    • 2007
  • In order to characterize the thermal conductivity and viscosity of grout materials used for backfilling ground heat exchangers, nine bentonite grouts and cement grouts being adapted in the United State have been considered in this study. The bentonite grouts indicate that the thermal conductivity and viscosity increase with the content of bentonite or filler (silica sand). In addition, material segregation can be observed when the viscosity of grout is relatively low. The saturated cement grouts appear to possess much higher thermal conductivity than the saturated bentonite grouts, and the reduction of thermal conductivity in the cement grouts after drying specimens is less than the case of the bentonite grouts. Maintaining the moisture content of grouts is a crucial factor in enhancing the efficiency of ground heat exchangers.

  • PDF

수직 밀페형 지증 열교환기용 뒤채움재의 열전도 및 점도특성 연구 (Experimental Study on Thermal Conductivity and Viscosity of Grouts for Backfilling Ground Heat Exchanger)

  • 최항석;이철호;길후정;최효범;우상백
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2007년도 추계학술대회 논문집
    • /
    • pp.529-532
    • /
    • 2007
  • In order to characterize the thermal conductivity and viscosity of grout materials used for backfilling ground heat exchangers, nine bentonite grouts and cement grouts being adapted in the United State have been considered in this study. The bentonite grouts indicate that the thermal conductivity and viscosity increase with the content of bentonite or filler (silica sand). In addition, material segregation can be observed when the viscosity of grout is relatively low. The saturated cement grouts appear to possess much higher thermal conductivity than the saturated bentonite grouts, and the reduction of thermal conductivity in the cement grouts after drying specimens is less than in case of the bentonite grouts. Maintaining the moisture content of grouts is a crucial factor in enhancing the efficiency of ground heat exchangers.

  • PDF

벨라이트시멘트를 사용한 콘크리트의 강도특성에 대한 실험적 연구 (An Experimental Study on the Strength of Concrete Using the Belite Cement)

  • 문한영;문대중;하상욱;김기수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.61-64
    • /
    • 1997
  • As construction technology advances, most of concrete structures are becoming larger and taller. Therefore, high strength and quality concrete is necessary for them. So, the proposal of using belite cement is investigated to satisfy high flowing, low heat, and high strength. In this study, the compressive strength, tensile strength, and modulous of elasticity of concrete using belite cement was considered according to the mix proposition condition as a water-cement ratio, unit cement content, and sand percentage.

  • PDF

개질 처리된 저발열 슬래그시멘트 특성에 관한 연구 (The research about properties of modified low heat slag cement)

  • 김홍주;김원기;김훈상;이원준;신진호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.677-680
    • /
    • 2008
  • 저발열형 고로슬래그 시멘트의 초기강도 발현 특성을 향상시키기 위하여 낮은 분말도의 고로슬래그 분말과 보통 포틀랜드시멘트를 혼합 분쇄하여 입자 표면을 개질하였다. 사전 분쇄한 고로슬래그 분말의 비표면적은 $2535cm^2/g$(BS2), $3245cm^2/g$(BS3)의 2가지를 사용하였으며, 고로슬래그 분말과 시멘트를 진동밀에 투입하여 10분부터 30분까지 혼합 분쇄하여 표면을 개질하였다. 시멘트에 대한 고로슬래그 분말의 혼합비는 60$^{\sim}$80%의 3수준으로 변화시켰으며 혼합분쇄 후 비표면적의 변화, 입도분표, 시멘트의 수화열, 몰탈의 압축강도를 측정하였다. 시판 삼성분계 저발열 시멘트(LHC)와 비교시험 결과, 7일 압축강도발현의 100%이상과 72시간 누적수화열 170J/g 이하의 값을 만족하는 배합 및 혼합분쇄 시간을 찾을 수 있었으며 저분말도 고로슬래그를 다량으로 활용한 저발열 슬래그시멘트의 가능성을 확인하였다.

  • PDF

개량형 3성분계 결합재를 사용한 조강형 저탄소 콘크리트의 기초적 특성 (A Engineering Properties of High Early Strength Low Carbon Concrete Using Modified Ternary Blended Cement)

  • 최현규;한상윤;김경민;박상준;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 추계 학술논문 발표대회
    • /
    • pp.55-56
    • /
    • 2011
  • This study is to investigate the engineering properties of low heat concrete incorporating improved ternary blended cement by combining OPC(original portland cement), blast furnace slag and fly ash. The results were summarized as following ; For ITB(Improved Ternary Blend)mixture was that setting time proved to be accelerated, and adiabatic temperature rises were low. The use of ITB resulted in an increase of initial compressive strength.

  • PDF

환원슬래그를 사용한 모르타르의 저온에서의 초기동해 방지에 관한 기초적 실험 (A Fundamental Experiment on Preventing Frost Damage at Early Age of Mortar in Low Temperature using Reduction Slag)

  • 민태범;문영범;김형철;최현국;김재영;이한승
    • 한국건축시공학회지
    • /
    • 제16권1호
    • /
    • pp.1-7
    • /
    • 2016
  • 본 연구에서는 $-5^{\circ}C$이하에서도 가열 양생이 없이 수화 반응시 수화열이 높게 발생되는 환원슬래그를 시멘트 분체와 치환사용 하여 영하의 온도에서도 콘크리트의 자체 발열로 인해 압축강도를 재령 3일 이내 5MPa를 발현시켜 초기동해를 방지시키는 것이 최종 연구의 목적이며 이에 대하여 환원슬래그의 물리적 특성 평가와 열적 특성 평가를 실시한 결과 환원슬래그는 높은 수화열을 발생시키기 때문에 저온에서도 압축강도 발현이 우수함을 알 수 있었다. 이는 환원 슬래그의 성분 중 $C_{12}A_7$$C_3A$에 의해 수화열이 높게 발생됨 저온에서도 압축강도가 발현되는 것으로 나타났다. 하지만 환원슬래그 단독 치환하였을 경우 $SO_3$함량 부족으로 급결이 발생하는 것을 알 수 있었다. 급결을 방지하기 위해서는 석고의 사용이 필수적으로 사용되어야 한다. 따라서 본 연구 결과 환원슬래그와 석고를 3성분계로 사용하였을 경우 저온에서도 재령 3일에서 5MPa 압축강도를 나타나는 것으로 보아 저온에서도 콘크리트의 초기동해를 방지할 수 있을 것으로 판단된다.

A Study on the High-Flowing Concrete with Low Unit Weight of Cement

  • Si Woo Lee;Hong Shik Choi;Sang Chel Kim;Gweon Heo
    • The Korean Journal of Ceramics
    • /
    • 제6권3호
    • /
    • pp.318-321
    • /
    • 2000
  • Most compressive strengths commonly used in the construction field are in a range of 240 to 300 kgf/$\textrm{cm}^2$ at 28 days. To get this rage of strengths, however, high-flowing concrete requires cementitious binders more than 400 to 450 kg/$\textrm{cm}^2$ for preventing segregation and sedimentation of aggregates. This amount of cementitious binder generates a large emission of excessive hydration heat, which may consequently induce harmful cracks in concrete structure. In order to reduce excessive hydration heat, thus, this paper aims at fabricating a high-flowing concrete under the condition that cement content is kept as low as 350kg/$\textrm{cm}^3$ by using viscose agents. In a parametric study, effects of cement types such as a ternary blended cement and Type V on he physical characteristics of high-flowing concrete were evaluated. In addition, the influence of viscosity was also investigated by applying two different viscose agents, one in a range of 6,000 to 10,000 cps and the others of 10,000 to 14,000 cps. In terms of chemical admixtures used in concrete mixture, the superplasticizer was Sulfonated Melamine-Formaldehyde Condensate with about 30,000 of molecular weight, and main component of viscose agent was HPMC (Hydroxy Propyl Methyl Cellulose). Slump flow was fixed at 50cm with different dosages of superplasticizer in weight.

  • PDF

원전 방사화 폐기물 저감을 위한 저방사화 시멘트의 개발 (Development of Low-activation Cement for Decreasing the Activated Waste in Nuclear Power Plant)

  • 이빛나;이종석;민지영;이장화
    • 한국건설순환자원학회논문집
    • /
    • 제5권3호
    • /
    • pp.223-229
    • /
    • 2017
  • 원전 구조물에 주로 사용되는 중량 콘크리트의 경우 중성자에 오랜 시간 노출되면 콘크리트 자체가 방사선을 방출하는 방사화가 발생하게 된다. 이러한 경우 원전 구조물 해체시 많은 양의 방사성 폐기물이 발생되고 이를 처리하기 위한 비용이 큰 폭으로 증가하게 된다. 따라서, 본 연구에서는 원전 해체시 폐기물의 처리비용을 저감하기 위하여 방사화에 밀접한 관련이 있는 Eu 및 Co를 포함하고 있는 시멘트를 대상으로 저방사화 시멘트를 제작하였다. 또한, 저방사화 시멘트 개발을 위하여 원재료 수급부터 제조방법을 제안하였으며 이를 일반 시멘트 및 저발열 시멘트와 비교 분석하였다. 방사화 분석 결과 Eu는 검출되지 않았으며, Co는 3.75ppm으로 보통포틀랜드 시멘트보다 낮게 측정되었으며, 물리적 화학적 특성 역시 1종 보통포틀랜드 시멘트와 4종 저발열 포틀랜드 시멘트 기준에 부합하는 것으로 나타났다.

고강도용 콘크리트의 온도상승 저감대책 (The Reduction of Temperature Rise in High Strength Concrete)

  • 문한영;문대중;하상욱;서정우
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 가을 학술발표회 논문집
    • /
    • pp.133-139
    • /
    • 1996
  • As construction technology advances, most of civil engineering structures are becoming larger and taller. Therefore, high strength concrete is necessary for them. For high strength concrete, it needs a large amount of unit cement content and low water-cement ratio inevitably, so that a large amount of heat occurs in concrete. The thermal cracks make the durability and quality of concrete structures become worse, result from temperature rise and thermal stress due to heat of hydration. In this study, the proposal of using ground granulated blast furnace slag, fly ash and chemical admixtures was investigated to decrease the temperature rise of concrete.

  • PDF