• 제목/요약/키워드: Low O/F Ratio

검색결과 114건 처리시간 0.029초

3% NaCl 수용액중에서 복합조직강의 부식피로 파괴거동에 미치는 주파수변화의 영향 (The Influence of the Changing of Cyclic Frequency on the Corrosion Fatigue Fracture Behavior of the Dual Phase Steel in 3% NaCl Solution)

  • 오세욱;신규동;김웅집
    • 한국해양공학회지
    • /
    • 제9권2호
    • /
    • pp.141-148
    • /
    • 1995
  • Fatigue tests were carried out by a rotary bending testing machine of cantilever type. M.E.F.(ferrite encapsulated islands of martensite) materials were made by a series of heat treatment from a low carbon steel(SM 20 C). The fatigue tests were conducted at stress levels of 302 MPa and with frequencies of 25Hz, 2.5 Hz and 0.5 Hz in 3% NaCl solution. The fatigue strength increased with frequency got higher. The microcracks and corrosion pits were generated at the boundary between the matrix and the 2nd phase. The cracks generated by the corrosion pits were coalesced with the pits around the notch and became the initial crack. The $N_i/N_f$ ratio increased as the frequency and stress level decreased. The interference phenomenon increased with stress level and frequency gots higher. The crack propagation rate was delayed as the stress level lowers and the frequency gets higher, however, the range of the stress intensity factor depended only on a stress level.

  • PDF

IC용 초정밀 박막저항소자의 제조와 특성연구 (Preparation of Precision Thin Film Resistor Sputtered by Magnetron Sputtering)

  • 하흥주;장두진;문상용;박차수;조정수;박정후
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 하계학술대회 논문집 C
    • /
    • pp.1236-1238
    • /
    • 1994
  • TiAlN thin films were prepared by a multi target r.f magnetron sputtering system under different conditions. We have investigated the resistivity and T.C.R. (Temperature Coefficient of Resistance) characteristics of TiAlN films deposited on $Al_2O_3$ and glass substrates by sputtering in an $Ar:N_2$ gas mixture. We used Al and Ti metal as Target Material and $Ar:N_2$ gas as working gas. We varied the partial pressure ratio of $N_2/Ar$ from 0.2/7 to 1.0/6.2 (SCCM). And the R.F power of Ti and Al Target also were varied as 160/240, 200/200 and 240/160(W). In this experiment, we can get the precision thin film resistor with a very low T.C.R. (Temperature Coefficient of Resistance) below 25 ppm ${\Omega}/^{\circ}C$.

  • PDF

메타카올린을 혼합한 재생골재 콘크리트의 역학적 특성 및 동결융해 저항성 (Mechanical Properties and Resistance to Freezing and Thawing of the Recycled Aggregate Concrete with Metakaolin)

  • 문한영;김양배;문대중
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제9권4호
    • /
    • pp.270-278
    • /
    • 2005
  • 재생골재 콘크리트의 강도 및 내구성은 천연골재를 사용한 콘크리트에 비하여 저하되므로 메타카올린을 사용하여 재생골재 콘크리트의 성질을 개선하였다.메타카올린의 주성분은 $SiO_2$$Al_2O_3$이며, 비표면적은 보통시멘트보다 약 9배 정도 크다. 실콘크리트 구조물에서 얻어진 재생골재(DRA)는 KS F 2573의 1종을 만족하였으나, 콘크리트를 제작하여 얻어진 재생골재(SRA)는 KS F 2573의 2종을 만족하지 않았다. 메타카올린을 시멘트 중량에 20% 대체한 경우, SRA 및 DRA를 사용한 콘크리트의 압축강도는 기준콘크리트에 비하여 약 40~64% 정도 크게 나타났다. 메타카올린을 20% 혼합하므로써 재생골재 콘크리트의 흡수율은 메타카올린을 혼합하지 않은 콘크리트에 비하여 약 2% 감소하였다. 또한, DRA를 사용한 콘크리트의 동결 융해 저항성은 메타카올린의 역할로 현저히 향상되었다. 그러나, 메타카올린을 20% 혼합하고 SRA를 사용한 콘크리트의 상대동탄성계수는 동결융해 싸이클 수 210에서 60% 이하로 나타났다.

개심술후에 발생한 지연성 심장압진증 (Deleyed Cardiac Tamponade After Open Heart Surgery (Two Cases Report))

  • 김병열
    • Journal of Chest Surgery
    • /
    • 제15권2호
    • /
    • pp.218-221
    • /
    • 1982
  • Delayed cardiac tamponade in an uncommon and frequently fatal complication after open-heart surgery. We had been experienced two cases of delayed cardiac tamponade as a complication of open-heart surgery and treated successfully by reinsertion of pericardial drain through subxiphoid route. First case was 60 years old female patient and underwent MVR under impression of MSi + Ti Second case was 19 years old male patient and underwent total correction of T.O.F.with Blalock shunt [Lt]. Both cases had Initial symptoms, which were epigastric pain, chest tightness, dropped blood pressure, and increased pulse rate and respiratory rate, mimic as low cardiac output syndrome after open-heart surgery. Roentgenogram of the chest showed a rapid increased cardiothoracic ratio. It is important to realize the presence of late cardiac tamponade for proper diagnosis of complication after open-heart surgery.

  • PDF

졸-겔 스핀코팅법에 의한 반사방지 및 정전기방지 복층막의 제조 및 특성 (Preparation and Characterization of Anti-reflective and Anti-static Double Layered Films by Sol-Gel Spin-Coating Method)

  • 이준종;최세영
    • 한국세라믹학회지
    • /
    • 제34권1호
    • /
    • pp.79-87
    • /
    • 1997
  • 졸-겔 스핀코팅법을 이용하여 VDT 기판에 반사방지 및 정전기방지 복층막을 코팅하고 코팅졸과 겔분말의 특성 및 코팅막의 전기적, 광학적, 기계적 특성을 조사하였다. 1층막은 복층막의 간섭조건을 만족시키는 굴절율을 얻기위해 투명 전도성 재료인 ATO(Antimony doped Tin Oxide) 졸과 SiO2 졸을 몰비 68:32로 혼합한 ATO-SiO2 복합졸을, 2층막에는 저굴절율의 SiO2 졸을 사용하였다. 각 코팅막을 45$0^{\circ}C$에서 30분간 열처리하였을 때 잔류 유기물은 완전히 제거되었다. ATO막의 표면저항은 3mol%의 Sb 첨가시 약 6$\times$107$\Omega$/$\square$로 최소를 나타내었고 SiO2 졸과의 혼합시 약 30mol% 까지는 표면저항이 완만히 증가하다가 그 이후에는 급격히 증가하는 경향을 나타내었으며, 간섭조건을 만족시키는 조성인 32mol%에서는 약 3$\times$108$\Omega$/$\square$를 나타내었다. 복층막의 반사율은 550nm의 기준파장에서 약 0.64%를 나타내었으며 광투과율은 약 3.20% 증가하였다. 복층막의 미소경도는 약 471.4kg.f/mm2로 코팅하지 않은 VDT기판의 경도와 유사한 값을 나타내었다.

  • PDF

Immunoblot법을 이용한 낭미충증(囊尾蟲症)진단에 있어서 각종 항원(抗原)의 적용가능성(適用可能性) 검토(檢討)에 관한 연구(硏究) (Studies on the Applicability of Various Antigen Preparations in the Immunoblot Diagnosis of Cysticercosis)

  • 고영태;주경환;정명숙;임한종
    • 농촌의학ㆍ지역보건
    • /
    • 제16권1호
    • /
    • pp.79-89
    • /
    • 1991
  • A systematic study was conducted to identify and isolate a serologically pertinent antigen with high specific activity and low cross reactivity from Cysticercus parenchymal antigen. Differential centrifugation of the homogenate yield three particulate and one soluble fractions ; the $480{\times}G$ pellets($CyL_2$), the $7650{\times}G$ pellet($CyL_3$), the $100000{\times}G$ pellet($CyL_4$), and $100000{\times}G$ supernatant($CyL_6$). We compared antigenicity of these antigens to that or cystic fluid antigens($CyF_1$), saline extract of cystic wall($CyL_1$), and n-butanol treated $GyL_4$ antigen ($CyL_6$) based on SDS-PAGE and immunoblot techniques. The data obtained were as follows : 1) The ratio of O.D. value of ELISA against cysticercosis positive pool sera to that of negative pool sera was highest when using $CyF_1$ as antigen. However the ratio was relatively low in case of $CyL_{3.4}$ and $CyL_5$. 2) We have noted in previous paper that most strong antigenic activities are present in 63Kd band with low cross reactivities. An effective serologic reagent must contain components that are recognized by most infected sera. 63Kd band met this criteria and could be considered as a reliable band for the diagnosis of cysticercosis. As far as 63Kd band concern, $CyL_5$ showed most strong activities without disturbance of cross reaction by EITB in spite of low applicability to microplate ELISA. 3) $CyL_5$ could detect the serum antibody of cysticercosis even in very low titers, around cut-off values of microplate ELISA, by immunoblot. It also could detect the cross reactivities of Echinococcus species, which showed high absorbance value in micro plate ELISA and some sparganosis cases. Further purification of this antigen will be able to represents a antigen that can be used in the diagnosis of cysticercosis.

  • PDF

촉매 연소기에서 희박 예혼합기의 연소특성 (Combustion Characteristics of Lean Premixed Mixture in Catalytic Combustors)

  • 서용석;강성규;신현동
    • 대한기계학회논문집B
    • /
    • 제22권12호
    • /
    • pp.1681-1690
    • /
    • 1998
  • The aim of this paper is to investigate combustion characteristics of lean premixed mixture stabilized by catalytic surface reaction. The catalytic combustor consisted of a catalyst bed and a thermal combustor. The catalyst bed was made of two stage, Pd catalyst in the first stage and Pt catalyst in the second stage. Auto ignition of lean mixture took place in the thermal combustor. Ignition temperature was about $810{\sim}820^{\circ}C$ at the fuel-air ratio of 1.5~3.0 % and the mixture velocity of 11~18m/sec. The position of flame front in the thermal combustor moved toward back as preheat temperature increased and fuel-air ratio decreased. The f1ame supported by surface reaction was stabilized without any flame stabilizers. NOx emissions from the catalytic combustor were below 2.0 ppm ($O_2$ 15 %) when gas temperature was limited below $1350^{\circ}C$. This result demonstrates that NOx emission from the catalytic combustor is much low comparing with conventional combustors.

낮은 C/N비 하수의 외부 탄소원 주입에 따른 생물학적 질소제거에서 미생물 군집 구조특성 (The Characteristics of Microbial Population Community Structure by an Addition of External Carbon Source in BNR Process for Low C/N Ratio Sewage Treatment)

  • 윤조희
    • 대한환경공학회지
    • /
    • 제30권8호
    • /
    • pp.831-838
    • /
    • 2008
  • 본 연구는 호기조에 유동상 접촉여재를 충전한 실험실 규모의 A$_2$O 공법을 이용하여 낮은 C/N비(COD$_{Cr}$/T-N = 1.24) 하수처리시에 외부 탄소원 주입량 여부에 따른 탈질 및 미생물 군집구조 변화특성을 검토하였다. 미생물 군집구조 특성 분석은 퀴논분석을 이용하여 수행하였다. 실험으로부터 얻어진 결론은 다음과 같다. C/N비가 낮은 유입하수의 미생물 군집특성은 유비퀴논(UQ) 동족체 비율이 UQ-8 > UQ-10 > UQ-9 > 기타의 순으로 감소하고 메나퀴논(MK) 동족체는 UQ 동족체에 비해 존재비(f)가 적고 단순하였다. MK/UQ비는 0.41 이하, 비유사도(D)는 0.26 이하이었다. 외부탄소원 미주입 경우, 각 공정에서의 미생물 군집 특성은 혐기조에서는 퀴논종이 3종으로 MK-8이 우점이고 DQ와 EQ값이 작았다. 무산소조에서는 UQ/MK비가 2.3으로 호기성 미생물의 존재비가 높았다. 호기조에서는 부유성인 경우 우점퀴논이 UQ-7이며, 접촉여재 부착성인 경우 우점 퀴논이 UQ-8이었다. 외부탄소원을 주입한 경우, 미생물 군집 구조특성은 미주입시보다 혐기조에서 MK-8 비가 감소하고 UQ-8비, 퀴논종수, DQ값과 EQ값는 증가하였다. 외부탄소원 주입시 탈질향상은 주로 무산소조에서 일어났으며 UQ/MK비가 2.3에서 1.4으로 감소하였다. 이는 주로 UQ-8의 감소와 MK-7 및 MK-8의 증가에 의한 요인으로 미생물군집구조가 Pseudomonas sp.에서 Bacillus 및 Micrococcus sp. 같은 종의 구조로 변화함을 의미한다. 호기조에서 부유성인 경우 우점퀴논이 UQ-7에서 UQ-8으로, 부착성인 경우 UQ-8에서 UQ-10으로 변하였는데 이는 부유성에서 Nitrosomonas가 부착성에서 Nitrobactor의 존재비가 증가하였음을 의미한다.

에탄올 블렌딩한 과산화수소 추력기의 성능평가 (Performance Evaluation of Ethanol Blended Hydrogen Peroxide Thrusters)

  • 이정섭;권세진
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2012년도 제38회 춘계학술대회논문집
    • /
    • pp.100-103
    • /
    • 2012
  • 친환경 추진제를 사용하는 추력기의 성능 향상을 위해서 미소량의 연료를 첨가하는 블렌딩 기법을 적용하였다. 친환경 추진제로는 90 wt.% 과산화수소를 사용하였으며, 혼합하는 연료는 에탄올을 사용하였다. 혼합비는 98 wt.% 과산화수소의 이론 성능을 상회하는 성능을 갖는 50으로 정하였다. 실험 결과 에탄올 블렌딩한 과산화수소의 반응기 온도가 과산화수소의 단열 분해 온도보다 높았다. 따라서 에탄올 블렌딩을 통해서 성능 증대를 꾀할 수 있었다. 또한 다양한 촉매 및 지지체의 비교를 통해 에탄올 블렌딩한 과산화수소 분해 및 연소에 적합한 촉매 조합을 파악하였다. 실험 결과 백금 촉매가 적합하다고 판단되며 이산화망간 촉매는 재사용 시 불안정성이 증가하였다. 고온 안정성이 높은 ${\alpha}-Al_2O_3$를 지지체로 사용할 경우 촉매의 분해 성능이 낮아 매우 불안정한 성능을 보였다.

  • PDF

End-burning 하이브리드 연소기 인젝터 분사각에 따른 연소 유동장의 수치적 연구 (Numerical Analysis of Combustion Field for Different Injection Angle in End-burning Hybrid Combustor)

  • 윤창진;김진곤;문희장
    • 한국항공우주학회지
    • /
    • 제35권12호
    • /
    • pp.1108-1114
    • /
    • 2007
  • end-burning 연소실의 주요 설계인자들을 구축하기 위해 기존에 수행되었던 인젝터 배열 및 포트 직경 변화, O/F비 변화 외에 산화제 분사각 변화에 따른 연소 특성을 해석하였다. 연료면과 평행한 분사각(Case 1), 연료면을 향해 기울여진 분사각(Case 2)과 노즐을 향해 기울여진 분사각(Case 3)을 설정하여 모델을 구성하였다. 연료면을 향한 분사각의 경우 상류에서 가장 효율적인 혼합특성을 보였으나 상당량의 미연가스가 노즐 밖으로 배출됨을 알 수 있었다. 반면 Case 1과 Case 3은 낮은 혼합특성을 보였으나 연소효율은 연료면을 향한 경우보다 월등한 것으로 판명되었다. Case 1, Case 3 모두 유사한 경향을 나타내었으나 노즐을 향한 Case 3은 짧은 체류시간으로 인해 연료면과 평행한 Case 1에 비해 낮은 연소성능을 갖는 것으로 평가되었다.