Investigation of degradation mechanism of phosphorescent and thermally activated delayed fluorescent organic light-emitting diodes through doping concentration dependence of lifetime

  • Song, Wook;Kim, Taekyung;Lee, Jun Yeob;Lee, Yoonkyoo;Jeong, Hyein
    • Journal of Industrial and Engineering Chemistry
    • /
    • 제68권
    • /
    • pp.350-354
    • /
    • 2018
  • Lifetime study of blue phosphorescent and thermally activated delayed fluorescent organic light-emitting diodes was carried out to understand the dominant degradation process during electrical operation of the devices. Doping concentration dependence of the phosphorescent and thermally activated delayed fluorescent organic light-emitting diodes was studied, which demonstrated long lifetime at low doping concentration in the phosphorescent devices and at high doping concentration in the thermally activated delayed fluorescent devices. Detailed mechanism study of the two devices described that triplet-triplet annihilation is the main degradation process of phosphorescent organic light-emitting diodes, whereas triplet-polaron annihilation is the key degradation factor of the thermally activated delayed fluorescent devices.

야간 시인성 확보를 위한 희토류 첨가 고내구성 장잔광 축광도료 제조에 관한 연구 (A study on the manufacturing of durable and long afterglow phosphorescent paints added with rare earths for night visibility of pavement)

  • 우은석;노윤석;이진호;최용욱;김종기
    • 한국표면공학회지
    • /
    • 제56권2호
    • /
    • pp.152-159
    • /
    • 2023
  • The night visibility of pavement is being considered as a global issue in the field of traffic safety. Although the spreading glass beads on the lane paints has been mainly used to secure night-visibility by utilizing the effect of retroreflection, obvious shortcoming of this method is that retroflection does not occur in the range where the headlights do not reach the glass beads. The use of functional paints including phosphorescent constituents could be a solution for overcoming fore-mentioned problem. SrAl2O4 based chemicals have not only good phosphorescent property, but also are chemically stable compared to existing ZnS based materials. However, this chemicals also need the improvement due to slightly reduced luminous effect in time. Herein, we developed novel paints showing enhanced phosphorescent properties by putting rare earth elements such as Eu, Dy and Y into SrAl2O4. These prepared phosphorescent pigments have displayed improved properties in terms of durability and long afterglow. For instance, the property of afterglow has been persisted after 5 hours with luminace of 20.6 mcd/m2.

축광노면표시의 실내 및 현장 휘도 성능분석과 디지털이미지를 이용한 휘도분석 사전연구 (Performance Analysis of Laboratory and Field Luminance for Phosphorescent Line Marking and Preliminary Study of Luminance Analysis Using Digital Images)

  • 김상태;이용문;김흥래;최기주
    • 한국도로학회논문집
    • /
    • 제18권6호
    • /
    • pp.145-152
    • /
    • 2016
  • OBJECTIVES : Visibility at night can be improved by using retroreflection for short distances and phosphorescent line markings for long distances. In this study, we analyzed the characteristics of the phosphorescent line marking through a laboratory luminance test. Field performance analysis was performed through tests conducted on the road. We also examined the luminance measurement methods using the digital image obtained during the phosphorescent visibility evaluation. METHODS : In this study, the laboratory luminance test of the phosphorescent line marking was conducted using seven specimens to characterize the luminance changes according to the type of the glass beads, the thickness of the phosphorescent line marking, and the brightness and irradiation time of the light source. Phosphorescent and general line markings were made at 150 m to investigate the field luminance performance. A preliminary review of the luminance measurement methods was made using a digital image from a digital single-lens reflex (DSLR) camera. The measured luminance ratio of the general and the phosphorescent line markings was compared with the calculated luminance ratio using luminance analysis. RESULTS : Through the laboratory luminance test, it was seen that the change in luminance, which corresponds to the brightness of the light source, appears large but the influence of the thickness and irradiation time is low. The field performance test of the phosphorescent line marking conducted on the road involved measuring the luminance on the day the marking was made and 7 days after the marking was made. The luminance was found to be $190mcd/m^2$ at 30 min after sunset and approximately $10-12mcd/m^2$ 4h after sunset. The results of the luminance test were captured using a digital image for each time group. The luminance ratio of the phosphorescent line marking, when compared to that of the general line marking, showed a similar trend within a 13% maximum error. Additionally, when this luminance ratio is compared to the direct field measurement, it could be confirmed that the luminance ratio, as captured in the digital image, showed a similar tendency. CONCLUSIONS : 1) The change in luminance corresponding to the brightness of the light source is significant in comparison with that corresponding to the thickness and the irradiation time. In addition, the results of the field test for the phosphorescent line marking satisfied the phosphorescent fire protection standard. 2) We examined the validity of the luminance measurement method using a digital image and we concluded that the change in the luminance ratio shows a similar tendency in both the cases. The results can form the basis for luminance measurement methodology for the construction and maintenance of phosphorescent line markings.

Long-lifetime Green Phosphorescent OLEDs for Low Power Displays

  • Weaver, Michael S.;Adamovich, Vadim I.;Xia, Sean C.;Fiordeliso, James J.;Kwong, Raymond C.;Brown, Julie J.;Lee, Kwan-Hee;Lim, Choon-Woo;Kim, Sung-Chul
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.38-41
    • /
    • 2009
  • We demonstrate a new commercial green phosphorescent organic light emitting device (OLED) in a bottom emission device and top emission microcavity. The bottom and top emitting phosphorescent OLEDs (PHOLED$^{TM}$s) had luminance efficiencies of 60cd/A and 137cd/A respectively, at a luminance of 1,000cd/$m^2$. The top emission microcavity was close to 1953 NTSC color requirements with 1931 CIE color coordinates of 0.231, 0.718. A record green PHOLED lifetime of >3,500hrs to LT95 from 4000cd/$m^2$ is demonstrated for the microcavity device.

  • PDF

Stimulation of Ovarian Development in a Tropical Damselfish by Prolonged Photoperiod using Pellets Containing Long-afterglow Phosphorescent Pigment

  • Imamura, Satoshi;Bapary, Mohammad Abu Jafor;Takeuchi, Yuki;Hur, Sung-Pyo;Takemura, Akihiro
    • Fisheries and Aquatic Sciences
    • /
    • 제17권2호
    • /
    • pp.223-227
    • /
    • 2014
  • The present study examined whether light emitted by long-afterglow phosphorescent pigments (LumiNova) would stimulate gonadal development in fish during the nonbreeding season. Pellets containing LumiNova powder (treatment group) were prepared and placed on the calvaria of specimens of the sapphire devil Chrysiptera cyanea, a reef-associated damselfish that requires long days for gonadal recrudescence. A pellet without LumiNova powder was placed on the calvaria of the control fish (control group). Fish were reared at $26^{\circ}C$ under a light-dark cycle (12 h photophase, 12 h scotophase; LD 12:12) for 4 weeks. No difference in the gonadosomatic index (GSI) or ovarian histology was observed among the control, sham-operation, and treatment groups 1 week after the start of the experiment. After 4 weeks, the GSI of the control and sham-operation groups remained at low levels, and ovaries contained immature oocytes at the perinucleolus stage. In contrast, the treatment group exhibited significantly higher values of GSI as well as developed ovaries with fully vitellogenic oocytes. These results demonstrated that long-day conditions were produced by light emitted from the LumiNova pellets, thus stimulating ovarian development in the damselfish. Therefore, long-afterglow phosphorescent pigments can be used as an alternative to standard light sources for purposes of artificial stimulation of gonadal development in fish.

($Eu^{2+}$, $Nd^{3+}$를 도핑시킨 $BaAl_{2}O_{4}$ 형광체의 광학 및 장잔광특성 (Optical and Long After-Glow Characteristics of $Eu^{2+}$, $Nd^{3+}$ doped $BaAl_{2}O_{4}$ Phosphorescent Crystals)

  • 김정환;김병규;이동규
    • 한국응용과학기술학회지
    • /
    • 제19권3호
    • /
    • pp.174-180
    • /
    • 2002
  • In recent days, the study of a new phosphorescent phosphor has been performed in order to overcome the defect of sulfide phosphor and increase the brightness and long after-glow characteristic of phosphorescent phosphor. Particularly, sulfide phosphor usually used is so chemically unstable that the study of oxide phosphors are processing. $Eu^{2+}$, $Nd^{3+}$ doped Ba-Al-O phosphors sintered at $600{\sim}1500^{\circ}C$ for 2hours had the PL emission spectrum and after-glow over $1200^{\circ}C$. In this system, as the mole concentration of alumina increases, emission bands of phosphors moved from 500nm to 380nm. The optimum concentration of flux was 5wt% and after-glow characteristics of phosphors were found at the host material molar ratio ($BaCO_{3}:Al_{2}O_{3}$), 1:1 and 1:3.

Novel host and electron blocking materials for efficient and long lifetime phosphorescent OLEDs

  • Vestweber, Horst;Gerhard, Anja;Kaiser, Joachim;Heil, Holger;Kroeber, Jonas;Pflumm, Christof;Stoessel, Philipp;Joosten, Dominik;Buesing, Arne;Fortte, Rocco;Parham, Amir;Boehm, Edgar
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.925-927
    • /
    • 2008
  • In order to improve the performance in green phosphorescent OLED devices, Merck has developed novel host and electron blocking materials. The newly developed host materials improve the device lifetime by a factor of 3. The newly developed electron blocking materials having not only electron but also exciton barrier properties increase the efficiency of the device by a factor of 1.4. Comparable results were achieved in phosphorescent red systems with further host materials.

  • PDF

착체중합법을 이용한 SrAl2O4: Eu2+, Dy3+ 축광성 형광체의 합성 (Synthesis and Characteristics of SrAl2O4: Eu2+, Dy3+ Long Afterglow Phosphors by Polymerized Complex Method)

  • 김태호;황해진;김진호;황광택;한규성
    • 한국재료학회지
    • /
    • 제26권10호
    • /
    • pp.561-569
    • /
    • 2016
  • $SrAl_2O_4$: $Eu^{2+}$ and $Dy^{3+}$ phosphorescent phosphors were synthesized using the polymerized complex method. Generally, phosphorescent phosphors synthesized by conventional solid state reaction show a micro-sized particle diameter; thus, this process is restricted to applications such as phosphorescent ink and paint. However, it is possible to synthesize homogeneous multi-component powders with fine particle diameter by wet process such as the polymerized complex method. The characteristics of $SrAl_2O_4$: $Eu^{2+}$ and $Dy^{3+}$ powders prepared by polymerized complex method with one and two step calcination processes were comparatively analyzed. Temperatures of organic material removal and crystallization were observed through TG-DTA analysis. The crystalline phase and crystallite size of the $SrAl_2O_4$: $Eu^{2+}$ and $Dy^{3+}$ phosphorescent phosphors were analyzed by XRD. Microstructures and afterglow characteristics of the $SrAl_2O_4$: $Eu^{2+}$ and $Dy^{3+}$ phosphors were measured by SEM and spectrofluorometry, respectively.

$SrAl_2O_4:Eu^{+2},\;Dy^{+3}$ 장잔광 형광체에 있어서 발광 및 장잔광특성에 미치는$B_2O_3$의 영향 (Effects of $ B_2O_3$ composition for the photoluminescence and after-glow charcteristics of $SrAl_2O_4:Eu^{+2},\;Dy^{+3}$ phosphors)

  • 이영기;엄기석
    • 한국결정성장학회지
    • /
    • 제14권3호
    • /
    • pp.123-128
    • /
    • 2004
  • 융제(flux)로서 $B_2O_3$의 농도를 0-10 wt%까지 변화시킨 $SrAl_2O_4$ : $Eu^{+2}$, $Dy^{+3}$계 장잔광 형광체를 고상반응법으로 합성한 후, $B_2O_3$의 첨가량에 따른 결정특성과 장잔광 축광재료로서 가장 중요한 발광 및 장잔광 특성을 조사하였다. $SrAl_2O_4$ : Eu$^{+2}$, $Dy^{+3}$계 형광체는 $B_2O_3$의 농도에 관계없이 520nm 파장을 최대 발광파장으로 하는 발광스펙트럼을 나타내었고, 3wt%의 $B_2O_3$ 농도에서 최대 발광강도를 나타내었다. 그리고 $SrAl_2O_4$ : Eu$^{+2}$, $Dy^{+3}$ 형광체의 잔광강도 역시 $B_2O_3$의 농도에 무관하게 시간에 따라 모든 시료에서 지수 함수적으로 감소하였으나, $B_2O_3$의 농도가 3wt%인 경우에 발광의 감쇠속도가 작은 뛰어난 장잔광특성을 나타내었다.

고상반응법과 착체중합법으로 합성된 SrAl2O4: Eu2+, Dy3+ 축광성 형광체의 특성 및 열적 안정성 평가 (Characteristics and thermal stability of SrAl2O4: Eu2+, Dy3+ long afterglow phosphors synthesized solid state reaction and polymerized complex method)

  • 김태호;황해진;김진호;황광택;한규성
    • 한국결정성장학회지
    • /
    • 제26권5호
    • /
    • pp.193-200
    • /
    • 2016
  • 고상반응법과 착체중합법 두 합성법에 의해 합성된 $SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$ 축광성 형광체 분말의 특성을 비교 분석하였다. 열적 안정성을 평가하기 위해 산업 도자 제조공정에서 사용되는 열처리 조건($1250^{\circ}C$, 1시간 유지, LPG 환원분위기)을 적용하여 고상반응법과 착체중합법으로 합성된 $SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$ 축광성 형광체 분말의 열처리 전후의 축광 특성변화를 관찰하였다. 두 합성법으로 합성된 분말과 고온 열처리 전후의 분말은 XRD 분석을 통해 결정구조 및 결정자 크기변화를 확인하였고, SEM과 PSA 분석을 이용하여 미세구조 및 입자 크기 변화를 관찰하였다. Spectrofluorometer 분석을 통해 $SrAl_2O_4:Eu^{2+}$, $Dy^{3+}$ 축광성 형광체의 여기 및 발광 특성, 장잔광 특성 변화를 확인하였다.