Synthesis of arsenic adsorbent using graft polymerization

  • SEKO Noriaki;TAMADA Hasao
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 2004년도 추계 총회 및 학술발표회
    • /
    • pp.199-203
    • /
    • 2004
  • Fibrous arsenic (As) adsorbent was synthesized by loading zirconium (Zr) on fibrous phosphoric adsorbent that was directly synthesized by radiation-induced graft polymerization of 2-hydroxyethyl methacrylate phosphoric acid on polyethylene-coated polypropylene nonwoven fabric. Zirconium reacted with phosphoric acid grafted in the polyethylene layer. Zirconium density of the resulting adsorbent was 4.1 mmol/g. The breakthrough curve of As(V) adsorption was independent of the flow rate up to $1300\;h^{-1}$ in space velocity. The total capacity of As(V) was 2.0 mmol/g-adsorbent at pH of 2. The adsorbed Zr(IV) could be evaluated by 0.4 M sodium hydroxide solution because negligible Zr(IV) could be found in the eluted solution.

  • PDF

임플랜트 상부구조의 재료가 반복하중 후 나사풀림에 미치는 영향 (AN INFLUENCE OF ABUTMENT MATERIALS ON A SCREW-LOOSENING AFTER CYCLIC LOADING)

  • 이태식;한중석;양재호;이재봉;김성훈
    • 대한치과보철학회지
    • /
    • 제45권2호
    • /
    • pp.240-249
    • /
    • 2007
  • Statement of problem: A phenomenon of screw-loosening in implant abutment is frequently occurred in a single and multiple implant restoration. Purpose: This study was performed to evaluate an effect of abutment material on screw-loosening before and after a cyclic loading. In a single-tooth implant, different materials of abutment, Type III Gold alloy and Zirconium composite$(ZrO_2/Al_2O_3)$ were used. Material and method: The Gold alloy(Type III) and Zirconium composite$(ZrO_2/Al_2O_3)$ were used to make a superstructure of implant, the one of types of UCLA, Each group was constituted of 5 sample with a 30-degree offset angulated loading platform. The external hexagonal fixture was rigidly hel d in a special holding zig to ensure solid fixation without rotation during the tightening and a cyclic loading. A Titanium-alloy screw was used to connect and controlled to be tighten in 20Ncm torque by a digital torque gauge. A 20 times of consecutive closing/opening cycle were performed to evaluate the immediate torque loss. In 5 sample of each material group, an initial opening torque was recorded during 3 closing/opening cycle, then 2Hz, 200N, 1,000,000 cyclic loadings were performed, then a opening torque was evaluated. Result & Conclusion: 1. In this limited study, titanium alloy screw tightened in 20Ncm, a cold-welding phenomen on was not observed during the 20 times of closing/opening cycle(p=0.11, p=0.18). 2. In titanium alloy abutment screw, repeated opening and closing of the screw caused to progressive decrease of opening torque(p=0.014). 3. The difference in preload of screw between gold alloy abutment and ceramic$(ZrO_2/Al_2O_3)$ abutment was not significant(p=0.78). 4. The difference in torque loss of screw between gold alloy abutment and ceramic$(ZrO_2/Al_2O_3)$ abutment was not significant after 2Hz,200N, 1,000,000 cyclic loading(p=0.92). 5. In titanium alloy abutment screw tightened by 20Ncm, the screw loosening was not significant on each group after 2Hz, 200Ncm, 1,000,000 cyclic loading(p=0.59).

Pulsed laser welding of Zr-1%Nb alloy

  • Elkin, Maxim A.;Kiselev, Alexey S.;Slobodyan, Mikhail S.
    • Nuclear Engineering and Technology
    • /
    • 제51권3호
    • /
    • pp.776-783
    • /
    • 2019
  • Laser welding is usually a more effective method than electron-beam one since a vacuum chamber is not required. It is important for joining Zr-1%Nb (E110) alloy in a manufacturing process of nuclear fuel rods. In the present work, effect of energy parameters of pulsed laser welding on properties of butt joints of sheets with a thickness of 0.5 mm is investigated. The most efficient combination has been found (8-11 J pulse energy, 10-14 ms pulse duration, 780-810 W peak pulse power, 3 Hz pulse frequency, 1.12 mm/s welding speed). The results show that ultimate strength under static loading can not be used as a quality criterion for zirconium alloys welds. Increased shielding gas flow rate does not allow to protect weld metal totally and contributes to defect formation without using special nozzles. Several types of imperfections of the welds have been found, but the major problem is branching microcracks on the surface of the welds. It is difficult to identify the cause of their appearance without additional research on improving the welding zone protection (gas composition and flow rate as well as nozzle configuration) and studying the hydrogen content in the welds.

동축 가공기용 드레싱 장치 개발 (Development of Dressing System for Co-axial Grinding Machine of Ferrule)

  • 이석우;최헌종;안건준;최동열
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.70-73
    • /
    • 2002
  • Using zirconium ceramics makes the ferrule, which is the part of optical communications. The quality of optical communications is directly affected by the concentricity of the optic ferrule. The products of optic ferrule should be meet the following general conditions which are the outer diameter of 2.5mm and the inner diameter of 0.125mm, and high quality conditions which are the concentricity of 0.1~$0.3\mu\textrm{m}$, the form accuracy of $0.2\mu\textrm{m}$, the roundness and the cylindricity of $0.1\mu\textrm{m}$ and the surface roughness of 10nm. Generally, the diamond wheel is used for the high efficiency and precision grinding of the materials. It is good for keeping the shape as it has little wear. Because of the loading phenomena, however, it is difficult to keep the fresh surface of the wheel. In grinding process, grinding fragments resemble fine powders rather than chips. It can easily get attached to the wheel surface and thus cause a loading. The loading takes place, in which the impurities stick to the wheel surface, and the grinding characteristics of wheel is deteriorated. To prevent all of these, a suitable dressing method should be used for the wheel. In this research, the dressing system fur co-axial grinding machine was designed and produced for the machining of ferrule, which is a high performance part. The performance of the developed dressing system was evaluated by measuring the form accuracy of ferrule, which is machined by the dressed wheel in developed dressing system.

  • PDF

Biomechanical three-dimensional finite element analysis of monolithic zirconia crown with different cement type

  • Ha, Seung-Ryong
    • The Journal of Advanced Prosthodontics
    • /
    • 제7권6호
    • /
    • pp.475-483
    • /
    • 2015
  • PURPOSE. The objective of this study was to evaluate the influence of various cement types on the stress distribution in monolithic zirconia crowns under maximum bite force using the finite element analysis. MATERIALS AND METHODS. The models of the prepared #46 crown (deep chamfer margin) were scanned and solid models composed of the monolithic zirconia crown, cement layer, and prepared tooth were produced using the computer-aided design technology and were subsequently translated into 3-dimensional finite element models. Four models were prepared according to different cement types (zinc phosphate, polycarboxylate, glass ionomer, and resin). A load of 700 N was applied vertically on the crowns (8 loading points). Maximum principal stress was determined. RESULTS. Zinc phosphate cement had a greater stress concentration in the cement layer, while polycarboxylate cement had a greater stress concentration on the distal surface of the monolithic zirconia crown and abutment tooth. Resin cement and glass ionomer cement showed similar patterns, but resin cement showed a lower stress distribution on the lingual and mesial surface of the cement layer. CONCLUSION. The test results indicate that the use of different luting agents that have various elastic moduli has an impact on the stress distribution of the monolithic zirconia crowns, cement layers, and abutment tooth. Resin cement is recommended for the luting agent of the monolithic zirconia crowns.

Response of osteoblast-like cells cultured on zirconia to bone morphogenetic protein-2

  • Han, Seung-Hee;Kim, Kyoung-Hwa;Han, Jung-Seok;Koo, Ki-Tae;Kim, Tae-Il;Seol, Yang-Jo;Lee, Yong-Moo;Ku, Young;Rhyu, In-Chul
    • Journal of Periodontal and Implant Science
    • /
    • 제41권5호
    • /
    • pp.227-233
    • /
    • 2011
  • Purpose: The aim of this study was to compare osteoblast behavior on zirconia and titanium under conditions cultured with bone morphogenetic protein-2. Methods: MC3T3-E1 cells were cultured on sandblasted zirconia and sandblasted/etched titanium discs. At 24 hours after seeding MC3T3-E1, the demineralized bone matrix (DBM) gel alone and the DBM gel with bone morphogenetic protein-2 (BMP-2) were added to the culture medium. The surface topography was examined by confocal laser scanning microscopy. Cellular proliferation was measured at 1, 4, and 7 days after gel loading. Alkaline phosphatase activity was measured at 7 days after gel loading. The mRNA expression of ALPase, bone sialoprotein, type I collagen, runt-related transcription factor 2 (Runx-2), osteocalcin, and osterix were evaluated by real-time polymerase chain reaction at 4 days and 7 days. Results: At 1, 4, and 7 days after loading the DBM gel alone and the DBM gel with BMP-2, cellular proliferation on the zirconia and titanium discs was similar and that of the groups cultured with the DBM gel alone and the DBM gel with BMP-2 was not significantly different, except for titanium with BMP-2 gel. ALPase activity was higher in the cells cultured with BMP-2 than in the other groups, but there was no difference between the zirconia and titanium. In ALPase, bone sialoprotein, osteocalcin, Runx-2 and osterix gene expression, that of cells on zirconia or titanium with BMP-2 gel was much more highly increased than titanium without gel at day 7. The gene expression level of cells cultured on zirconia with BMP-2 was higher than that on titanium with BMP-2 at day 7. Conclusions: The data in this study demonstrate that the osteoblastic cell attachment and proliferation of zirconia were comparable to those of titanium. With the stimulation of BMP-2, zirconia has a more pronounced effect on the proliferation and differentiation of the osteoblastic cells compared with titanium.

지르코니아 세라믹과 레진 시멘트의 결합강도 (BOND STRENGTH OF RESIN CEMENTS TO ZIRCONIA CERAMIC)

  • 장문숙;김지혜;조석규;복원미;송광엽;박주미
    • 대한치과보철학회지
    • /
    • 제43권4호
    • /
    • pp.426-437
    • /
    • 2005
  • Statement of problem : Although zirconium oxide ceramics are more and more commonly used in restorative dentistry, for many clinical applications only limited data can be found in the literature. However it is quite clear that hydrofluoric acid etching is impossible with zirconia ceramics. Therefore, other bonding techniques are required in order to lute these materials adhesively. Purpose : The purpose or this study was to evaluate the effects of surface treatments on shear bond strengths between two resin cements and a zirconia ceramic. Materials and methods : Experimental industrially manufactured yttrium-oxide-partially-stabilized zirconia ceramic discs (Adens, Korea) were used for this study. The ceramic specimens divided into five experimental groups and a control group (as received). Five surface treatments were studied 1) sandblasting with 110$\mu$m $Al_2O_3$ at 3 bars pressure 13 seconds at a distance of 10 mm, 2) flame-treated with the Silano-Pen for 5 $s/cm^3$, 3) grinding with a diamond bur. 4) sandblasting + Silano-Pen treatment, 5) diamond bur preparation + Silano-Pen treatment. Acrylic plastic tube (5 mm in height and 3 mm in diameter) were filled with composite to fabricate composite cylinders The composite cylinders were bonded to the ceramic specimens with either Superbond C&B or Panavia F resin luting agents. All cemented specimens were tested under shear loading until fracture on universal testing machine at a crosshead speed 1mm/min; the maximum load at fracture was recorded. Sheat bond strength data were analyzed with oneway analysis of variance and Tukey HSD tests (P<.05). Treated ceramic surfaces and fracture surfaces after shear testing were examined morphologically using scanning electron microscope. Results: Ceramic surface treatment with Silano-Pen after sandblasting improved the bond strength of Superbond C&B resin cement. Supevbond C& B resin cement at Silano-Pen aiker sandblasting($27.4{\pm}3.8MPa$) showed statistically higher shear bond strength than the others. Conclusion: Within the limitation of this study, Superbond C& &B resin cement are suitable for cementation of zirconia ceramics and flame-treated with the Silano-Pen after sandblasting is required to enhance the bond strength.