• 제목/요약/키워드: Large-diameter pipe

검색결과 138건 처리시간 0.033초

대구경 해상 강관말뚝의 설계지지력 확인을 위한 여러 가지 재하시험의 적용 (Case Studies of Several Load Tests for Large Diameter Battered Steel Pipe Piles Constructed on the Offshore Area.)

  • 이정학;서덕동;정헌주
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.291-298
    • /
    • 2001
  • It is very difficult to accomplish load tests of piles with large diameter constructed on the offshore area, because of requirement for large scaled loading equipment and bad testing conditions. Therefore, so far in many cases pile driving dynamic formulas have applied to quality control, and recently dynamic load test method is widely used for confirming bearing capacities of such piles. However, in cases of piles with very large diameter about 2,500mm, it is nearly impossible for regular type load test methods of piles such as static and dynamic to apply owing to very large design load. This is case studies of load tests such as modified static and dynamic load tests of piles and point load tests of rock samples for estimating rational allowable bearing capacity of very large diameter piles constructed on the marine area.

  • PDF

도시가스 수직 배관 내 정지된 수소-메탄 혼합가스의 성층화 현상 연구 (A Study on Stratification Phenomena of Still Hydrogen-Methane Gas Mixture in a Vertical Urban Gas Pipe)

  • 김태균;조정민;성재용
    • 한국가시화정보학회지
    • /
    • 제22권1호
    • /
    • pp.68-78
    • /
    • 2024
  • The stratification phenomena of still hydrogen (20%) and methane (80%) gas mixture in a vertical urban gas pipe have been investigated by simulating the flows based on a mixture model. The stratification is accompanied with the natural convection by the buoyancy force. The hydrogen volume fraction in the upper sections of the pipe increases with time but the increasing rate gets smaller due to the weaker buoyancy force. The pipe with a smaller diameter exhibits a higher peak of hydrogen concentration. The size of vortices is proportional to the pipe diameter. The slip velocity between hydrogen and methane oscillates with a large amplitude at the earlier stage of stratification and then the amplitude decreases sharply. The slip velocity decreases with the diameter, making the stratification become slower. The length of pipe does not affect the stratification since the pipe is sufficiently long relative to the size of vortices.

모세관 삽입 룸 에어컨용 액.가스 열교환 배관에 관한 실험적 연구 (An Experimental Study of Liquid.Gas Heat Exchange Pipe Inserted Capillary Tube for Room Air-Conditioner)

  • 김재돌
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제30권6호
    • /
    • pp.702-708
    • /
    • 2006
  • This study shows the experimental characteristics of the double pipe inserted liquid pipe with small diameter in the gas pipe with large diameter for circulating of a liquid of high temperature, pressure and a gas of low temperature, pressure at the same time. So the functions of pipe and pipe's expansion and heat transfer are presented simultaneously. In the result, the temperature of gas refrigerant at the inlet of compressor increased about $5^{\circ}C$ by the heat transfer with liquid refrigerant in case of the double pipe. And liquid gas refrigerant which the temperature at the inlet of evaporator decreased about $3^{\circ}C$ comparing with the existing type flows into an evaporator COP of the double pipe increased about $7{\sim}10%$ comparing with that of the conventional pipe. And the noise of the double pipe at capillary tube is less than that of the conventional type about 3dB. Consequently. it is convinced the superiority of the double pipe in the heat loss and soundproofing aspect.

다공성소결윅구조에 따른 루프 히트파이프에서 압력손실의 이론적 분석 (Theoretical Analysis of the Pressure Drop in Loop Heat Pipe by Sintered Porous Wick Structure)

  • 이기우;이욱현;박기호;이계중;전원표;인현만
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.1225-1230
    • /
    • 2004
  • In this paper, the pressure drops were investigated according to the sintered porous wick structure in loop heat pipe(LHP) by theoretical analysis. LHP has the wick only in evaporator for the circulation of working fluid, so utilizes porous wick structure which pore diameter is very small for large capillary force. This paper investigates the effects of different parameters on the pressure drops of the LHP such as particle diameter of sintered porous wick, wick porosity, vapor line diameter, thickness of wick and heating capacity. Working fluid is water and the material of sintered porous wick is copper. According to the these different parameters, capillary pressure, pressure drop in wick were analized by theoretical design method of LHP.

  • PDF

항타시공성을 고려한 대구경 항타강관말뚝의 폐색효과 분석(CEL해석) (Analysis of Plugging Effect for Large Diameter Steel Pipe Piles Considering Driveability (CEL Method))

  • 정상섬;송수민;고준영
    • 한국지반공학회논문집
    • /
    • 제33권12호
    • /
    • pp.21-33
    • /
    • 2017
  • 본 연구에서는 항타시공성(BPM, blow per meter)을 고려하여 대구경 항타강관말뚝을 시공하였을 때 발생하는 폐색효과를 분석하였다. Coupled Eulerian-Lagrangian(CEL)해석 시 적용된 항타에너지는 파동방정식을 이용하여 산정하였고, CEL 대변형 3차원 유한요소 해석을 수행하여 말뚝 항타시공 과정을 모사하였다. 본 연구 결과, 말뚝 직경이 증가함에 따라 목표 깊이까지 소요되는 항타에너지는 증가(일정한 BPM인 경우에 해당함) 하였으며, 그 결과 soil plugging index(SPI)는 서로 유사하게 나타나지만 폐색효과는 감소함을 알 수 있었다. 또한, 말뚝의 근입 깊이가 증가할수록 SPI는 서로 유사한 값을 나타냈으나 관내토에서 발생하는 수평토압이 증가하게 되어 폐색효과는 오히려 증가하는 것으로 나타났다. 본 연구결과, 폐색효과의 대표적 영향인자인 말뚝 직경, 말뚝 근입 깊이, 지반 탄성계수, BPM에 따른 관내토의 수평토압계수 분포 경향을 제안하였다.

Experimental Study of Load Characteristics of Buried and Exposed Large-Diameter Pipelines Using Fiber-Optic Strain Sensor

  • Chung, Joseph Chul;Lee, Michael Myung-Sub;Kang, Sung Ho
    • 한국해양공학회지
    • /
    • 제34권3호
    • /
    • pp.194-201
    • /
    • 2020
  • In this study, an optical-fiber sensor was used to measure loads that could act in an environment similar to the loading conditions that exist in an actual pipe. The structure and the installation method of the optical-fiber strain sensor were applied considering the actual large pipe and the buried pipe environment. Load tests were performed using a displacement sensor and sandbags to determine the deflection of the pipe according to the external load, and the linear measurement results were verified. Considering the conditions that could exist in the actual pipe, the test method was presented, and the strain of the buried pipe generated at this time was measured.

대구경 상수도관 부식 손상부의 고분자 필러와 복합슬리브 성능 평가 (Performance assessment of polymeric filler and composite sleeve technique for corrosion damage on large-diameter water pipes)

  • 이호민;박정수;박정주;배철호
    • 상하수도학회지
    • /
    • 제37권4호
    • /
    • pp.203-214
    • /
    • 2023
  • In this study, the physical properties and fracture characteristics according to the tensile load are evaluated on the materials of the polymeric filler and carbon fiber-based composite sleeve technique. The polymeric filler and the composite sleeve technique are applied to areas where the pipe body thickness is reduced due to corrosion in large-diameter water pipes. First, the tensile strength of the polymeric filler was 161.48~240.43 kgf/cm2, and the tensile strength of the polyurea polymeric filler was relatively higher than that of the epoxy. However, the tensile strength of the polymeric filler is relatively very low compared to ductile cast iron pipes(4,300 kgf/cm2<) or steel pipes(4,100 kgf/cm2). Second, the tensile strength of glass fiber, which is mainly used in composite sleeves, is 3,887.0 kgf/cm2, and that of carbon fiber is up to 5,922.5 kgf/cm2. The tensile strengths of glass and carbon fiber are higher than ductile cast iron pipe or steel pipe. Third, when reinforcing the hemispherical simulated corrosion shape of the ductile cast iron pipe and the steel pipe with a polymeric filler, there was an effect of increasing the ultimate tensile load by 1.04 to 1.06 times, but the ultimate load was 37.7 to 53.7% compared to the ductile cast iron or steel specimen without corrosion damage. It was found that the effect on the reinforcement of the corrosion damaged part was insignificant. Fourth, the composite sleeve using carbon fiber showed an ultimate load of 1.10(0.61T, 1,821.0 kgf) and 1.02(0.60T, 2,290.7 kgf) times higher than the ductile cast iron pipe(1,657.83 kgf) and steel pipe(2,236.8 kgf), respectively. When using a composite sleeve such as fiber, the corrosion damage part of large-diameter water pipes can be reinforced with same level as the original pipe, and the supply stability can be secured through accident prevention.

Air-Water Countercurrent Flow Limitation in a Horizontal Pipe Connected to an Inclined Riser

  • Kang, Seong-Kwon;Chu, In-Cheol;No, Hee-Cheon;Chun, Moon-Hyun;Sung, Chang-Kyung
    • Nuclear Engineering and Technology
    • /
    • 제31권6호
    • /
    • pp.548-560
    • /
    • 1999
  • An experimental investigation has been peformed to examine the effects of various geometrical parameters and an initial operating condition on the air-water countercurrent How limitation (CCFL) in a simulated PWR hot leg. A total of 118 experimental data for the onset of CCFL and zero liquid penetration were obtained for various combinations of test parameters. It was observe that the CCFL can be classified into three different categories: (the onset of CCFL, (the partial liquid delivery, and (r) the zero liquid penetration. The observed mechanisms of the onset of CCFL were different depending on the inlet water flow rate. The parametric effects of pipe diameter, horizontal pipe length, horizontal pipe length-to-diameter (L/D) ratio, and initial water level in the horizontal pipe of the test section on the onset of air-water CCFL were also examined. An empirical correlation for the onset of CCFL in a horizontal pipe connected to an inclined riser was developed in terms of Wallis flooding parameters for the low inlet water flow rate region. Comparisons of the present empirical correlation with the air-water CCFL data of large pipe diameters show that the present correlation agrees more closely with the experimental data than the existing CCFL correlations.

  • PDF

Manufacturing and Temperature Measurements of a Sodium Heat Pipe

  • 이병인;이성홍
    • Journal of Mechanical Science and Technology
    • /
    • 제15권11호
    • /
    • pp.1533-1540
    • /
    • 2001
  • A high-temperature sodium stainless steel heat pipe was fabricated and its performance has been investigated. The working fluid was sodium and it was sealed inside a straight tube container made of stainless steel. The amount of sodium occupied approximately 20% of the total volume of the heat pipe and its weight was 65.7gram. The length of a stainless steel container is 1002mm and its outside diameter is 25.4mm. Performance tests were carried out in a room air condition under a free convective environment and the measured temperatures are presented. The start-up behavior of the heat pipe from a frozen state was investigated for various heat input values between 600W and 1205W. In steady state, axial temperature distributions of a heat pipe were measured and its heat transfer rates were estimated in the range of vapor temperature from 50$0^{\circ}C$ to 63$0^{\circ}C$. It is found that there are small temperature differences in the vapor core along the axial direction of a sodium heat pipe for the high operating temperatures. But for the range of low operating temperatures there are large temperature drops along the vapor core region of a sodium heat pipe, because a small vapor pressure drop makes a large temperature drop. The transition temperature was reached more rapidly in the cases of high heat input rate for the sodium heat pipe.

  • PDF

조립식 집수암거의 개량과 이용에 관한 연구 (A Study on Use and improvement of Construction type infiltration gallery)

  • 함준호
    • 한국농공학회지
    • /
    • 제14권2호
    • /
    • pp.2593-2602
    • /
    • 1972
  • Plastic pipes Wrapped with synthetic filter are recently used for drainage or Collecting of Underground water. But it's use is possible only for small size of diameter less than 300mm, because large size plastic pipes are not readily availabe. For large diameter infiltration gallery, porous concrete pipes are now used, but it's heavy weight brings difficulties in making, moving and setting of the pipes. With it's conventional method of filter setting, fine sands are brought into the pipes to make trouble to lifting pumps and channels Therefore, initial construction cost and maintenance cost become high. To solve-this problem, new method is developed and tested. Small PVC pipes(diameter 14mm) are assembled at the site of construction to newly devised I beam type circls. The size of circular inpiltration gallery is optionally determined by I beam type circle which support small PVC pipes and is made of PVC amterial. This gallery are wrappd with syntheitc filter to prevent sand instruction. In this test, the diameter of 300, 400, 500mm were used. I beam type circles were made with PVC plated with thickness. t=6, 9, 12mm. Water quantity collected through the PVC circulor gallery are measured and the strengths of the gallery. 1. Allowable setting depth of gallery pipe below graund for the case of t=6mm, D=500mm is 2.72m. 2. Collected water quantity depends on soil texture, depth of water grandient of water surface, filter material angle of setting etc. 3. About 126% of water quantity collected from the one gallery pipe measured in two gallery pipes of two parallel installation.

  • PDF