고분자 감웅성 LB막을 이용한 One-channel 가스센서의 개발연구 (A Study on Development of One-channel Gas Sensor Using Polymeric Sensitive LB Films)

  • 강현욱;김정명;권영수
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1996년도 추계학술대회 논문집 학회본부
    • /
    • pp.261-263
    • /
    • 1996
  • The study on the development of one-channel gas sensor using the quartz crystal analyzer were attempted. The adsorption and desorption behavior of organic gases were investigated using the resonant frequency and resistance method of quartz crystal. The sensitive materials were deposited on the quartz crystal analyzer(QCA) by using Langmuir-Blodgett method. To investigate the response characteristics of organic vapours and response mechanism, resonant frequency-resonant resistance (F-R) diagram was used. In our experimental results, the response mechanism between sensitive LB film and organic vapours was obtained using F-R diagram. And the position of each organic vapour were different as to the kind and injection amount. Thus F-R diagram can be applied to one-channel gas sensor using the QCA and useful to analyze the response mechanism between organic vspours and sensitive LB films.

  • PDF

Local Photoswitching Effects of Cytochrome c/Viologen/GFP Hetero-Thin Film

  • 유창준;최정우;박세정;남윤석;오병근;이원홍
    • 한국생물공학회:학술대회논문집
    • /
    • 한국생물공학회 2001년도 추계학술발표대회
    • /
    • pp.823-826
    • /
    • 2001
  • In the initial process of photosynthesis, a biological electron transfer system, photoelectric conversion occurs and then long-range electron transfer takes place very efficiently in one direction through the biomolecules. The metal/insulator/metal structured device consisting of GFP, viologen, cytochrome c hetero-thin film was presented based on the biomimesis. GFP, viologen, and cytochrome c was used as an electron sensitizer, a mediator, and an electron acceptor. Cytochrome c molecules and viologen molecules were deposited by Langmuir-Blodgett (LB) technique, and GFP molecules were adsorbed by self-assembly method (SAM). Surface morphology of hetero-thin film was analyzed by scanning tunneling microscopy (STM). Local photoswitching effects of a proposed photodiode were verified by current-voltage measurements using hybrid STM/I-V measurement system.

  • PDF

Langmuir-Blodgett(LB) 박막의 열자격 전류 연구 (A study on the Thermally stimulated current(TSC) of the Langmuir-Blodgctt(LB) films)

  • 이호식;김우연;이원재;김태완;;강도열
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 추계학술대회 논문집
    • /
    • pp.199-202
    • /
    • 1996
  • This paper describes the thermally stimulated current (TSC) measurements of arachidic acid and polyamic acid alkylamine salt(PAAS) LB film, which is a precursor of polyimide(PI). The measurements were performed from room temperature to about 25$0^{\circ}C$ and the temperature was increased at a rate of 0.02 K/s linearly. It shows that peaks of TSC are observed at about 8$0^{\circ}C$ in the arachidic acid and about 8$0^{\circ}C$, 16$0^{\circ}C$ in the PAAS LB films. Results of these measurements indicate that one peak at 8$0^{\circ}C$ is resulted from alkyl group; the other peak at 16$0^{\circ}C$ is due to alkyl and C-O group of PAAS. Additional large peak at about 16$0^{\circ}C$ is due to dipole moments in the PAAS films. The DSC and TGA of PAAS, arachidic acid and octadesylamine are measured. Thermal imidization was performed at 30$0^{\circ}C$ far 1 hour by our pre study

  • PDF

적외선 분광법을 이용한 Perfluorostearic Acid의 이온화 연구 (Infrared Spectroscopic Studies on the Ionization of Perfluorostearic Acid)

  • 김욱수;하기룡
    • 공업화학
    • /
    • 제19권1호
    • /
    • pp.111-116
    • /
    • 2008
  • 적외선 분광법을 이용하여 하부상의 다양한 pH(3~11) 변화 및 금속이온($Na^+$, $Ca^{2+}$, $La^{3+}$) 존재에 따른 perfluorostearic acid(PFS)의 이온화 거동에 관한 연구를 수행하였다. Langmuir-Blodgett (LB) 수조의 하부상에 존재하는 pH 변화 및 금속이온의 종류에 따른 PFS의 -COOH의 C = O 신축진동 피크와 $COO^-$ 피크의 이동 및 강도의 변화를 관찰한 결과 하부상 수용액의 pH가 같은 경우에는 PFS의 -COOH 그룹의 C = O 피크 세기의 감소가 $La^{3+}$ > $Ca^{2+}$ > $Na^+$의 순으로 나타났다. 이는 PFS에 대한 친화도가 $La^{3+}$가 가장 크며, $Ca^{2+}$$Na^+$의 순서로 감소한다는 것을 알 수 있다. 또한 증류수 하부상에서 생성된 perfluorostearate 이온의 몰분율을 측정한 IR 스펙트럼으로부터 계산한 결과 약 pH 3의 낮은 pH 값에서도 50% 이상의 perfluorostearate 이온이 생성되는 것을 관찰하였으며, 이러한 결과는 PFS의 이온화도가 stearic acid (SA)보다 높은 것을 나타낸다.

말레에이트계 공중합체 I-l3막의 공기/물에서의 계면 특성 (The Air/water Interface Characteristics of Maleate Copolymer LB Films)

  • 신훈규;권영수;이범종;장정수;배진호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1995년도 춘계학술대회 논문집
    • /
    • pp.220-223
    • /
    • 1995
  • Stable polyion-complexed polymeric monolayrers were prepared by spreading perfluoroalkyl monomaleatd copolymers. C$_2$F$\_$8/MA-VE$_2$ and C$_2$F$\_$8/Mv-VE$_3$ on aqueous poly(allylamine) subphase. The monolayer properties have been studied by the surface pressure-area($\pi$-A) isotherms. The C$_2$F$\_$8/MA-VE$_3$containing longer oligoethyleneglycol pendant showed more expaned monolayer phase than the C$_2$F$\_$8/MA-VE$_2$ The polyion-complexed monolayers were transferable on various substrates, and the resulting Langmuir-Blodgett(LB) films were characterized b ET-IR spectroscopy and scanning electron microscopy(SEM) Two-dimensional crosslinking to from a polymer network was achieved by amide formation through heat treatment under vacuum with concurrent removel of perfluoroalkyl tails. SEM observation of this film ona porous membrane filter showed that the four layer film was sufficiently stable to cover the filter pore size of 0.1$\mu\textrm{m}$. The C$_2$F$\_$8/MA-VE$_3$revealed better covering capability than the C$_2$F$\_$8/MA-VE$_2$Immersion of this film in water or in benzend did not cause any change in its appearance and in FT-IR spectra.

  • PDF

LB법으로 제작한 백색 EL소자의 발광특성 (Emission Properties of EL Device Fabricated by LB Method)

  • 김주승;이경섭;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.351-354
    • /
    • 2001
  • We fabricated organic electroluminescent(EL) devices with mixed emitting layer of poly (N- vinylcarbazole) ( PVK) , 2,5-bis (5-tert-butyl -2- benzoxaBoly) thiophene ( BBOT) , N,N-diphenyl-N,N- (3-methyphenyl) -1,1-biphenyl-4, 4-thiamine(TPD) and poly(3-hexylthiophene) (P3HT) deposited by LB(Langumuir-Boldgett) method. From the AFM(atomic force microscope) images, the monolayer containing 30% of AA(arachidic acid) showed a roughness value of 28$\AA$. In the voltage-current characteristics of ITO/Emitting layer/BBOT/LiF/A1 devices, current density much smaller than that of the spin-coated devices having a same thickness.

  • PDF

Langmuir-Blodgett(LB) Films의 광학적 및 전기적 특성 (Polyamic Acid Alkylamine Salts(PAAS))

  • 이승엽;강도열;김태완
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 춘계학술대회 논문집
    • /
    • pp.277-280
    • /
    • 1997
  • It is important to investigate the molecular arrangement and the orientational distribution in the study of LB films. Polarized UV/visible absorption spectra make it possible to reveal the molecular arrangement and the orientational distribution. It is clarified that the PAAS LB films have specific directions in the molecular arrangement and the orientational distribution, which art different in intensity corresponding to the surface pressure. Unpolarized UV/visible absorption spectra reveal that the surface pressure is proportional to the finn thickness and is related to the molecular orientation. Current-Voltage(I-V) measurements provide that the current decreases as the surface pressure increases and there are certain phenomena called switching phenomena. Switching effort indicates that the current flows in high conductivity during on-state and suddenly decreases into low conductivity during off-state.

  • PDF

Au/Pl/Au구조의 유기박막 절연성에 관한 연구 (A Study on the Insulation Characteristics of Organic Thin Films of Au/Pl/Au structure)

  • 전동규;김영근;조제황;이경섭;최영일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 D
    • /
    • pp.1468-1470
    • /
    • 1998
  • Using a solution of polyamic acid salt obtained in combination with polyimide acid, we successfully prepared thermally stable multilayers(41, 35, 31 layers) films disilane-containing polyimide by Langmuir-Blodgett(LB) technique. We studied the electrically phenomena occurring at the metal(Au)/polyimide(Pl) LB film/metal(Au). Also, we then examined the of Pl LB films by means of current-voltage (I-V) and resistance measurement.

  • PDF

LB법을 이용한 polyimide 초박막의 제작 (Fabrication of Ultrathin Polyimide Films by LB Technique)

  • 김재환;유덕선;김영관;손병청;강도열
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1993년도 정기총회 및 추계학술대회 논문집 학회본부
    • /
    • pp.174-177
    • /
    • 1993
  • The polyimide films were prepared by imidizing the polyamic acid long-chain alkylamine (dimethylhexadecylamine) salt films with a thermal and chemical treatment, where the polyamic acid alkylamine salt film were formed on various substrates by using Langmuir-Blodgett (LB) method. The imidization of polyamic acid alkylamine salt films with various thickness were identified with FT-IR and UV-visible absorption spectroscopies. Atomic Force Microscopy (AFM) have been used to investigate the surface morpology of polyamic acid alkylamine salt and imidized films.

  • PDF

광학시스템을 이용한 메로시아닌 색소 LB막의 표면 모폴로지 해석 (The Surface Analysis of the Merocyanine Dye LB film using Optical system)

  • 강기호;신훈규;장정수;권영수
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 하계학술대회 논문집 C
    • /
    • pp.1714-1716
    • /
    • 2000
  • We fabricated the optical system of merocyanine dye using Langmuir-Blodgett(LB) technique because quite uniform orientation could be obtained, which is one of the most important factors to affect to its optical characteristics. The resonance frequency and other electrical parameters at the parallel resonance state were measured using the impedance analyser(HP 4294 A). Also the morphological changes of dye molecules after UV irradiation were observed using AFM. The parallel resonance frequency and resistance by electrical equivalent circuit were decreased with the UV irradiation and these aspects are different from general mass adsorption process. Therefore the structural changes of dye molecules are being considered, that is, the aggregated molecules become dissociated. It indicates that the shifts of the resonance frequency and the others occurred without mass absorption.

  • PDF