Fabrication of Titanium alloy by Electromagnetic Continuous Casting (EMCC) Method for Medical Applications (전자기 연속 주조법을 이용한 의료용 타이타늄 합금 제작에 관한 연구)

  • Choi, Su-Ji;Lee, Hyun-Jae;Baek, Su-Hyun;Hyun, Soong-Keun;Jung, Hyun-Do;Moon, Byung-Moon
    • Journal of Korea Foundry Society
    • /
    • v.38 no.1
    • /
    • pp.9-15
    • /
    • 2018
  • Electromagnetic continuous casting (EMCC) was used to fabricate Ti-6Al-4V alloys with properties suitable for medical applications. Ti-6Al-4V alloy ingots fabricated by EMCC were subjected to heat treatment, such as residual stress removing (RRS), furnace cooling after solution treatment (ST-FC) and water-cooling after solution treatment (ST-WC), in order to obtain characteristics suitable for the standard. After component analysis, the microstructure and mechanical properties (tensile strength and elongation) were evaluated by ICP, gas analysis, OM, SEM, a Rockwell hardness tester and universal testing machine. The Ti-6Al-4V alloy ingot fabricated by EMCC was fabricated without segregation, and the lamellar structure was observed in the RRS and ST-FC specimens. The ST-WC specimen showed only martensite structure. As a result of evaluating the mechanical properties based on the microstructure results, we found that the water-cooled heat treatment condition after the solution treatment was most suitable for the Ti-6Al-4V ELI standard.

The Effects of Physical States of Phospholipids on $Ca^{2+}$-ATPase Activity of Biological Membranes (지질의 물리학적 성상이 $Ca^{2+}$-ATPase 활성도에 미치는 영향)

  • Hah, Jong-Sik
    • The Korean Journal of Physiology
    • /
    • v.22 no.2
    • /
    • pp.163-177
    • /
    • 1988
  • The $Ca^{2+}-ATPase$ of sarcoplasmic reticulum (SR) was solubilized and reconstituted into a mixture of phosphatidylcholine (PC) and phosphatidylethanolamine (PE) of varying ratios in order to assess the effect of physical states of phospholipids on the incorporation and functions $Ca^{2+}-ATPase$. On the basis of the spectral data of Ca-arsenazo III, the $Ca^{2+}$ uptake of SR was increased linearly as the PC content increased in the reconstituted vesicles. The ATP hydrolysis activity also increased as PC content increased up to 25% and then decreased slightly as the PC content further increased. On the other hand the incorporation of $Ca^{2+}-ATPase$ into the reconstituted vesicls occured maximally at 25% PC and 75% PE mixture which is known to have a non-bilayer structure in reconstitution system. From the above results it is clear that preexisting defects in the lipid bilayer promote protein incorporation into the bilayer during reconstitution and lamellar structure of the bilayer facilitates the $Ca^{2+}-ATPase$ function.

  • PDF

Formation of Nanocrystalline Ferrite by Planetary Ball Milling in a Low Carbon Steel (저탄소강에서 Planetary 볼밀링에 의한 나노결정 페라이트의 형성)

  • Lee, Hye Jung;Lee, Sang Woo;Oh, Myung-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.18 no.1
    • /
    • pp.29-40
    • /
    • 2005
  • Formation of nanocrystalline ferrite was investigated using milled powders obtained by planetary ball milling of chips, which were made by high speed mechanical cutting of a low carbon steel(0.15%C-1.1%Mn-0.01%Ti). After 4 hour milling the chips were changed to powders of $50{\mu}m$ in average size, and with increasing milling time the powders were refined to about $3{\mu}m$ for 128 hour and showed more equiaxed shapes. Nanocrystalline(nc) region appeared in the surfaces of powders milled for 1 hour, and the 4 hour milled powders were almost filled with nc region. Hardness of nc region was much higher than that of work-hardened(WH) region. With increasing milling time, ferrite and cementite in pearlite were severely deformed and lamellar spacing was decreased, and then cementites began to disappear after 4 hour milling due to dissolution into ferrite. Deformation bands formed in lightly work-hardened region showed large width and similar crystallographic orientations. Spacing of deformation bands was decreased with deformation and the layered microstructure consisting of narrow deformation bands subdivided into variously oriented small grains was formed by more deformation, and eventually this structure seemed to be evolved to the nc structure by further deformation. It is also conjectured the growth of nc ferrite grains occurred through the coalescence of nanocrystalline ferrites rather than the nucleation and growth of recrystallized grains.

A Characteristic of Microstructures in Bonding Interlayer of Brazed Titanium to Copper (브레이징한 Ti/Cu 접합계면부의 미세조직 특성)

  • 김우열;정병호;이성렬
    • Journal of Welding and Joining
    • /
    • v.13 no.3
    • /
    • pp.106-115
    • /
    • 1995
  • To know the bonding phenomena of Ti/Cu brazed joint, a characteristic of microstructures in bonding interlayer of vacuum brazed pure Ti to Cu has been studied in the temperature range from 1088 to 1133K for various bonding times using Ag-28wt%Cu filler metal. Also intermediate phases formed in bonded interlayer and behavior of layer growth have been investigated. The obtained results in this study are as follows: 1) Liquid insert metal width at the each brazing temperature was proportional to the square root of brazing time, and it was considered that the liquid insert metal width was controlled by the diffusion rate process of primary .alpha.-Cu formed at the Ti side. 2) Intermediate phases formed near the Ti interface were .betha.-Ti and intermetallic compounds TiCu, Ti$_{2}$Cu, Ti$_{3}$Cu, and TiCu. 3) .betha.-Ti formed in Ti base metal durig brazing transformed to lamellar structure, .alpha.-Ti + Ti$_{2}$Cu. The structure came from the eutectoil decomposition reaction in cooling. And the width of .betha.-Ti layer was proportional to the square root of brazing time, and it was considered that the growth of .betha.-Ti layer was controlled by interdiffusion rate process in .betha.-Ti. 4) The layer growth of TiCu, Ti$_{3}$Cu$_{4}$ and TiCu, phases formed near the Ti interface was linerface was linearly proportional to the brazing time, and it was considered that the layer growth of these phases was controlled by the chemical reaction rate at the interface.

  • PDF

Fine Structure of the Epithelial Apoptosis in the Anuran Tadpole Rana nigromaculata (참개구리(Rana nigromaculata) 유생기 상피 세포사의 미세구조)

  • Lee, Hye-Won;Moon, Myung-Jin
    • Applied Microscopy
    • /
    • v.40 no.2
    • /
    • pp.81-88
    • /
    • 2010
  • The fine structural characteristics of the apoptotic cells in the cutaneous epithelium of the anuran tadpole of the black-spotted frog, Rana nigromaculata was examined using the TUNEL (Terminal deoxynucleotidyl transferase-mediated biotinylated d-Uridine triphosphate Nick End Labeling) staining technique and TEM (transmission electron microscopy) observations. The cutaneous epithelium of the tadpole was composed of stratified cuboidal cells and the apoptotic cell death was observed continuously during the tail degeneration stages from the Shumway stage number 31 to 33. The early apoptotic cells shown in the epithelium demonstrated condensation and margination of the chromatin material at the nuclear periphery, and nuclear breakdown and cytoplasmic condensation were followed. Subsequent cytoplasmic degeneration of the apoptotic cell were produced by membrane-bounded cell fragments with relatively well preserved organelles. Following the processes of autophagic degradation, the late apoptotic cells being phagocytosed by other surrounding cells. These nearby cells, presumptive intraepithelial macrophages, contain a variety of lysosomal residual bodies which fuses with other cell organelles or other cytoplasmatic material to form secondary lysosomes. They are soon transformed into lamellar shaped vesicles and finally disappeared during the process of degradation.

Ultrastructural Studies on Mercury Poisoning in the Liver, Kidney and Gills of Carassius carassius L. (수은중독에 의한 붕어(Carassius carassiusr L.) 장기의 미세구조 변화)

  • 등영건;유관희;최춘근;최임순
    • The Korean Journal of Zoology
    • /
    • v.21 no.3
    • /
    • pp.87-102
    • /
    • 1978
  • Electron microscopic studies were made to investigate changes in the fine structure of the liver, kidney and gills of Carassius carassius L. following exposure to 1 and 2.5 ppm of $HgCl_2$. The following results were obtained: 1. In the mercury-treated liver cells, an increase in the number of lysosomes were noticed. These lysosomes appeared to be of two types; round ones containing some crystalline structures and others with phagocytosed glycogen granules and mitochondria. Also observed were mitochondrial swelling where the matrix appeared less electrondense, and segregation of the nucleoli in the nucleus. 2. In the kidney, mercury treatment resulted in thickening of the basement membrane of the glomerulus, and appearance of vacuoles and cytoplasmic bodies in the proximal convoluted tubule. The vacuoles seemed to be formed from mitochondria. Nuclear shrinkage was also noticed at 2.5 ppm of $HgCl_2$. 3. Many large and small lysosomes appeared in response to mercury in the epithelial cells of the gill lamella. Also the lamellar membrane became fuzzy in appearance. 4. It can be concluded from these results that mercury-induced changes in the fine structure are associated with activation of detoxication processes and impairment of energy metabolism.

  • PDF

The Effect of Comonomer Type and Content on the Properties of Ziegler-Natta Bimodal High-Density Polyethylene (공단량체의 종류 및 조성이 지글러-나타 중합된 이중 분자량 분포 고밀도 폴리에틸렌의 물성에 미치는 영향)

  • Meng, Weijuan;Li, Hongbo;Li, Jianwei;Chen, Biaohua
    • Journal of the Korean Chemical Society
    • /
    • v.55 no.4
    • /
    • pp.673-679
    • /
    • 2011
  • Bimodal high-density polyethylenes with different comonomer type and content were synthesized by polymerization of ethylene using Ziegler-Natta catalyst. Their structure and properties were studied using GPC, NMR, DSC and tensile test. It was found that ethylene/1-hexene copolymer exhibits higher tensile strength and elongation at break than that of ethylene/1-butylene copolymer with similar comonomer content. The molecular weight decreases as the comonomer content of the polymer increases. Short chain branching affects the crystallinity and thus the morphology and consequently the mechanical properties of the corresponding bimodal high-density polyethylenes. After SSA treated, the multiple endothermic peaks were observed. Multiple endothermic peaks are mainly attributed to the heterogeneity of ethylene sequence length and lamellar thickness. The difference of broadness index indicates that SCB distribution of polyethylene containing higher comonomer content has improved uniformity.

Formation of Liquid Crystalline with Hydrogenated Lecithin and Its Effectiveness (수소첨가레시친을 이용한 액정 젤의 형성과 보습효과)

  • Kim, In-Young;Lee, Joo-Dong;Ryoo, Hee-Chang;Zhoh, Choon-Koo
    • Journal of the Society of Cosmetic Scientists of Korea
    • /
    • v.30 no.2
    • /
    • pp.159-165
    • /
    • 2004
  • This study described about method that forms liquid crystal gel (LCG) by main ingredient with hydrogenated lechin (HL) in O/W emulsion system. Result of stability test is as following with most suitable LCG's composition. Composition of LCG is as following, to form liquid crystal, an emulsifier used 4.0wt% of cetostearyl alcohol (CA) by 4.0wt% of HL as a booster. Moisturizers contained 2wt% of glycerin and 3.0wt% of 1,3-butylene glycol (1,3-BG). Suitable emollients used 3.0wt% of cyclomethicone, 3.0wt% of isononyl isononanoate (ININ), 3.0wt% of cerpric/carprylic triglycerides (CCTG), 3.0wt% of macademia nut oil (MNO) in liquid crystal gel formation. On optimum conditions of LCG formation, the pHs were formed all well under acidity or alkalinity conditions (pH=4.0-11.0). Considering safety of skin, pH was the most suitable 6.0${\pm}$1.0 ranges. The stable hardness of LCG formation appeared best in 32 dyne/$\textrm{cm}^2$. Particle of LCG is forming size of 1-20$\mu\textrm{m}$ range, and confirmed that the most excellent LCG is formed in 1-6$\mu\textrm{m}$ range. According to result that observe shape of LCG with optical or polarization microscope, LCG could was formed, and confirmed that is forming multi -layer lamellar type structure around the LCG. Moisturizing effect measured clinical test about 20 volunteers. As a result, moisturizing effect of LCG compares to placebo cream was increased 36.6%. This could predicted that polyol group is appeared the actual state because is adsorbed much to round liquid crystal droplets to multi-lamellar layer's hydrophilic group. It could predicted that polyol group is vast quantity present phase that appear mixed because is adsorbed to round liquid crystal to multi-lamellar layer's hydrophilic group. This LCG formation theory may contribute greatly in cosmetics and pharmacy industry development.

Layered structure of sialoliths compared with tonsilloliths and antroliths

  • Buyanbileg Sodnom-Ish;Mi Young Eo;Yun Ju Cho;Mi Hyun Seo;Hyeong-Cheol Yang;Min-Keun Kim;Hoon Myoung;Soung Min Kim
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.50 no.1
    • /
    • pp.13-26
    • /
    • 2024
  • Objectives: The aim of this study was to perform a comparative analysis of the ultrastructural and chemical composition of sialoliths, tonsilloliths, and antroliths and to describe their growth pattern. Materials and Methods: We obtained 19 specimens from 18 patients and classified the specimens into three groups: sialolith (A), tonsillolith (B), and antrolith (C). The peripheral, middle, and core regions of the specimens were examined in detail by histology, micro-computed tomography (micro-CT), scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy, and transmission electron microscopy (TEM). Results: In the micro-CT, group A showed alternating radiodense and radiolucent layers, while group B had a homogeneous structure. Group C specimens revealed a compact homogeneous structure. Histopathologically, group A showed a laminated, teardrop-shaped, globular structure. Group B demonstrated degrees of immature calcification of organic and inorganic materials. In group C, the lesion was not encapsulated and showed a homogeneous lamellar bone structure. SEM revealed that group A showed distinct three layers: a peripheral multilayer zone, intermediate compact zone, and the central nidus area; groups B and C did not show these layers. The main elemental components of sialoliths were O, C, Ca, N, Cu, P, Zn, Si, Zr, F, Na, and Mg. In group B, a small amount of Fe was found in the peripheral region. Group C had a shorter component list: Ca, C, O, P, F, N, Si, Na, and Mg. TEM analysis of group A showed globular structures undergoing intra-vesicular calcification. In group B, bacteria were present in the middle layer. In the outer layer of the group C antrolith, an osteoblastic rimming was observed. Conclusion: Sialoliths had distinct three layers: a peripheral multilayer zone, an intermediate compact zone and the central nidus area, while the tonsillolith and antrolith specimens lacked distinct layers and a core.

Engineering Properties of Mylonite in the Youngju Area (영주지역 압쇄암의 공학적 특성 연구)

  • Kim, Sung-Wook;Choi, Eun-Kyeong;Yang, Tae-Sun;Lee, Kyu-Hwan
    • Journal of the Korean Geotechnical Society
    • /
    • v.27 no.10
    • /
    • pp.35-43
    • /
    • 2011
  • The area to be studied is the place where the main line rail way will be constructed in accordance with the scheduled construction project of Yeongju dam, and is a fold and mylonite zone over several km that is formed by ductile-shearing effect. The ductile shear zone, which has been transformed by faulting for long geological time, shows a complicated geological structure. Due to the recrystallization of mineral caused by transformation in deep underground (>8km), a mylonite zone with lamellar structure has properties distinguished from other fault zones formed by transformation near earth surface <2km). To see the properties of mylonite, this study analyzed the transformation rate of sample rocks and the shape of constriction structure accompanied with transformation. While the transformation of fault zone shows a round oblate, the mylonite zone shows a prolate form. Transformation rate in fault zone was measured to be less than 1.2 compared to the state before transformation while the measured rate in mylonite zone was 2.5 at most. Setting the surface of discontinuity as the base, the unconfined compressive strength of slickenside can be categorized in sedimentary rocks, and a change of strength was observed after water soaking over certain time. Taking into account that the weathering resistance of the rock based on mineral and chemical organization is relatively higher, its engineering properties seems to result from the shattered crack structure by crushing effect. When undertaking tunnel construction in mylonite zone, there should be a special care for the expansion of shattered cracks or the fall of strength by influx of ground water.