Luminescent Properties of Two-Ions Doped Phosphors for LED Application

  • Kim, Tae-Gon;Kim, Young-Sic;Im, Seoung-Jae
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.52-55
    • /
    • 2009
  • A red phosphor, $(Sr,Ca)_2P_2O_7:Eu^{2+},Mn^{2+}$, for UV-LED was synthesized under a reducing atmosphere, and its luminescent properties were investigated. The phosphor absorbs ultraviolet light at around 400 nm and efficiently emits red light at approximately 610 nm through an energy transfer from $Eu^{2+}$ to $Mn^{2+}$. Using the varied input current test for the phosphor-loaded LED lamps, it was found that the luminescent efficiency of the phosphor decreased with increasing light flux. This might be due to an increased probability of excited-state absorption and the consequent non-radiative relaxation in $Mn^{2+}$ ions in the condition of high photon influx.

  • PDF

유로피움-활성화 칼슘 알루미늄 실리케이트 형광체 연구 (Study of Europium-activated Calcium Aluminium Silicate Phosphors)

  • 황정하;박주석;장보윤;남산;김준수;유순재
    • 한국전기전자재료학회논문지
    • /
    • 제19권11호
    • /
    • pp.1020-1024
    • /
    • 2006
  • Europium$(Eu^{2+}\;or\;Eu^{3+})$-activated calcium aluminium silicate phosphors were synthesized for the first time and the structures and luminescence characteristics of these phosphors were investigated. The phosphors in this study emitted blue, green, and even red light depending on the starting milterials and annealing conditions for synthesis. In addition, the structure was also changed when the different starting materials were used. When $CaCO_3$ was used as a starting material, tetragonal $Ca_2Al_2SiO_7$ was formed. However, pure green light was emitted when the annealing was conducted in reduced atmosphere and red one was emitted by annealing in air. In the case of $CaSiO_3$ as a starting material, triclinic $CaAl_2Si_2O_8$ was formed and only pure blue emission was observed. Moreover, this blue phosphor exhibited higher intensity than that of commercial YAG:Ce phosphor, which showed the possibility of application on the phosphor for new light source such as a UV-LED.

따뜻한 백색 LED의 제조를 위한 Sr3SiO5:Eu2+ 형광체에서의 융제 첨가 영향 (Influence of Fluxing Agents in Sr3SiO5:Eu2+ Phosphors for Fabrication of Warm White Light Emitting Diodes)

  • 김현호;정강섭;이승원;김병규
    • 한국세라믹학회지
    • /
    • 제49권1호
    • /
    • pp.105-110
    • /
    • 2012
  • In this paper, a yellow phosphor $Sr_3SiO_5:Eu^{2+}$ that emits efficiently at the 450 nm excitation for warm white LED is studied. In addition, the effects of various flux $BaF_2$, $NH_4Cl$ on the emission spectra were investigated. The samples were synthesized through conventional solid state reaction under reducing atmosphere of 95% $N_2$-5% $H_2$ mixture at the high temperature. All phosphors showed a excitation band from 450 nm and broad band emission peaking at region of 580 nm. The optimal concentration of $BaF_2$ flux is 3 wt% for $Sr_3SiO_5$ with doping 0.05mol Eu phosphors fired in a reductive atmosphere. The phosphor showed highest emission peaking at 582 nm.

CaYAlO4:Tb3+/Eu3+/Ce3+형광체의 광학적 특성 분석 (Optical Properties of CaYAlO4:Tb3+/Eu3+/Ce3+ Phosphors)

  • 강태욱;류종호;김종수;김광철
    • 반도체디스플레이기술학회지
    • /
    • 제16권4호
    • /
    • pp.86-90
    • /
    • 2017
  • $Tb^{3+}$ or $Eu^{3+}$ or $Ce^{3+}$-doped $CaYAlO_4$ phosphor were synthesized by solid-state method. $CaYAlO_4:Tb^{3+}$ is shown that the $Tb^{3+}$-doping concentration has a significant effect on the $^5D_4/^5D_3{\rightarrow}7F_J$ (J=6,...,0) emission intensity of $Tb^{3+}$. The $CaYAlO_4:Tb^{3+}$ phosphors show tunable photoluminescence from blue to yellow with the change of doping concentration of $Tb^{3+}$ ions. The $CaYAlO_4:Eu^{3+}$ phosphors exhibit a red-orange emission of $Eu^{3+}$ corresponding to $^5D_0$, $_{1,2}{\rightarrow}^7F_J$ (J=4,...,0) transitions. The $CaYAlO_4:Ce^{3+}$ phosphors show a blue emission due to $Ce^{3+}$ ions transitions from the 5d excited state to the $^2F_{5/2}$ and $^2F_{7/2}$ ground states. The decay time of $CaYAlO_4:Tb^{3+}$ phosphors decrease from 1.33 ms to 0.97 ms as $Tb^{3+}$ concentration increases from 0.1 mol% to 7 mol%. The decay time of $CaYAlO_4:Eu^{3+}$ phosphors increase from 0.94 ms to 1.17 ms as $Eu^{3+}$ concentration increases from 1 mol% to 9 mol%.

  • PDF

Improving color gamut of white LED for LCD B/L application

  • Lee, H.J.;Yoo, J.S.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2006년도 6th International Meeting on Information Display
    • /
    • pp.1100-1102
    • /
    • 2006
  • A three-band white LED was fabricated by combining a blue LED with SrGa2S4:Eu (green) and CaS:Eu (red) phosphors for improving the color gamut, which is favorable to full color image.

  • PDF

고연색 LED용 적색 Sr2Si5N8:Eu2+ 형광체의 합성 및 발광특성 연구 (Synthesis and Luminescence of Sr2Si5N8:Eu2+ Red Phosphor for High Color-Rendering White LED)

  • 이성훈;김종수;강태욱;류종호;이상남
    • 반도체디스플레이기술학회지
    • /
    • 제16권4호
    • /
    • pp.11-15
    • /
    • 2017
  • Red phosphors, $Sr_2Si_5N_8:Eu^{2+}$, were synthesized as a single-phase crystal structure by optimizing carbon and $Eu^{2+}$ contents in a carbothermal reduction nitridation method. With increasing $Eu^{2+}$ contents, the photoluminescence spectra were red-shifted from 600 nm peak for 1 mol% for to 700 nm for 7 mol%. It was suggested that this red shift is attributed to the energy transfer from one low-energy sited $Eu^{2+}$ (1) to other high-energy sited $Eu^{2+}$ (2). Finally, the best red sample (620 nm emission peak and 80 nm half width for 3 mole% of $Eu^{2+}$) was packaged on a Blue LED together with two additional green and yellow phosphors, the fabricated White LED showed a high color-rendering index of 90 and white color coordinates of x= 0.321 and y = 0.305.

  • PDF

Highly Luminescent (Zn0.6Sr0.3Mg0.1)2Ga2S5:Eu2+ Green Phosphors for a White Light-Emitting Diode

  • Jeong, Yong-Kwang;Cho, Dong-Hee;Kim, Kwang-Bok;Kang, Jun-Gill
    • Bulletin of the Korean Chemical Society
    • /
    • 제33권8호
    • /
    • pp.2523-2528
    • /
    • 2012
  • Green phosphors $(Zn_{1-a-b}M_aM^{\prime}_b)_xGa_yS_{x+3y/2}:Eu^{2+}$ (M, M' = alkali earth ions) with x = 2 and y = 2-5 were prepared, starting from ZnO, MgO, $SrCO_3$, $Ga_2O_3$, $Eu_2O_3$, and S with a flux $NH_4F$ using a conventional solidstate reaction. A phosphor with the composition of $(Zn_{0.6}Sr_{0.3}Mg_{0.1})_2Ga_2S_5:Eu^{2+}$ produced the strongest luminescence at a 460-nm excitation. The observed XRD patterns indicated that the optimized phosphor consisted of two components: zinc thiogallate and zinc sulfide. The characteristic green luminescence of the $ZnS:Eu^{2+}$ component on excitation at 460 nm was attributed to the donor-acceptor ($D_{ZnGa_2S_4}-A_{ZnS}$) recombination in the hybrid boundary. The optimized green phosphor converted 17.9% of the absorbed blue light into luminescence. For the fabrication of light-emitting diode (LED), the optimized phosphor was coated with MgO using magnesium nitrate to overcome their weakness against moisture. The MgO-coated green phosphor was fabricated with a blue GaN LED, and the chromaticity index of the phosphor-cast LED (pc-LED) was investigated as a function of the wt % of the optimized phosphor. White LEDs were fabricated by pasting the optimized green (G) and the red (R) phosphors, and the commercial yellow (Y) phosphor on the blue chips. The three-band pc-WLED resulted in improved color rendering index (CRI) and corrected color temperature (CCT), compared with those of the two-band pc-WLED.

Synthesis and Luminescent Properties of $RE^3+(Eu^3+\;and\;Tb^3+$) Ions Activated CaGd4O7 Novel Phosphors

  • Pavitra, E.;Raju, G.Seeta Rama;Ko, Yeong-Hwan;Yu, Jae-Su
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.359-359
    • /
    • 2012
  • Trivalent rare-earth ($RE^{3+}=Eu^{3+}\;and\;Tb^{3+}$) ions activated $CaGd_4O_7$ phosphors were synthesized by a sol-gel process. After annealing at $1,500^{\circ}C$, the XRD patterns of the phosphor confirmed their monoclinic structure. The photoluminescence excitation spectra of $Eu^{3+}$ and $Tb^{3+}$ doped $CaGd_4O_7$ phosphor shows the broad-band excitations in the shorter wavelength region due to charge transfer band of completely filled $O^{2-}$ to the partially filled $Eu^{3+}$ ions and f-d transitions of $Tb^{3+}$ ions, respectively. The photoluminescence spectra show that the reddish-orange ions and green emission for $Eu^{3+}$ and $Tb^{3+}$ ions, respectively. Owing to the importance of thermal quenching property in the technological parameters, the temperature-dependent luminescence properties of these phosphors were measured for examing the suitability of their applications in the development of light emitting diodes (LEDs). In addition to those measurements, the cathodoluminescence properties were examined by changing the acceleration voltage and filament current. The calculated chromaticity coordinates of these phosphors were close proximity to those of commercially available phosphors for LED and field emission display devices.

  • PDF

사파장 백색 발광 다이오드의 발광 특성 (Luminescent Properties of Four-Band White Light Emitting Diodes)

  • 허영덕;임수미
    • 대한화학회지
    • /
    • 제47권4호
    • /
    • pp.370-375
    • /
    • 2003
  • 보라색 발광 다이오드에 의해 여기되어 청색, 녹색, 적색을 발광하는 형광체로 각각 $BaMg_2Al_16O_27:Eu,\SrGa_2S_4:Eu$, ZnCdS:Ag,Cl 형광체를 선택하였다. 보라색 발광 다이오드의 발광에서 형광체에 의해서 완전히 흡수되지 않고 나오는 보라색 발광과 $BaMg_2Al_16O_27:Eu,\SrGa_2S_4:Eu$, ZnCdS:Ag,Cl 형광체에서 나오는 청색, 녹색, 적색 발광을 조합하여 사파장 백색 발광 다이오드를 만들었다. 사파장 백색 발광 다이오드의 발광 특성을 확인하였다.

백색 LED용 ZnS:Mn,Cu 황색 형광체의 발광 특성 (Luminescent characteristic of ZnS:Mn,Cu yellow phosphors for Light Emitting Diodes)

  • 이지영;유일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.141-141
    • /
    • 2010
  • ZnS:Mn yellow phosphors doped with Cu for white light emitting diodes were synthesized by solid state reaction method. Photoluminescence excitation spectra originated from $Mn^{2+}$ were ranged from 450 nm to 500 nm. The yellow emission at around 580 nm was associated with $^4T_1{\rightarrow}^6A_1$ transition of $Mn^{2+}$ ions in ZnS:Mn,Cu phosphors. The highest photoluminescence intensity of the phosphors under 405 nm excitation was obtained at Cu concentration of 0.02 mol%.

  • PDF