• 제목/요약/키워드: L-particles

검색결과 931건 처리시간 0.034초

Dispersion of Li[Ni0.2Li0.2Mn0.6]O2 Powder by Surfactant for High-power Li-ion Cell

  • Yun, Su-Hyun;Park, Yong-Joon
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권7호
    • /
    • pp.1598-1602
    • /
    • 2009
  • The particle size of Li[$Ni_{0.2}Li_{0.2}Mn_{0.6}]O_2$ cathode powder was controlled effectively by dispersion using lauric acid as a surfactant. The samples treated by lauric acid showed smaller particles of approximately half the original size compared to the particles of a pristine sample. A structural change due to the dispersion of Li[$Ni_{0.2}Li_{0.2}Mn_{0.6}]O_2$ powder was not detected. The rate performance of the Li[$Ni_{0.2}Li_{0.2}Mn_{0.6}]O_2$ cathode was improved by dispersion using lauric acid, which was likely due to the decrease of the particle size. In particular, a sample dispersed pristine powder using lauric acid (L2) presented a greatly enhanced discharge capacity and capacity retention at a high C rate. The discharge capacity of a pristine sample was only 133 m$Ahg^{-1}$ (3C rate) and 96 m$Ahg^{-1}$ (12C rate) at the tenth cycle. In contrast, the L2 electrode delivered higher discharge capacities of 160 m$Ahg^{-1}$ (3C rate) and 129 m$Ahg^{-1}$ (12C rate) at the tenth cycle. The capacity retention at a rate of 12C/2C was also enhanced from ~ 45% (pristine sample) to 57% (L2) by treatment with lauric acid.

수용성 블록공중합물에서 산화티탄 분말의 흡착 안정화 (Adsorption Stabilization of $TiC_{2}$ Particles in Water Soluble Block Copolymers)

  • 권순일;정환경;최성옥;남기대
    • 한국응용과학기술학회지
    • /
    • 제18권2호
    • /
    • pp.118-126
    • /
    • 2001
  • Micelle formation and adsorption at the $Ti0_{2}$ interface of a series of polystyrene-polythylene oxide(PS-PEO) block copolymer in aqueous solution was studied using fluorescence probing and small-angle X-ray methods. Further, the stability of aqueous $Ti0_{2}$ dispersion in the presence of copolymer was investigated by microelectrophoresis, optical density and sedimentation measurements. The dissolution of pyrene as fluorescent probe in aqueous surfactant solution leads to a slow decrease of the $I_{1}/I_{3}$ ratio, as the copolymer concentration increase; $I_{1}$ and $I_{3}$ are respectively the intensities of the first and third vibrionic peaks in the pyrene fluorescence emission. The behaviour was due to the characteristics of the copolymers and/or to the copolymer association efficiency in water. Moreover, the adsorption at the plateau level increases with decreasing PEO until chain length. The zeta potential of $TiO_{2}$ particles decreases with increasing copolymer concentration and reaches a plateau value. Finally, stabilization using block copolymers was more effective with samples having higher weight fractions of PS block.

무전해 니켈 도금된 폴리스티렌 복합 입자 제조 및 도금 조건의 영향 (Preparation of Composite Particles via Electroless Nickel Plating on Polystyrene Microspheres and Effect of Plating Conditions)

  • 김병철;박진홍;이성재
    • 폴리머
    • /
    • 제34권1호
    • /
    • pp.25-31
    • /
    • 2010
  • 무전해 니켈 도금법을 사용하여 단분산 폴리스티렌 입자 표면에 니켈이 도금된 고분자 코어/금속 쉘의 복합 입자를 제조하였다. 단분산 입자는 분산중합으로 제조하였는데 사용한 분산매질의 종류에 따라 다양한 크기의 단분산 폴리스티렌 입자를 제조할 수 있었다. 그 중 직경 $3.4\;{\mu}m$ 크기의 단분산 폴리스티렌 입자를 선택하여 무전해 니켈 도금을 시도하였다. 니켈 도금에 영향을 미치는 도금 조건을 파악하기 위하여 활성화제인 $PdCl_2$의 농도, 착화제인 glycine의 농도와 니켈 도금액의 투여 시간에 따른 니켈 도금된 폴리스티렌 복합 입자의 모폴로지를 관찰하였다. 본 연구조건하에서는 $PdCl_2$의 농도 0.4 g/L, glycine 농도 1 M 이상인 경우 폴리스티렌 입자 위에 균일한 두께의 니켈층을 형성하였고 석출되는 니켈도 적었다. 도금 시간 2 시간 중에서 동일양의 도금액을 투여 속도를 달리하며 도금한 경우 모폴로지 상의 뚜렷한 차이는 없었으나 0.15 mL/min 속도로 1시간 동안 투여한 경우가 상대적으로 균일한 도금 특성을 보여 주었다.

생균제의 부형제(운반체)로서의 난각분말의 특성 (Characteristics of Eggshell Powder as Carriers of Probiotics)

  • 이우도;우개민;임정민;이권정;이봉주;김강웅;김경덕;허상우;한현섭;김수기
    • 생명과학회지
    • /
    • 제28권1호
    • /
    • pp.90-98
    • /
    • 2018
  • 계란 가공 부산물인 난각(ES: Eggshell)은 탄산칼슘 함량이 높아 사료에 첨가하여 칼슘원으로 이용되고 있다. 본 연구에서는 ES를 생균제의 부형제인 운반체로서 활용 가능성을 처음으로 시도하였다. L. plantarum을 대두박(SBM: Soybean meal), 난각조각(ESL: Eggshell powder with large particles), 난각미세분말(ESF: Eggshell powder with fine particles), 그리고 이들의 복합운반체인 SBM+ESL과 SBM+ESF에 생균제를 흡착시켜 그 부착상태를 주사전자현미경으로 확인하였다. 이 중 복합운반체인 SBM+ESF는 상온에서 4주 동안 pH 7~8을 유지하면서 L. plantarum의 가장 높은 생존율을 보였다. 본 연구에 사용한 모든 생균제들은 보존기간 동안 $4^{\circ}C$에서는 높은 생존율을 보였다. $30^{\circ}C$에서는 유산균수는 크게 감소하였으나, B. licheniformis는 높은 생존율을 유지하였고 B. subtilis, B. amyloliquefaciens와 S. cerevisiae는 $2{\log}_{10}$ (CFU/g)정도 감소하였다. 상기 연구결과는 사료의 칼슘원으로 이용되는 난각미세분말(ESF)을 대두박과 혼합하여 사용하면 B. licheniformis를 비롯한 일부 생균제의 생존성을 향상시켜 부형제(운반체)로도 사용할 수 있음을 밝혔다.

한국산 나리류에서 분리한 바이러스에 관한 연구 I. Broad Bean Wilt Virus 및 Cucumber Mosaic Virus (Studies on Viruses Isolated from Lilium spp. In Korea I. Broad Bean Wilt Virus and Cucumber Mosaic Virus)

  • 장무웅;정재동
    • 한국식물병리학회지
    • /
    • 제3권3호
    • /
    • pp.223-235
    • /
    • 1987
  • 황색 모자이크 괴저조반, 위축, 기형, colour breaking의 병미을 나타내고 있는 나리류를 한국의 남부지역에서 채집하였다. 전자현미경에 의해 2종의 바이러스 입자가 분리되어, 이들의 기주범위, 혈청반응, 조즙액중의 부활화 한계, 진딧물의 전반성, 감염엽세포에 있어서 바이러스 입자의 소재양식에 의하여 2종의 바이러스를 동정하였다. Broad bean wilt virus(BBWV) : 이 바이러스는 즙액접종에 의해 8과 23종의 검정식물에 감염이 확인되었다. 복숭아혹진딧물에 의해 쉽게 전반되었다. 내열성은 $70\%$, 내희석성은 1,000배, 내보존성은 6일이였다. 바이러스 입자의 형태는 직경 약 28nm의 소구형이다. 혈청시험에서 본 바이러스는 BBWV의 항혈청과 특이적인 반응대를 형성했다. 병엽절편의 전자현미경적관찰에서는 엽육세포의 세포질, 액포, 핵내에서 바이러스 입자의 응집괴 및 결정배열상이 확인되엇고, 특히 세포질내에서는 vesicular body의 발달이 확인되었다. Cncumber mosaic virus(CMV) : 이 바이러스 입자의 형태는 직경 약30nm의 소구형이다. 본 바이러스 CMV-Y의 항혈청과 특이적인 반응대를 형성했다. 감염엽조직의 전자현미경적관찰에서는 엽육세포의 세포질 및 액포내에서 바이러스 입자의 응집괴 도는 결정배열상이 확인되었다. BBWV와 CMV를 건전한 나리류(Lilium tigrium, L. concolor, L. auratum)에 재접종한 결과 BBWV의 접종주에서는 가벼운 병징 또는 colour breaking를 나타내었고, CMV의 접종수에서는 황색 모자이크 또는 괴저조반을 나타냈다.

  • PDF

탄소나노튜브 및 실리카 입자로 강화된 하이브리드 복합재료의 기계적, 전기적 물성에 관한 연구 (Investigation of Mechanical and Electrical Properties of Hybrid Composites Reinforced with Carbon Nanotubes and Micrometer-Sized Silica Particles)

  • 오윤;유병일;안지호;이교우
    • 대한기계학회논문집A
    • /
    • 제40권12호
    • /
    • pp.1037-1046
    • /
    • 2016
  • 본 연구에서는 기계적 물성을 개선함과 동시에 전기 절연성을 부여하기 위해 에폭시 수지에 탄소나노튜브와 실리카 입자를 혼입하여 하이브리드 복합재료를 제작하였다. 두 충전제의 함량을 변화시켜 제작한 시편으로 인장강도, 영률, 동적기계분석 그리고 전기 비저항을 측정하였으며, 이를 통해 기계적, 전기적 물성을 고찰하였다. 또한 하이브리드 복합재료 시편의 기계적 물성을 평가하고자 영률을 측정한 결과와 미시역학 모델을 이용해 계산한 결과를 비교하였다. 탄소나노튜브 함량 0.6 wt%와 실리카 함량 50 wt%를 첨가하여 제작한 하이브리드 복합재료 시편에서 인장강도 및 영률은 에폭시 복합재료 시편 대비 각각 약 11 %와 35 %의 증가를 보여 가장 높은 기계적 물성을 나타내었다. 에폭시 수지에 전도성 충전제인 탄소나노튜브를 분산시키면 전기 전도성이 향상되었으며, 여기에 절연성 충전제인 실리카를 추가로 혼입한 하이브리드 복합재료 시편에서는 개선된 기계적 물성과 더불어 전기 절연성을 증대시킬 수 있었다.

Arsenic Removal from Water Using Various Adsorbents: Magnetic Ion Exchange Resins, Hydrous Ion Oxide Particles, Granular Ferric Hydroxide, Activated Alumina, Sulfur Modified Iron, and Iron Oxide-Coated Microsand

  • Sinha, Shahnawaz;Amy, Gary;Yoon, Yeo-Min;Her, Nam-Guk
    • Environmental Engineering Research
    • /
    • 제16권3호
    • /
    • pp.165-173
    • /
    • 2011
  • The equilibrium and kinetic adsorption of arsenic on six different adsorbents were investigated with one synthetic and four natural types (two surface and two ground) of water. The adsorbents tested included magnetic ion exchange resins (MIEX), hydrous ion oxide particles (HIOPs), granular ferric hydroxide (GFH), activated alumina (AA), sulfur modified iron (SMI), and iron oxide-coated microsand (IOC-M), which have different physicochemical properties (shape, charge, surface area, size, and metal content). The results showed that adsorption equilibriums were achieved within a contact period of 20 min. The optimal doses of adsorbents determined for a given equilibrium concentration of $C_{eq}=10\;{\mu}g/L$ were 500 mg/L for AA and GFH, 520-1,300 mg/L for MIEX, 1,200 mg/L for HIOPs, 2,500 mg/L for SMI, and 7,500 mg/L for IOC-M at a contact time of 60 min. At these optimal doses, the rate constants of the adsorbents were 3.9, 2.6, 2.5, 1.9, 1.8, and 1.6 1/hr for HIOPs, AA, GFH, MIEX, SMI, and IOC-M, respectively. The presence of silicate significantly reduced the arsenic removal efficiency of HIOPs, AA, and GFH, presumably due to the decrease in chemical binding affinity of arsenic in the presence of silicate. Additional experiments with natural types of water showed that, with the exception of IOC-M, the adsorbents had lower adsorption capacities in ground water than with surface and deionized water, in which the adsorption capacities decreased by approximately 60-95%.

Angiostrongylus cantonensis: Scanning Electron Microscopic Observations on The Cuticle of Moulting Larvae

  • Zeng, Xin;Wei, Jie;Wang, Juan;Wu, Feng;Fung, Feng;Wu, Xiaoying;Sun, Xi;Zheng, Huanqing;Lv, Zhiyue;Wu, Zhongdao
    • Parasites, Hosts and Diseases
    • /
    • 제51권6호
    • /
    • pp.633-636
    • /
    • 2013
  • Angiostrongylus cantonensis is a parasitic nematode that needs to develop in different hosts in different larval stages. Freshwater snails, such as Pomacea canaliculata, are the intermediate host, and rats are the definitive host. Periodic shedding of the cuticle (moulting) is an important biological process for the survival and development of the parasite in the intermediate and definitive hosts. However, there are few studies on the cuticle alterations between different stages of this parasite. In this study, we observed the ultrastructural appearance and changes of the cuticle of the 2nd/3rd stage larvae (L2/L3) and the 3rd/4th stage larvae (L3/L4) using a scanning electron microscope. We also first divided L2/L3 into late L2 and early L3. The late L2 lacked alae, but possessed a pull-chain-like fissure. Irregular alignment of spherical particles on the cuticle were noted compared to the L3. Alae appeared in the early L3. The old cuticle turned into a thin filmlike structure which adhered to the new cuticle, and spherical particles were seen regularly arranged on the surface of this structure. Regular rectangular cavities were found on the surface of L3/L4. The caudal structure of L3/L4 was much larger than that of L3, but caudal inflation, such as seen in L4, was not observed. These results are the first to reveal the ultrastructural changes of the cuticle of A. cantonensis before and after moulting of L2/L3 and L3/L4.

점토와 조류입자의 제타전위가 부상분리 효율에 미치는 영향 (Effect of Zeta Potential of Clay and Algae Particles on Flotation Efficiency)

  • 최도영;김성진;정흥조;이세일;백도현;이재욱;곽동희
    • 상하수도학회지
    • /
    • 제19권4호
    • /
    • pp.437-445
    • /
    • 2005
  • Zeta potential is a key parameter of double layer repulsion for individual particles and can usually be used to interpret the trend of coagulation efficiency. This study focused on the measurement of zeta potential of algae and clay under various experimental conditions including water characteristics (pure water, stream water, reservoir water) and coagulant dose (10~50 mg/L). Results showed that the variation of zeta potential was highly sensitive depending on the water characteristics and coagulation conditions. Zeta potential of two genera of algae (anabaena sp. and microcystis sp.) were changed highly with coagulant dosage, especially. On the basis of trajectory analysis, bubble-floc collision efficiency simulated in terms of zeta potential was fitted well with removal efficiency of chlorophyll-a from algae particles. It was found that the control of zeta potential was important for effective removal of algae particles.

패러데이 케이지와 에어로졸 하전기의 설계 및 성능평가 (Design and Performance Evaluation of a Faraday Cage and an Aerosol Charger)

  • 지준호;배귀남;황정호
    • 대한기계학회논문집B
    • /
    • 제28권3호
    • /
    • pp.315-323
    • /
    • 2004
  • An electrical cascade impactor is a multi-stage impaction device to separate airborne particles into aerodynamic size classes using particle charging and electrical detection techniques. A Faraday cage and an aerosol charger, which are basic components of the electrical cascade impactor, were designed and evaluated in this study. The low-level current response of the Faraday cage was investigated with changing particle size and air flow rate by using sodium chloride (NaCl) particles. The response of the prototype Faraday cage was very similar to that of a commercial aerosol electrometer (TSI model 3068) within ${\pm}$5% for singly-charged particles. The response linearity of the prototype Faraday cage could be extended up to flow rate of 30 L/min. For the performance evaluation of the aerosol charger the monodisperse liquid dioctyl sebacate (DOS) particles, with diameters of 0.1∼0.8$\mu\textrm{m}$, were generated using spraying from an atomizer followed by evaporation-condensation process. Typical performance parameters of the aerosol charger such as P$.$n, wall loss, and elementary charges per particle were evaluated. The performance of the prototype aerosol charger was found to be close to that of the aerosol charger used in an electrical low pressure impactor (ELPI, Dekati).