• 제목/요약/키워드: Iron-based

검색결과 1,246건 처리시간 0.027초

산화철 폐촉매로부터 수상 자성유체 제조방법 (Preparation of Water-based Magnetic Fluids with Spent Iron Oxide Catalyst)

  • 이효숙;소혜평;김종오
    • 한국자기학회지
    • /
    • 제15권1호
    • /
    • pp.37-41
    • /
    • 2005
  • 70% 이사의 결정질 마그키타이트를 함유한 산화철 폐촉매를 Attritor에서 미립화하고 계면활성제 종류별로 마그네타이트 미립자를 피복하여 물에 분산하므로 수상 자성유체를 제조하였다. Attritor를 사용하여 볼 : 시료 : 물의 중량비가 최적조건인 2000 : 100 : 100에서 60시간 동안 산화철 폐촉매를 미립화하고, 여기에 계면활성제 oleic acid 20 ml를 넣고 한시간 동안 가열한 후 물에 분산하므로 자화값이 22emu/g인 수상 자성유체를 제조하였다.

Relative Availability of Iron in Mined Humic Substances for Weanling Pigs

  • Kim, S.W.;Hulbert, L.E.;Rachuonyo, H.A.;McGlone, J.J.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • 제17권9호
    • /
    • pp.1266-1270
    • /
    • 2004
  • Humic substances include several biological active and inactive compounds that are commonly used for improving soil fertility. Use of humic substances in swine diets is a novel concept. Humic substances contain 8,700 mg/kg of iron but its bioavailability is unknown. This study was conducted to test the bioavailability of iron in humic substances for nursery pigs. One hundred twenty five pigs (Newsham, Colorado Springs, CO) were not given supplemental iron while nursing for 21 d. Pigs were weaned on d 21 and allotted to one of five treatments (four control treatments with different levels of supplemented iron; 0, 30, 70 and 88 mg/kg from ${FeSO}_4$ and one treatment with 70 mg/kg iron from humic substances). Pigs were fed diets for 5 wk ad libitum and water was accessible freely. Body weight and feed intake were measured weekly. Blood samples were taken from pigs on d 28 to measure the number of red blood cells and hemoglobin concentration. Pigs fed a diet with the humic substances grew faster (p<0.05) during the first week postweaning, but performance was not different during the entire 5 wk period. Feed intake and gain/feed were the same among treatments. The slope ratio technique was used to estimate relative iron bioavailability. The concentration of blood hemoglobin did not respond to dietary iron levels using this model. However, the number of red blood cells (106/$\mu$l) was modeled by 4.438+0.017${\times}$ 'ron (mg/kg) from ${FeSO}_4$'0.012${\times}$'ron (mg/kg) from the humic substances' Based on the comparison between the slopes (0.012 from humic substances and 0.017 from ${FeSO}_4$), iron in humic substances was 71% as available as the iron in ${FeSO}_4$. The slopes for dietary feed intake of ${FeSO}_4$ and the iron in humic substances did not differ (p>0.05). Humic substances can replace ${FeSO}_4$ as an alternative iron source for pigs at 71% relative bioavailability.

리튬-철 산화물 전극의 제조 및 전류전위 순환 특성에 관한 연구 (A Study on the Fabrication of Lithium Iron Oxide Electrode and its Cyclic Voltammetric Characteristics)

  • 정원중;주재백;손태원
    • 전기화학회지
    • /
    • 제2권3호
    • /
    • pp.156-162
    • /
    • 1999
  • 본 연구에서는 리튬전지 내 양극 재료로서 리튬-철계 산화물의 응용가능성을 모색하기 위하여 여러 제조방법에 따라 변화되는 전기화학적 특성을 고찰하고자 하였다. 철산화물에 대한 기본적인 양극 전기화학적 특성을 관찰하기 위해 철판, 철분말을 산화시켜 제작한 전극과 FeOOH 분말로 제작한 전극을 전류전위 순환실험을 실행하였다. 그 결과 철판과 FeOOH분말 전극의 경우 거의 리튬 층간의 산화-환원 반응이 일어나지 않음을 알 수 있었으며 철 분말의 산화물 전극에서는 리튬이온의 환원반응 피크는 보이나 산화반응은 거의 관찰되지 않았다. 또한 출발 물질 $FeCl_3-6H_2O,\;NaOH.\;LiOH$를 혼합하여 저온으로 가열하여 층상의 $LiFeO_2$를 합성하였으며, 출발 물질의 조성비를 바꾸어 그 영향을 조사하였다. 그 결과 NaOH의 첨가량이 증가할수록 전극의 용량과 효율은 감소하나 용량의 감소율은 작아짐을 알 수 있었다. $NaOH/FeCl_3/LiOH$의 몰 비를 2/1/7로 조성하여 합성하였을 때 가장 큰 용량을 보였으나 효율은 30회 순환 후 급격히 감소하였다.

고고학 자료로 본 흉노의 철기문화 -중국 중원계 철기와의 비교를 중심으로- (New Perspectives on the Xiongnu Iron Works based on Archaeological Study)

  • 문재범
    • 헤리티지:역사와 과학
    • /
    • 제46권4호
    • /
    • pp.64-77
    • /
    • 2013
  • 현재의 몽고와 바이칼(Baikal) 호 서부, 투바(Tuva), 카자흐스탄(Kazakhstan), 중국 황하 상류 지구 및 신강(新疆) 등 광대한 지역에 분포했던 흉노의 철기문화는 전체적으로 유목문화의 특징을 선명하게 보여주고 있다. 철기제조기술 발생 이후 농업경제 위주의 중국 중원지구에서는 식량생산량의 증가가 명백하게 일어났다. 이것은 철제 농공구가 청동제 농공구에 비하여 내마모성과 인장강도가 강하며 파손 시 수리가 용이한 점 등 농경에 더욱 적합한 기계적 성능을 지녔기 때문이다. 때문에 농경지구에서는 다양한 철제 농경도구가 생산되었다. 그러나 흉노는 유목경제에 기초하고 있었기 때문에 철제생산도구의 사용이 유발하는 식량 생산력의 증가와 생산구조의 변화 정도가 높지 않았다. 다만, 군사 무기 방면에서의 변화는 비교적 컸다. 철기제작기술 보급 이후 원사무기(遠射武器) 위주의 흉노 무기 체계의 위력이 눈에 띄게 강해졌다. 게다가 이 시기에 흉노가 말 위에서 활을 쏘며 돌격하는 기사전술(騎射戰術)을 적극 활용하면서 흉노의 철제무기의 위력은 더욱 배가되었다. 이처럼 철기가 생산도구의 생산성 향상에 미친 영향보다 전쟁무기의 성능 향상에 미친 영향이 더욱 컸던 것이 유목경제를 기반으로 하고 있는 흉노 철기문화의 중요한 특징 중 하나이다. 비록 중국 중원계 철기문화의 영향력이 강하기는 하나 두 지역의 자연환경과 경제구조의 차이가 크기 때문에 철기문화가 발생한 이후 중원지역과 흉노지역은 사회 발전 방향의 차이가 발생했으며, 이러한 점은 철기문화에도 그대로 반영되어 나타난다. 철기제작기술이 전래된 뒤에도 흉노는 자신들의 경제방식을 계속 유지하였다. 때문에 그들이 사용했던 철제 생산도구는 앞선 시기의 청동제 생산도구와 형태상의 변화가 거의 없으며 흉노의 영역 내에서 철기문화의 공통성은 광범위하게 유지되었다.

전기분해를 이용한 난삭재의 다이아몬드 미세가공 (Diamond micro-cutting of the difficult -to -cut materials using Electrolysis)

  • 손성민;손민기;임한석;안중환
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 추계학술대회 논문집
    • /
    • pp.951-954
    • /
    • 2000
  • This paper presents a new cutting method, i.e. diamond cutting, aided by electrolysis, in order to cut ferrous materials with diamond tools. Diamond cutting is widely applied in manufacturing ultraprecision parts such as magnetic disk, polygon mirror, spherical/non-spherical mirror and copier drum, etc. because of the diamond tool edge sharpness. In general, however, diamond cutting cannot be applied to cutting steels, because diamond tools wear excessively in cutting iron based materials like steel due to their high chemical interaction with iron in high temperature. In order to suppress the diffusion of carbon from the diamond tool and to reduce increase of cutting force due to size effect, we attempt to change chemically the compositions of iron based materials using electrolysis in a limited part which will be soon cut. Through experiments under several micro-machining and electrolysis conditions, cutting using electrolysis, compared to conventional cutting, was found to result in a great decrease of the cutting force, a better surface and much less wear tool.

  • PDF

구상 흑연 주철의 고온 변형 거동 (The High Temperature Deformation Behavior of Ductile Cast Iron)

  • 유위도;나영상;이종훈
    • 한국주조공학회지
    • /
    • 제22권1호
    • /
    • pp.11-16
    • /
    • 2002
  • Hot deformation behavior of GCD-50 cast iron has been investigated by employing the compressive test. Phenomenological deformation behaviors, which were modeled based on the dynamic materials model and the kinetic model, have been correlated with the microstructural change taken place during compression. Microstructural investigation revealed that the adiabatic shear band caused by the locallized deformation was taken place in low temperature and high strain rate. On the other hand, the wavy and curved grain boundaries, which repersent the occurrence of dynamic microstructure change such as dynamic recovery and dynamic recrystallization, were observed in high temperature and low strain rate. Deformation model based on hyperbolic sine law has also been suggested.

P-Q Circle Diagram Based Parameter Measurement for Permanent Magnet Synchronous Motor Including Iron Loss

  • Urasaki, Naomitsu;Senjyu, Tomonobu;Uezato, Katsumi
    • Journal of Power Electronics
    • /
    • 제3권1호
    • /
    • pp.55-61
    • /
    • 2003
  • This paper presents parameter measurement for permanent magnet synchronous motors based on the P-Q circle diagram. Three electrical parameters of permanent magnet synchronous motors, i.e., the equivalent iron loss resistance, armature inductance, and electrical motive force (emf) coefficient are simultaneously measured. The advantages of this method are that it can be implemented under constant excitation and it dispenses with the generating test for the emf coefficient. The proposed method is applied to a 160w permanent magnet synchronous motor, and then the measurement results are analyzed.

니켈계 용사층의 조직 및 열피로 특성 (Microstructure and Thermal Fatigue Properties of Flame-Sprayed Nickel-Based Coatings)

  • 김형준;권영각
    • 한국표면공학회지
    • /
    • 제29권3호
    • /
    • pp.163-175
    • /
    • 1996
  • Flame-sprayed Ni-based coatings are investigated in order to improve the thermal fatigue properties of gray cast iron in the presence of water spraying. The results of thermal cycling tests from room temperature to $1100^{\circ}C$ indicate that thermal fatigue endurance is increased in the order of Ni-20%Cr, NiCr-6%Al, and Ni-5%Al. The thermal fatigue failure is caused by the formation of iron oxides between the coating and the substrate and then the thermal fatigue cracks have propagated either along the brittle iron oxide layer resulting in the spatting of the coatings in case of Ni-5%Al and NiCr-6%Al coatings or to the substrate resulting in the whole specimen fracture in case of Ni-20%Cr coating. It seems that the most governing factor for thermal fatigue resistance is the thermal expansion coefficient difference between the coating and the substrate. Microstructural variations before and after the tests are also discussed.

  • PDF

Identification of Proteins Affected by Iron in Saccharomyces cerevisiae Using Proteome Analysis

  • Lieu Hae-Youn;Song Hyung-Seok;Yang Seung-Nam;Kim Jae-Hwan;Kim Hyun-Joong;Park Young-Doo;Park Cheon-Seok;Kim Hae-Yeong
    • Journal of Microbiology and Biotechnology
    • /
    • 제16권6호
    • /
    • pp.946-951
    • /
    • 2006
  • To study the effect of iron on Saccharomyces cerevisiae, whole-cell proteins of Saccharomyces cerevisiae were extracted and subjected to two-dimensional polyacrylamide gel electrophoresis (2D-PAGE), and differentially expressed proteins were identified. The proteins separated were further identified by matrix-assisted laser desorption/ionization time-of-flight (MALDI-TOF) mass spectrometry and were compared with a protein database. Of more than 300 spots separated by molecular weight and isoelectric points, 27 differentially expressed spots were identified. Ten proteins were found to be differentially expressed at high iron concentration. Triosephosphate isomerase (TPI), YDR533C hypothetical protein, superoxide dismutase (SOD), 60 kDa heat-shock protein (HSP60), pyruvate dehydrogenase beta subunit 1 (PDB1), and old yellow enzyme 2 (OYE2) were upregulated, whereas thiol-specific antioxidant (TSA), regulatory particle non-ATPase subunit 8 (RPN8), thiol-specific peroxiredoxin 1 (AHP1), and fructose-1, 6-bisphosphate adolase (FBA) were downregulated by iron. Based on the result, we propose that SOD upregulated by iron would protect the yeast from oxidative stress by iron, and that TSA downregulated by iron would render cells hypersensitive to oxidative stress.

전통 제철실험을 통해 생산된 단조박편의 재료과학적 특성 연구 (A Study on the Metallurgical Characteristic of Hammer Scale Produced through Traditional Iron-making Experiments)

  • 조성모;조남철
    • 보존과학회지
    • /
    • 제37권6호
    • /
    • pp.738-747
    • /
    • 2021
  • 제철원료별 직접제련법 복원실험으로 생산된 단조박편의 재료과학적 분석을 통해 금속학적 특성을 규명하였다. 제련을 위해 경주감포사철과 양양철광석을 이용하며, 각각 4개의 그룹을 설정하였다. 분석은 주성분, 광물 동정, 미세조직 관찰을 하였다. 주성분 분석 결과 정련·단접이 진행될수록 Fe의 함량은 증가하고 비금속개재물의 함량은 감소하였다. 광물을 동정한 결과 산화철 계열의 광물이 확인되었다. 미세조직 관찰 결과 Wüstite, Fayalite가 관찰되었으며, 일부에는 응집된 Wüstite가 관찰되었다. 일부 다각형, 장주상의 Magnetite도 확인되었다. 또한, 공극 및 불순물, 비금속개재물은 점차 감소하였다. 차후 다양한 제철원료를 이용한 복원실험을 통해 생산된 단조박편의 재료과학적 분석을 통해 금속학적 특성을 규명하고, 이를 유적에서 출토된 단조박편과 비교·검토하는 것이 필요하다.