PURPOSES : This study was performed to evaluate the possibility of Indirect Tensile Strength (ITS) as a testing method that can predict cracking on pavement. METHODS : Three asphalt binders and one kind of aggregate were used in this study, and all asphalt mixtures were produced using Gyratory Compactor followed asphalt mix design. The ITS test was performed for the mixture which are artificially short-term aged using the oven. The ITS properties were analyzed by air void, compaction temperature, asphalt content, and asphalt binder. RESULTS : The results of this study indicated that (1) the compaction temperature did not show relationship with the ITS test; (2) there was no specific trend between the asphalt content and the ITS test; (3) the ITS could reveal the property of kinds of asphalt binders; (4) the asphalt mixture that were produced at optimum temperature suggested by manufacturer did not exhibit optimum result for all asphalt binder. CONCLUSIONS : The possibility of ITS was confirmed from this study for replacement of the Marshall Stability method. However, it needs to perform in further studies of aggregate and compaction property to suggest a new ITS standard value.
The indirect tensile strengths (ITSs) of different cemented paste backfill mixes with different curing times were determined by considering crack initiation and fracture toughness concepts under different loading conditions of steel loading arcs with various contact angles, flat platens and the standard Brazilian test jaw. Because contact area of the ITS test discs developes rapidly and varies in accordance with the deformability, ITSs of curing materials were not found convenient to determine under the loading apparatus with indefinite contact angle. ITS values increasing with an increase in contact angle can be measured to be excessively high because of the high contact angles resulted from the deformable characteristics of the soft paste backfill materials. As a result of the change of deformation characteristics with the change of curing time, discs have different contact conditions causing an important disadvantage to reflect the strength change due to the curing reactions. In addition to the experimental study, finite element analyses were performed on several types of disc models under various loading conditions. As a result, a comparison between all loading conditions was made to determine the best ITSs of the cemented paste backfill materials. Both experimental and numerical analyses concluded that loading arcs with definite contact angles gives better results than those obtained with the other loading apparatus without a definite contact angle. Loading arcs with the contact angle of $15^{\circ}$ was found the most convenient loading apparatus for the typical cemented paste backfill materials, although it should be used carefully considering the failure cracks for a valid test.
PURPOSES : The objective of this study is to evaluate the physical properties of recycled asphalt mixtures reinforced with glass fiber. METHODS : Firstly, mixing design was conducted on recycled asphalt mixture for use of 50% recycled aggregate. Various laboratory tests were performed on four types of recycled asphalt mixtures with different glass fiber content to evaluate the physical properties. The laboratory tests include indirect tensile strength test, dynamic modulus test, Hamburg wheel tracking test and tensile-strength ratio to evaluate cracks, rutting and moisture resistance of mixtures. RESULTS : The indirect tensile strength of fiber reinforced glass increased about 139.4%. As a result of comparing the master curves obtained by the dynamic modulus test, the elasticity was low in the low temperature region and high in the high temperature region when the glass fiber was reinforced. The glass fiber contents of PEGS 0.3%, Micro PPGF 0.1% and Macro PPGF 0.3% showed the highest moisture resistance and rutting resistance. CONCLUSIONS : The test results show that use of glass fiber reinforcement can increase the resistance to cracking, rutting, and moisture damage of asphalt mixtures. It is also necessary to validate the long-term performance of recycled asphalt mixtures with glass fiber using full scale pavement testing and field trial construction.
본 연구는 폐폴리에틸렌필름(폐비닐)을 아스팔트 혼합물에 첨가하여 아스팔트 포장재료의 품질특성을 향상시키고 환경적으로 문제가 되고 있는 폐비닐을 재활용하기 위한 연구의 일환으로 수행되었다. 폐비닐 사용시 나타날 수 있는 포장체의 특성을 파악하기 위하여 국내에서 가장 많이 수거되는 LDPE 폐비닐을 사용하여 현장에서의 실용성을 고려한 건식혼합법으로 아스팔트 혼합물을 제조하였다. 제조한 혼합물에 대하여 마샬안정도 시험, 간접인장강도 시험, 반복주행시험 및 피로시험을 수행한 결과 폐비닐을 혼합한 혼합물이 일반혼합물에 비하여 인장강도가 향상되고 윤하중에 의한 소성변형 저항성 및 피로균열 저항에 크게 효과적인 것으로 나타났다.
본 연구에서는 회수아스팔트 혼합물의 재활용을 위해서 상온재생 아스팔트 혼합물과 재래식 밀입도 13mm 아스팔트 혼합물을 사용하여 아스팔트 혼합물의 실험적 공용특성을 파악하기 위하여 간접인장강도 시험과 피로파괴 시험을 수행하였다. 간접인장강도 시험은 $10^{\circ}C,\;20^{\circ}C$에서 수행되었으며, 피로파괴시험은 500kgf, 400kgf 그리고 300kgf의 반복하중 아래에서 수행되었다. 간접인장강도 시험결과 재생 아스팔트 혼합물은 재래식 아스팔트 혼합물에 대해서 각 온도대별 약 90%의 성능을 보였으며, 피로파괴 시험의 결과에 의하면 재생 밀입도 아스팔트 혼합물은 반복하중 500kgf, 400kgf, 및 300kgf에 대해서 각각 재래식 아스팔트 혼합물의 70%, 55%, 30%의 성능을 보여주었다.
This paper investigates the effect of the jaw's curvature, also known by contact angle and jaw arc central angle (2α), of the Brazilian test apparatus on indirect tensile strength of various rock types. That's why, ten rock samples including limestone, marble, skarn, granite, diorite, and granodiorite were collected from some quarries in different provinces of Iran. Petrographic, mineralogical and textural investigations were performed using thin section analyses. Physical properties of the selected rock samples namely dry and saturated unit weights, porosity, water absorption, and specific gravity were determined for the rock samples. In addition, Brazilian tensile strength at different 2α angles (i.e., 2α = 0°, 10°, 15°, 20°, 45°, and 60°) were determined for the rocks in the laboratory. Results show that the parameter for the rocks is between 3.81 MPa at 2α=0° and 54.76 MPa at 2α=60°. This means that Brazilian tensile strength increased with increasing 2α angle from 0° to 60°. Also, it was found that the highest change rate of the Brazilian tensile strength occurs in range of 2α=15°-30° for most studied rock samples. In some tested samples, the parameter is decreased only at 2α = 60°. The values of Brazilian tensile strength of the rocks tested by flat and standard jaws are near to each other.
본 연구는 동절기에 많이 발생하는 포장의 저온균열에 대한 폴리머 개질 아스팔트 혼합물의 저항 특성을 알아보기 위하여 수행하였다. 저온에서의 간접인장강도를 측정 분석한 결과 혼합물들이 $-10^{\circ}C의 저온 대에서 최대 인장강도를 나타냈다. 최대 인장강도를 보이는 온도 이하에서는 시차열 응력이 인장강도 이상으로 발생하여 내부에 손상이 발생하기 때문에 나타나는 인장강도 저하현상을 ITS 시험으로 증명하여 보였다. 저온의 시험 결과는 폴리머 개질 아스팔트 혼합물이 일반 아스팔트 혼합물에 비하여 보다 낮은 온도에서까지도 강도가 높게 나타나 폴리머 개질에 따른 효과를 보였으며, 바인더가 저온균열에 대한 저항에 큰 영향을 미치는 것으로 나타났다. 따라서 추운 지역에서는 저온균열을 예방하기 위하여 폴리머 개질 아스팔트의 사용이 추천된다.
Garcia, Victor J.;Marquez, Carmen O.;Zuniga-Suarez, Alonso R.;Zuniga-Torres, Berenice C.;Villalta-Granda, Luis J.
International Journal of Concrete Structures and Materials
/
제11권2호
/
pp.343-363
/
2017
The objective of this work was finding out the most advisable testing conditions for an effective and robust characterization of the tensile strength (TS) of concrete disks. The independent variables were the loading geometry, the angle subtended by the contact area, disk diameter and thickness, maximum aggregate size, and the sample compression strength (CS). The effect of the independent variables was studied in a three groups of experiments using a factorial design with two levels and four factors. The likeliest location where failure beginning was calculated using the equations that account for the stress-strain field developed within the disk. The theoretical outcome shows that for failure beginning at the geometric center of the sample, it is necessary for the contact angle in the loading setup to be larger than or equal to a threshold value. Nevertheless, the measured indirect tensile strength must be adjusted to get a close estimate of the uniaxial TS of the material. The correction depends on the loading geometry, and we got their mathematical expression and cross-validated them with the reported in the literature. The experimental results show that a loading geometry with a curved contact area, uniform load distribution over the contact area, loads projected parallel to one another within the disk, and a contact angle bigger of $12^{\circ}$ is the most advisable and robust setup for implementation of BT on concrete disks. This work provides a description of the BT carries on concrete disks and put forward a characterization technique to study costly samples of cement based material that have been enabled to display new and improved properties with nanomaterials.
폐타이어 재활용 아스팔트 콘크리트의 기술개발과 기초 자료의 확립을 위해서 건식공법 및 습식공법으로 생산되어진 폐타이어 재활용 아스팔트 콘크리트와 재래식 밀입도 아스팔트 콘크리트 공시체를 제작하여 아스팔트 혼합물의 내구성을 평가할 수 있는 간접인장강도시험과 회복 탄성계수시험을 수행하였다. 간접인장강도시험 결과 골재 입도의 영향으로 간접인장강도는 재래식 아스팔트 콘크리트가 폐타이어 재활용 아스팔트 콘크리트보다 우수하게 나타났지만, 인성과 최대수직변형률의 경우 골재 입도의 영향에도 불구하고 폐타이어 재활용 아스팔트 콘크리트가 우수하게 나타났다. 또한, 회복 탄성계수시험 결과에서도 폐타이어 재활용 아스팔트 콘크리트가 재래식 아스팔트 콘크리트보다 우수한 성능을 보여줌으로써 폐타이어 재활용 아스팔트 콘크리트의 공학적 특성이 우수하게 나타났다. 특히, 습식공법 활용 폐타이어 재활용 아스팔트 콘크리트의 모든 공용특성은 건식공법활용 혼합물보다 우수한 것으로 평가되었다.
본 연구에서는 시멘트 고결토 내에 실린더를 내장시킨 다음 유압으로 공시체 내부에서 인장력을 가하여 공시체를 직접 파괴시키는 직접인장시험 방법에 대한 연구를 수행하였다. 또한 기존 아령모양의 공시체를 이용한 직접인장시험과 대표적인 간접인장시험인 쪼갬인장시험을 실시하여 인장시험 방법에 따른 차이를 비교하였다. 인장시험용 공시체는 모래/시멘트비를 3:1 또는 1:1로 제작한 다음 7일 및 28일 동안 대기중 양생하였으며, 동일한 경우에 대해 10개의 공시체를 실험하여 평균값을 비교하였다. 한편 일축압축시험도 실시하여 일축압축강도와 인장강도의 비를 분석하였다. 내장형 실린더를 이용한 직접인장시험으로부터 얻은 인장강도는 아령모양 공시체를 이용한 직접인장시험으로부터 얻은 값보다 다소 높은 인장강도를 보였지만, 아령모양 공시체를 이용한 시험방법은 공시체 제작이 불편하고 시험 중 변곡부에서 파괴되는 경우가 자주 발생하였다. 탄성파괴를 일으키는 콘크리트나 암석에 적용하는 쪼갬인장시험방법으로 부터 얻은 인장강도는 표준편차가 가장 컸을 뿐 아니라, 시멘트 고결토와 같이 강도가 상대적으로 약해 탄소성파괴를 일으키는 재료에는 적용하기 어려웠다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.