• 제목/요약/키워드: INCONEL600

검색결과 119건 처리시간 0.017초

선삭가공에서 초내열합금 Inconel 600의 가공성 평가 (Estimation of Machinability for Super Heat-resistant Alloys Inconel 600 in Turning Process)

  • 원종식;임은성;정윤교
    • 한국기계가공학회지
    • /
    • 제10권6호
    • /
    • pp.1-8
    • /
    • 2011
  • Recently, super heat-resistant alloy Inconel 600 come into spotlight as the material of airplane parts but this material causes lots of problems that is, reduction of machinability and attritious wear and breakage of cutting tool during turning processing due to high temperature strength and cohesion between tool material and Inconel 600. Therefore, in this study, it was purposed to determine tool material kind and to select of proper cutting range when turning process was carried out for Inconel 600. In order to these Purpose, coated carbide tool and ceramic tool was used in this experiment and the machinability of Inconel 600 was investigated from perspective of the cutting force, chipping and wear of tool and deposition phenomenon of chip.

겹치기 마찰교반접합된 Inconel 600/SS 400 합금의 미세조직과 기계적 특성 평가 (Evaluation of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Inconel 600/SS 400)

  • 송국현
    • 한국재료학회지
    • /
    • 제22권3호
    • /
    • pp.123-129
    • /
    • 2012
  • The microstructures and mechanical properties of friction stir welded lap joints of Inconel 600 and SS 400 were evaluated; friction stir welding was carried out at a tool rotation speed of 200 rpm and welding speed of 100 mm/min. Electron back-scattering diffraction and transmission electron microscopy were introduced to analyze the grain boundary characteristics and the precipitates, respectively. Application of friction stir welding was notably effective at reducing the grain size of the stir zone. As a result, the reduced average grain size of Inconel 600 ranged from $20{\mu}m$ in the base material to $8.5{\mu}m$ in the stir zone. The joint interface between Inconel 600 and SS 400 showed a sound weld without voids and cracks, and MC carbides with a size of around 50 nm were partially formed at the Inconel 600 area of lap joint interface. However, the intermetallic compounds that lead to mechanical property degradation of the welds were not formed at the joint interface. Also, a hook, along the Inconel 600 alloy from SS 400, was formed at the advancing side, which directly brought about an increase in the peel strength. In this study, we systematically discussed the evolution of microstructures and mechanical properties of the friction stir lap joint between Inconel 600 and SS 400.

오스테나이트계 스테인리스강과 니켈합금의 해수 농도 변화에 따른 전기화학적 부식 손상 특성 (Electrochemical Corrosion Damage Characteristics of Austenite Stainless Steel and Nickel Alloy with Various Seawater Concentrations)

  • 허호성;김성종
    • Corrosion Science and Technology
    • /
    • 제20권5호
    • /
    • pp.281-288
    • /
    • 2021
  • Due to advancement of the industry, operation of a device in a harsh environment is increasing. Especially, the marine environment contains Cl- ions which causes localized corrosion such as pitting and crevice corrosion of stainless steel and various metals. In this study, electrochemical corrosion behaviors of austenitic stainless steel (STS 316L) and nickel alloy (Inconel 600) with different seawater concentrations (fresh water, seawater, mixed water) were investigated. The STS 316L and Inconel 600 were etched in 10% oxalic acid and composed of an austenitic phase. Results of Tafel analysis in seawater showed that STS 316L and Inconel 600 presented the highest corrosion current densities of 7.75 × 10-4 mA/cm2 and 1.11 × 10-4 mA/cm2 and the most negative pitting potentials of 0.94 V and 1.06 V, respectively. The maximum damage depths and surface damage ratio by pitting corrosion increased with chloride concentration. The STS 316L had higher PREN than Inconel 600. However, the surface damage and weight loss of Inconel 600 were superior to STS 316L. It was difficult to compare the pitting resistance of STS 316L based on Fe and Inconel 600 based on Ni with PREN simply.

Inconel 600 및 690 튜브 재질의 일반 부식에 관한 실험적 연구 (An Experimental Research on Uniform Corrosion of Inconel 600 and 690 Tubing Material)

  • 염유선;황정래;전인섭;김숭평;윤장희
    • 방사성폐기물학회지
    • /
    • 제4권2호
    • /
    • pp.103-116
    • /
    • 2006
  • 본 논문은 국내 PWR 발전소에서 S/G tube 재질로 사용되고 있는 Inconel 600 및 690에 대한 부식 실험을 수행함으로써 작업자들의 주요 피폭원인 $^{58}Co,\;^{60}Co,\;^{51}Cr,\;^{54}Mn,\;^{59}Fe$의 생성량을 예측하고자 하였다. 이를 위해 Inconel 600 및 690 재질로 총 12개의 시편을 제작하여 실제 발전소의 운전조건과 유사하거나 가혹한 조건에서 전면 부식실험을 pH별로 20일씩 총 60일간 수행하였고, 실험 결과를 정량적으로 분석하기 위해 GDS(Glow Discharge Spectrometer) 장비를 사용하였다. GDS 장비를 이용하여 정량적으로 분석한 결과 pH 7 및 9에서는 Inconel 600이 Inconel 690에 비해 부식이 잘 되는 것으로 나타난 반면, pH 4에서는 Inconel 690이 부식이 더 잘 되는 것으로 평가되었다. 이러한 경향을 보이는 것은 과도상태의 영향이 과도하게 반영된 것에 기인한 것으로 비교적 정확한 결론을 도출하기 위해서는 장시간의 부식 실험을 수행함으로써 과도상태에 의한 영향을 최소화해야 할 것으로 판단된다.

  • PDF

nconel 600위에 증착된 TiN 박막의 고온 NaCl 수용액에서의 CPP 실험에 의한 핏팅저항성의 연구 (A Study on Pitting Resistance of TiN Film Coated on Inconel 600 by CPP Test in High Temperature NaCl Solution)

  • 김용일;정한섭;김홍회;이원종
    • 한국세라믹학회지
    • /
    • 제32권11호
    • /
    • pp.1301-1307
    • /
    • 1995
  • Pitting corrosion of TiN film deposited on Inconel 600 by plasma assisted chemical vapor deposition (PACVD) was investigated. Cyclic potentiodynamic polarization (CPP) tests were conducted in order to determine the pit nucleation potentials, Enp, of the TiN-deposited sample and the bare Inconel 600 in deaerated NaCl solution at 25, 135 and 20$0^{\circ}C$. The effects of the TiN film thickness, the solution temperature and the Cl- concentration on Enp were studied. Enp of the TiN-deposited sample which had the film thickness above 1${\mu}{\textrm}{m}$ were higher than those of the bare Inconel 600 by 300~600mV at all the solution temperatures, implying the pitting resistance improvement of the TiN film. The morphologies of the pits generated after immersion test were examined with a scaning electron microscopy. The higher was the solution temperature, the more corrosion products, mainly composed of Cr and Ni oxides, were formed.

  • PDF

공기중에서 인코넬-지르칼로이 접촉의 프레팅 마멸특성 (Fretting Wear Characteristics of Inconel-Zircaloy Contact in Air)

  • 노규철;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제29회 춘계학술대회
    • /
    • pp.310-316
    • /
    • 1999
  • The fretting wear characteristics of the contact between Zircaloy-4 tube and Inconel 600 tube have investigated. Zircaloy-4 is used for fuel rod in nuclear reactor and Inconel 600 is used for tube In steam generator of nuclear power plant. A fretting wear tester was designed to be suitable for this fretting test. In this study, the number of cycles, slip amplitude and normal load were selected as main factors of fretting wear. This study shows that the wear scar length of Zircaloy-4 and Inconel 600 increases as number of cycles, normal load and slip amplitude increase and the wear scar length of Zircaloy-4 is more longer than that of Inconel 600 due to the surface hardness.

  • PDF

상온 대기 중에서 인코넬 600과 690의 슬라이딩 마모 (Sliding wear of Inconel 600 and 690 in room temperature air)

  • 홍동석;김경국;김준기;김선진
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 추계학술발표강연 및 논문개요집
    • /
    • pp.91-91
    • /
    • 2003
  • Sliding wear behaviors of Inconel 600 and 690 were investigated at room temperature in air. In the present study, Archard's equation which has low reliability was modified. In the prediction of wear volume by Archard's equation, the reliabilities of Inconel 600 and 690 were about from 26.3% to 45.7% and from 69. l% to 88.6%, respectively, The sliding wear behaviors of Inconel 600 and 690 turned out to be influenced by their stacking fault energy, and the fact was confirmed by using TEM and micro-hardness test Based on experimental results, the wear coefficient was modified as a function of the sliding distance. The calculation with the modified wear equation showed that the reliability of Inconel 600 tested with 409 ferritic stainless steel increased from 45.7% to 93.4%.

  • PDF

고온 리튬용융염에서 Ni 200 및 Ni-base 합금의 부식거동 (Corrosion Behavior of Ni 200 and Ni-base Alloys in Hot Lithium Molten salt)

  • 조수행;임종호;윤기석;박성원
    • 한국재료학회지
    • /
    • 제14권4호
    • /
    • pp.251-259
    • /
    • 2004
  • In the development of the advanced spent fuel management process based on the molten salt technology, it is essential to choose the optimum material for the process equipment handling molten salt. Corrosion behavior of Ni 200 and Ni-base alloys in molten salt of LiCl-$Li_2$O under oxidation atmosphere was investigated in the temperature range of $650~800^{\circ}C$ for 24~312 hrs. The order of corrosion rate was Ni 200 > Inconel 690 > Inconel 601 > Inconel 600. Inconel 600 alloy showed the highest corrosion resistance among the examined alloys, but Ni 200 exhibited the highest corrosion rate. Corrosion products of Inconel 600 and Inconel 601 were $Cr_2$$O_3$ and $NiFe_2$$O_4$. In case of Inconel 690, a single layer of $CrO_2$$O_3$ was formed in the early stage of corrosion and an outer layer of $NiFe_2$O$_4$ and inner layer of $Cr_2$$O_3$ were formed with increase of corrosion time. Inconel 600 showed local corrosion behavior and Inconel 601, 690 showed uniform corrosion behavior.

Magnetic NDE for Sensitization of Inconel 600 Alloy

  • Kikuchi, Hiroaki;Sumimoto, Takaki;Kamada, Yasuhiro;Kobayashi, Satoru
    • Journal of Magnetics
    • /
    • 제18권3호
    • /
    • pp.348-351
    • /
    • 2013
  • Inconel 600 alloy, Ni base alloy, is widely used for steam generator tubings where sensitization occurs at grain boundaries and sensitization will induce tubing failures. This alloy has usually paramagnetic property, however, it transforms into ferromagnetic property along grain boundaries when sensitization occurs: this means NDE using magnetism for sensitization is possible. Therefore, in this study, Inconel 600 alloys were heat treated at 873 K from 0 to 400 hours so as to generate sensitization and their magnetic properties were investigated in detail. The saturation and the residual magnetization increase with increasing heat treatment time and take a maximum. On the other hand, the coercive force decreases with the increase in time of heat treatment. We confirmed that characteristics at only grain boundaries change into ferromagnetic phase by a MFM observation. As a trial for industrial application, heat treated Inconel 600 alloy was scanned by a magnetic field sensor, and the variations in magnetization were obtained nondestructively. The results indicate a feasibility of magnetic NDE for sensitization of Inconel 600 alloy.