An Experimental Study for the Failure Mode and the Ductility of a High Pier with a Hollow Section using a High Strength Cocnrete and Steel (고성능 중공단면 교각의 파괴모드 및 연성에 관한 실험적 연구)

  • Oh Byung Hwan;Choi Seung Won;Park Young Ho;Pang Gi Sung
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05a
    • /
    • pp.63-66
    • /
    • 2005
  • Six RC pier were tested under a constant axial load and a cyclically reversed horizontal load to investigate the performance of RC piers used in the high strength concrete and the high strength rebar. It is designed with a hollow section according to the Korean Bridge Design Standard. The variables of the test were concrete strength, rebar strength, a ratio of lap splice and a ratio of transvere rebar. The test results show that the performance of a RC Pier; failure mode, crack pattern, maximum load and ductility.

  • PDF

An Experimental Study on Structural Behavior of High-strength Concrete Members with Compressive Strength of 80 MPa Subjected to Flexure (휨을 받는 압축강도 80 MPa 수준의 고강도 콘크리트 부재의 구조거동 실험 연구)

  • Yang, In-Hwan;Hwang, Chul-Sung;Kim, Kyoung-Chul;Joh, Chang-Bin
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.4
    • /
    • pp.1-12
    • /
    • 2017
  • This paper concerns the structural behavior of high-strength concrete beams with compressive strength of 80 MPa subjected to flexure. Main test variables were nominal yielding strength of longitudinal rebar including normal strength rebar(SD 400) and high strength rebar(SD 600), reinforcement ratio from 0.98 to 1.58% and beam section size with $200{\times}250$, $200{\times}300mm$. The nine beams were cast and tested under flexure. The study investigated ultimate flexural strength, load-deflection relationship, crack patterns, failure patterns and ductility of the test beams. Test results indicate that when rebar ratio increased flexural strength increased and ductility decreased. In addition, the number of cracks increased and the crack width decreased as the reinforcement ratio increased. The yield strength of rebar did not affect significantly load-crack width relationship. Nonlinear analysis of test beams was performed and then test results and analytical results of ultimate load were compared. Analytical results of high-strength concrete beams overall underestimated flexural strength of test beams.

Bonding between high strength rebar and reactive powder concrete

  • Deng, Zong-Cai;Jumbe, R. Daud;Yuan, Chang-Xing
    • Computers and Concrete
    • /
    • v.13 no.3
    • /
    • pp.411-421
    • /
    • 2014
  • A central pullout test was conducted to investigate the bonding properties between high strength rebar and reactive powder concrete (RPC), which covered ultimate pullout load, ultimate bonding stress, free end initial slip, free end slip at peak load, and load-slip curve characteristics. The effects of varying rebar buried length, thickness of protective layer and diameter of rebars on the bonding properties were studied, and how to determine the minimum thickness of protective layer and critical anchorage length was suggested according the test results. The results prove that: 1) Ultimate pull out load and free end initial slip load increases with increase in buried length, while ultimate bonding stress and slip corresponding to the peak load reduces. When buried length is increased from 3d to 4d(d is the diameter of rebar), after peak load, the load-slip curve descending segment declines faster, but later the load rises again exceeding the first peak load. When buried length reaches 5d, rebar pull fracture occurs. 2) As thickness of protective layer increases, the ultimate pull out load, ultimate bond stress, free end initial slip load and the slip corresponding to the peak load increase, and the descending section of the curve becomes gentle. The recommended minimum thickness of protective layer for plate type members should be the greater value between d and 10 mm, and for beams or columns the greater value between d and 15 mm. 3) Increasing the diameter of HRB500 rebars leads to a gentle slope in the descending segment of the pullout curve. 4) The bonding properties between high strength steel HRB500 and RPC is very good. The suggested buried length for test determining bonding strength between high strength rebars and RPC is 4d and a formula to calculate the critical anchorage length is established. The relationships between ultimate bonding stress and thickness of protective layer or the buried length was obtained.

Bond behavior between high volume fly ash concrete and steel rebars

  • Liang, Jiong-Feng;Hu, Ming-Hua;Gu, Lian-Sheng;Xue, Kai-Xi
    • Computers and Concrete
    • /
    • v.19 no.6
    • /
    • pp.625-630
    • /
    • 2017
  • In this paper, 54 pull-out specimens and 36 cubic specimens with different replacement ratios of fly ash in the concrete (i.e., 0%, 20%, 30%, 40%, 50%, 60%) were fabricated to evaluate the bond at the interface between fly ash concrete and steel rebar. The results showed that the general shape of the bond-slip curve between fly ash concrete and steel rebar was similar to that for the normal concrete and steel rebar. The bond strength between fly ash concrete and the steel rebar was closer to each other at the same rebar diameter, irrespective of the fly ash replacement percentage. On the basis of a regression analysis of the experimental data, a revised bond strength mode and bond-slip relationship model were proposed to predict the bond-slip behaviour of high volume fly ash concrete and steel rebar.

Mitigation of Steel Rebar Corrosion Embedded in Mortar using Ammonium Phosphate Monobasic as Hreen Inhibitor (제 1 인산 암모늄 사용량에 따른 시멘트 모르타르의 철근방청성능 평가에 관한 실험적 연구)

  • Tran, Duc Thanh;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.112-113
    • /
    • 2021
  • Phosphate based inhibitor is playing a decisive role in inhibiting the corrosion of steel rebar in chloride condition. We have used different amount of ammonium phosphate monobasic (APMB) as corrosion inhibitor in mortar with different amount of chloride ions. The compressive strength, flexural strength, open circuit potential (OCP), electrochemical impedance spectroscopy (EIS), potentiodynamic polarization resistance (PPR), scanning electron microscopy (SEM) and Raman spectroscopy were performed to access the effect of inhibitor on corrosion resistance. As the amount of inhibitor is increased, the compressive strength increased. The electrochemical results show that as the amount of inhibitor and chloride ions are increased, the total impedance and corrosion resistance of steel rebar increased attributed to the formation of the stable oxide films onto the steel rebar surface. It is suggested that APMB can work in high concentration of chloride ions present in concrete where phosphate ion helps in formation of stable and protective phosphate based oxide film.

  • PDF

Mock-up Test for Nuclear Power Plant Rebar Modulation Applying Febrication (선조립공법을 활용한 원전구조물 철근모듈화 Mock-up 실험연구)

  • Lim, Sang-Jun;Lee, Byung-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2015.05a
    • /
    • pp.13-14
    • /
    • 2015
  • To minimize construction of nuclear facility, it is required to reduce reinforcing bar amount and solve reinforcing bar concentration and for this, it is necessary to develop appication design technology and modular of high strength reinforcing bar. Hence, KHNP reduces excessive reinforcing bar amount which can cause possibility of poor construction of concrete through design standard development and modular of nuclear facility structure using high strength reinforcing bar to raise economics and has its purpose to maintain high-level safety and durability as they are. After reviewing the rebar drawing of the NPP structures and performing the mock-up test, the rebar modulation method in the various area of the NPP Structure has been established.

  • PDF

An Empirical Study for Cost Saving Effect Analysis When Using Seismic Reinforcing Bar (내진 보강용 철근 사용 시 비용 절감 효과 분석을 위한 실증적 연구)

  • Lee, Jong-Sik
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.20 no.4
    • /
    • pp.120-127
    • /
    • 2016
  • Due to the enlargement and high-rise of reinforced concrete structure, the application of high functional material is required. However, high-strength bar is recently introduced to the country and the material is insufficient to measure the variation of quantity of rebar quantitatively when using high-strength bar. For these reasons, this study is to provide useful data in cost decision making when applying high-strength bar at a stage of architectural project planning. For residence-commerce complex buildings, we set up six types of conditions such as in case of using only rebar, in case of using only high-strength bar, in case of using rebar mixed with high-strength bar and so on. With the standard of study model 1 that applies only SD400 regardless of rebar diameter, the analyzed result of rebar variation and the cost change of construction in other study model is as follows. When the rebar amount and cost in study model I was 100%, each ratio was 88.3% and 90.5% in study model II, 80.2% and 83.4% in study model III, 91.9% and 93.5% in study model IV, 88.9% and 87.7% in study model V and 82.4% and 85.5% in study model VI. Therefore, in case of rebar amount and construction cost, study model III was evaluated as the best that was applied only SD600.

The Effect of Variation of Design Parameters on the Flexural Behavior of UHPFRC Beams (UHPFRC 보 휨 거동에 대한 설계변수 변동의 영향)

  • Yang, In-Hwan;Kim, Kyung-Chul;Park, Ji-Hun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.2
    • /
    • pp.138-145
    • /
    • 2018
  • This paper studies the bending behavior of ultra-high-performance fiber-reinforced concrete (UHPFRC) beams focused on the effect of variation in major material design parameters such as tensile strength, elastic modulus of UHPFRC, and rebar ratio. Analytical results show that the variation in the range of ${\pm}20%$ in the tensile strength of UHPFRC causes the significant difference in ${\pm}8{\sim}9%$ of bending strength compared to the reference condition. The variation of elastic modulus in UHPFRC rarely causes the effect on the bending strength of the UHPFRC section, whereas causes the difference in the slopes of moment-curvature curves, indicating different bending stiffness of UHPFRC sections. For the rebar with yield strength of 400MPa, the bending strength of SC120f is increased by 30, 67, and 99% when the rebar ratio is 1.0, 1.5, and 20%, respectively, compared to the rebar ratio of 0.5%. Therefore, it is observed that the variation of rebar ratio significantly affects the difference in bending strength of UHPFRC beams. However, as the compressive strength of UHPFRC becomes greater, the effect of rebar ratio on the increase of bending strength is decreased.

The properties of hybrid FRP rebar for concrete structures (콘크리트 보강용 하이브리드 FRP 리바의 특성)

  • 원종필;박찬기;황금식;윤종환
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.255-260
    • /
    • 2003
  • The corrosion of steel rebars has been the major cause of the reinforced concrete deterioration. It is FRP rebar that is developed to solve problem of such steel rebar. FRP rebar in concrete structures should be used as a substitute of steel rebars for that cases in which aggressive environment produce high steel corrosion, or lightweight is an important design factor, or transportation cost increase significantly with the weight of the materials. But FRP rebar have only linearly elastic behavior; whereas, steel rebar has linear elastic behavior up to the yield point followed by large plastic deformation and strain hardening. Thus, the current FRP rebars are not suitable concrete reinforcement where a large amount of plastic deformation prior to collapse in required. The main objective of this study was to develop new type of hybrid FRP rebar. The manufacture of the hybrid FRP rebar was achieved pultrusion, braiding and filament winding techniques. Tensile and interlaminar shear test results of hybrid FRP rebar can provide its excellent tensile strength-strain behavior and interlaminar stress-strain behavior.

  • PDF

Effect of cover depth and rebar diameter on shrinkage behavior of ultra-high-performance fiber-reinforced concrete slabs

  • Yoo, Doo-Yeol;Kwon, Ki-Yeon;Yang, Jun-Mo;Yoon, Young-Soo
    • Structural Engineering and Mechanics
    • /
    • v.61 no.6
    • /
    • pp.711-719
    • /
    • 2017
  • This study investigates the effects of reinforcing bar diameter and cover depth on the shrinkage behavior of restrained ultra-high-performance fiber-reinforced concrete (UHPFRC) slabs. For this, twelve large-sized UHPFRC slabs with three different rebar diameters ($d_b=9.5$, 15.9, and 22.2 mm) and four different cover depths (h=5, 10, 20, and 30 mm) were fabricated. In addition, a large-sized UHPFRC slab without steel rebar was fabricated for evaluating degree of restraint. Test results revealed that the uses of steel rebar with a large diameter, leading to a larger reinforcement ratio, and a low cover depth are unfavorable regarding the restrained shrinkage performance of UHPFRC slabs, since a larger rebar diameter and a lower cover depth result in a higher degree of restraint. The shrinkage strain near the exposed surface was high because of water evaporation. However, below a depth of 18 mm, the shrinkage strain was seldom influenced by the cover depth; this was because of the very dense microstructure of UHPFRC. Finally, owing to their superior tensile strength, all UHPFRC slabs with steel rebars tested in this study showed no shrinkage cracks until 30 days.