Basic Mixing and Mechanical Tests on High Ductile Fiber Reinforced Cementless Composites (고인성 섬유보강 무시멘트 복합체의 기초 배합 및 역학 실험)

  • Cho, Chang-Geun;Lim, Hyun-Jin;Yang, Keun-Hyeok;Song, Jin-Kyu;Lee, Bang-Yeon
    • Journal of the Korea Concrete Institute
    • /
    • v.24 no.2
    • /
    • pp.121-127
    • /
    • 2012
  • Cement has been traditionally used as a main binding material of high ductile fiber reinforced cementitious composites. The purpose of this paper is to investigate the feasibility of using alkali-activated slag and polyvinyl alcohol (PVA) fibers for manufacturing high ductile fiber reinforced cementless composites. Two mixture proportions with proper flowability and mortar viscosity for easy fiber mixing and uniform fiber dispersion were selected based on alkali activators. Then, the slump flow, compression, uniaxial tension and bending tests were performed on the mixes to evaluate the basic properties of the composites. The cementless composites showed an average slump flow of 465 mm and tensile strain capacity of approximately 2% of due to formation of multiple micro-cracks. Test results demonstrated a feasibility of manufacturing high ductile fiber reinforced composites without using cement.

Modeling of a Ductile Fracture Criterion for Sheet Metal Considering Anisotropy (판재의 이방성을 고려한 연성파단모델 개발)

  • Park, N.;Huh, H.
    • Transactions of Materials Processing
    • /
    • v.25 no.2
    • /
    • pp.91-95
    • /
    • 2016
  • This paper is concerned with modeling of a ductile fracture criterion for sheet metal considering anisotropy to predict the sudden fracture of advanced high strength steel (AHSS) sheets during complicated forming processes. The Lou−Huh ductile fracture criterion is modified using the Hill’s 48 anisotropic plastic potential instead of the von Mises isotropic plastic potential to take account of the influence of anisotropy on the equivalent plastic strain at the onset of fracture. To determine the coefficients of the model proposed, a two dimensional digital image correlation (2D-DIC) method is utilized to measure the strain histories on the surface of three different types of specimens during deformation. For the derivation of an anisotropic ductile fracture model, principal stresses (𝜎1,𝜎2, 𝜎3) are expressed in terms of the stress triaxiality, the Lode parameter, and the equivalent stress (𝜂𝐻, 𝐿,) based on the Hill’s 48 anisotropic plastic potential. The proposed anisotropic ductile fracture criterion was quantitatively evaluated according to various directions of the maximum principal stress. Fracture forming limit diagrams were also constructed to evaluate the forming limit in sheet metal forming of AHSS sheets over a wide range of loading conditions.

Evaluation of Seismic Performance of High Strength Reinforced Concrete Exterior Beam-Column Joints Using High Ductile Fiber-Reinforced Mortar (고인성섬유 복합모르타르를 활용한 고강도 철근콘크리트 외부 보-기둥 접합부의 내진성능평가)

  • Ha, Gee-Joo;Shin, Jong-Hak
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.4
    • /
    • pp.419-428
    • /
    • 2013
  • In this study, experimental research was carried out to evaluate the constructability and seismic performance of high strength R/C exterior beam-column joints regions, with or without the shear reinforcement, using high ductile fiber-reinforced mortar. Five specimens of retrofitted the exterior beam-column joint regions using high ductile fiber-reinforced mortar are constructed and tested for their retrofit performances. Specimens designed by retrofitting the exterior beam-column joint regions (BCJNSP series) of existing reinforced concrete building showed a stable mode of failure and an increased its maximum load-carrying capacity by 1.09~2.03 times in comparison with specimen of BCJNS due to the effect of enhancing dispersion of crack control at the time of initial loading and bridging of fiber from retrofitting new high ductile materials during testing. Specimens of BCJNSP series attained its maximum load carrying capacity by 0.92~0.96 times and increased its energy dissipation capacity by 1.62 times when compared to standard specimen of BCJC with a displacement ductility of 4.

A Study on Improvement of Seismic Performance of High Strength Reinforced Concrete Interior Beam-Column Joints Using High Ductile Fiber-Reinforced Mortar and Advanced Reinforcing Detailings (고인성섬유 복합 모르타르 및 고성능 배근상세를 활용한 고강도 철근콘크리트 내부 보-기둥 접합부의 내진성능 개선 연구)

  • Ha, Gee-Joo;Yi, Dong-Ryul;Hong, Kun-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.2
    • /
    • pp.233-240
    • /
    • 2013
  • In this study, experimental research was carried out to evaluate and improve the seismic performance of high strength R/C interior beam-column joints regions using advanced reinforcing detailings and high ductile fiber-reinforced mortar. Five specimens of retrofitted the beam-column joint regions using advanced reinforcing detailings and high ductile fiber-reinforced mortar were constructed and tested for their retrofitring performances. Specimens designed by retrofitting the interior beam-column joint regions (IJIR series) of existing reinforced concrete building showed a stable mode of failure and an increase in load-carrying capacity. Specimens of IJIR series, designed by the retrofitting of advanced reinforcing detailings and high ductile fiber-reinforced mortar in reinforecd beam-column joint regions increased its maximum load carrying capacity by 114.2~123.5% and its energy dissipation capacity by 1.55~1.85 times in comparison with the standard specimen of SIJC with a displacement ductility of 5.

Assessment of Flexural Ductility in RC Beams with High-Strength Reinforcement (고장력 철근을 사용한 RC 보의 휨연성 평가)

  • 권순범;윤영수;이만섭;임철현
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.897-902
    • /
    • 2001
  • Recently, structure performance is maximized by using high strength concrete. In design of structure, concrete need combination with reinforcement, but use of common strength reinforcement make member complex bar placement, so high strength concrete members require increased strength reinforcement. If common strength reinforcement replaced by equal tension area of high strength reinforcement, reinforcement ratio increase and brittle failure of member may occur by material change. So, adequate upper limit of strength ratio is required to affirm ductile behavior in application of high strength reinforcement. In this study, ductility behavior was analysed by factor of reinforcement ratio, strength of concrete and reinforcement. The result indicate that ductile failure is shown under 0.35 $\rho_{b}$ in any reinforcement strength of same section and high strength concrete of 800kg/$cm^{2}$ used commonly is compatible with reinforcement of 5500kg/$cm^{2}$.

  • PDF

Improvement of Shear Performance for High Ductile Fiber-Reinforced Mortar Slab-Column Connection in Flat Plate Structural System (고인성 복합섬유 모르타르를 이용한 플랫 플레이트 구조 슬래브-기둥 접합부의 전단성능 개선)

  • Ha Gee Joo;Kim Yun Yong;Shin Jong Hak;Yang Seung Hyeok;Hong Kun Ho;Kim Joung Su
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.145-148
    • /
    • 2005
  • Recently the construction of high-rise reinforced concrete building is progressively increased as the social demands. It is significantly important factors such as economy, the safety of structure, and the flexibility of internal space. Therefore new structural system is also required to be attained the reduction of story height, the flexibility and efficient use of space. The most suitable structural system is with the economy and flexibility, flat plate slab system in high-rise reinforced concrete building. In this research, it was focused in the improvement of shear performance in the flat plate system using high ductile fiber reinforced mortar. It was evaluated the shear performance in the critical region of slab-column connection. The flat plate system, designed by the high performance and safety, was developed as a new technique in the application of high-rise R/C building.

  • PDF

Design for Warm Forming of a Mg El-cover Part Using a Ductile Fracture Criterion (연성파괴이론에 의한 마그네슘 합금 EL-cover 부품 온간 성형 공정 설계)

  • Kim, S.W.;Lee, Y.S.
    • Transactions of Materials Processing
    • /
    • v.23 no.4
    • /
    • pp.238-243
    • /
    • 2014
  • Recently, magnesium alloys have been widely used in the automotive, aerospace and electronics industries with the advantages of high specific strength, excellent machinability, high electrical conductivity, and high thermal conductivity. Deep drawn magnesium alloys not only meet the demands environmentally and the need for lighter products, but also can lead to remarkably improved productivity and more rapid qualification of the product The current study reports on a failure prediction procedure using finite element modeling (FEM) and a ductile fracture criterion and applies this procedure to the design of a deep drawing process. Critical damage values were determined from a series of uniaxial tensile tests and FEM simulations. They were then expressed as a function of strain rate and temperature. Based on the plastic deformation histories obtained from the FEM analyses of the warm drawing process and the critical damage value curves, the initiation time and location of fracture were predicted. The proposed method was applied to the process design for fabrication of a Mg automotive compressor case and verified with experimental results. The final results indicate that a Mg case part 39% lighter than an Al die casting part can be produced without any defects.

Flexural Design and Ductile Capacity of Reinforced High Strength Concrete Beams (고강도 철근 콘크리트 보의 휨 설계 및 연성능력)

  • 신성우;유석형;안종문;이광수
    • Magazine of the Korea Concrete Institute
    • /
    • v.8 no.6
    • /
    • pp.141-149
    • /
    • 1996
  • The reinforced high-strength-concrete beam subjected to flexure moment behaves more brittly than the moderate-strength-concrete beam reinforced with equal reinforcement ratio($\rho$/$\rho_b$). Test results show that when the concrete strength exceeds 830kg/$cm^2$, the maximum reinforcement ratio should be less than $0.6{\rho}_b$ for ductile behavior (${\rho}_b$=balanced steel ratio). The ratio of flexural strength between experimental results and analytical results with rectangular stress block decrease as the compressive strength of concrete increase. The shape of the compressive stress block distributed triangularly. because the ascending part of the stress-strain curve shows fairly linear response up to maximum stress in contrast to the nonlinear behavior of the medium and low strength specimens.

Full-Scale Shaker Testing of Non-Ductile RC Frame Structure Retrofitted Using High-Strength Near Surface Mounted Rebars and Carbon FRP Sheets (고강도 표면매립용철근과 탄소섬유시트로 보강된 비연성 철근콘크리트 골조의 실물 진동기 실험)

  • Shin, Jiuk;Jeon, Jong-Su;Wright, Timothy R.
    • Journal of the Earthquake Engineering Society of Korea
    • /
    • v.23 no.1
    • /
    • pp.43-54
    • /
    • 2019
  • Existing reinforced concrete frame buildings designed for only gravity loads have been seismically vulnerable due to their inadequate column detailing. The seismic vulnerabilities can be mitigated by the application of a column retrofit technique, which combines high-strength near surface mounted bars with a fiber reinforced polymer wrapping system. This study presents the full-scale shaker testing of a non-ductile frame structure retrofitted using the combined retrofit system. The full-scale dynamic testing was performed to measure realistic dynamic responses and to investigate the effectiveness of the retrofit system through the comparison of the measured responses between as-built and retrofitted test frames. Experimental results demonstrated that the retrofit system reduced the dynamic responses without any significant damage on the columns because it improved flexural, shear and lap-splice resisting capacities. In addition, the retrofit system contributed to changing a damage mechanism from a soft-story mechanism (column-sidesway mechanism) to a mixed-damage mechanism, which was commonly found in reinforced concrete buildings with strong-column weak-beam system.

Comparative Evaluation of the Characteristics of High Si-High Mo Ductile Cast Iron, High Si-High Mo C. V. Cast Iron and Ni-resist Cast Iron (고규소 고몰리브덴 구상흑연주철, 고규소 고몰리브덴 C. V. 주철 및 Ni-resist 주철 특성의 비교 평가)

  • Ju, Young-Kyu;Choe, Kyeong-Hwan;Lee, Sang-Mok;Kim, Myung-Ho;Yun, Sang-Weon;Lee, Kyong-Whoan
    • Journal of Korea Foundry Society
    • /
    • v.29 no.3
    • /
    • pp.120-127
    • /
    • 2009
  • The characterestics of high Si-high Mo ductile cast iron, high Si-high Mo C.V. cast iron and Ni-resist cast iron were compared and evaluated. The nodule count of the last one was lower and the nodularity was higher than those for the first one, respectively. The first two had ferritic matrices with small amounts of molybdenum carbides. The first one had the highest tensile strength and the last one the lowest elongation. This had the highest high temperature strength and that of the second one was greatly increased from the room temperature strength. The volumes of the first two were decreased during cooling and that of the last one changed little. The thermal expansion coefficient of the last one was the highest and the first one the lowest. During high temperature oxidation, even though the volume of the first one was increased, the weight was decreased and the volume and weight of the second one were increased. The change of the increased weight of the last one was more than that of thickness.