• 제목/요약/키워드: Heat stability

검색결과 1,569건 처리시간 0.025초

Concepts of heat dissipation of a disposal canister and its computational analysis

  • Minseop Kim;Minsoo Lee;Jinseop Kim;Seok Yoon
    • Nuclear Engineering and Technology
    • /
    • 제55권11호
    • /
    • pp.4173-4180
    • /
    • 2023
  • The stability of engineered barriers in high-level radioactive waste disposal systems can be influenced by the decay heat generated by the waste. This study focuses on the thermal analysis of various canister designs to effectively lower the maximum temperature of the engineered barrier. A numerical model was developed and employed to investigate the heat dissipation potential of copper rings placed across the buffer. Various canister designs incorporating copper rings were presented, and numerical analysis was performed to identify the design with the most significant temperature reduction effect. The results confirmed that the temperature of the buffer material was effectively lowered with an increase in the number of copper rings penetrating the buffer. Parametric studies were also conducted to analyze the impact of technical gaps, copper thickness, and collar height on the temperature reduction. The numerical model revealed that the presence of gaps between the components of the engineered barrier significantly increased the buffer temperature. Furthermore, the reduction in buffer temperature varied depending on the location of the gap and collar. The methods proposed in this study for reducing the buffer temperature hold promise for contributing to cost reduction in radioactive waste disposal.

전부도재수복물을 위한 수종의 코어 세라믹의 반투명도 및 색 안정성 (Translucency and Color Stability of Various Core Ceramics for All-Ceramic Restoration)

  • 오상천;이해형;신미란;박광수
    • 구강회복응용과학지
    • /
    • 제23권2호
    • /
    • pp.157-170
    • /
    • 2007
  • Purpose: This investigation was designed to determine the translucency and color stability of various core ceramics for all-ceramic restoration using the CIE $L^*a^*b^*$ system. Material and Methods: IPS e.max Press ceramic(Ivoclar-Vivadent, Liechtenstein), $LAVA^{TM}$ All Ceramic(3M-Espe, Germany), Cercon Smart Ceramic(Dentsply, Germany), and Z-match Ceramic(DentAim, Korea) were used for this study. For the specimens of zirconia oxide ceramics, the as-sintered cylindrical blanks($11.0{\times}25.0mm$) were machined into the shape of a disk(0.4, 0.8, 1.5 mm in thickness, 10 mm in diameters) with a diamond grind machine. The IPS e.max Press specimens ($0.8{\times}10mm$) were fabricated using the "lost wax" technique. CIE $L^*a^*b^*$ coordinates and light transmission were recorded for each specimen with a spectrophotometer(CM-2600d, Minolta, Japan). Color differences were calculated using the equation, ${\Delta}E^*ab=[({\Delta}L^*)2+({\Delta}a^*)2+({\Delta}b^*)2]1/2$. Results: The results were obtained as follows: 1. The most translucent group was IPS e.max Press ceramic that is a glass-ceramic, and $Lava^{TM}$ and Z-match ceramic were more translucent than Cercon Smart ceramic in zirconia ceramic group. 2. In the all groups, there was no significant translucent change after 6 times heat-treatments required to make a final restoration. 3. Colored zirconia was showed more yellowish and dark than uncolored zirconia. 4. After heat-pressing, IPS e.max Press ceramic was showed high ${\Delta}E^*ab$ value(4.1 of eM1, 6.8 of eM2) that means to be more whiter than before heat-pressing. However, there was no color change after additive heat treatments for final restoration. 5. In the colored zirconia groups, there was no significant color change after some heat-treatments required to make a final restoration.

용융염 코팅이 열지에 미치는 영향 (Effect of Molten Salt Coating on Heat Papers)

  • 임채남;이정민;강승호;정해원
    • 한국전기전자재료학회논문지
    • /
    • 제27권8호
    • /
    • pp.528-534
    • /
    • 2014
  • Thermal batteries are primary reserve batteries that use inorganic salt as electrolytes which are inactive at room temperature. The two principal heat sources that have been used in thermal batteries are heat paper and heat pellets. As soon as the heat paper, which is ignited by the initiator, in turn ignites the heat pellets, all the solid electrolytes are melted into excellent ionic conductors. However, the high combustion temperature by heat papers in thermal batteries causes thermal decomposition at the cathode, eventually leading to a thermal runaway. In this paper, we have attempted to prepare $Zr/BaCrO_4$ heat papers coated with KCl molten salt. We have also investigated the effect of a molten salt coating on the heat papers through the thermal characteristics such as calorimetric value, combustion temperature and burning rate. The calorimetric value and combustion temperature of heat papers were reduced with an increase in the molten salt coating. As a result, the molten salt coating on heat papers greatly reduced risk of a thermal runaway and improved the stability of thermal batteries.

Trichosporon의 CMCase 활성에 관하여 (On the CMCase Activity from Two species of Trichosporon)

  • 전순배;박종영
    • 미생물학회지
    • /
    • 제17권4호
    • /
    • pp.187-192
    • /
    • 1979
  • Dennis (1972) reported that Trichosporon cutaneum FRI-425 from the petioles of Pheum rhamponticum var, had showed the celluloytic activity. Chun (1977) also suggested that Trichoporon pullulons 225 isolated from the saline water of the Yeoung San River had a similar properties. However, the assay conditions for enzyme activity were not yet investigated. Thus, the present work was undertaken to examine some conditions for CMCase activity and at the same time to compare the activities of crude enzyme produce from above two species of Trichosporon pullulans. The results are as follows; 1. The maximum production of total reducing sugar by crude enzyme of Tr. pululans was after 30 minutes, whereas that of Tr. cutanuem FRI-425 was after 90 minutes. This fact showed that the reaction velocity of enzyme from Tr. pullulans 225 was more faster than that of Tr. cutaneum FRI-425. 2. Two species showed a similar trend to increase the production of reducing sugar in proportion to the increment in substrate concentration and to arrive at maximum level at lmg/ml of substrate concentration. However, Tr. pullulans 225 produced more $50{\mu}g$ of reducing sugar compared to Tr. cutaneum. 3. The optimum PH for CMCase activity is 5.0 for Tr. pullulans 225 as well as Tr. cutaneum FRI-425, and PH stability lie within the range of 6 and 8. In the activity and stability of enzyme on PH changes, enzyme of Tr. cutaneum FRI-425 was more unstable than that of TY. pullulans 225. 4. The optimum temperature for CMCase activity was $40^{\circ}C$, and enzyme activity from Tr. pullulans 225 was more sensitive to temperature changes compared with that of TY. cutaneum. The heat stability was within $40^{\circ}C$, but that was rapidly decreased above $40^{\circ}C$. In comparison of the heat stability for enzyme of Tr. cutaneum FRI-425 with that of Tr. pullulans 225 at the same temperature of $80^{\circ}C$, the former was some 10 percent more stable than the latter.

  • PDF

건축용 내화강재(FR 490) 적용 H형강 보부재의 고온내력 연구 (Study of Structural Stability for H-section Beams Made of Fire Resistant Steels (FR 490) at High Temperatures by Analytical Method)

  • 권인규
    • 한국화재소방학회논문지
    • /
    • 제28권5호
    • /
    • pp.52-57
    • /
    • 2014
  • 구조용 강재는 고온 시 물질 내부의 구성 물질의 결합력 약화로 인하여 내력과 변형이 추가적으로 발생됨으로써, 구조적 성능이 저하되고, 국부 및 연속적 붕괴로 이어질 수 있다. 따라서 강재로 구성된 구조부재는 화재 시 열영향부를 최소화하기 위한 수단이 강구되는 내화설계가 요구된다. 건축용 내화강재(FR 490)는 용접 구조용 강재(SM 490)와 상온시 특성은 동일하나, 고온 시의 내력유지 성능이 우수한 강종으로써 이로 구성된 보부재의 고온 시 내력 평가 자료는 거의 없다. 따라서 본 연구에서는 FR 490강재로 구성된 보부재의 고온 시 거동을 고온 시 재료 특성과 이론적 방법을 통하여 해석적으로 평가하고, 이를 SM 490강재보와 비교함으로써 내화성능을 확인하고자 하였으며, 그 결과 FR 490강재보의 경우 SM 490강재보에 비해서 고온 시 내력유지 성능이 우수하였다.

지중 송전관로 되메움용 순환골재의 현장실증시험을 통한 적용성 평가 (Assessment on Applicability of Recycled Aggregates for Backfill Materials of Underground Transmission Lines Based on Field Demonstration Tests)

  • 강성철;이강렬;안태봉
    • 한국건설순환자원학회논문집
    • /
    • 제3권1호
    • /
    • pp.72-83
    • /
    • 2015
  • 지중 송전선은 전기저항에 의한 발열현상이 늘 있으며, 그 주변의 되메움재를 통하여 열을 방출하게 된다. 따라서, 송전관로의 설계에는 발생하는 열을 주변 지반이 효과적으로 외부에 전달하여, 열적 안정성을 확보하는 것이 매우 중요한 설계 요소가 된다. 본 연구에서는 지중 송전관로 되메움재용 순환골재의 현장 적용성을 향상시키기 위하여, 순환골재의 품질기준 및 시공기준을 제시하고, 현장 실증시험을 통하여 송전관로의 열안정성을 분석하였다. 현장 실증시험에서는 순환골재 두 종류와 현재 되메움재로 사용하고 있는 모래의 열적 거동을 비교하였다. 시험 결과, 순환골재는 시간경과와 관로에서의 이격거리에 따라 온도와 함수비 변화가 모래와 유사하게 나타났다. 따라서 순환골재는 지중 송전관로 되메움재로서 일반 모래를 대체하여 적용 가능할 것으로 판단된다.

리튬 이차전지용 텅스텐 산화물 전해 도금 박막 제조 (Preparation of Electrolytic Tungsten Oxide Thin Films as the Anode in Rechargeable Lithium Battery)

  • 이준우;최우성;신헌철
    • 한국재료학회지
    • /
    • 제23권12호
    • /
    • pp.680-686
    • /
    • 2013
  • Tungsten oxide films were prepared by an electrochemical deposition method for use as the anode in rechargeable lithium batteries. Continuous potentiostatic deposition of the film led to numerous cracks of the deposits while pulsed deposition significantly suppressed crack generation and film delamination. In particular, a crack-free dense tungsten oxide film with a thickness of ca. 210 nm was successfully created by pulsed deposition. The thickness of tungsten oxide was linearly proportional to deposition time. Compositional and structural analyses revealed that the as-prepared deposit was amorphous tungsten oxide and the heat treatment transformed it into crystalline triclinic tungsten oxide. Both the as-prepared and heat-treated samples reacted reversibly with lithium as the anode for rechargeable lithium batteries. Typical peaks for the conversion processes of tungsten oxides were observed in cyclic voltammograms, and the reversibility of the heat-treated sample exceeded that of the as-prepared one. Consistently, the cycling stability of the heat-treated sample proved to be much better than that of the as-prepared one in a galvanostatic charge/discharge experiment. These results demonstrate the feasibility of using electrolytic tungsten oxide films as the anode in rechargeable lithium batteries. However, further works are still needed to make a dense film with higher thickness and improved cycling stability for its practical use.

물질이동 억제 버퍼층 형성을 통한 페로브스카이트 태양전지 장기 안정성 확보 (Long-term Stability of Perovskite Solar Cells with Inhibiting Mass Transport with Buffer Layers)

  • 배미선;정민지;장효식;양태열
    • 마이크로전자및패키징학회지
    • /
    • 제28권3호
    • /
    • pp.17-24
    • /
    • 2021
  • 페로브스카이트 태양전지는 용액공정으로 제작되어 공정 중 전구체 조성제어를 통해 밴드갭을 용이하게 조절할 수 있다. 탠덤 태양전지의 상부셀로 활용하여 실리콘 태양전지와 접합 시 30% 이상의 효율 달성이 가능하지만, 페로브스카이트 태양전지의 낮은 안정성이 상용화의 걸림돌로 작용하고 있다. 아이오딘 이온 및 전극 물질 확산이 주된 열화기구로 알려져 있어 장기 안정성을 확보하기 위해서는 이러한 이온 이동의 방지가 필요하다. 본 연구에서는 층간소재와 페로브스카이트 광활성층 사이의 이온이동에 의한 열화현상을 관찰하고, 이를 억제하기 위해 페로브스카이트 소재와 은전극 사이에 버퍼층을 도입하여 소자의 안정성을 확보하였다. 85℃에서 300시간 이상 보관 시 버퍼가 없는 소자는 페로브스카이트 층이 PbI2 및 델타상으로 변화하며 변색되었으며 AgI가 형성되는 것을 확인했다. LiF와 SnO2 버퍼 도입 시 이온이동 억제 효과를 통해 페로브스카이트 태양전지의 열안정성이 향상되었다. LiF버퍼층 적용 및 봉지를 한 소자는 85℃-85%RH damp heat 시험 200시간 후 효율감소가 발생하지 않았으며 추가로 AM 1.5G-1SUN 하에서 최대출력점을 추적하였을 때 200시간 후 초기 효율의 90% 이상 유지하는 것을 확인했다. 이 결과는 버퍼층 형성을 통한 층간 물질이동 억제가 장기안정성을 확보하기 위한 필요조건임을 보여준다.

열처리 잣나무 정각재의 재색 변화 및 물성 조사 (Investigation of the Color Change and Physical Properties of Heat-treated Pinus koraiensis Square Lumbers)

  • 임호묵;홍승현;강호양
    • Journal of the Korean Wood Science and Technology
    • /
    • 제42권1호
    • /
    • pp.13-19
    • /
    • 2014
  • 국내의 주 생산 수종인 잣나무 $90{\times}90mm$ 각재의 적정한 열처리 조건을 찾기 위해 3가지 열처리 스케줄을 적용하여 재색과 물성에 미치는 영향을 연구하였다. 1차 열처리시 온도는 $170^{\circ}C$$190^{\circ}C$, 시간은 예비가열시간 1시간을 포함하여 9시간과 13시간을 적용하였다. 2차와 3차 열처리는 모든 공시 각재에 동일하게 $190^{\circ}C$-9시간을 적용하였다. 열처리 횟수가 증가할수록 백색도 $L^*$는 직선적으로 감소하였으며 표준편차도 감소하였다. 열처리 횟수가 증가할수록 색차 ${\Delta}E^*$는 직선적으로 증가하였으며, 표준편차가 커지는 경향이 있었다. 알려진 바와 달리 열처리 시편의 평균 종압축강도가 무처리 시편보다 9% 높았다. 항팽윤율과 중량증가율을 측정하여 열처리 시편의 치수안정성이 무처리보다 크게 증가하였음을 보였다.

알칼리와 열처리에 의한 임플란트의 표면 특성 및 골유착 안정성에 관한 연구 (Surface characteristics and stability of implants treated with alkali and heat)

  • 송윤석;조인호
    • 대한치과보철학회지
    • /
    • 제46권5호
    • /
    • pp.490-499
    • /
    • 2008
  • 생체 활성 재료는 생체 내에서 자가적으로 인회석 층 (apatite layer)을 형성하여, 골과의 생화학적 결합이 가능해야 한다. 알칼리와 열처리를 통하여 생체 활성 표면을 얻을 수 있는 것으로 보고되고 있다. 본 실험에서는 알칼리 및 열처리를 시행한 임플란트들의 안정성을 평가하고자 하였다. 실험군의 분류로 1군은 대조군인 선반 가공 임플란트군, 2, 3군은 $60^{\circ}C$, 5 M의 NaOH 용액에 24시간 처리한 후, 각각 대기 중 및 진공 상태 $600^{\circ}C$에서 1시간 동안 열처리하였다. 처리된 시편은 FESEM, XPS, TF-XRD 및 AFM을 이용하여 표면 특성을 관찰하고, 임플란트의 안정성을 위해 공진 주파수와 페리오테스트 및 역 토오크를 측정하고, 골유착 안정성에 관한 차이를 비교 분석하여 다음과 같은 결과를 얻었다. 1. 표면 특성: 알칼리 및 열처리를 시행한 2, 3군은 비슷한 양상의 거친 표면을 보여주었다. 알칼리 처리를 시행한 2군과 3군에서 1군과는 달리 높은 함량의 나트륨 이온이 검출되었으며, 결정구조 분석 결과 2군에서 예추석 (antase)과 금홍석 (rutile)이 혼재된 상태로 금홍석이 우세한 양상을 보여주었다. 2. 공진 주파수 분석: 군간 비교에서 12주에 2군이 1, 3군에 비해 통계적으로 유의하게 높은 측정치를 보였다. 주간 비교시, 1, 2군은 4주 이후에 유의한 증가를 보여주었고, 3군은 2주와 4주에서 각각 유의한 증가를 보여주었다 (P < .05). 3. 페리오테스트 분석: 주간 비교에서 1, 2군은 4주 이후에 유의하게 감소를, 3군은 2주와 4주에서 각각 유의한 감소를 보여주었다 (P< .05). 4. 역 토오크 분석: 군간 비교에서는 2, 4, 8주에서는 2군이 1, 3군에 비해 유의하게 높은 측정값을 보여주었다. 주간 비교에서는 1, 3군은 4주, 12주에서 유의한 증가를 보여주었고, 2군은 4주부터 유의한 증가를 보여주었다 (P < .05). 이상의 결과로 볼 때, 알칼리 및 대기 중 열처리를 통해서 적절한 결정 구조의 산화막을 가진 생체 활성화된 무정형의 나트륨 티탄산염 층을 얻을 수 있었고, 알칼리 및 진공 상태 열처리만으로도 나트륨이 함유된 생체 활성화된 표면을 얻을 수 있었다고 사료된다. 또한 이런 처리 과정으로 형성된 표면층들은 임플란트의 초기 골유착에 도움을 줄 수 있는 유용한 방법 중 하나라고 사료된다.