The Effects of 3-(3,4-dichloro phenyl)-1,1-dimethylurea on the Cure of Epoxy/Dicyandiamide System (3-(3,4-dichloro phenyl)-1,1-dimethylurea이 Epoxy/Dicyandiamide계의 경화에 미치는 영향)

  • Kim, Hyung-Soon;Kim, Wan-Young;Kim, Young-Ja
    • Applied Chemistry for Engineering
    • /
    • v.7 no.5
    • /
    • pp.963-969
    • /
    • 1996
  • Cure characteristics of DGEBA(diglycidyl ether of bisphenol A)/dicy(dicyandiamide) system containing diuron(3-(3,4-dichloro phenyl) -1,1-dimethylurea) as an accelerator was investigated. The system has shelf life of six months because dicy is insoluble in liquid/solid resins at room temperature. It is generally known that dicy is an adequate curing agent for one component adhesive due to its highly latent property. With increasing the amount of added dicy, reaction heat of DGEBA/dicy system increased and degree of conversion was not varied. For DGEBA/dicy/diuron system, cure temperature decreased about $40^{\circ}C$ and cure reaction became fast by the addition of diuron which activates dicy. $T_g$ of the mixed resin decreased with the amount of accelerator. which was interpreated with molecular structure forming loose chain. Cure kinetics of DGEBA/dicy and DGEBA/dicy/diuron system were explained using Kamal's autocatalytic reaction model. The effect of acceleration was confirmed with that reaction model.

  • PDF

A Study on the Heat-Curing of Acrylic Resin using Ring Furnace (Ring Furnace를 이용한 Acrylic Resin의 온성에 관한 연구)

  • Choi, Seog-Soon
    • Journal of Technologic Dentistry
    • /
    • v.13 no.1
    • /
    • pp.27-31
    • /
    • 1991
  • The purpose of this study was to evaluate the effect of curing time and curing temperature on the hear - Curing of acrylic resin using ring furnace. Specimens were fabricated from 2 kinds(Laboron, Bertex) heat-cured resin. Total 200 samples were divided into 4 groups(70$^{\circ}C$, 100$^{\circ}C$, 13$^{\circ}C$, 150$^{\circ}C$) and each group was divided into 5 small groups(30 min., 45min., 60min., 75min., 90min.). A microscope(Olympus Coll Co. Japan) was used to examine a randomly selected central zone, midzone and surface for each complete specimen. The results of the experiment were as follows : 1. To obtain non-polymerzation, cure the resin for 30 minutes at 70$^{\circ}C$ and 100$^{\circ}C$ in a ring furnace. 2. To obtain with porosity, cure the resin for 45 minutes, 60 minutes and 75 mintes at 70$^{\circ}C$ and for 90 minutes at 150$^{\circ}C$ in ring furnace. Porosity appears in Laboron for 30 minutes, 45 minutes at 150$^{\circ}C$ in a ring furnace. 3. Every other specimens connot get a sight of special problem with makes eye in the made surface.

  • PDF

Thermal Stability and Cure Behavior of Waterborne Phenol-Formaldehyde Resin (수용성 페놀-포름알데히드 수지의 열안정성 및 경화거동)

  • Yoon, Sung Bong;Kim, Jin Woo;Cho, Donghwan
    • Journal of Adhesion and Interface
    • /
    • v.7 no.1
    • /
    • pp.16-22
    • /
    • 2006
  • In this work, the effect of cure temperature and time on the thermal stability and the exothermic cure reaction peak of a waterborne resol-type phenol-formaldehyde resin, which may be used for preparing phenolic sheet molding compounds (SMC), has been investigated using a thermogravimetric analyzer and a differential scanning calorimeter. The weight loss of waterborne phenol-formaldehyde resin was mainly occurred at three temperature stages: near $200^{\circ}C,\;400^{\circ}C$, and $500^{\circ}C$. The carbon yield at $750^{\circ}C$ for the cured resin was about 62%~65%. Their thermal stability increased with increasing cure temperature and time. Upon cure, the exothermic reaction was taken placed in the range of $120^{\circ}C{\sim}190^{\circ}C$ and the maximum peak was found in between $165^{\circ}C$ and $170^{\circ}C$. The shape and the maximum of the exothermic curves depended on the given cure temperature and time. To remove $H_2O$ and volatile components, the uncured resin needed a heat-treatment at $100^{\circ}C$ for 60 min at least prior to cure or molding. Curing at $130^{\circ}C$ for 120 min made the exothermic peak of waterborne phenol-formaldehyde resin completely disappeared. And, post-curing at $180^{\circ}C$ for 60 min further improved the thermal stability of the cured resin.

  • PDF

Physical Properties Effect of Dry-Heat and Microwave-Cured Acrylic Resins depending on the Irradiation-Induced Changes (유도광선변화에 따른 건식중합과 마이크로파중합 아크릴레진의 물리적 성질영향)

  • Kim, Gyu-Ri
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.7
    • /
    • pp.4388-4397
    • /
    • 2015
  • The purpose of this study was to research the property change of acrylic resins depending on the induced-beam change and research the improved physical property of dry-heat and microwave-cured dental place acrylic resin in order to develop the acrylic resins with the optimum characteristic. As a result of observing flexural rigidity, hardness and color difference, the dry-heat-cured specimens of Vertex RS and Paladent 20 showed ideal property at 5, 15, and 25 kGy irradiation. The microwave-cured specimens of Vertex RS and Paladent 20 showed ideal property at 5 kGy irradiation. The correlation analysis showed a positive correlation among ARD, flexural rigidity (0 418), E coefficient (0.675) and Barcol hardness (0 588). The radiation cure technology is helpful for relieving the contamination caused by the manufacture of polymer composite. It can significantly contribute to the fusion of ultra violet cure technology and nano technology and the improvement of mechanical property without giving effect to the workability of polymer.

Cure Characteristics, Mechanical Properties, Abrasion Property and Thermal Properties of EVM/EPM Blends Containing Flame Retardants

  • Sung, Il Kyung;Lee, Won Ki;Park, Chan Young
    • Elastomers and Composites
    • /
    • v.52 no.2
    • /
    • pp.105-113
    • /
    • 2017
  • The curing behavior, mechanical properties, hot-air aging resistance, abrasion properties,thermal properties, etc., of EVM/EPM/APP (ammonium polyphosphate)/DPER (dipentaerythritol)/EG (expandable graphite) and EVM/EPM/ATH (aluminium trihydroxide) flame retarding systems in ethylene vinyl acetate rubber (EVM) blends with EPM (ethylene propylene rubber) were sequentially examined. For both flame retarding systems, the torque values increased with the content of EPM rubber and with the vulcanization time. As the content of EPM rubber increased, the scorch time became shorter, whereas the optimum cure time followed an increasing trend. For the EVM/EPM/APP/DPER/EG flameretarding system, as the content of EPM rubber increased, the hardness did not change,whereas the tensile strength and elongation at break decreased. A hot-air aging resistance test at $150^{\circ}C$ showed that the heat resistance decreased with the EPM content regardless of the kinds and contents of flame retardants. As the EPM content increased, the abrasion rate became higher and the abrasion resistance of the EVM/EPM/APP/DPER/EG flame retarding systems exceeded that of the EVM/EPM/ATH flame retarding counterparts. In comparison with the EVM/EPM/ATH flame retarding systems, the thermal stability of the EVM/EPM/APP/DPER/EG flame retarding system showed an increasing tendency.

Deceleration stage and modeling of hydration heat flow for fly ash cement paste (플라이애쉬 시멘트 페이스트의 수화열류 감속 단계 분석 및 모델링에 대한 실험적 연구)

  • Wang, Zihao;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2022.04a
    • /
    • pp.13-14
    • /
    • 2022
  • This study investigated the effect of fly ash content on the isothermal hydration heat of cement pastes. Two different pastes with fly ash content were studied to cure at 35℃. The hydration heat flow deceleration stage of slurry was simulated and compared by Jander Equation and Ginstling-Brounshtein Equation. The results show that Jander Equation and Ginstling-Brounshtein Equation have certain defects in the modeling of the deceleration stage of the heat flow of cement fly ash paste, and the fitted curve can not describe the deceleration stage well.

  • PDF

A Study on the Pathogenic Factors and Treatments of Exogenous Febrile Disease with Time (외감열병(外感熱病)의 원인(原因)과 치법(治法)에 대한 통시적(通時的) 고찰(考察))

  • Yang, Kwang-Yeol
    • Journal of Korean Medical classics
    • /
    • v.21 no.1
    • /
    • pp.295-302
    • /
    • 2008
  • Until the middle of the 20th century, exogenous febrile disease was the most common disease that threatened the human health. For a long time, oriental medicine doctors developed many ways to cure this disease by studying pathogenic factors. The phthogenic factors and treatments of exogenous febrile disease with time are as followings. "Naegyeong(內經)" : Cold pathogen. Diaphoretic therapy, purgation therapy. Hwata : Cold pathogen. Diaphoretic therapy, emetic therapy, purgation therapy. Jangjunggyeong(張仲景) : Cold pathogen. Eight principal therapeutic methods except diaphoretic therapy with pungent and cool properties. Yuhagan(劉河間) : Fire pathogen. Diaphoretic therapy with pungent and cool properties. Idongwon(李東垣) : Improper diet and overstrain. Reinforcing therapy. Ouga(吳又可) : Epidemic pathogenic factors. Diaphoretic therapy with pungent and cool properties, Heat-reducing therapy. purgation therapy Seopcheonsa(葉天士) : Warm pathogen. diaphoretic therapy, Heat-reducing therapy, expel Heat therapy, cooling the blood and eliminating stagnation of blood. Oguktong(吳鞠通) : Six pathogenic factors. Eight principal therapeutic methods including diaphoretic therapy with pungent and cool properties.

  • PDF

Confirmation of Applicability of Heating and Curing Method of Concrete in Winter Using Electric Heating System (전기열풍기를 이용한 동절기 콘크리트 가열양생공법 적용 및 적정성 효과 검증)

  • Kim, Se-Jong;Park, Jong-Hoon
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2022.04a
    • /
    • pp.131-132
    • /
    • 2022
  • Looking at recent construction cases at winter construction sites, there is a risk that heat sources such as kerosene fans and fossil fuels (brown coal, molded carbon) used in concrete will cure rapidly, so in situations where further curing is impossible after formwork removal, the outer wall and the entire slab are exposed to rapid external deterioration, resulting in delays in concrete strength expression and until collapse accidents. In this study, we applied kerosene fans and tropical circulating electric heat fans mainly used as curing heat sources at construction sites, comparative analysis. also verified the performance of structures during concrete curing due to thermal convention / circulation performance, concrete demand strength expression, and implementation of electric heat fans by heavy disaster methods.

  • PDF

Cure Kinetics of Epoxy/Diamine System Modified with Malononitrile by Barrett Method and Integral Method (Malononitrile에 의해 개질된 Epoxy/Diamine계의 경화반응 속도론: Barrett Method와 Integral Method)

  • Cheon, In-Suk;Don, Yun-Seung;Sim, Mi-Ja;Kim, Sang-Uk
    • Korean Journal of Materials Research
    • /
    • v.4 no.5
    • /
    • pp.574-580
    • /
    • 1994
  • This study is about cure kinetics of DGEBA/MDA/MN(malononitrile) system by Barrett method and Integral method using DSC dynamic run. Curing behavior was shown through DSC and the heat change involved in a reaction could be measured directly with DSC. The kinetic parameters such as activation energy, pre-exponential factor and reaction order were given by Barrett method and Integral method obtained in an assumption that the area of DSC enthalpic analysis curve was propotional to the enthalpic change.

  • PDF

A study on the vulcaniz러on characteristic of combined antioxidants in NR and SBR compounds (NR 및 SBR의 노화방지제(老化防止劑) 병용효과(倂用效果)에 의(依)한 가황특성(加黃特性) 연구(硏究))

  • Choi, Jae-Woon;Lee, Ki-Jong
    • Elastomers and Composites
    • /
    • v.17 no.2
    • /
    • pp.77-90
    • /
    • 1982
  • The purpose of this study is to get comparative results on the combined antioxidant systems comprised of MHPPD with IPPD, MHPPD with PBN and MHIPPD with MB when they are individually added to NR and SBR compound. Vulcanization characterstics and physical properties of the combined antioxidants have been studied by means of the Mooney viscometer, the Monsanto disc rheometer and so on. According to the test results, MHPPD with IPPD system has shown faster cure rate, better optimum cure time and shorter scorch time than other systems. The vulcanizate comprised of the MHPPD with IPPD antioxidant system has taken advantage of heat resistance, fluid resistance and antiozone resistance.

  • PDF