Microstructure and Strength of the Microjoined Electrode for the Lamp of the LCD Backlight Unit (TFT-LCD 백라이트 유닛(BLU) 램프용 전극 미세 접합부의 강도 및 미세조직)

  • Kim, Gwang-Soo;Kim, Sang-Duck
    • Korean Journal of Materials Research
    • /
    • v.19 no.1
    • /
    • pp.7-12
    • /
    • 2009
  • TFT-LCD is the most popular type of flat display panel in the information technology field. The back light unit is a main part of the structure of a TFT-LCD panel. Occasionally, studies have shown that failures of the CCFL of the BLU occur due to the poor weld characteristics of these materials. The aim of this study was to prepare some technical data and to characterize a microjoined electrode for the CCFL. Microstructure examinations, microhardness measurements, resistance measurements and microtensile tests of the microjoined electrode were carried out. The result indicates that a large amount of grain coarsening exists in the heat-affected zone (HAZ) of the weld between the cup and the pin. This grain coarsening of the HAZ between the cup and pin is caused by the welding cycle, which may have an influence on the lowest microhardness values. Fracturing of the microjoined electrode also occurred at the HAZ close to the cup between the weld holding the cup and the pin. Additionally, no specific changes of the electrical resistance among the cup, pin, and lead wire themselves or in the microjoined electrode were observed.

High-Temperature Oxidation Kinetics and Scales Formed on P122 Steel Welds in Air (P122강 용접부의 대기중 고온산화 부식속도와 스케일 분석)

  • Bak, Sang-Hwan;Lee, Dong-Bok
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.9
    • /
    • pp.699-707
    • /
    • 2011
  • P122 steel, with a composition of Fe-10.57%Cr-1.79%W-0.96Cu-0.59Mn was arc-welded and oxidized between $600^{\circ}C$ and $800^{\circ}C$ in air for up to 6 months. The oxidation rates increased in the order of the base metal, weld metal, and heat-affected zone (HAZ), depending on the microstructure. The scale morphologies of the base metal, weld metal, and HAZ were similar because it was determined mainly by the alloy chemistry. The scale consisted primarily of a thin $Fe_2O_3$ layer at $600^{\circ}C$ and $700^{\circ}C$ and an outer $Fe_2O_3$ layer and an inner ($Fe_2O_3$, $FeCr_2O_4$)-mixed layer at $800^{\circ}C$. The microstructural changes resulting from heating between $600^{\circ}C$ and $800^{\circ}C$ coarsened the carbide precipitates, secondary Laves phases, and subgrain boundaries in the matrix, resulting in softening of the base metal, weld metal, and HAZ.

An Experimental Study on Corrosion Fatigue Strength of TMCP Steel in Consideration of NaCl Salinity (염분농도변화에 따른 TMCP강의 부식피로강도에 관한 실험적 연구)

  • 강성원;김철현;이해우
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.40 no.3
    • /
    • pp.54-60
    • /
    • 2003
  • Fatigue strength of offshore structures or ship structures is significantly decreased due to corrosive environment condition such as sea water and/or coal, crude oil of cargoes, compared to that of on shore structures. In corrosive environment, fatigue strength of structures also depends on characteristics of weld material heat affected zone(HAZ). In this research work, rotary bending fatigue tests of parent material and HAZ of TMCP steel were performed in order to investigate the initiation and propagation of cracks both in air and in NaCl solution. Comparison of fatigue strength In relation with the salinity of NaCl were carried out as well. According to the test results weld material or HAZ of TMCP steel showed higher fatigue strength than that of the parent material. The fatigue strength of TMCP steel decreases drastically in NaCl solution compared to that of in air environment. In particular, more reduced fatigue strength is observed in 1% NaCl solution than in 3% NaCl solution.

Evaluation on Mechanical Properties with Welding Processes for Off Shore Wind Tower Application (TMCP강을 적용한 해상용 풍력타워의 용접 공정에 따른 기계적 물성 평가)

  • Ji, Changwook;Choi, Chul Young;Nam, Dae-Geun;Kim, Hyoung Chan;Jang, Jae Ho;Kim, Ki Hyuk;Park, Yeong-Do
    • Journal of Welding and Joining
    • /
    • v.32 no.1
    • /
    • pp.15-21
    • /
    • 2014
  • FCAW(Flux Cored Arc Welding), SAW(Submerged Arc Welding), EGW(Electro Gas Welding), and three-pole SAW are applicable in manufacturing the offshore wind tower. In this paper, mechanical properties of these welded-joints for TMCP steels were evaluated in all above welding processes. The tensile strength of welded-joints for all the welding methods satisfied the standard guideline (KS D 3515). No cracking on weldment was found after the bending test. Changes of weldedments hardness with welding processes were observed. In a weld HAZ (heat-affected zone), a softened HAZ-zone was formed with high heat input welding processes (SAW and EGW). However, the welded-joint fractures were found in the base metal for all cases and small decrease in welded-joint strength was caused by a softened zone. The multi-pole SAW welds exhibited similar mechanical properties comparing to the one with one-pole SAW process.

Effect of Silicon on Intergranular Corrosion Resistance of Ti-stabilized 11 wt% Cr Ferritic Stainless Steels (11 wt% 크롬이 함유된 Ti 첨가 페라이트스테인리스강의 입계부식에 미치는 규소의 영향)

  • Hyun, Youngmin;Kim, Heesan
    • Corrosion Science and Technology
    • /
    • v.12 no.6
    • /
    • pp.265-273
    • /
    • 2013
  • Ti-stabilized 11 wt% Cr ferritic stainless steels (FSSs) for automotive exhaust systems have been experienced intergranular corrosion (IC) in some heat-affected zone (HAZ). The effects of sensitizing heat-treatment and silicon on IC were studied. Time-Temperature-Sensitization (TTS) curves showed that sensitization to IC was observed at the steels heat-treated at the temperature lower than $650^{\circ}C$ and that silicon improved IC resistance. The sensitization was explained by chromium depletion theory, where chromium is depleted by precipitation of chromium carbide during sensitizing heat-treatment. It was confirmed with the results from the analysis of precipitates as well as the thermodynamical prediction of stable phases. In addition, the role of silicon on IC was explained with the stabilization of grain boundary. In other words, silicon promoted the formation of the grain boundaries with low energy where precipitation was suppressed and consequently, the formation of Cr-depleted zone was retarded. The effect of silicon on the formation of grain boundaries with low energy was proved by the analysis of coincidence site lattice (CSL) grain boundary, which is a typical grain boundary with low energy.

Creep-Fatigue Crack Growth at CrMo Steel Weld Interface (CrMo강 용접계면균열의 크리프-피로 균열성장거동)

  • Baek, Un-Bong;Yoon, Kee-Bong;Lee, Hae-Moo;Suh, Chang-Min
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.12
    • /
    • pp.3088-3095
    • /
    • 2000
  • Creep-fatigue crack growth behavior was experimentally measured particularly when a crack was located in the heat affected region of lCr-5Mo steel. Load hold times of the tests for trapezoidal fatigue waveshapes were varied among 0, 30, 300 and 3,600 seconds. Time-dependent crack growth rates were characterized by the $C_r$parameter. It was found that the crack growth rates were the highest when the crack path was located along the fine-grained heat affected zone(FGHAZ). Cracks located in other heat affected regions had a tendency to change the crack path eventually to FGHAZ. Creep-fatigue crack growth law of the studied case is suggested in terms of (da/dt)$_{avg}$ vs. ($C_t$)$_{avg}$ for residual life assessment.

Investigation into the Effects of Process Parameters of DED Process on Deposition and Residual Stress Characteristics for Remanufacturing of Mechanical Parts (기계 부품 재제조를 위한 DED 공정 조건에 따른 적층 및 잔류응력 특성 분석)

  • Kim, D.A.;Lee, K.K.;Ahn, D.G.
    • Transactions of Materials Processing
    • /
    • v.30 no.3
    • /
    • pp.109-118
    • /
    • 2021
  • Recently, there has been an increased interest in the remanufacturing of mechanical parts using metal additive manufacturing processes in regards to resource recycling and carbon neutrality. DED (directed energy deposition) process can create desired metallic shapes on both even and uneven substrate via line-by-line deposition. Hence, DED process is very useful for the repair, retrofit and remanufacturing of mechanical parts with irregular damages. The objective of the current paper is to investigate the effects DED process parameters, including the effects of power and the scan speed of the laser, on deposition and residual stress characteristics for remanufacturing of mechanical parts using experiments and finite element analyses (FEAs). AISI 1045 is used as the substrate material and the feeding powder. The characteristic dimensions of the bead shape and the heat affected zone (HAZ) for different deposition conditions are obtained from the experimental results. Efficiencies of the heat flux model for different deposition conditions are estimated by the comparison of the results of FEAs with those of experiments in terms of the width and the depth of HAZ. In addition, the influence of the process parameters on residual stress distributions in the vicinity of the deposited region is investigated using the results of FEAs. Finally, a suitable deposition condition is predicted in regards to the bead formation and the residual stress.

A Study of New Technique Development for Creep Evaluation of Heat Resistant Steel Weldment(I) (내열강 용접부의 크리프 평가 신기술 개발에 관한 연구)

  • 유효선;백승세;권일현;이송인
    • Journal of Welding and Joining
    • /
    • v.20 no.6
    • /
    • pp.30-30
    • /
    • 2002
  • It has been reported that the creep characteristics on weldment which is composed of weld metal(W.M), fusion line(F.L), heat-affected zone(HAZ), and base meta(B.M) could be unpredictably changed in severe service conditions such as high temperature and high pressure. However, the studies done on creep damage in power plant components have been mostly conducted on B.M and not the creep properties of the localized microstructures in weldment have been thoroughly investigated yet. In this paper, it is investigated the creep characteristics for three microstructures like coarse-grain HAZ(CGHAZ), W.M, and B.M in X20CrMoV121 steel weldment by the small punch-creep-(SP-Creep) test using miniaturized specimen(l0×10×0.5mm). The W.M microstructure possesses the higher creep resistance and shows lower creep strain rate than the B.M and CGHAZ. In the lower creep load the highest creep strain rate is exhibited in CGHAZ, whereas in the higher creep load the B.M represents the high creep strain rate. The power law correlation for all microstructures exists between creep rate and creep load at 600℃. The values of creep load index (n) based on creep strain rate for B.M, CGHAZ, and W.M are 7.54, 4.23, and 5.06, respectively and CGHAZ which shows coarse grains owing to high welding heat has the lowest creep loade index. In all creep loads, the creep life for W.M shows the highest value.

A Study on New Technique Development for Creep Evaluation of Heat Resistant Steel Weldment (I) (내열강 용접부의 크리프 평가 신기술 개발에 관한 연구(I))

  • 유효선;백승세;권일현;이송인
    • Journal of Welding and Joining
    • /
    • v.20 no.6
    • /
    • pp.754-761
    • /
    • 2002
  • It has been reported that the creep characteristics on weldment which is composed of weld metal(W.M), fusion line(F.L), heat-affected zone(HAZ), and base meta(B.M) could be unpredictably changed in severe service conditions such as high temperature and high pressure. However, the studies done on creep damage in power plant components have been mostly conducted on B.M and not the creep properties of the localized microstructures in weldment have been thoroughly investigated yet. In this paper, it is investigated the creep characteristics for three microstructures like coarse-grain HAZ(CGHAZ), W.M, and B.M in X20CrMoV121 steel weldment by the small punch-creep-(SP-Creep) test using miniaturized specimen($10{\times}10{\times}0.5mm$). The W.M microstructure possesses the higher creep resistance and shows lower creep strain rate than the B.M and CGHAZ. In the lower creep load the highest creep strain rate is exhibited in CGHAZ, whereas in the higher creep load the B.M represents the high creep strain rate. The power law correlation for all microstructures exists between creep rate and creep load at $600^{\circ}C$. The values of creep load index (n) based on creep strain rate for B.M, CGHAZ, and W.M are 7.54, 4.23, and 5.06, respectively and CGHAZ which shows coarse grains owing to high welding heat has the lowest creep loade index. In all creep loads, the creep life for W.M shows the highest value.

Microstructure Evolution of UFG Steel Weld by Hybrid and Laser Welding (하이브리드 용접과 레이저 용접에 의한 세립강 용접부의 미세조직변화에 관한 연구)

  • Dong, H.W.;Lee, M.Y.;Ahn, Y.S.
    • Journal of Power System Engineering
    • /
    • v.14 no.3
    • /
    • pp.58-63
    • /
    • 2010
  • A laser beam welding and an electric arc welding were combined, and the positive points of each welding method are drawn such as high speed, low thermal load, deep penetration, and high productivity. The fiber laser-MIG conjugated welding. namely the hybrid welding has been studied mainly for the automation industry of a pipeline welding. In this study, the MIG welding was combined with a fiber laser welding to make up the hybrid welding. The weld shapes, microstructures and mechanical properties for weld zones after the hybrid welding or only fiber laser welding were investigated on the 700 MPa grade Ultra Fine Grained(UFG) high strength steel. The amount of acicular ferrite in weld metals and HAZ(heat affected zone) was observed larger after hybrid welding compared with after only laser welding. The Vickers hardness of the top area of the fusion zone after fiber laser welding was higher compared with after hybrid welding.