고주파 유도용접 현상의 3차원 해석 (Three Dimensional Analysis of High Frequency Induction Welding Phenomena)

  • 김현중;윤성기
    • 대한기계학회논문집A
    • /
    • 제30권7호
    • /
    • pp.865-872
    • /
    • 2006
  • High frequency induction welding is widely employed for longitudinal seam welding of small scale tubes and pipes because of its relatively high processing speed and efficiency. This research is aimed at understanding the variables that affect the quality of the high frequency induction welding. The welding variables include the welding frequency, weld speed, V-angle and tube thickness. Temperature distribution of the tube is calculated through three dimensional coupled electromagnetic and thermal FE analysis. The skin and proximity effects are considered in the electromagnetic analysis. The influence of the impeder is also analyzed. The effects of the operating welding variables on the temperature distribution are investigated quantitatively by exhibiting the heat affected zone (HAZ). The results explain the mechanism of significant enhancement of welding efficiency when the impeder is used. The proper welding conditions without the overheated edge are obtained through FE analysis.

펄스형 Nd:YAG레이저로 용접된 Inconel Tube의 전단강도 (Shear Strength of lnconel Tube Welded with Pulsed Nd:YAG Laser)

  • 장웅;김재도;정진만;김철중
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1995년도 추계학술대회 논문집
    • /
    • pp.125-128
    • /
    • 1995
  • The remote sleeve repair-welding technology using the pulsed Nd:YAG laser for increasing the lifetime of the steam generator tube in the nuclear power plant has been developed. The laser welding has many advantages on deep penetration depth and narrow heat affect zone(HAZ). The inconel 600 tube and inconel 690 sleeve used high temperature and high pressure service have been welded as round lap welds. It is found that the relation between the connection width and welding parameters. It is found that the shear strength in proportion to the connection width by conducting tensile-shear tests.

  • PDF

용접(鎔接)이음한 구조용강(構造用鋼)의 피노귀열진전거동(疲勞龜裂進展擧動) (The Propagation Behavior of the Fatigue Crack of the Welded Structural Steel)

  • 정영화;김익겸;이형근;정진석
    • 산업기술연구
    • /
    • 제18권
    • /
    • pp.117-124
    • /
    • 1998
  • In recently, according to increase the construction rate of steel bridge, it is necessary to develop the high strength, high toughness steel. Thus, this study show to evaluate the fatigue characteristic of SWS 570 B first used within a country. With the weld-joined compact tension specimens compared with each other, that is, transverse and lengthwise about the crack propagation, high and low in the input heat level, the fatigue test were performed. The log-log curves between the fatigue crack propagation rate da/dN and the transition range of the stress intensity factor ${\Delta}K$ ahead the crack tip were drawed, with these data. By using this curve, we obtained C and m which is material constant from Paris-Erdogan power law. The obtained results from this study indicate that fatigue crack growth rate of SWS 570 B is not influenced by softening effect which occurs in the HAZ(heat-affected zone) when high and low heat input weld is carried out. Softening effects, which affect fatigue properties, are shown that it is not affected to the fatigue growth rates significantly.

  • PDF

A study on the welding conditions that affect thermal deformation and mechanical property of Al 5083 non-ferrous alloy for eco-environmental leisure ships

  • Moon, Byung Young;Kim, Kyu Sun;Lee, Ki Yeol
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제38권10호
    • /
    • pp.1190-1199
    • /
    • 2014
  • As a considerable, experimental approach, an autocarriage type of $CO_2$ welding machine and a MIG(metal inert gas) welding robot in the inert gas atmosphere were utilized in order to realize Al 5083 welding to hull and relevant components of green leisure ships. This study aims at investigating the effect of welding conditions(current, voltage, welding speed, etc.) on thermal deformation that occurs as welding operation and tensile characteristics after welding, by using Al 5083, nonferrous material, applied to manufacturing of eco-environmental leisure ships. With respect to welding condition to minimize the thermal deformation, 150 A and 16 V at the wire-feed rate of 6 mm/sec were acquired in the process of welding Al 5083 through an auto carriage type of $CO_2$ welding feeder. As to tensile characteristics of Al 5083 welding through a MIG welding robot, most of tensile specimens showed the fracture behavior on HAZ(heat affected zone) located at the area joined with weld metal, except for some cases. Especially, for the case of the Al specimen with 5 mm thickness, 284.62 MPa of tensile strength and 11.41 % of elongation were obtained as an actual allowable tensile stress-strain value. Mostly, after acquiring the optimum welding condition, the relevant welding data and technical requirements might be provided for actual welding operation site and welding procedure specification (WPS).

순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(II) - 맞대기 용접 특성 - (A Study of Weldability for Pure Titanium by Nd:YAG Laser(II) - Welding Properties of Butt Welding -)

  • 김종도;곽명섭;송무근;박성하
    • Journal of Welding and Joining
    • /
    • 제27권6호
    • /
    • pp.68-73
    • /
    • 2009
  • Recently, as titanium and titanium alloys are being increasingly used in wide areas, there are on-going researches to obtain high quality weld zone. In particular, growing interest is being drawn to laser welding, which involves low heat input and large aspect ratio in various welding processes and can facilitate shield in atmospheric condition compared with electron beam welding. The first report covered the analysis of embrittlement by the bead color of weld zone through quantitative analysis of oxygen and nitrogen and measurement of hardness as basic experiment to apply laser welding to titanium. Results indicated that the element that affect embrittlement the most was nitrogen, and as embrittlement and oxygenation go on, bead color changed to silver, gold, brown, blue and gray. This study performed butt welding of pure titanium and STS304 by using 1kW CW Nd:YAG laser, and to find out basic physical properties, evaluated welding performance by laser output, welding speed, root gap and misalignment etc, and examined mechanical properties through tensile stress and Erichsen test. The reason particles of pure titanium welded metal and HAZ are greater than STS304 is because they are pure metal and do not include many impure elements that work as nuclei in case of resolidification, thus becoming coarse columnar crystals eventually. In addition, the reason STS304 requires more energy during welding than pure titanium is because the particle size of base metal is smaller.

초음파 반사 패턴과 주파수 대역 분할 신호처리를 이용한 다층구조인 노내 간극 측정 (Multi-layered Gap Measurement on In-Vessel Cerium Retention Using Ultrasonic Wave Reflective Pattern Analysis and Frequency Diversity Signal Processing)

  • 구길모;심철무;김종환;김상백;김희동;박치승
    • 비파괴검사학회지
    • /
    • 제20권4호
    • /
    • pp.314-321
    • /
    • 2000
  • 모의 원자로내 용융물 냉각 실증 실험 결과 용융물 $Al_2O_3/Fe$ thermite 와 lower head vessel사이에 간극이 발생된다. 간극을 정량적으로 측정하기 위한 기존의 초음파 방법은 구조물의 복잡성과 $2300^{\circ}C$ 에서 용융되는 thermite $Al_2O_3/Fe,\;Al_2O_3$의 영향으로 발생되는 lower head의 열영향부위(HAZ)의 금속학적인 결정입자 크기의 변화로 결정 계면으로부터 발생되는 잡음신호와 초음파 산란, 감쇠, 모드 변환 등이 발생되어 신뢰성이 떨어지고 있다. 간극을 정량적으로 측정하기 위해서 thermite와 lower head 사이에 물이 채워진 형태의 즉 고체, 액체, 고체의 다층구조에서 초음파의 진행 및 반사 형태를 분류 및 분석하였다. 결정립의 잡음을 억제하기 위하여 주파수대역의 확률 처리 방식인 PT(polarity threshold) 알고리즘을 이용하여 약 6dB 신호 대 잡음비의 개선효과를 가져왔다.