The Effect of Current on Characteristics of Stellite 12 Alloy Overlayer by PTA Process (PTA법에 의한 스텔라이트 12 합금 육성층의 특성에 미치는 전류의 영향)

  • Jung, B.H.;Kim, M.K.;Ahan, Y.S.;Kim, M.Y.;Lee, S.Y.
    • Journal of Power System Engineering
    • /
    • v.5 no.3
    • /
    • pp.88-94
    • /
    • 2001
  • Stellite 12 alloy-powders were overlaid on 410 stainless steel valve seat using plasma transferred arc(PTA) process. Variation of the microstructure, hardness, wear and corrosion of overlaid deposit with current change was investigated. The deposit showed hypoeutectic microstructure, which was consisted of primary cobalt dendrite and networked $M_7C_3$ type eutectic carbides. As current increased, the amount of eutectic carbide decreased and its dendritic secondary arm spacing increased. Hardness of the deposit was decreased with increase of current. Stress relief heat treatment at $600^{\circ}C$ for two hours resulted in slight increase of hardness in the deposit and showed uniform hardness distribution in base metal without any hardened layer in HAZ. Specific wear decreased with increase of sliding distance. The deposit of high hardness with a lot of eutectic carbide showed relatively low specific wear. Initial corrosion current density of the deposit in 0.1N sulfuric acid was lower than those of 410 stainless steel, and showed a little variation with PTA current.

  • PDF

Fundamental Electro-Mechanical Characteristics of Ballooning-Resistant Bi-2223 HTS Tapes (벌루닝 손상에 강한 Bi-2223 테이프의 기본적인 전기-기계적 특성)

  • Dizon, John Ryan C;Shin, Hyung-Seop;Ha, Dong-Woo;Cho, Jeon-Wook;Oh, Sang-Soo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.11a
    • /
    • pp.26-27
    • /
    • 2006
  • The fundamental mechanical characteristics under tensile and bending deformations of hermetically-sealed reinforced Bi-2223 tape and CTOP processed Bi-2223 tape were examined at 77K. Also, the Tensile strain dependence of the critical current, $I_c$, was obtained at 77K and self-field. The reinforced hermetic tape showed higher tensile strength and a better Tensile strain tolerance than the CTOP processed tape. For bending tests, a rho-shaped sample holder was used giving multiple bending strains. in increasing order. In the same case under bending deformation, the hermetic tape showed a higher bending strain tolerance than the CTOP processed tape. This higher strength of the hermetic tape can be attributed to the thick hardened copper reinforcement layer.

  • PDF

A Study on the Dry Wear Characteristics of Austempered Ductile Cast Iron (오스템퍼링 處理된 球狀黑鉛鑄鐵의 乾燥磨滅 特性에 관한 硏究)

  • 강명순;전태옥;김형자;박흥식
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.12 no.3
    • /
    • pp.489-496
    • /
    • 1988
  • This paper is studied to know wear mechanism in variation of austempering temperature and holding time of austempered ductile cast iron against mating material SM45C hardened by heat treatment. The wear tests were carried out by rubbing the annular surface of two test pieces in dry sliding friction. The wear mechanism was investigated by scanning electron microscopy and the retained austenite volume fraction was investigated by X-ray diffractometer. The experimental results show that the wear characteristics depend largely on the oxidation of the testing materials which is influenced by the sliding velocity and distance. The retained austenite has a negative effect during frictional contact because it has increased severe wear by softened surface layer. It is shown experimentally that hard metals have lower frictional resistance and hence the resistance to adhesion is increased due to stronger interatomic linking bonds and increase in the surface energy.

Acoustic Characteristics of High Intensity Focused Ultrasound for Necrosis of CTO (CTO 괴사를 위한 고강도 집속 초음파의 음향학적 특성)

  • Park, Chan Hee;Jeong, Sang Hwa
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.24 no.5
    • /
    • pp.481-488
    • /
    • 2015
  • It is difficult to see a therapeutic effect from cardiovascular disease treatment methods in the case of a hardened chronic total occlusion (CTO), owing to the calcification of the deposition materials. However, lesion cells, such as CTOs, can be selectively necrotized without affecting the normal tissue using high-intensity ultrasound focused on one point. In this study, a phantom CTO was necrotized by a high-intensity focused ultrasound (HIFU) energy system, and the acoustic characteristics in the focal region were analyzed. An experimental HIFU device was constructed to discover the appropriate conditions for the necrosis of a phantom CTO. The transfer characteristics of the ultrasound changed in the focal region by the density difference of the phantom CTO. These changes were acoustically analyzed to choose the available frequency band for each density. On-off temperature control in the focal region was applied to prevent rapid temperature rises, which would otherwise affect normal tissue.

Sliding Wear Behavior of Pure Metal, Fe and Cu Having a Cubic Crystal System (입방정계 순 금속 Fe, Cu의 미끄럼 마멸 거동)

  • Yi, S.K.;Kim, Y.S.
    • Transactions of Materials Processing
    • /
    • v.19 no.6
    • /
    • pp.357-362
    • /
    • 2010
  • Dry sliding wear behavior of pure Fe and Cu which have BCC and FCC crystal structure, respectively, was investigated. The wear characteristics of the pure metals with different crystal structure were compared. Dry sliding wear tests were carried out using a pin-on-disk wear tester at various loads under the constant sliding speed condition of 0.15 m/s against a silica ball at room temperature. Sliding distance was fixed as 600 m for all wear tests. Wear rate of a specimen was calculated by dividing the weight loss of the specimen after the test by the specific gravity and sliding distance. Worn surfaces and wear debris were analyzed by SEM. The wear of both pure Fe and Cu proceeded with surface deformation, resulting in similar wear rates despite of their structure difference under the current test conditions. Wear rates of both metals were low if the surface deformation due to wear forms thick surface-deformation layer that is strain hardened beneath the wearing surface. The pure Cu specimens showed a lot of oxides on the worn surface when tested at low loads less than 5 N, which resulted in very low wear rate.

A Study on Formation of Thick Hardened Layer on Al Alloy Surface by PYAW Process (PTAW법에 의한 Al 합금 표면의 후막경화층 형성에 관한 연구)

  • 임병수;김봉수;오세훈;황선효;서창제
    • Journal of Welding and Joining
    • /
    • v.15 no.5
    • /
    • pp.92-103
    • /
    • 1997
  • The purpose of this study is to improve the wear resistance and hardness of Al alloy by making a formation of the thick surface hardening layers. The thick surface hardening layers were formed by PTAW(Plasma Transferred Arc Welding), with the addition of metal powders (Cu), ceramics powders (NbC, TiC), and mixture powders (Cu+NbC) in Al alloy (A1050, A5083). Mechanical properties of overlaid layers (wear resistance, hardness) were investigated in relation to the microstructure. The results obtained are summarized as follows: The depth of penetration was increased with increasing powder feeding rate. It is considered that these increase were due to the thermal pinch effect by the addition of powders, especially, for the Cu powders, were due to the heat of reaction with the matrix. The hardness and wear resistance of overlaid layers were improved with increasing powder feeding rate. For the Cu powders, it is considered that these increase were due to the increase of the formation of ${\theta}(CuAl_2)$ phase with increasing feeding rate of Cu powers.

  • PDF

Effects of Processing Time and Temperature on the Surface Properties of AISI 316L Stainless steel During Low Temperature Plasma Nitriding After Low Temperature Plasma Carburizing (AISI 316L stainless steel에 저온 플라즈마 침탄처리 후 질화처리 시 처리시간과 온도가 표면특성에 미치는 영향)

  • Lee, Insup
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.6
    • /
    • pp.357-362
    • /
    • 2008
  • The 2-step low temperature plasma processes (the combined carburizing and post-nitriding) were carried out for improving both the surface hardness and corrosion resistance of AISI 316L stainless steel. The effects of processing time and temperature on the surface properties during nitriding step were investigated. The expanded austenite (${\gamma}_N$) was formed on all of the treated surface. The thickness of ${\gamma}_N$ was increased up to about $20{\mu}m$ and the thickness of entire hardened layer was determined to be about $40{\mu}m$. The surface hardness reached up to $1,200HV_{0.1}$ which is about 5 times higher than that of untreated sample ($250HV_{0.1}$). The thickness of ${\gamma}_N$ and concentration of N on the surface were increased with increasing processing time and temperature. The corrosion resistance in 2-step low temperature plasma processed austenitic stainless steels was enhanced more than that in the untreated austenitic stainless steels due to a high concentration of N on the surface.

Corrosion Resistance and Low Friction Property of Sintered Steel Parts via Chromizing Treatment (크로마이징 처리 된 철계 소결 부품의 내식성 및 저 마찰특성)

  • Kim, Sang-Gweon;Park, Yong-Jin;Yeo, Kuk-Hyun;Lee, Jae-Hoon
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.11
    • /
    • pp.809-815
    • /
    • 2012
  • Recently, as the interest in improving energy efficiency has grown, the demand for vehicle and machine parts that are resistant in high temperature corrosive conditions and abrasive environments has increased. Pack chromizing treatment of sintered steels is a profitable method that satisfies both corrosion resistance and low friction properties. Since austenitic stainless steels have good corrosion resistance but low mechanical hardness, if they are replaced by sintered steel parts with pack chromizing treatment, all the desirable properties such as low price, easy molding, high hardness, low frictional coefficient, and high corrosion resistance, can be obtained. The higher corrosion resistance of the chromized parts over that of the austenitic stainless steels was acquired by coating chromium carbides and a thin chromium oxides layer on the surface. Moreover, the surface morphology of chromized parts, which were composed of chromium rich phases and hardened chromium carbides by diffusing and alloying, had a peak-and-valley shape so that the dimple effect by the wrinkled morphology and high hardness induced a low friction coefficient.

Design optimization for analysis of surface integrity and chip morphology in hard turning

  • Dash, Lalatendu;Padhan, Smita;Das, Sudhansu Ranjan
    • Structural Engineering and Mechanics
    • /
    • v.76 no.5
    • /
    • pp.561-578
    • /
    • 2020
  • The present work addresses the surface integrity and chip morphology in finish hard turning of AISI D3 steel under nanofluid assisted minimum quantity lubrication (NFMQL) condition. The surface integrity aspects include microhardness, residual stress, white layer formation, machined surface morphology, and surface roughness. This experimental investigation aims to explore the feasibility of low-cost multilayer (TiCN/Al2O3/TiN) coated carbide tool in hard machining applications and to assess the propitious role of minimum quantity lubrication using graphene nanoparticles enriched eco-friendly radiator coolant based nano-cutting fluid for machinability improvement of hardened steel. Combined approach of central composite design (CCD) - analysis of variance (ANOVA), desirability function analysis, and response surface methodology (RSM) have been subsequently employed for experimental investigation, predictive modelling and optimization of surface roughness. With a motivational philosophy of "Go Green-Think Green-Act Green", the work also deals with economic analysis, and sustainability assessment under environmental-friendly NFMQL condition. Results showed that machining with nanofluid-MQL provided an effective cooling-lubrication strategy, safer and cleaner production, environmental friendliness and assisted to improve sustainability.

Corrosion Fatigue Characteristics of SUS316L Steel with Ti Undercoat using Plasma Spray Method (플라즈마 스프레이방법을 이용하여 Ti 언더코트를 제작한 SUS316L강의 부식피로 특성)

  • Han, Chang-Suk;Kim, Woo-Suk
    • Korean Journal of Materials Research
    • /
    • v.31 no.3
    • /
    • pp.172-180
    • /
    • 2021
  • In this study, using the plasma spray method, tensile and compression fatigue tests are performed in saline solution to examine the effect of Ti undercoat on corrosion fatigue behavior of alumina-coated specimens. The alumina-coated material using Ti in the undercoat shows better corrosion fatigue strength than the base material in the entire stress amplitude range. Fatigue cracking of UT specimens occurs in the recess formed by grit-blasting treatment and progresses toward the base metal. Subsequently, the undercoat is destroyed at a stage where the deformation of the undercoat cannot follow the crack opening displacement. The residual stress of the UT specimen has a tensile residual stress up to about 100 ㎛ below the surface of the base material; however, when the depth exceeds 100 ㎛, the residual stress becomes a compressive residual stress. In addition, the inside of the spray coating film is compressive residual stress, which contributes to improving the fatigue strength characteristics. A hardened layer due to grit-blasting treatment is formed near the surface of the UT specimen, contributing to the improvement of the fatigue strength characteristics. Since the natural potential of Ti spray coating film is slightly higher than that of the base material, it exhibits excellent corrosion resistance; however, when physiological saline intrudes, a galvanic battery is formed and the base material corrodes preferentially.