A STUDY ON THE CHANGE OF IMPLANT STABILITY USING RESONANCE FREQUENCY ANALYSIS

  • Park Chan-Jin;Kim Yung-Soo;Kim Chang-Whe;Cho Lee-Ra;Yi Yang-Jin
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.41 no.3
    • /
    • pp.271-287
    • /
    • 2003
  • Statement of problem: Resonance frequency analysis (RFA) has been increasingly served as a non-invasive and objective method for clinical monitoring of implant stability. Many clinical studies must be required for standardized baseline data using RFA. Purpose: This study was performed to evaluate RFA value changes in two stage surgery group and one stage surgery group in patients. Material and method: Forty-seven mandibles in consecutively implant installed patients were selected for this study and 141 fixtures were installed. Ninety-three fixtures were double threaded, machined surface design ($Br{\aa}anemark^{(R)}$ MK III, Nobel Biocare AB, Goteborg, Sweden) and 48 fixtures were root form, threaded, HA-coated surface one ($Replace^{TM}$, Steri-Oss/Nobel Biocare AB, USA). Among those, each 10 fixture was installed in one stage group patients. ISQ values were measured using $Osstell^{TM}$ (Integration Diagnostics Ltd. Sweden) during fixture installation, at healing abutment connection and in the loading period for two stage surgery group patients and during at each 4, 6, 8, 10, 12week and in the loading phase for one stage surgery group patients and evaluated the changes according to the time and fixture type. Results: In two stage surgery group, mean and SO of ISQ values of machined surface implants were $76.85{\pm}3.74,\;75.76{\pm}5.04,\;75.73{\pm}4.41$ and those of HA-coated surface implant were $75.05{\pm}6.23,\;77.58{\pm}5.23,\;78.32{\pm}4.29$ during fixtures installation, at healing abutment connection and in the loading period, respectively. In one-stage surgery group, the ISQ values of machined surface and HA-coated surface implants decreased until 4 or 6 week and maintained at plateau for 1-3 week and increased to the loading period. Conclusions: Machined and HA-coated surface implants showed minimal ISQ changes with time if they were installed at the sites showing at least intact cortical plate and good bone qualities. And HA-coated implants had a tendency to show somewhat increased ISQ values with time.

EFFECT OF VARIOUS MECHANICAL TREATMENTS OF HYDROXYAPATITE-COATED IMPLANT SURFACES (Hydroxyapatite 피막 처리된 임프란트에 대한 여러가지 기계적 표면처리방법이 임프란트 표면조도 및 성상에 미치는 영향)

  • Yang, Kyung-Ran;Jung, Oh-Chul;Lee, Jae-Mok;Suh, Jo-Young
    • Journal of Periodontal and Implant Science
    • /
    • v.24 no.1
    • /
    • pp.131-143
    • /
    • 1994
  • For maintenance of exposed implant in healthy state, it is necessary to treat the surface of implant fixture and provide the surface adjustable to surrounding tissues. Variable techniques have been introduced such as citric acid and air-abrasive system to treat the failed implant. Although when the rough surface of HA coated implant was exposed to oral environment, the surface treatment method with citric acid or air-abrasive system is effective for removal of bacterial endotoxin, it is unsuccessful to prevent plaque deposition due to difficulty in removal of rough surface of HA coated implant. Thus, in this study the method that removes bacterial endotoxin and makes smooch surface without alteration of surface characteristics was studied. HA coated disc manufactured by IMZ Co. Was treated with high speed diamond bur, low speed diamond bur, stone bur, rubber point, jetpolisher. And then its surface state was examined with profilometer and SEM to evaluate the surface smoothness, and its surface component was analyzed with EDX to evaluate wheter the surface characteristics were altered or not. As a result, following results were obtained. When the surface roughness of each implant disc was measured by profilometer, the group I showed a $R_{max}\;2.11{\mu}m$ and the group II, III, IV, V showed a $R_{max2}\;4.17{\mu}m$, $7.28{\mu}m$, $8.61{\mu}m$ and $39.44{\mu}m$ respectively. That is, surface smoothness was highest in the group I and it has been gradually decreased in the group II, III, IV and V. Under the SEM examination, the group I showed relatively smooth surface and the group II showed slightly rougher surface than the group I due to partially remaining HA particles while most HA particle was removed. The group III and IV showed rough topography due to HA particles that was not grinded, and HA coated surface in group V showed very irregular surface with deep groove and prominence. In cross-sectional view, the group I showed uniform surface, and the group III, IV showed rough surface due to remaining HA particles but the thickness of HA coating was remarkably reduced. The group II has similar pattern in group I, and the group V showed about $40{\mu}m$ thickness although it was not constant. By analysis of surface component with EDX, the group II in which the grinding was effective showed a small quantity of calcium and phosphorous and the group III, IV, in which the grinding was incomplete showed calcium and phosphorus peak. In all experimental group, no other than titanium, aluminum, calcium, phosphorus was observed.

  • PDF

HISTOLOGIC COMPARATIVE STUDY ON THE BONE-IMPLANT INTERFACE OF HYDROXYLAPATITE AND TITANIUM PLASMA SPRAY COATED IMPLANTS (Hydroxylapatite 및 Titanium Plasma Spray 피복임프란트와 골조직 계면의 조직학적 비교 연구)

  • Cho, Ju-Oh;Song, Kwang-Yeob;Park, Charm-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.33 no.3
    • /
    • pp.492-516
    • /
    • 1995
  • This study evaluated the responses of mandibular bones of mongrel dogs to loaded hydro xylapatite(HA) and titanium plasma spray(TPS) coated endosseous dental implants, using unloaded ones as the control group. after HA and TPS coated implants were implanted, their bone reactions with vital bones have been observed with light and scanning electron microscope(SEM) at the three periods of the 4th, 12th and 20th week. These reactions have been also compared in a histomorphometric method. The elemental distribution state of implants and the interface neighboring bone tissues have been measured with the energy dispersive analysis of X-rays(EDAX). The following results were obtained ; 1. The light microscopic analysis showed osseointegration in both the control group and the occlusal force loaded group ; Its degree was shown to be higher in the long-maintained and occlusal force groups. 2. The SEM analysis showed that both groups had osseointegration, In the case of TPS-coated implants, the coated layer was divided on the bone interface. In the case of HA-coated implants, there appeared a division between the metal and coated interface. 3. In the histomorphometric analysis, the measured ratio contaction bone of TPS-coated implants was $70{\pm}19$% in the case of no occlusal force ; it was $84{\pm}13$% in the case of occlusal force. The measured ratio contacting bone of HA-coated implants was $75{\pm}18$% in the case of no occlusal force ; it was $94{\pm}9$% in the case of occlusal force. However, there was no significant difference statistically(p>0.05). 4. Both groups showed that the ratio of calcium and phosphorous increased more in the bone tissues than on the bone to implant interface.

  • PDF

Micromorphometric change of implant surface conditioned with tetracycline-HCI;HA and oxidized surface (표면처리 시간에 따른 임플란트 미세구조의 변화;HA와 양극산화 표면 임플란트)

  • An, Sang-Ho;Park, Joon-Bong;Kwon, Young-Hyuk;Herr, Yeek;Chung, Jong-Hyuk
    • Journal of Periodontal and Implant Science
    • /
    • v.35 no.4
    • /
    • pp.891-905
    • /
    • 2005
  • The present study was performed to evaluate the effect of tetracycline-HCL on the change of implant surface microstructure according to application time. Implant with pure titanium machined surface. HA-coated surface and TiUniteTM surface were utilized. Implant surface was rubbed with 50mg/ml tetracycline-HCL solution for $\frac{1}{2}min.$, 1min., $1\frac{1}{2}min.$, 2min., and $2\frac{1}{2}min.$ respectively in the test group. Then, specimens were processed for scanning electron microscopic observation. The results of this study were as follows. 1. Both test and control group showed a few shallow grooves and ridges in pure titanium machined surface implants. There were not significant differences between two groups. 2. In HA-coated surfaces, round particles were deposited irregularly. The roughness of surfaces conditioned with tetracycline-HCL was lessened and the cracks were increased relative to the application time. 3. The anodic oxidized surfaces showed the craterous structures. The surface conditioning with tetracycline-HCl didn't influence on its micro-morphology. In conclusion, the detoxification with 50mg/ml tetracycline-HCL must be applied respectively with different time according to various implant surfaces.

The histometric analysis of osseointegration in hydroxyapatite surface dental implants by ion beam-assisted deposition

  • Kim, Min-Kyung;Choi, Jung-Yoo;Chae, Gyung-Joon;Jung, Ui-Won;Kim, Sung-Tae;Lee, In-Seop;Cho, Kyoo-Sung;Kim, Chong-Kwan;Choi, Seong-Ho
    • Journal of Periodontal and Implant Science
    • /
    • v.38 no.sup2
    • /
    • pp.363-372
    • /
    • 2008
  • Purpose: This study compared the effects of coating implants with hydroxyapatite (HA) using an ion beam-assisted deposition (IBAD) method prepared with machined, anodized, sandblasted and large-grit acid etched (SLA) surfaces in minipigs, and verified the excellency of coating method with HA using IBAD. Material and Methods: 4 male Minipigs(Prestige World Genetics, Korea), 18 to 24 months old and weighing approximately 35 to 40 kg, were chosen. All premolars and first molars of the maxilla were carefully extracted on each side. The implants were placed on the right side after an 8 week healing period. The implant stability was assessed by resonance frequency analysis (RFA) at the time of placement. 40 implants were divided into 5 groups; machined, anodized, anodized plus IBAD, SLA, and SLA plus IBAD surface implants. 4 weeks after implantation on the right side, the same surface implants were placed on the left side. After 4 weeks of healing, the minipigs were sacrificed and the implants were analyzed by RFA, histology and histometric. Results: RFA showed a mean implant stability quotient (ISQ) of $75.625{\pm}5.021$, $76.125{\pm}3.739$ ISQ and $77.941{\pm}2.947$ at placement, after 4 weeks healing and after 8 weeks, respectively. Histological analysis of the implants demonstrated newly formed, compact, mature cortical bone with a nearby marrow spaces. HA coating was not separated from the HA coated implant surfaces using IBAD. In particular, the SLA implants coated with HA using IBAD showed better contact osteogenesis. Statistical and histometric analysis showed no significant differences in the bone to implant contact and bone density among 5 tested surfaces. Conclusion: We can conclude that rough surface implants coated with HA by IBAD are more biocompatible, and clinical, histological, and histometric analysis showed no differences when compared with the other established implant surfaces in normal bone.

Effect of Titanium Coating on Cell Adhesion and Extracellular Matrix Formation in Human Osteoblast-like MG-63 Cells

  • Lee, Jae-Bum;Seo, Sang-Hui;Kim, Yu-Ri;Shin, Sang-Wan;Kim, Meyoung-Kon;Ryu, Jae-Jun
    • Molecular & Cellular Toxicology
    • /
    • v.4 no.3
    • /
    • pp.192-198
    • /
    • 2008
  • A variety of titanium (Ti) and its alloys are used in the clinical procedures of bone regeneration for periodontal and dental implant therapies. This study was performed to determine the effect of different surface dental implant materials on biologic responses of a MG-63 human osteoblast-like cell line. MG-63 cells were cultured on Ti coated with hydroxyapatite (HA), calcium metaphosphate (CMP), anodized (A), which compared with non-coated Ti (control). The appearances of surface of dental implant materials and the morphology of these cells were assessed by scanning electron microscopy (SEM). The gene expression profiles of MG-63 cells cultured on Ti were examined by human cDNA microarray (1,152 elements). The expression of several genes was up- and down-regulated by different surfaces of dental implant materials. Interesting, the genes correlated with cellular adhesion and extra cellular matrix (ECM) formation were enhanced, in accordance surface morphology of the dental implant materials used.

COMPARATIVE STUDY OF OSSEOINTEGRATION OF 4 DIFFERENT SURFACED IMPLANTS IN THE TIBIA OF DOGS (성견 경골에서 표면처리방법이 다른 4종의 임프란트 골유착에 관한 비교연구)

  • Hong, Who-Suk;Kim, Tae-Hee;Ryu, Seong-Hee;Kook, Min-Suk;Park, Hong-Ju;Oh, Hee-Kyun
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.31 no.1
    • /
    • pp.46-54
    • /
    • 2005
  • Purpose: This study was performed in order to compare the osseointegration of 4 different surfaced implants in the dog's tibia which has thick dense cortical bone and loose marrow space. Materials & methods: Four mongrel dogs and four different surface types of implants, smooth surfaced AVANA implants, RBM surfaced AVANA implants, HA-coated Steri-Oss implants and SLA Bicon implants, were used in this study. The animals were divided into 4 groups on the basis of implant surface characteristics: Control group, RBM group, HA group, and SLA group. Three implants of each group were installed into the metaphysis of tibia of adult dogs. The animals were sacrificed at 8 weeks after implantation. The undecalcified specimens were prepared for histological examination and histomorphometric analysis of implant-bone contact ratios. Results: Radiographically and histologically good osseointegration of implant was observed in the dense cortical bone, but poor osseointegration was observed in the marrow space. Histologically more bone apposition to implant surface was found in rough surfaced groups than the smooth surfaced, Control group. In histomorphometric findings of cortical bone the average bone-implant contact ratios of HA group (95.4%, p<0.01), RBM group (87.1%, p<0.05), and SLA group (86.0%, p<0.05) were significantly higher than that of Control group (75.9%). In marrow space the average bone-implant contact ratios of HA group (76.1%, p<0.01) and SLA group (45.4%, p<0.05) were significantly higher than that of Control group (29.6%). The ratio of RBM group was higher than that of Control group but there was no significantly difference between RBM group and Control group. Conclusion: These results suggest that the rough surfaced implants can obtain the better osseointegration than the smooth surfaced implant in the cortical and marrow space and that HA-coated implants can obtain the best osseointegration in the marrow space among them.

Hydroxyapatite-coated implant: Clinical prognosis assessment via a retrospective follow-up study for the average of 3 years

  • Jung, Jun-Hong;Kim, Sang-Yun;Yi, Yang-Jin;Lee, Bu-Kyu;Kim, Young-Kyun
    • The Journal of Advanced Prosthodontics
    • /
    • v.10 no.2
    • /
    • pp.85-92
    • /
    • 2018
  • PURPOSE. This research evaluated clinical outcomes of two types of hydroxyapatite (HA)-coated implants: OT (Osstem TS III-HA, Osstem implant Co., Busan, Korea) and ZM (Zimmer TSV-HA, Zimmer dental, Carlsbad, USA). MATERIALS AND METHODS. The research was conducted on 303 implants (89 of OT, 214 of ZM), which were placed from January 16, 2010 to December 20, 2012. The prognosis was evaluated in terms of success rates, survival rates, annual marginal bone loss, and implant stability quotients (ISQ). The samples were classified into immediate, early, conventional, and delayed groups according to the loading time. RESULTS. Overall, there were no significant differences between OT and ZM in success rates, survival rates, and annual marginal bone loss, except for the result of secondary stability. OT showed $77.83{\pm}8.23ISQ$, which was marginally higher than $76.09{\pm}6.90ISQ$ of ZM (P<.05). In terms of healing periods, only immediate loading showed statistically significant differences (P<.05). Differences between OT and ZM were observed in terms of two indices, the annual marginal bone loss ($0.17{\pm}0.58mm/year$ < $0.45{\pm}0.80mm/year$) and secondary stability ($84.36{\pm}3.80ISQ$ > $82.48{\pm}3.69ISQ$) (P<.05). OT and ZM did not have any statistically significant differences in early, conventional, and delayed loading (P>.05). CONCLUSION. OT (97.75%) and ZM (98.50%) showed relatively good outcomes in terms of survival rates. In general, OT and ZM did not show statistically significant differences in most indices (P>.05), although OT performed marginally better than ZM in the immediate loading and 1-stage surgery (P<.05).

Bone Ingrowth and Enhancement of Bone Bonding Strength at Interface between Bone and HA Coated Stainless Steel (HA 코팅된 스테인레스강과 뼈의 계면에서의 경조직 성장 및 결합력 향상)

  • Kim, C.S.;Kim, S.Y.;Kim, D.H.;Khang, G.
    • Proceedings of the KOSOMBE Conference
    • /
    • v.1996 no.05
    • /
    • pp.133-136
    • /
    • 1996
  • We investigated how hydroxyapatite (HA) coating onto a porous super stainless steel (S.S.S, 22Cr-20Ni-6Mo-0.25N) affects bone ingrowth in a dog transcortical femoral model. Implants were histologically evaluated after 4 and 48 weeks of implantation, and the bone bonding strength at the bone/implant interface was examined by employing the pull-out test. The direct osseous tissue bonding onto the HA-coated S.S.S was observed, but the uncoated stainless steels had thin fibrous tissue layers. The mean interface strength of the HA-coated S.S.S was 1.5 and 2.5 times greater than those of the S.S.S and the 316L SS after one year of implantation, respectively. In preliminary studies, no toxic responce was observed from a cytotoxicity test of the S.S.S, having similar corrosion resistance to titanium. Our results suggest that early osteoconductive nature of HA coating may induce long term osteointegration for a bioinert substrate.

  • PDF