고로슬래그 콘크리트의 구조체 보정강도(mSn) 산정을 위한 고로슬래그 혼입 구조체 콘크리트의 적산온도법 적용에 관한 실험적 연구 (An Experimental Study on the Application of the Maturity Method of Ground Granulated Blast Furnace Slag(GGBFS) Concrete to Calculate the Concrete Strength Correction Value(mSn))

  • 김한솔;정민구;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 가을학술발표대회논문집
    • /
    • pp.147-148
    • /
    • 2023
  • Recently, as blast furnace slag concrete has become widely used, managing the strength of concrete has become important. mSn is a method of correcting the difference in strength between standard cured specimens and concrete exposed to changes in temperature. In this study, the predicted strength based on the maturity of the central and outer parts of the blast furnace slag concrete structure is compared with the actual strength measured through coring. As a result, the actual strength difference between the center and the outer part of the concrete mixed with blast furnace slag was larger than the predicted strength difference.

  • PDF

동절기 슬래그 혼입 콘크리트의 실용화기술개발 (Development and Application of Concrete using Ground Granulated Blast Slag in Winter Season)

  • 유조형;김우재;홍석범
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.256-257
    • /
    • 2014
  • Concrete made with ground granulated blast-furnace slag(GGBS) has many advantage, including improved durability, workability and economic benefits. GGBS concrete is that its strength development is considerably slower under standard 20℃ curing conditions than that of portland cement concrete, although the ultimate strength is higher for same water-binder ratio. GGBS is not therefore used in application where high early age strength is required. However, hydration of GGBS is much more sensitive to temperatures, the strength development of GGBS concrete is significantly enhanced.

  • PDF

광물질 혼화재 및 석고를 사용한 고강도 콘크리트의 슬럼프 손실 (Slump Loss of High Strength Concrete Containing Mineral Admixture and Gypsum)

  • 김기형;최재진
    • 한국안전학회지
    • /
    • 제12권1호
    • /
    • pp.101-107
    • /
    • 1997
  • High strength concrete(HSC) using high range water reducing admixture (HRWR) has the defect which severe slump loss occurs according to elapsed time. For using HSC without any trouble, special caution and countermeasure against this problem are necessary. In this study, for minimizing the slump loss of HSC, mineral admixture( flyash, ground granulated blast furnace slag ) and gypsum were used experimentally. Flyash and ground granulated blast furnace slag are effective in reducing the slump loss of HSC. Especially, the slump loss of HSC containing mineral admixture and gypsum Is minimized by the aggregation inhibiting action of gypsum. Cement substituted with flyash 30% or ground granulated blast furnace slag 50% by weight are very effective in minimizing the slump loss.

  • PDF

CaO-Al2O3계 무기결합재 사용량에 따른 고로슬래그 미분말의 응결특성 (Setting Properties of GGBS Powder According to Replacement of Ratio of CaO-Al2O3 Based Inorganic Binder)

  • 최덕진;이영재;최세진;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.78-79
    • /
    • 2013
  • As a part of study to maximize the amount used of the ground granulated blast-furnace slag, the study deals with setting properties of paste that is mixed the ground granulated blast-furnace slag with CaO-Al2O3 based inorganic blinder. The results of the experiment show that the setting time is most fast in the mix of 25% rate of CaO-Al2O3 based inorganic blinder. It is generally needed 2 hours for work time in precast concrete products. In this study, this requirement is achieved when using the retarder of 0.5%.

  • PDF

고로슬래그 미분말의 치환율을 고려한 압축강도예측모델에 관한 실험적 연구 (An Experimental Study on the Prediction Model for the Compressive Strength of Concrete according to Replacement Ratio of Ground Granulated blast-furnace slag)

  • 양현민;박원준;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.89-90
    • /
    • 2013
  • This study is to predict the compressive strength for the concrete of ground granulated blast-furnace slag, and use Plowman's, Gompertz's model. The results are as follows; The prediction compressive strength were simiar using Rastrup's equivalent age model. but The prediction compressive strength using Freiesleben's equivalent age model weren't simiar in bfs replacement Ratio of 50%, because it is analyzed as the activation energy.

  • PDF

Study on the characteristics of grout material using ground granulated blast furnace slag and carbon fiber

  • Kim, Daehyeon;Park, Kyungho
    • Geomechanics and Engineering
    • /
    • 제19권4호
    • /
    • pp.361-368
    • /
    • 2019
  • This study aims to evaluate the applicability of a grout material that is mixed with carbon fiber, biogrout, ground granulated blast furnace slag (GGBS) powder and cement. Uniaxial compressive strength tests were performed on homo-gel samples at days of 1, 3, 7, 14 and 28. In addition, the variation of permeability with the mixing ratios was measured. Based on the uniaxial compressive strength test, it was confirmed that the uniaxial compressive strength increased by 1.2times when carbon fiber increased by 1%. In addition, as a result of the permeability test, it was found that when the GGBS increased by 20%, the permeability coefficient decreased by about 1.5times. Therefore, the developed grout material can be used as a cutoff grouting material in the field due to its strength and cut-off effect.

고로슬래그 미분말을 혼입한 폴리머 시멘트 모르타르의 성질 (Properties of Polymer-Modified Mortars Using Ground Granulated Blast-Furnace Slag)

  • 주명기;연규석;이윤수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.1035-1040
    • /
    • 2001
  • The effects of polymer-binder ratio and slag content on the properties of combined wet/dry-cured polymer-modified mortars using granulated blast-furnace slag (slag) are examined. As a result, the flexural and compressive strengths of polymer-modified mortar using slag reaches a maximum at a slag content of 40%, and is inclined to increase with increasing polymer-binder ratio. The water absorption, carbonation depth and chloride ion penetration depth tend to decrease with increasing polymer-binder ratio and slag content.

  • PDF

슬래그부산물을 자극제로 활용한 고활성 고로슬래그 미분말 모르타르의 압축강도 발현 특성 (Properties of Compressive Strength of Mortar Based on High-activated Blast Furnace Slag using the Slag by-product as an Activator)

  • 이보경;김규용;구경모;신경수
    • 한국건축시공학회지
    • /
    • 제14권1호
    • /
    • pp.37-44
    • /
    • 2014
  • 건설산업에서는 탄산가스 저감을 위해 산업부산물을 다량 활용하는 기술개발을 위한 연구가 이루어지고 있다. 산업부산물 중 특히 고로슬래그 미분말은 잠재수경성에 기인하여 장기강도는 우수하나 초기강도가 낮기 때문에 많은 양을 대체하는데 한계가 있다. 이에 본 연구에서는 철강공정 중 용선예비처리 공정에서 발생하는 슬래그부산물을 활용하여 고활성 고로슬래그 미분말을 시험 제조후 고활성 고로슬래그 미분말의 모르타르 압축강도 강도발현 특성을 검토하였다. 또한, 고활성 고로슬래그 미분말 단독으로도 경화가 가능한 특징을 고려해서 2차 콘크리트 제품용 결합재로서 활용 가능성을 검토하고자 배합조건에 따른 콘크리트 제조 및 압축강도 발현특성을 검토하였다. 실험변수로써 슬래그부산물의 분말도, 치환율, 양생조건 및 W/B를 설정하였다. 그 결과 슬래그부산물을 자극제로 활용한 고활성 고로슬래그 미분말 모르타르의 압축강도 향상을 확인하였으며 고활성 고로슬래그 미분말이 단독으로도 경화가 가능하기 때문에 양생 및 배합조건을 고려하면 고활성 고로슬래그 미분말을 콘크리트 2차 제품용 결합재로서 활용 가능할 것으로 판단된다.

플라이애시 및 고로슬래그 미분말을 사용한 콘크리트의 강도 발현 예측 모델식 연구 (A Study on Estimation Model of Strength Development of Concrete Using Fly Ash and Ground Granulated Blast-Furnace Slag)

  • 최연왕;박만석;정재권;최병걸;김경환
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제17권5호
    • /
    • pp.87-93
    • /
    • 2013
  • 최근 콘크리트 산업은 $CO_2$ 가스 배출 저감을 목적으로 플라이애시 및 고로슬래그 미분말 등의 혼화재 사용량이 증가되고 있다. 그러나 국내의 경우 구조설계기준에서 사용되고 있는 강도 발현 예측 모델은 시멘트 종류 및 양생방법에 따른 상수값 ${\beta}_{sc}$를 포틀랜드시멘트에 관해서만 규정함에 따라 플라이애시 및 고로슬래그 미분말을 혼합 사용한 콘크리트의 시간에 따른 강도 발현 특성을 반영하지 못하는 실정이다. 따라서 본 논문에서는 플라이애시 및 고로스래그 미분말을 혼합한 보통강도 및 고강도 영역의 콘크리트의 시간에 따른 강도를 평가하였으며, 혼화재 종류 및 혼합률에 따른 콘크리트 강도발현 상수 ${\beta}_{sc}$ 값을 제안하였다.

고성능 쉴드 세그먼트용 고로슬래그 미분말을 혼입한 콘크리트의 역학적 특성 및 증기양생 효과 분석 (Mechanical characteristics of high-performance concrete shield segment containing ground granulated blast furnace slag and their improvement by steam curing)

  • 김병권;이진섭;이규필;장수호;배규진
    • 한국터널지하공간학회 논문집
    • /
    • 제13권3호
    • /
    • pp.233-242
    • /
    • 2011
  • 본 연구에서는 쉴드터널에 사용되는 세그먼트의 성능향상과 경제성향상을 위하여 고로슬래그 미분말을 혼합한 고강도 콘크리트에 대한 기초 연구를 실시하였다. 특히, 설계강도가 60 MPa 세그먼트용 콘크리트에 대해서 고로슬래그 미분말의 최적 치환율과 최적의 증기양생 조건을 도출하고자 하였다. 이상의 결과로부터, 고로슬래그 치환율 50%와 단위수량 125 kg/$m^3$ 일 경우가 성능과 경제적인 측면에서 가장 적합한 배합조건으로 나타났다. 또한 표준양생 조건과 비교할 때 증가양생에 의하여 약 110~442%의 강도증진 효과를 기대할 수 있는 것으로 확인되었다.