Expansion Properties of Mortar Using Waste Glass and Industrial By-Products (폐유리와 산업부산물을 사용한 모르터의 팽창특성)

  • 박승범;이봉춘
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.3
    • /
    • pp.440-448
    • /
    • 2002
  • Waste glass has been increased with the development of industry. The utilization of waste glass for concrete can cause the concrete to be cracked and to be weakened due to an expansion by alkali-silica reaction(ASR). In this study, ASR expansion and properties of strength were analyzed in terms of waste glass color(amber, emerald-green), industrial by-products(ground granulated blast-furnace slag, fly ash), and the content of industrial by-products for reducing ASR expansion caused by the waste glass. The possibility of using glass ground as pozzolanic properties was also analyzed. From the result of this study, the pessimum size of waste glass was 2.5∼1.2 mm regardless of waste glass color. And the smaller than 2.5∼1.2 mm waste glass is, the more decreasing expansion of ASR is. Also, the combination of waste glass with industrial by-products have an effect on reducing the expansion and strength loss caused by ASR between the alkali in the cement paste and the silica in the waste glass, and the glass ground of less than 0.075 mm is applicable as a pozzolanic material.

Strength and durability of ultra fine slag based high strength concrete

  • Sharmila, Pichaiya;Dhinakaran, Govindasamy
    • Structural Engineering and Mechanics
    • /
    • v.55 no.3
    • /
    • pp.675-686
    • /
    • 2015
  • The use of ground granulated blast furnace slag (GGBFS) from steel industries waste is showing perspective application in civil engineering as partial substitute to cement. Use of such waste conserves natural resources and minimizes the space required for landfill. The GGBFS used in the present work is of ultra fine size and hence serves as micro filler. In this paper strength and durability characteristics of ultra fine slag based high strength concrete (HSC) (with a characteristic compressive strength of 50 MPa) were studied. Cement was replaced with ultra fine slag in different percentages of 5, 10, and 15% to study the compressive strength, porosity, resistances against sulfate attack, sorptivity and chloride ion penetration. The experiments to study compressive strength were conducted for different ages of concrete such as 7, 28, 56, and 90 days. From the detailed investigations with 16 mix combinations, 10% ultra fine slag give better results in terms of strength and durability characteristics.

Physical/Chemical Characterization of Ordinary Portland Cement/Ground Granulated Blast Furnace Slag Pastes Containing Low Carbon Steel as Reinforcements

  • Hwang, Jin-Ha
    • Korean Journal of Materials Research
    • /
    • v.13 no.2
    • /
    • pp.94-100
    • /
    • 2003
  • The interface between low carbon steel and blended cement pastes containing slag was investigated using impedance spectroscopy. In addition, the pastes were characterized by several analytical methods (XRD, EDX, electrode potential, pH and ICP). The electrical behavior of the interface in the blended slag systems is correlated to its corresponding pore solution chemistry and the products present in the interface. Passivation occurred at the paste/steel interfaces, in cement pastes up to containing from 0 to 75% slag content. 100% slag paste induced corrosion of the low carbon steel, which could be explained by the influence of sulfur on the system.

An Experimental Study on the Properties of Drying Shrinkage for Alkali-Activated Slag Mortar (알칼리 자극제를 혼입한 고로슬래그 모르타르의 건조수축 특성에 관한 실험적 연구)

  • Chun Jung-Hwan;Kim Jae-Hun;Jee Nam-Yong
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2006.05a
    • /
    • pp.97-100
    • /
    • 2006
  • This paper report the result of the investigation on the properties of drying shrinkage for alkali-activated slag mortar in different relative humidity Commonly we know that drying shrinkage means lost more moisture but the mechanism of drying shrinkage of alkali activated slag mortar is not entirely due to the quantity of weight loss of water from mortar. pore size distribution and the calcium silicate hydrate gel characteristics have a critical influence on the magnitude of drying shringkage to alkali activated slag mortar. For this investigation, Ca(OH)2, Na2SiO4 were as alkali activator with 5 dosages(6%, 9%, 12%, 15%, 20%) and curing condition were three different relative humidity(35%, 65%, 95%) at $20{\pm}3^{\circ}C$

  • PDF

Evaluation of Curing Conditions for Improving the Various Properties of Aerated Concrete Incorporating Slag Powder (슬래그 혼입 기포콘크리트의 성능향상을 위한 양생조건의 평가)

  • Park, Jong-Beom;Yoon, Hyun-Sub;Yang, Keun-Hyeok
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.6
    • /
    • pp.527-532
    • /
    • 2018
  • The objective of the present study is to evaluate a practical approach for enhancing the compressive strength and minimizing deforming of aerated concrete. Test results measured in the aerated concrete mixes that were produced using 40% ground granulated blast-furnace slag (GGBS) as a replacement of cement and cured under different conditions (i.e., high temperatures of $40^{\circ}C$ and $60^{\circ}C$ for 10 hrs or 15 hrs) were compared with those obtained from the specimens cured under room temperature. No deforming was observed in the mixes with 40% GGBS. The compressive strength of the prepared aerated concrete cured under high temperature was higher than that of the concrete cured at room temperature, even at the lower ranges of the apparent dry density. However, the curing time is needed to be controlled as not exceeding 10 hrs at the temperature of $60^{\circ}C$ to prevent the decrease in the compressive strength due to foam mergences.

Properties of Fresh Concrete admixed with Blast-Furnace Slag Powder with variations of Blaine and Content (분말도 및 치환율 변화에 따른 고로슬래그 미분말 혼입 콘크리트의 초기물성)

  • 최진만;김형래;임정수;김상규;이도현;변승호;윤철현;최현국
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.10a
    • /
    • pp.297-300
    • /
    • 1999
  • This study was carried out to present the properties of fresh concrete made with ground granulated blast-furnace slag (BFS) powder with variations of blaine and content, and to estimate the utilization of the BFS concrete as admixtural materials for concrete structures of the building. According to the results, the fluidity of concrete which BFS dosage rate was 45% had the considerable difference from that of concrete which BFS dosage rate was not bigger than 35%. Also, the diminution of bleeding was appeared with the increase of blaine and content of BFS. It is concluded that BFS concrete of low blaine can be used effectively in concrete structures of the building.

  • PDF

A Experimental Study on the High Performance Concrete for Bridge Decks (고성능 콘크리트의 교량 바닥판 적용을 위한 실험적 연구)

  • Suh, Jin-Won;Rhee, Ji-Young;Cheong, Hai-Moon;Ku, Bon-Sung;Shin, Do-Chul
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.53-56
    • /
    • 2006
  • To develop more durable concrete deck, performance characteristic test of HPC(High Performance Concrete) mixtures was carried out. The parameters used in this project were ; the mineral admixture details were 4 types such as ordinary portland cement(OPC), 20% fly ash (FA), 20% fly ash and 4% silica fume(FS), and 40% ground granulated blast-furnace slag(BS). Their design compressive strengths were 27MPa and 35MPa respectively. The results showed the compressive strength of concrete did not much affect the durability of concrete. HPC with blast-furnace slag(BS) showed the good durability but was prone to crack. HPC with fly ash(FA) or with fly ash and silica fume(FS) had the good durability and crack resistance.

  • PDF

Effect of W/C and the Kinds of Cement on the Chloride Invasion Resistance of the Offshore Concrete (물-시멘트비 및 시멘트 종류가 해양콘크리트의 내염해성에 미치는 영향)

  • Shin Hong Chol;Yoo Jae Kang;Park Sang Joon;Kim Young Jin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05b
    • /
    • pp.165-168
    • /
    • 2005
  • This paper investigated the effect of W/C and the kinds of cement on the chloride invasion resistance of the offshore concrete. W/C set up 0.30, 0.35, 0.40 and The kinds of cement were used four(ordinary portland cement, ground granulated blast-furnace slag cement, belite cement, low heat portland cement). For the electrical migration test, NT BUILD 492's method was used to estimate the migration coefficient of chloride ion. As a result, the migration coefficients of chloride ion of concrete according to w/c were shown reducing with the w/c increasing, and according to kinds of cement were shown discrepancy in chloride invasion resistance. Especially blast-furnace slag cement was most low it. In the each cement, the compressive strength was shown related to the migration coefficient.

  • PDF

A Study on the Applicability of Estimation of Apparent Activation Energy of Blast Furnace Slag Contained Cement Using Calorimeter (열량계를 이용한 고로슬래그 혼입 페이스트의 겉보기 활성화 에너지 산정에 관한 연구)

  • Kim, Han-Sol;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.78-79
    • /
    • 2021
  • It is necessary to calculate Apparent Activation Energy(Ea) in order to apply the equivalent age formula to predict compressive strength using the maturity method. For carbon reduction, it is necessary to consider the change of Ea by condition of GGBFS concrete, which is widely used today. In this study, as a basic study for the design of the compressive strength model of GGBFS concrete, the apparent activation energy of the GGBFS mixed paste was calculated through a calorimeter. The experiment was carried out at a hydration temperature of 10 to 30℃ with a paste test specimen having a GGBFS content of 0 to 80%. As a result, the GGBFS replacement rate of the paste increased, and Ea tended to increase as the temperature decreased.

  • PDF

A Study on the Prediction of Concrete Strength Based on Maturity Method for Calculating the Concrete Strength Correction Value (mSn) of Two-Component Concrete (2성분계 콘크리트의 구조체 보정강도(mSn) 산정을 위한 적산온도 기반 콘크리트의 압축강도 예측 연구)

  • Kim, Han-Sol;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.05a
    • /
    • pp.129-130
    • /
    • 2023
  • The compressive strength of concrete is greatly affected by the temperature inside the concrete at the initial age immediately after pouring. In the KCI Concrete Standard Specification, only the temperature correction strength (Tn) according to the curing temperature is applied in the mixing strength calculation formula, and mSn is not considered. The formula based on the Chrino model of the blast furnace slag concrete was calculated, and the strength of the structural concrete and the strength of the water cured specimen in the same mixture were compared with the predicted strength. As a result, the error between the predicted strength and the measured strength was greater in the structural concrete than in the concrete specimen.

  • PDF