Influence of Tempering Temperature and Microstructure on Wear Properties of Low Alloy PM Steel with 1-2% Ni Addition

  • Tekeli, Suleyman;Gural, Ahmet;Guru, Metin
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1004-1005
    • /
    • 2006
  • The effect of tempering temperature and microstructure on dry sliding wear behavior of quenched and tempered PM with 0.3% graphite and 1-2% Ni steels was investigated. The sintered specimens were quenched from $890^{\circ}C$ and then tempered at $200^{\circ}C$ and $600^{\circ}C$ for 1 hr. Wear tests were carried out on the quenched$\neq$tempered specimens under dry sliding wear conditions using a pin-on-disk type machine at constant load and speed. The experimental results showed that the wear coefficient effectively increased with increasing tempering temperature and decreased with increasing Ni content.

  • PDF

Synthesis of Cu-coated Ni-based Bulk Metallic Glass Powders by Gas Atomization and Spray Drying Process

  • Kim, Byoung-Kee;Kim, Yong-Jin;Kim, Jin-Chun
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.936-936
    • /
    • 2006
  • Bulk amorphous materials have been intensively studied to apply for various advanced industry fields due to their high mechanical, chemical and electrical properties. These materials have been produced by several techniques such as mechanical alloying, melt spinning and gas atomization, etc. Among them, the atomization is the most potential technique for commercialization due to high cooling rate during solidification of the melt and mass productivity. However, the amorphous powders still have some limitations because of their low ductility and toughness. Therefore, intensive efforts have to be carried out to increase the ductility and toughness. In this study, the Ni-based amorphous powder was produced by the gas atomization process. And in order to increase the ductile toughness, ductile Cu phase was coated on the Ni amorphous powder by spray drying process. The characteristics of the as-synthesis powders have been examined and briefly mentioned. The master alloy with $Ni_{57}Zr_{20}Ti_{16}Si_2Sn_3$ was prepared by vacuum induction melting furnace with graphite crucible and mold. The atomization was conducted at $1450^{\circ}C$ under the vacuum of $10^{-2}$ torr. The gas pressure during atomization was varied from 35 to 50 bars. After making the Ni amorphous powders, the spray drying was processed to produce the Cu -coated Ni amorphous composite powder. The amorphous powder and Cu nitrate solution were mixed together with a small amount of binder and then it was sprayed at temperature of $130^{\circ}C$ and rotating speed of 15,000 R.P.M.

  • PDF

Microstructural and Mechanical Characteristics of In Situ Synthesized Chromium-Nickel-Graphite Composites

  • Pirso, Juri;Viljus, Mart;Letunovits, Sergei;Juhani, Kristjan
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.631-632
    • /
    • 2006
  • Cr-C-Ni composites were synthesized in situ from elemental powders of Cr, Ni and C by high energy milling followed by reactive sintering. The milled powders with the grain size in nano-scale were pressed to compacts and sintered. During the following thermal treatment at first the chromium carbide was formed and then the $Cr_3C_2-Ni$ cermets were sintered in one cycle. The interface between the binder phase and the carbide grains of the in situ composite has a good bonding strength as it is not contaminated with oxidation films or other detrimental surface reactions.

  • PDF

NCM계 리튬이온 배터리 양극재의 그라파이트 첨가 탄산화 배소와 수침출에 의한 Li 회수 (Lithium Recovery from NCM Lithium-ion Battery by Carbonation Roasting with Graphite Followed by Water Leaching)

  • 이소연;이대현;이소영;손호상
    • 자원리싸이클링
    • /
    • 제31권4호
    • /
    • pp.26-33
    • /
    • 2022
  • 리튬이온배터리의 수요가 증가함에 따라 향후 발생할 폐리튬이온배터리 중의 유가금속 회수가 필요하다. 대량의 폐리튬이온배터리 리사이클링에는 건식제련이 적합하지만 Li이 슬래그나 분진으로 손실되는 문제점이 있다. 본 연구에서는 폐리튬이온배터리의 NCM계 양극재로부터 Li을 회수하기 위해 그라파이트 첨가에 따른 탄산화 배소와 수침출 거동에 대해 조사하였다. 그라파이트를 10 wt% 첨가 시, Ar 및 CO2 분위기에서 승온 중 약 850 K에서 급격한 무게 감소와 함께 CO 및 CO2 가스가 배출되었다. 급격한 무게 감소 후 NCM은 금속 산화물 및 순금속으로 분해되고 환원되었다. 따라서 블랙파우더(NCM+그라파이트)의 탄산화 배소에서는 NCM의 분해에 의해 O2가 발생하면서 Li2O, NiO 등의 산화물이 생성되고, 이어서 Li2O가 CO2와 반응하여 Li2CO3를 생성하며, NiO의 일부는 그라파이트에 의해 환원되어 금속 Ni을 생성한다. 그리고 탄산화 배소 후 수침출에 의해 약 99.95 % 순도의 Li2CO3를 최대 94.5 %까지 회수하였다.

EFFECT OF ADDED Si ON DENSIFICATION OF Ni-AI INTERMETALLIC COATING ON SPHEROIDAL GRAPHITE CAST IRON SUBSTRATES

  • Kim, Tetsuro ata;Keisuke Uenishi;Akira Ikenaga;Kojiro F. Kobayashi
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.726-731
    • /
    • 2002
  • Reaction synthesis is a process to form ceramics, intermetallics and their composites from elemental powder mixture. Application of this process to a surface modification techniques has a possibilities to enable the process at a lower temperature or for a shorter time, although synthesized materials are likely to include voids and unreacted elements. This paper intend to examine the effect of Si addition to the mixture of Al and Ni on the densification of synthesized Ni-Al intermetallic compounds and to evaluate the surface properties of obtained coatings. By the Si addition, exothermic reaction temperature to form Ni-Al intermetallic was lowered to be below the melting point of Al. Si soluted $Al_3$Ni$_2$, $Al_3$Ni and $Al_{6}$Ni$_3$Si were mainly formed in the coating layer when powder mixture was heated to 973K for 300s. Besides, densification was enhanced by increasing hot press pressure, Si additions and heating rate. When the composition of eutectic Al-Si reaches 78%, void ratio of sintered compact reduced to 0.4%. It is caused by higher flowability of Al-Si liquid phase generated and its infiltration into the void. Since the hardness of NiAl(Si) compound (about 600HV) formed in the coating layer is higher than that of Ni-Al compound (about 400HV), coating layer with high density and superior wear property is obtained by hot press using reaction synthesis from Al-Ni-Si powder mixture.

  • PDF

고체산화물 연료전지를 위한 플라즈마 용사코팅 Ni/YSZ 음극 복합체의 특성평가 (Characterization of Ni/YSZ Anode Coating for Solid Oxide Fuel Cells by Atmospheric Plasma Spray Method)

  • 박수동;윤상훈;강기철;이창희
    • Journal of Welding and Joining
    • /
    • 제26권4호
    • /
    • pp.50-54
    • /
    • 2008
  • In this research, anode for SOFC has been manufactured from two different kinds of feedstock materials through thermal spraying process and the properties of the coatings were characterized and compared. One kind of feedstock was manufactured from spray drying method which includes nano-components of NiO, YSZ (300 nm) and graphite. And the other is manufactured by blending the micron size NiO coated graphite, YSZ and graphite powders as feedstock materials. Microstructure, mechanical properties and electrical conductivity of the coatings as-sprayed, after oxidation and after hydrogen reduction containing nano composite which is prepared from spray-dried powders were evaluated and compared with the same properties of the coatings prepared from blended powder feedstock. The coatings prepared from the spray dried powders has better properties as they provide larger triple phase boundaries for hydrogen oxidation reaction and is expected to have lower polarization loss for SOFC anode applications than that of the coatings prepared from blended feedstock. A maximum electrical conductivity of 651 S/cm at $800^{\circ}C$ was achieved for the coatings from spray dried powders which much more than that of the average value.

Effect of Alloying on the Microstructure and Fatigue Behavior of Fe-Ni-Cu-Mo P/M Steels

  • Bohn, Dmitri A.;Lawley, Alan
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 1997년도 춘계학술강연 및 발표대회 강연 및 발표논문 초록집
    • /
    • pp.34-34
    • /
    • 1997
  • The effect of alloying mode and porosity on the axial tension-tension fatigue behavior of a P/M steel of nominal composition Fe-4w/o Ni-1.5w/o Cu-O.5w/o Mo-O.5w/o C has been evaluated. Alloying modes utilized were elemental powder mixing, partial alloying(distaloy) and prealloying by water atomization; in each case the carbon was introduced as graphite prior to sintering. Powder compacts were sintered($1120{\circ}C$/30 min.) in 7Sv/o $H_2$/25v/o $N_2$ to densities in the range 6.77-7.2 g/$cm^3$. The dependence of fatigue limit response on alloying mode and porosity was interpreted in terms of the constituent phases and the pore and fracture morphologies associated with the three alloying modes. For the same nominal composition, the three alloying modes resulted in different sintered microstructures. In the elemental mix alloy and the distaloy, the major constituent was coarse and fine pearlite, with regions of Ni-rich ferrite, Ni-rich martensite and Ni-rich areas. In contrast, the prealloy consisted primarily of martensite by with some Ni-rich areas. From an examination of the fracture surfaces following fatigue testing it was concluded that essentially all of the fracture surfaces exhibited dimpled rupture, characteristic of tensile overload. Thus, the extent of growth of any fatigue cracks prior to overload was small. The stress amplitude for the three alloying modes at 2x$l0^6$ was used for the comparison of fatigue strengths. For load cycles <3x$l0^5$, the prealloy exhibited optimum fatigue response followed by the distaloy and elemental mix alloy, respectively. At load cycles >2x$l0^6$, similar fatigue limits were exhibited by the three alloys. It was concluded that fatigue cracks propagate primarily through pores, rather than through the constituent phases of the microstructure. A decrease in pore SIze improved the S-N behavior of the sintered steel.

  • PDF

금속수소화물-팽창흑연 복합체의 열전달 특성 및 수소 저장 특성 (Heat Transfer Characteristics and Hydrogen Storage Kinetics of Metal Hydride-Expended Graphite Composite)

  • 이평종;김종원;배기광;정성욱;강경수;정광진;박주식;김영호
    • 한국수소및신에너지학회논문집
    • /
    • 제31권6호
    • /
    • pp.564-570
    • /
    • 2020
  • Metal hydride is suitable for safe storage of hydrogen. The hydrogen storage kinetics of the metal hydride are highly dependent on its heat transfer characteristics. This study presents a metal hydride-expended graphite composite with improved thermal conductivity and its hydrogen storage kinetics. To improve the heat transfer characteristics, a metal hydride was mixed and compacted with a high thermal conductivity additive. As the hydrogen storage material, AB5 type metal hydride La0.9Ce0.1Ni5 was used. As an additive, flakes-type expended graphite was used. With improved heat transfer characteristics, the metal hydride-expended graphite composite stores hydrogen four times faster than metal hydride powder.

Correlation between Component Fatigue Performance and Results from Plane Bending Fatigue Tests on Notched Samples

  • Bergmark, Anders;Dizdar, Senad;Bengtsson, Sven;Luk, Sydney
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.381-382
    • /
    • 2006
  • A comparative study is made on root bending fatigue performance of spur gears and plane bending fatigue performance of notched test bars. R = 0 root bending fatigue tests are made on small spur gears with critical root radius 1.0 mm. The results are compared to plane bending fatigue tests of 0.9 mm radius notched specimens. Results are presented for tests on 4%Ni/2%Cu/1.5%Mo prealloyed PM steel with addition of about 0.6% graphite. Predicted values from the test bars coincide well with the results obtained from the gear root fatigue tests.

  • PDF

Effect of Repeated Quenching Heat Treatment on Microstructure and Dry Sliding Wear Behaviour of Low Carbon PM Steel

  • Gural, Ahmet;Tekeli, Suleyman;Ozyurek, Dursun;Guru, Metin
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.570-571
    • /
    • 2006
  • The mixed atomized iron powders with 0.3% graphite and 1% Ni powders were cold pressed and sintered at $1200^{\circ}C$ for 30 min under pure Ar gas atmosphere. Some of the sintered specimens were intercritically annealed at $760^{\circ}C$ and quenched in water (single quenching). The other sintered specimens were first fully austenized at $890^{\circ}C$ and water quenched. These specimens were then intercritically annealed at $760^{\circ}C$ and re-quenched in water. The experimental results showed that the wear coefficient effectively decreased in the double quenched specimen.