• 제목/요약/키워드: Grain growth mechanism

검색결과 124건 처리시간 0.024초

비정질 실리콘의 ELC 공정에 대한 광학적 연구 (An Optical Study on ELC Process of Amorphous Silicon)

  • 김우진;윤창환;박승호;김형준
    • 한국레이저가공학회지
    • /
    • 제6권2호
    • /
    • pp.9-17
    • /
    • 2003
  • Due to the heat confinement in the shallow region of the target for a short time scale, pulsed laser annealing has received an increasing interest for the fabrication of poly-Si thin film transistors(TFTs) on glass as a low cost substrate in the flat panel displays. The formation and growth mechanisms of poly silicon(poly-Si) grains in thin films are investigated using an excimer laser crystallization system. To understand the crystallization mechanism, the grain formations are observed by FESEM photography. The optical reflectance and transmittance during the crystallization process are measured using HeNe laser optics. A two-step ELC(Excimer Laser Crystallization) process is applied to enhance the grain formation uniformity.

  • PDF

열간 유동응력 예측을 위한 물리식 기반 동적 재결정 모델 (A Physically Based Dynamic Recrystallization Model for Predicting High Temperature Flow Stress)

  • 이호원;강성훈;이영선
    • 소성∙가공
    • /
    • 제22권8호
    • /
    • pp.450-455
    • /
    • 2013
  • In the current study, a new dynamic recrystallization model for predicting high temperature flow stress is developed based on a physical model and the mean field theory. In the model, the grain aggregate is assumed as a representative volume element to describe dynamic recrystallization. The flow stress and microstructure during dynamic recrystallization were calculated using three sub-models for work hardening, for nucleation and for growth. In the case of work hardening, a single parameter dislocation density model was used to calculate change of dislocation density and stress in the grains. For modeling nucleation, the nucleation criterion developed was based on the grain boundary bulge mechanism and a constant nucleation rate was assumed. Conventional rate theory was used for describing growth. The flow stress behavior of pure copper was investigated using the model and compared with experimental findings. Simulated results by cellular automata were used for validating the model.

WC기 초경합금중 WC/WC界面의 구조와 입계편석 (Stucture and Intergranular Segregation of WC/WC Grain Boundaries in WC-Based Cemented Carbides)

  • 신순기
    • 한국재료학회지
    • /
    • 제10권9호
    • /
    • pp.612-618
    • /
    • 2000
  • WC-Co와 WC-Co 초경합금중 WC/WC 입계의 구조와 입계 편석상태를 알아볼 목적으로 HRTEM과 EDS를 이용하여 연구하였다. 일부의 입계들은 액상에 의하여 분리된 상태로 관찰되었으나, 상당수는 원자적 상태의 연소계면이었다. 또 연속계면 중 WC-Co 합금에서는 Co 상이 편석되어 있었으며, WC-VC-Co 합금에서는 Co와 V이 동시에 편석되어 있음을 알 수 있었다. 그 편석의 폭은 약6nm이었다. 연속 계면 중 V의 편석은 소결 또는 열처리 시에 일어나는 입계 이동을 억제하는 데 효과적인 역할을 할 것으로 여겨졌다. 동시에 이것은 WC-Co 초경합금에서 VC 첨가에 의한 입성상 억제기구를 설명할 수 있는 것으로 사료되었다.

  • PDF

변동하중하에서의 피로크랙 지연현상과 지연기구에 관한 연구 - 균열성장 지연현상에 미치는 균열 가지의 영향 - (A Study on Fatigue Crack Retardation and Retardation Mechanism in Variable Loading)

  • 송삼홍;권윤기
    • 한국정밀공학회지
    • /
    • 제14권6호
    • /
    • pp.83-89
    • /
    • 1997
  • In order to study on fatigue crack retardation and retardation mechanism in variable loading, the effects of crack tip branching in fatigue crack growth retardation were examined. The characteristics of crack tip banching behavior was considered to micro structure. It was examined that the variation of crack tip branching angle. Crack tip branching was observed along the grain boundary of ferrite and pearlite structure. It was found that the abanching angle ranges from 25 to 53 degrees. Using the finite element method, the variable of crack driving force to branching angle was examined. The effective crack driving force ( $K_{\eff}$ ) decreased as the braching angle increases. The rate of decrease was 33% for the kinked type and 29% for the forked one. It was confirmed that the effect of crack tip branching is a very important factor in fatigue crack growth retardation. Therefore, crack branching effect should be considered building the hypoth- etical model to predict crack growth retardation.

  • PDF

밀어닐링 온도가 Ti-6Al-4V 합금의 미세조직 및 경도에 미치는 영향 (Effects of Mill Annealing Temperature on the Microstructure and Hardness of Ti-6Al-4V Alloys)

  • 서성지;권기훈;최호준;이기영;정민수
    • 열처리공학회지
    • /
    • 제32권6호
    • /
    • pp.263-269
    • /
    • 2019
  • The mechanism of microstructure and hardness changes during mill annealing of Ti-6Al-4V alloy was investigated. The annealing heat treatments were performed at $675{\sim}795^{\circ}C$ in vacuum for 2 hours, followed by air cooling. The microstructure was observed by using an optical microscope and X-ray diffraction, and hardness was measured by using a Rockwell hardness tester and micro Vickers hardness tester. The average grain size becomes smaller at $675^{\circ}C$ to $735^{\circ}C$ due to the formation of new grains rather than grain growth, but becomes larger at $735^{\circ}C$ to $795^{\circ}C$ due to growth of the already-formed grains rather than formation of new grains. The mill annealing temperature becomes higher, the ${\beta}$ phase fraction decreases and ${\alpha}$ phase fraction increases at room temperature. This is because the higher annealing temperature, the smaller amount of V present in the ${\beta}$ phase, and thus the ${\beta}$ to ${\alpha}$ transformation occurs more easily when cooled to room temperature. As the mill annealing temperature increases, the hardness value tends to decrease, mainly due to resolution of defects such as dislocations from $675^{\circ}C$ to $735^{\circ}C$ and due to grain growth from $735^{\circ}C$ to $795^{\circ}C$, respectively.

FeCo의 결정성 및 조성 제어를 통한 자기 특성 향상 (Enhanced magnetic properties of FeCo alloys by engineering crystallinity and composition)

  • 김단비;김지원;엄누시아;박성흠;임재홍
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2018년도 춘계학술대회 논문집
    • /
    • pp.32.1-32.1
    • /
    • 2018
  • Novel soft magnetic materials can be achieved by altering material properties such as morphology, composition, crystallinity, and grain size of soft magnetic alloys. Especially, magnetic properties (i.e., saturation magnetization, coarcivity) of soft magnetics are significantly affected by grain boundaries which act as a control of magnetic domain wall movement. Thus, we herein develop a two-step electroless plating method to control morphology and grain size of FeCo films for excellent magnetic properties. Accordingly, the chemical composition to control the degree of polarization of FeCo alloys was altered by electroless deposition parameters; for example, electrolyte concentration and temperature. The grain size and crystallinity of FeCo alloys was dramatically affected by the reaction temperature because the grain growth mechanism dominantly occurs at $90^{\circ}C$ where as the neucleation only happens at $50^{\circ}C$. By simply controlling the temperature, the micron-sized FeCo grains embedded FeCo film was synthesized where the large grains allow high magnetization originated from larger magnetic domain with low corecivity and the nano-sized grains allow excellent soft magnetic properties due to the magnetic correlation length.

  • PDF

기계적 밀링법으로 제조된 마그네슘 분말의 밀링시간에 따른 미세구조 변화와 부식거동 (Corrosion Behavior and Microstructural Evolution of Magnesium Powder with Milling Time Prepared by Mechanical Milling)

  • 안진우;황대연;김긍호;김혜성
    • 대한금속재료학회지
    • /
    • 제49권6호
    • /
    • pp.454-461
    • /
    • 2011
  • In this study, the relationship between corrosion resistance and microstructural characteristics such as grain size reduction, preferred orientation, and homogenous distribution of elements and impurity by mechanical milling of magnesium powder was investigated. Mechanical milling of pure magnesium powder exhibited a complex path to grain refinement and growth together with preferred orientation reversal with milling time. It was also found that anisotropic formation of dislocation on the basal plane of magnesium was initially the dominant mechanism for grain size reduction. After 60 hrs of milling, grain coarsening was observed and interpreted as a result of the strain relaxation process through recrystallization. In spite of the finer grain size and strong (002) texture developed in the sample prepared by spark plasma sintering at $500^{\circ}C$ for 5 min after mechanical milling for 2hrs, the sample showed a higher corrosion rate. The results from this study will be helpful for better understanding of the controlling factor for corrosion resistance and behaviors of mechanical milled magnesium powders.

Study on the Formation Mechanism of Hard Chrome Surface Morphology by Atomic Force Microscopy

  • Lee, B.K.;Park, Y.;Kim, Man;S.C. Kwon
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2002년도 춘계학술발표회 초록집
    • /
    • pp.35-35
    • /
    • 2002
  • Atomic force microscopy was applied to study the formation and growth mechanism of thin chrome layers prepared under various pulse plating conditions. The chrome was electro-deposited from an electrolyte bath containing 250 gl-l of chromic acid, 25 gl-l of sulfuric acid using direct current density of $1.6{\;}mA.$\textrm{mm}^{-2} and pulse currents with on-off time from 5 to 900 ms. The higher current density enhanced nucleation rate which resulted in refining grain size. The chrome growth kinetics determining nodule size and shape significantly depends on the duration of on-time rather than duration of off-time and on/off time ratio.

  • PDF

Co첨가에 의한 WC의 비정상입성장 (Effect of Co additive on the Abnormal Grain Growth of WC)

  • 이동범;채기웅
    • 한국세라믹학회지
    • /
    • 제41권2호
    • /
    • pp.131-135
    • /
    • 2004
  • WC에 소량의 Co를 첨가하여 그에 따른 미세조직의 변화를 관찰하였다. 순수한 WC를 성형하여 그 윗부분에 Co를 올려놓고 195$0^{\circ}C$에서 소결을 행한 결과, WC시편에서는 Co상이 놓여 액상을 형성한 영역으로부터 거리에 따라 입자의 크기와 모양이 다른 활발한 비정상입성장이 관찰되었다. 그러나, Co상이 놓인 영역으로부터 떨어진 시편 아래 영역에서는 낮은 치밀화와 함께 비정상입성장은 일어나지 않았다. 즉, Co 액상량은 WC의 비정상입성장 현상에 지대한 영향을 주었으며, 이러한 비정장입정장 현상은 2차원 핵생성 기구와 그에 따른 입성장기구로 설명이 가능하였다.

Ni-NiAl 확산대에서 $Ni_3Al$ 상의 형성과 반응확산 (Reaction diffusion and formation of$Ni_3Al$ phase at the Ni-NiAl diffusion couple)

  • 정승부
    • Journal of Welding and Joining
    • /
    • 제15권3호
    • /
    • pp.128-135
    • /
    • 1997
  • Reaction diffusion and formation of $Ni_3Al$phase with $L1_2$ structure have been studied in temperature range of 1432K to 1573K using the diffusion couple of (Ni-40, 5at%Al)/(Ni-14, 1at%Al) and (Ni-49, 2at%Al)/ (Nickel). The layer growth of Ni$_{3}$Al pyhase in the annealed diffusion couple was measured by optical microscope and electron probe microanalyzer (EPMA). The layer growth of $Ni_3Al$phase in diffusion zone obeyed the parabolic law without any indication of grain boundary effects. The layer growth of $Ni_3Al$phase in temperature range of 1423K to 1573K was mainly controlled by the volume diffusion mechanism. The rate of layer growth of $Ni_3Al$phase was found to be colsely related to the composition of intermetallic compound NiAl phase. The activation energy for layer growth of $Ni_3Al$phase was calculated to be 127kJ/mol.

  • PDF