The Properties on Ceramic/glass Composites of SiO2-B2O3-R(CaO, BaO, ZnO, Bi2O3 Borosilicate Glass System for Low Temperature Ceramics (저온 소결 세라믹스용 SiO2-B2O3-R(CaO, BaO, ZnO, Bi2O3 붕규산염계 세라믹/유리 복합체의 특성)

  • Kim, Kwan-Soo;Yoon, Sang-Ok;Shim, Sang-Heung;Park, Jong-Guk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.1
    • /
    • pp.19-24
    • /
    • 2007
  • The effects of $B_2O_3-SiO_2-R(R;CaO,\;BaO,\;ZnO,\;Bi_2O_3)$ borosilicate glass system on the sintering behavior and microwave dielectric properties of ceramic/glass composites were investigated as functions of modifier, glass addition ($30{\sim}50\;vol%$) and sintering temperature ($500{\sim}900^{\circ}C$ for 2 hrs). The addition of 50 and 45 vol% glass ensured successful sintering below $900^{\circ}C$. Sintering characteristics of the composites were well described in terms of modifier. Borosilicate glass enhanced the reaction with $Al_{2}O_{3}$ to form pores, second phases and liquid phases, which was responsible to component of modifier. Dielectric constant (${\varepsilon}_{r},\;Q{\times}f_{o}$) and temperature coefficient of resonant frequency (${\tau}_{f}$) of the composite with 50 and 45 vol% glass contents($B_{2}O_{3}:SiO_{2}:R=25:10:65$) demonstrated A-CaBS(7.8, 2,560 GHz, -81ppm/$^{\circ}C$), A-BaBs(5.8, 3.130 GHz, -64 ppm/$^{\circ}C$), A-ZnBS(5.7, 17,800 GHz, -21 ppm/$^{\circ}C$), A-BiBs(45 vol% glass in total)(8.3, 2,700 GHz, -45 ppm/$^{\circ}C$) which is applicable to substrate requiring an low dielectric properties.

Formation of $Al_2O_3$-Ceramics by Reactive Infiltration of Al-alloy into Insulation Fiber Board (Al-합금의 단열섬유판 반응침투에 의한 $Al_2O_3$-세라믹스의 형성)

  • 김일수
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.5
    • /
    • pp.483-490
    • /
    • 1997
  • Al2O3/metal composites were fabricated by oxidation and reaction of molten Al-alloy into two types of commercial Al2O3-SiO2 fibrous insulation board. The growth rate, composition and microstructure of these materials were described. An AlZnMg(7075) alloy was selected as a parent alloy. Mixed polycrystalline fiber and glass phase fiber were used as a filler. The growth surface of an alloy was covered with and without SiO2. SiO2 powder was employed as a surface dopant to aid initial oxidation of Al-alloy. Al-alloy, SiO2, fiber block and growth inhibitor CaSiO3 were packed sequentially in a alumina crucible and oxidized in air at temperature range 90$0^{\circ}C$ to 120$0^{\circ}C$. The growth rate of composite layer was calculated by measuring the mass increasement(g) per unit surface($\textrm{cm}^2$). XRD and optical microscope were used to investigate the composition and phase of composites. The composite grown at 120$0^{\circ}C$ and with SiO2 dopant showed rapid growth rate. The growth behavior differed a little depending on the types of fiber used. The composites consist of $\alpha$-Al2O3, Al, Si and pore. The composite grown at 100$0^{\circ}C$ exhibited better microstructure compared to that grown at 120$0^{\circ}C$.

  • PDF

Evaluation of surface gloss of composite resins (복합레진의 표면 광택에 대한 평가)

  • Ji-Eun Byun
    • Journal of Korean Academy of Dental Administration
    • /
    • v.11 no.1
    • /
    • pp.38-46
    • /
    • 2023
  • Composite resins, commonly used in clinical practice, have been developed to improve aesthetics to obtain smooth surfaces. Although the restored composite resin has a smooth surface, it gradually becomes rough over time. Therefore, this study measured glossiness to evaluate the surface of various composite resins and attempted to evaluate the maintenance of glossiness of composite resins by observing surfaces that change to roughness. Specimens were produced using resin used in clinical practice: Gradia direct anterior (GA), Tetric N-Ceram (TN), Ceram.X Sphere TEC one (CX), Filtek Z350XT (FT), Estelite sigma quick (ES). After creating a smooth surface with slide glass, five locations were randomly selected to measure surface gloss, and the average was the representative value of the specimen. Roughness was applied to the specimen under water pouring at the same speed and pressure using SiC paper #2400, 1200, and 400. The gloss unit of different SiC papers was measured. To evaluate the gloss unit and gloss retention between composite resins, one-way analysis of variance and Tukey multiple comparisons test were used. As a result of the study, there was a difference in gloss unit of specimens produced under the same conditions. Although the degree differed depending on the composite resin, there was also a difference in gloss retention. Based on the findings, composite resins show differences in gloss due to their different characteristics. Ceram.X Sphere TEC one (CX) showing the lowest gloss retention and Estelite sigma quick (ES) showing the highest.

Effects of SiC Particle Size and Inorganic Binder on Heat Insulation of Fumed Silica-based Heat Insulation Plates

  • Jo, Hye Youn;Oh, Su Jung;Kim, Mi Na;Lim, Hyung Mi;Lee, Seung-Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.4
    • /
    • pp.386-392
    • /
    • 2016
  • Heat insulation plates of fumed silica were prepared by mixing fumed silica, SiC powder and chopped glass fiber by a high speed mixer followed by pressing of the mixture powder in a stainless steel mold of $100{\times}100mm$. Composition of the plates, particle size of SiC, and type of inorganic binder were varied for observation of their contribution to heat insulation of the plate. The plate was installed on the upper portion of an electric furnace the inside temperature of which was maintained at $400^{\circ}C$ and $600^{\circ}C$, for investigation of heat transfer through the plate from inside of the electric furnace to outside atmosphere. Surface temperatures were measured in real time using a thermographic camera. The particle size of SiC was varied in the range of $1.3{\sim}17.5{\mu}m$ and the insulation was found to be most excellent when SiC of $2.2{\mu}m$ was incorporated. When the size of SiC was smaller or larger than $2.2{\mu}m$, the heat insulation effect was decreased. Inorganic binders of alkali silicate and phosphate were tested and the phosphate was found to maintain the heat insulation property while increasing mechanical properties.

Effect of Glass Composition on the Properties of Glass-infiltrated Alumina(I) : Effect of Al2O3 (유리가 침투된 알루미나 복합체의 물성에 미치는 유리조성의 영향(I): Al2O3의 영향)

  • 이재희;김철영
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.3
    • /
    • pp.301-308
    • /
    • 2003
  • Glass-infiltrated alumina, which can be used as an all-ceramic dental crown, was prepared. The glasses in the system of SiO$_2$-B$_2$O$_3$-Al$_2$O$_3$-CaO-La$_2$O$_3$with various amount of $Al_2$O$_3$infiltrated into a porous sintered alumina. The effect of $Al_2$O$_3$on the infiltration characteristics and its mechanical strength were studied. The corrosion of the sintered alumina by infiltrated glasses was prevented by increasing the amount of $Al_2$O$_3$in the glass batches, this increased the bending strength of the glass infiltrated alumina composite. The crack like voids in the sintered alumina was a cause of the deteriorating the mechanical strength of the composite, and this can be eliminated by sintering the alumina at 130$0^{\circ}C$. Glass infiltration under the vacuum atmosphere enhanced the hording strength of the composite up to 453$\pm$31 MPa.

Synthesis and Characterization of Particle-filled Glass/G lass-Ceramic Composites for Microelectronic Packaging (I)

  • Hong, Chang-Bae;Lee, Kyoung-Ho
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.6 no.1
    • /
    • pp.11-21
    • /
    • 1999
  • For microelectronic packaging application, the crystallizable glass powder in CaO-$A1_2O_3-SiO_2-B_2O_3$system was mixed with various amounts of alumina inclusions (\approx 4 $\mu \textrm{m}$), and its sintering behavior, crystallization behavior, and dielectric constant were examined in terms of vol% of alumina and the reaction between the alumina and the glass. Sintering of the CASB glass powder alone at $900^{\circ}C$ resulted in full densification (99.5%). Sintering of alumina-filled composite at $900^{\circ}C$ also resulted in a substantial denslfication higher than 97% of theoretical density, In this case, the maximum volume percent of alumina should be less than 40%. XRD analysis revealed that there was a partial dissolution of alumina into the glass. This alumina dissolution, however, did not show the particle growth and shape accommodation. Therefore, the sintering of both the pure glans and the alumina-filled composite was mainly achieved by the viscous flow and the redistribution of the glass. Alumina dissolution accelerated the crystallization initiation time at $1000^{\circ}C$ and hindered the densification of the glass. Dielectric constants of both the alumina-filled glass and the glass-ceramic composites were increased with increasing alumina content and followed rule of mixture. In case of the glass-ceramic matrix composites showed relatively lower dielectric constant than the glass matrix composite. Furthermore, as alumina content increased, crystallization behavior of the glass was changed due to the reaction between the glass and the alumina. As alumina reacted with the glass matrix, the major crystallized phase was shifted from wollastonite to gehlenite. In this system, alumina dissolution strongly depended on the particle size: When the particle size of alumina was increased to 15 $\mu\textrm{m}$, no sign of dissolution was observed and the major crystallized phase was wollastonite.

  • PDF

High Frequency Dielectric Properties of $CaF_2$ filled Glass-Composites ($CaF_2$가 Filler로 첨가된 유리복합체의 고주파 유전특성)

  • Kim, Sun-Young;Lee, Kyoung-Ho;Kim, Sung-Won
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05c
    • /
    • pp.277-281
    • /
    • 2003
  • Effects of $CaF_2$ addition as a filler on the high frequency dielectric properties and sintering of CaO-$Al_2O_3-SiO_2-B_2O_3$(CASB) and ZnO-MgO-$B_2O_3-SiO_2$(ZMBS) glass composites were investigated. The optimal glass composition in the CASB system was 33.0CaO-$17.0Al_2O_3-35.0SiO_2-15.0B_O_3$(in wt%). The corresponding dielectric properties were k=8.1 and $Q{\times}fo$=1,200GHz. The sintering temperature was $800{\mu}m$. In case of 2MBS system, 25.0ZnO-25.0MgO-20.0$B_2O_3-30.0SiO_2$(in wt%) glass showed k=6.8 and $Q{\times}fo$=5,200GHz when it was sintered at $750^{\circ}C$. The maximum amount of $CaF_2$ in the CASB and 2MBS glass system without any detrimental effect on the sintering was 25.0 v/o and 15.0 v/o, respectively. The addition of $CaF_2$ in the glass systems improved the high frequency dielectric properties. In case of CASB+$CaF_2$ composite, k was 7.1 and $Q{\times}fo$ was 2,300GHz. And in case of 2MBS+$CaF_2$ composite, k was 5.9 and $Q{\times}fo$ was 8,100GHz. $CaF_2$ addition also reduced sintering temperature. Effects of $CaF_2$ on the dielectric and sintering properties was analyzed in terms of viscosity and crystallization behavior changes due to the interaction between $CaF_2$ and the glass systems.

  • PDF

Organic-inorganic Nano Composite Membranes of Sulfonated Poly(Ether Sulfone-ketone) Copolymer and $SiO_2$ for Fuel Cell Application

  • Lee, Dong-Hoon;Park, Hye-Suk;Seo, Dong-Wan;Kim, Whan-Gi
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.487-488
    • /
    • 2006
  • Novel bisphenol-based wholly aromatic poly(ether sulfone-ketone) copolymer containing pendant sulfonate groups were prepared by direct aromatic nucleophilic substitution polycondensation of 4,4-difluorobenzophenone, 2,2'-disodiumsulfonyl-4,4'-fluorophenylsulfone (40mole% of bisphenol A) and bisphenol A. Polymerization proceeded quantitatively to high molecular weight in N-methyl-2-pyrrolidinone at $180^{\circ}C$. Organic-inorganic composite membranes were obtained by mixing organic polymers with hydrophilic $SiO_2$ (ca. 20nm) obtained by sol-gel process. The polymer and a series of composite membranes were studied by FT-IR, $^1HNMR$, differential scanning calorimetry (DSC) and thermal stability. The proton conductivity as a function of temperature decreased as $SiO_2$ content increased, but methanol permeability decreased. The nano composite membranes were found to posse all requisite properties; Ion exchange capacity (1.2meq./g), glass transition temperatures $(164-183\;^{\circ}C)$, and low affinity towards methanol $(4.63-1.08{\times}10^{-7}\;cm^2/S)$.

  • PDF

Investigation on Lead-Borosilicate Glass Based Dielectrics for LTCC (Lead-Borosilicate Glass계 LTCC용 유전체에 대한 고찰)

  • Yoon, Sang-Ok;Oh, Chang-Yong;Kim, Kwan-Soo;Jo, Tae-Hyun;Shim, Sang-Heung;Park, Jong-Guk
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.6 s.289
    • /
    • pp.338-343
    • /
    • 2006
  • The effects of lead-borosilicate glass frits on the sintering behavior and microwave dielectric properties of ceramic-glass composites were investigated as functions of glass composition of glass addition ($10{\sim}50vol%$), softening point (Ts) of the glass, and sintering temperature of the composites ($500{\sim}900^{\circ}C$ for 2 h). The addition of 50 vol% glass ensured successful sintering below $900^{\circ}C$. Sintering characteristics of the composites were well described in terms of Ts. PbO addition in to the glass enhanced the reaction with $Al_{2}O_3$ to form liquid phase and $PbAl_{2}Si_{2}O_8$, which was responsible to lower Ts. Dielectric constant(${\epsilon}_r$), $Q{\times}f_0$ and temperature coefficient of resonant frequency (${\tau}_f$) of the composite with 50 vol% glass contents ($B_{2}O_{3}:PbO:SiO_{2}:CaO:Al_{2}O_3$ = 5:40:45:5:5) demonstrated 8.5, 6,000 GHz, $-70\;ppm/^{\circ}C$, respectively, which is applicable to substrate requiring a low dielectric constant. When the same glass composition was applied sinter $MgTiO_3\;and\;TiO_2,\;at\;900^{\circ}C$ (50 vol% glass in total), the properties were 23.8, 4,000 GHz, $-65ppm/^{\circ}C$ and 31.1, 2,500 GHz, $+80ppm/^{\circ}C$ respectively, which is applicable to filter requiring an intermidiate dielectric constant.

Effect of $Al_2O_3$ Particle Size on Thermal Properties of Glass-Ceramics for LTCC Material (저온동시소성용 결정화 유리의 필러 사이즈가 열적 특성에 미치는 영향)

  • Kim, Jin-Ho;Hwang, Seong-Jin;Lee, Sang-Wook;Kim, Hyung-Sun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.281-281
    • /
    • 2007
  • Low Temperature Co-fired Ceramic (LTCC) technology has been used in electronic device for various functions. LTCC technology is to fire dielectric ceramic and a conductive electrode such as Ag or Cu thick film below the temperature of $900^{\circ}C$ simultaneously. The glass-ceramic has been widely used for LTCC materials due to its low sintering temperature, high mechanical properties and low dielectric constants. To obtain the high strength, addition of filler, the microstructure should have various crystals and low pores in a composite. In this study, two glass frits were mixed with different alumina size(0.5, 2, 3.7um) and sintered at the range of $850{\sim}950^{\circ}C$. The microstructure, crystal phases, thermal and mechanical properties of the composites were investigated using FE-SEM, XRD, TG-DTA, Dilatomer. When the particle size of $Al_2O_3$ filler increased, the starting temperatures for the densification of the sintered bodies, onset point of crystallization, peak crystallization temperature in the glass-ceramic composites decreased gradually. After sintered at $900^{\circ}C$, the glass frits were crystallized as $CaAl_2Si_2O_8\;and\;CaMgSi_2O_6$. The purpose of our study is to understand the relationship between the $Al_2O_3$ particle size and thermal properties in composites.

  • PDF