• 제목/요약/키워드: Gas Pressure Sintering

검색결과 88건 처리시간 0.025초

유기바인더를 이용한 통기성 금형제작에 관한 연구 (A study on porous metal mold using organic binder)

  • 김경래;정성일;임용관;정해도;이석우;최헌종
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.1026-1029
    • /
    • 2002
  • Outlet of gas has been a big problem in deforming rubber or plastic in pressing mold. Air vent has been used to solve the problem, but it has weak points such as the increased cost, the increased number of process, and vent marks on the surface of a produce. In this study, the sintering method is used for making porous metal mold. Porous metal mold has many open pores, which are very small. When Porous metal mold is used for pressing mold, all process would be made short, produce cost would be down, and it would not leave vent marks on the surface of a produce. Porosity varies from sintering and pressing conditions, which are the pressure of compacting powder, the length of sintering time, sintering temperature and sintering atmosphere etc. This study will find optimized sintering temperature condition for the Porous metal mold.

  • PDF

Impact of Sintering Gas Pressure on Deep-red EuSi2O2N2 Phosphors

  • Deressa, Gemechu;Kim, Jongsu;Kim, Gwangchul
    • 반도체디스플레이기술학회지
    • /
    • 제19권2호
    • /
    • pp.22-25
    • /
    • 2020
  • Deep red EuSi2O2N2 phosphors were synthesized under various sintering gas pressures (1 atm, 2 atm, and 3 atm). They were in good agreement with the standard EuSi2O2N2 ICSD card # 41-6046 (a monoclinic crystal system with space group of P21/a). Their photoluminescence intensities were significantly increased with increasing the gas pressures. They showed a broad band emission peaking at 680 nm due to 4f65d1 - 4f7 of Eu2+ ion, which can be efficiently excited in the visible range up to 550 nm. The best one at 3 atm was applied for red LED based on blue chip, which showed the strong deep red emission.

질화규소의 가스압 소결 (GPS) 시간에 따른 마모거동 (Wear Behavior of Silicon Nitride Depending on Gas Pressure Sintering Time)

  • 이수완;김성호
    • 한국재료학회지
    • /
    • 제10권1호
    • /
    • pp.83-89
    • /
    • 2000
  • $Si_3N_4$에 2wt% $Al_2O_3$와 6wt% $Y_2O_3$을 첨가한 분말을 가스압 소결 방법으로 시편을 제조하였다. 이때 소결시 시간변화에 따른 공기 중에서 마모 특성을 비교하였다. 소결 시간에 따른 마모 특성의 변화는 기계적 성질, 즉, 파괴인성 등이 영향을 주는 것으로 나타났다. 소결 시간이 길어지면 큰 elongated 입자의 과잉성장에 따라 곡강도 및 파괴인성이 낮아져 이 결과 마모가 증가되었다. 이때 나타난 결과에 의하면 공기 중에서 질화규소의 마모특성에 영향을 주는 인자는 여러 가지 기계적 특성 중에서 파괴인성 및 곡강도가 미치는 영향이 크게 나타났다.

  • PDF

배향된 $\beta-Si_3N_4$ Whisker를 함유하는 $Si_3N_4$ 복합체의 기계적 특성에 미치는 소결조제와 소결온도의 영향 (Effect of Sintering Additives and Sintering Temperature on Mechanical Properties of the $Si_3N_4$ Composites Containing Aligned $\beta-Si_3N_4$ Whisker)

  • 김창원;최명제;박찬;박동수
    • 한국세라믹학회지
    • /
    • 제37권1호
    • /
    • pp.21-25
    • /
    • 2000
  • Gas pressure sintered silicon nitride based composites with 5 wt% $\beta$-Si3N4 whiskers were prepared, and the variations depending on sintering additives and sintering temperature were studied. Sintering additives were 6 wt% Y2O3-1 wt% MgO(6Y1M), 6 wt%Y2O3-1 wt% Al2O3(6Y1A), 6 wt% Y2O3-1 wt% SiO2(6Y1S), and whiskers were unidirectionally oriented by a modified tape casting technique. Samples were fully densified by gas pressure sintering at 2148 K and 2273 K. As the sintering temperature increased, the size of large elongated grains was increased. Three point flexural strength of 6Y1M and 6Y1M samples was higher than that of 6Y1S sample, and the strength decreased as the sintering temperature increased. The indentation crack length became shorter for the sample sintered at higher temperature, and the difference between the cracks length parallel to and normal to the direction of whisker alignment was decreased. In case of cracks 45$^{\circ}$off the whisker alignment direction, the crack length anisotropy disappeared.

  • PDF

절삭 공구용 다이아몬드 복합체의 저온 저압 소결 합성 및 후속 도전형 박막 공정 특성 연구 (A Study on the Sintering of Diamond Composite at Low Temperature Under Low Pressure and its Subsequent Conductive PVD Process for a Cutting Tool)

  • 조민영;반갑수
    • 한국산업융합학회 논문집
    • /
    • 제23권1호
    • /
    • pp.25-32
    • /
    • 2020
  • Generally, high-temperature, high-pressure, high-priced sintering equipment is used for diamond sintering, and conductivity is a problem for improving the surface modification of the sintered body. In this study, to improve the efficiency of diamond sintering, we identified a new process and material that can be sintered at low temperature, and attempted to develop a composite thin film that can be discharged by doping boron gas to improve the surface modification of the sintered body. Sintered bodies were sintered by mixing Si and two diamonds in different particle sizes based on CIP molding and HIP molding. In CVD deposition, CVD was performed using WC-Co cemented carbide using CH4 and H2 gas, and the specimen was made conductive using boron gas. According to the experimental results of the sintered body, as the Si content is increased, the Vickers hardness decreases drastically, and the values of tensile strength, Young's modulus and fracture toughness greatly increase. Conductive CVD deposited diamond was boron deposited and discharged. As the amount of boron added increased, the strength of diamond peaks decreased and crystallinity improved. In addition, considering the release processability, tool life and adhesion of the deposition surface according to the amount of boron added, the appropriate amount of boron can be confirmed. Therefore, by solving the method of low temperature sintering and conductivity problem, the possibility of solving the existing sintering and deposition problem is presented.

Effects of the Addition of $La_2O_3$ on Mechanical Properties and Machinability of $Si_3N_4$ Ball

  • Sang Yang Lee;Sung Ho Kim;Soo Wohn Lee
    • The Korean Journal of Ceramics
    • /
    • 제6권4호
    • /
    • pp.364-369
    • /
    • 2000
  • Silicon nitride with adding La$_2$O$_3$ was sintered by gas pressure sintering (GPS) technique at $1950^{\circ}C$, in $N_2$ gas at 3 MPa, for 2h. Mechanical properties such as hardness, flexural strength, and fracture toughness were determined as a function of the GPS holding time and the contents of La$_2$O$_3$ in silicon nitride. Also machinability of silicon nitride ball with various GPS holding time and amount of La$_2$O$_3$ was evaluated by magnetic fluid grinding (MFG) method. In this study it was found that machinability was influenced significantly with La$_2$O$_3$ contents. However, the different GPS holding time did not affect the machinability very much.

  • PDF

소결금속을 이용한 LPG 용기용 안전 밸브의 개발 (The Development of the Safety Valve for LP Gas Cylinder Using the Sintered Metal)

  • 임종국
    • 한국안전학회지
    • /
    • 제21권1호
    • /
    • pp.48-52
    • /
    • 2006
  • This study is a research of safety valve development for LP gas cylinder which use sintering metal. Re-searcher wishes to apply technology of sintering metal for safety valve development and do gas flow control. The basis of this study is most suitable fluid examination that to reduce gas accident. This research concluded following results. 1. When press pin length is 42mm to 45mm powder quantity is 0.25g, in case of press pin length 36mm to 42mm powder quantity is 0.2g, displayed fluid optimization. 2. When press pin length is 39mm and powder quantity is 0.25g, press pressure displayed fluid optimization at all interests from $1.2\;tons/cm^{2}\;to\;2\;tons/cm^{2}$. 3. When apparent density is about $5.0g/cm^{3}\;to\;4.5g/cm^{3}$, fluid optimization becomes.

Lu2O3-SiO2계 소결조제를 포함하는 Silicon Nitride의 소결 특성 및 기계적 거동 (Densification and Mechanical Properties of Silicon Nitride Containing Lu2O3-SiO2 Additives)

  • 이세훈;조춘래;박영조;고재웅;김해두
    • 한국세라믹학회지
    • /
    • 제48권5호
    • /
    • pp.384-389
    • /
    • 2011
  • Gas pressure sintering (GPS) of reaction bonded silicon nitride (RBSN) was performed using $Lu_2O_3-SiO_2$ additive and the properties were compared with those of specimens prepared using high purity $Si_3N_4$ powder. The relative density of RBSN and compacted $Si_3N_4$ powder were 68.9 and 47.1%, and total linear shrinkage after sintering at $1900^{\circ}C$ were 14.8 and 42.9%, respectively. High nitrogen partial pressure (5MPa) was required during sintering at $1900^{\circ}C$ in order to prevent the decomposition of the nitride and to promote the formation of SiC. The relative density and 4-point bending strength of RBSN and $Si_3N_4$ powder compact were 97.7%, 954MPa and 98.2%, 792MPa, respectively, after sintering at $1900^{\circ}C$. The sintered RBSN also showed high fracture toughness of 9.2MPam$^{1/2}$.

액상소결법에 의한 탄화규소 제조시 소결조제와 온도의 영향 (Influence of Sintering Additives and Temperature on Fabrication of LPS-SiC)

  • 정헌채;윤한기
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.266-270
    • /
    • 2004
  • SiC materials have been extensively studied for high temperature components in advanced energy system and advanced gas turbine because it has excellent high temperature strength, low coefficient of thermal expansion, good resistance to oxidation and good thermal and chemical stability etc. However, the brittle characteristics of SiC such as low fracture toughness and low strain-to fracture still impose a severe limitation on practical applications of SiC materials. For these reasons, SiC/SiC composites can be considered as a promising for various structural materials, because of their good fracture toughness compared with monolithic SiC ceramics. But, high temperature and pressure lead to the degradation of the reinforcing jiber during the hot pressing. Therefore, reduction of sintering temperature and pressure is key requirements for the fabrication of SiC/SiC composites by hot pressing method. In the present work, monolithic Liquid Phase Sintered SiC (LPS-SiC) was fabricated by hot pressing method in Ar atmosphere at $1800^{\circ}C$ under 20MPa using $Al_2O_3,\;Y_2O_3\;and\;SiO_2$ as sintering additives in order to low sintering temperature and sintering pressure. The starting powder was high purity $\beta-SiC$ nano-powder with all average particle size of 30mm. The characterization of LPS-SiC was investigated by means of SEM and three point bending test. Base on the composition of sintering additives-, microstructure- and mechanical property correlation, tire compositions of sintering additives are discussed.

  • PDF

Fe-TiC 복합재료 분말의 상압소결과 방전플라즈마소결 (Pressureless Sintering and Spark-Plasma Sintering of Fe-TiC Composite Powders)

  • 이병훈;배상원;배선우;;김지순
    • 한국분말재료학회지
    • /
    • 제22권4호
    • /
    • pp.283-288
    • /
    • 2015
  • Two sintering methods of a pressureless sintering and a spark-plasma sintering are tested to densify the Fe-TiC composite powders which are fabricated by high-energy ball-milling. A powder mixture of Fe and TiC is prepared in a planetary ball mill at a rotation speed of 500 rpm for 1h. Pressureless sintering is performed at 1100, 1200 and $1300^{\circ}C$ for 1-3 hours in a tube furnace under flowing argon gas atmosphere. Spark-plasma sintering is carried out under the following condition: sintering temperature of $1050^{\circ}C$, soaking time of 10 min, sintering pressure of 50 MPa, heating rate of $50^{\circ}C$, and in a vacuum of 0.1 Pa. The curves of shrinkage and its derivative (shrinkage rate) are obtained from the data stored automatically during sintering process. The densification behaviors are investigated from the observation of fracture surface and cross-section of the sintered compacts. The pressureless-sintered powder compacts show incomplete densification with a relative denstiy of 86.1% after sintering at $1300^{\circ}C$ for 3h. Spark-plasma sintering at $1050^{\circ}C$ for 10 min exhibits nearly complete densification of 98.6% relative density under the sintering pressure of 50 MPa.