This report presents a new technical approach for evaluating the fiber orientation of composites using small-angle light scattering (SALS). Glass fiber (GF)/polypropylene (PP) composites with different fiber orientations were prepared by drawing compression-molded specimens. The drawn samples were remelted and then annealed at $150^{\circ}C$ in order to induce a crystalline structure on the fiber surface, and then underwent SALS analysis. The samples showed a combination of circular and streak patterns. The model calculations demonstrated that the number of nuclei on the fiber surface and the thickness of the transcrystalline layer affected the sharpness and intensity of the streak pattern. In addition, the azimuthal angle of the streak pattern was found to be dependent on the direction of the transcrystalline layer, which correlated with the fiber direction. This correlation suggests that the fiber orientation in the composites can be easily evaluated using SALS.
최근에 널리 쓰이고 있는 섬유강화 복합재료는 플라스틱 재료가 갖고 있는 가공성의 장점을 충분히 발휘한 재료로서 모재인 수지와 강화재인 강화섬유로 구성되며 사용된 섬유의 종류에 따라 유리섬유강화플라스틱(GFRP : glass fiber reinforced plastic)과 탄소섬유강화플라스틱(CFRP : carbon fiber reinforced plastic)으로 구분된다. 이 두 복합재료가 건설, 선박, 자동차 그리고 우주항공분야에 이르기까지 거의 모든 산업에서 다양하게 이용되고 있다. (중략)
산업부산물의 플라이애쉬와 실리카흄 및 국내 부존자원이 풍부한 규사분말, 생석회 및 발포용 알루미늄 분말과 취성개선을 위한 보강용 섬유를 사용한 경량 고강도의 시멘트복합체의 개발을 위하여 오토클래브 양생에 의한 열수 알카리분위기에서의 섬유 자체의 열화현상을 조사함과 아울러 배합요인별로 건재용 경량섬유보강 규산칼슘계 시멘트복합에를 제조하여 그 역학적 특성에 관한 연구를 수행하였다. 시험결과, 탄소섬유 및 내알카리성 유리섬유는 보강용 섬유로서 적합함이 확인되었으며, 경량 섬유보강 규산칼슘계 시멘트복합체의 압축, 인장, 휨강도는 플라이애쉬와 실리카흄 혼입율 및 섬유혼입율이 증가함을 따라 증가하는 경향을 나타내었고 또한 섬유혼입율 증가에 따라 현저히 휨인성이 증가하였으며, 탄소섬유보강의 경유가 유리섬유보강의 경우에 비하여 압축, 인장, 휨강도 및 휨인성은 다소 높은 경향을 나타내었다.
이 연구에서는 조적벽체의 내진보강을 위하여 프리스트레스트 강봉 및 유리섬유 망을 이용하여 개발된 비부착 공법의 구조적 효율성을 평가하였다. 주요 실험변수는 강봉 및 유리섬유 망의 개별 보강과 강봉과 유리섬유 망의 복합 보강이다. 실험결과 제안된 보강공법은 조적벽의 내력, 강성 및 연성향상에 효율적이었다. 보강되지 않은 조적벽의 횡하중 내력, 최대내력 이전의 강성 및 에너지소산 능력과 비교할 때, 유리섬유 망으로 보강된 벽체에서의 그 증가비는 각각 110%, 120% 및 360%이며, 프리스트레스트 강봉으로 보강된 벽체에서의 그 증가비는 각각 140%, 130% 및 510%이며, 유리섬유 망과 강봉으로 보강된 벽체에서의 그 증가비는 각각 160%, 130% 및 840%이었다. 제시된 기술로 보강된 조적벽의 횡하중 내력은 Yang et al.의 제안식을 이용한 예측값과 비교적 잘 일치하였다. 즉, 제안된 기술은 조적벽체의 내진보강을 위한 적용성으로서 구조적 잠재력이 높았다.
Kim, Namil;Lee, Jung-Seok;Hwang, Byung-Kook;Bae, Seokhu;Yoon, Jeong-Hwan;Yun, Juho
Elastomers and Composites
/
제54권2호
/
pp.135-141
/
2019
Polyphenylene sulfide (PPS) was filled with glass fiber (GF), aramid fiber (AF), and solid lubricants to improve the mechanical properties and wear resistance. The addition of GF effectively enhanced the tensile strength, flexural modulus, and impact strength of PPS, while solid lubricants such as polytetrafluoroethylene (PTFE), molybdenum disulfide ($MoS_2$), and tungsten disulfide ($WS_2$) lowered the friction coefficients of the composites to below 0.3. The ball nut and motor pulley of the electric power steering (EPS) were manufactured using the PPS composites, and feasibility was ascertained thereafter by conducting the durability test. The composites filled with GF and AF showed high mechanical strength, but slip occurred at the interface between the pulley and belt while testing above $50^{\circ}C$. When small amounts of lubricants were added, the slip was no longer detected because of the suppression of friction heat. It is realized that the low friction as well as high mechanical properties is important to ensure the reliability of plastic pulleys.
폐 디스플레이에서 발생하는 플라스틱을 재활용하여 실용적이고 경제성 있는 재생복합소재의 개발에 기여할 목적으로 ABS/PE(50/50과 20/80), ABS/GF (90/10) 복합 소재의 조성이 연신율에 미치는 효과를 연구하였다. PE 함량을 50%에서 80%로 증가시킨 폐플라스틱 재생복합소재의 인장시험 결과 전반적으로 연신율이 2.4%에서 13%로 증가하는 것이 관찰되었으나 유리섬유 첨가 시 인장강도와 연신율 모두 현저하게 감소하였다. 이러한 사실에 비추어 볼 때 PE의 함량에 따라 인장강도 등 다양한 기계적 특성의 조절이 가능함을 알 수 있었고 무엇보다도 플라스틱 사출성형에 투입되는 재생복합소재의 특성 중 아주 중요한 연신율을 향상시키는데 PE의 효과가 현저함을 알 수 있었다. 이는 ABS 자체의 우세한 비정질성이 결정성을 띈 PE의 첨가로 인해서 광범위하게 결정화된 결과 폐플라스틱 입자들 사이의 전단 응력이 감소하기 때문인 것으로 간주된다.
압축하중 및 굽힘하중을 받는 유리섬유플라스틱(GFRP) 표피/ 알루미늄 하니컴 코어(GF-AH) 하이브리드 복합재료의 음향방출(AE) 특성을 다양한 파괴과정과 연결시켜 연구하였다. 표피층 파괴, 표피/코어간의 계면박리, 하니컴 알루미늄 벽의 국부적인 소성항복 좌굴 및 셀벽간의 접착수지 박리와 같은 다양한 파괴모드가 하니컴 코어/GFRP표피 복합재를 이용한 AE주파수 분포 해석과 진폭분포 해석결과를 통해 분류되었다. 높은 진폭을 가진 AE 사상율의 분포는 셀벽 접착수지의 파괴, 표피층과 심층 사이의 박리및 미세파괴, 섬유파단에 대응하였으며 다른 피크 주파수의 분포는 알루미늄 셀벽의 소성변형, 셀벽간의 마찰로부터 발생한 것이다. 결론적으로 GF-AH 하이브리드 복합재료의 파괴거동 특성은 AE기법을 활용한 비파괴 평가를 통해 분석 가능하였다.
Thermosetting matrix composites have disadvantages in terms of moulding time, repairability and manufacturing cost. Thus the high-performance thermoplastic composites to eliminate such disadvantages have been developed so far. As a result of environmental and economical concerns, there is a growing interest in the use of thermoplastic composites. However, since their mechanical properties are very sensitive to the environment such as moisture, temperature etc., those behaviors need to be studied. Particularly the temperature is a very important factor influencing the mechanical behavior of thermoplastic composites. The effect of temperature have not yet been fully quantified. Since engineering applications of reinforced composites necessitate their fracture mechanic characterization, work is in progress to investigate the fracture and related failure behavior. An approach which predicts the tensile strength was perpormed in the tensile test. The main goal of this work is to study the effect of temperature on the result of tensile test with respect to GF/PE composite. The tensile strength and failure mechanisms of GF/PE composites were investigated in the temperature range 6$0^{\circ}C$ to -5$0^{\circ}C$. The tensile strength increased as the fiber volume fraction ratio increased. The tensile strength showed the maximum at -5$0^{\circ}C$, and it tended to decrease as the temperature increased from -5$0^{\circ}C$. The major failure mechanism was classified into the fiber matrix debonding, the fiber pull-out, the delamination and the matrix deformation.
This study has been investigated about the influence of moisture environment properties in the unidirectional and cross laminated carbon fiber/epoxy and glass fiber/epoxy composites. As a results, it was found that the weight gain of water increased with the immersion time and the mechanical properties were decreased with the weight gain of water. And it was also shown that the mechanical properties of carbon fiber/epoxy laminates were better than those of glass fiber/epoxy laminates. And a gap of the mechanical properties between the two kinds of laminates was increasing with the immersion time in distilled water of 80$^{\circ}C $. Mechanical properties which decreased by moisture absorption in the CF and GF reinforced laminates were recovered up to some extent by drying in oven at 80$^{\circ}C $ for 10 days.
In the study, tensile, compression and in-plane tests about longitudinal direction of glass fiber were performed. Also, to obtain the material properties of GFRP fabric composite, tensile test was performed. All test were performed by the test method of ASTM. Maximum compressive strength was smaller than the maximum tensile strength at the longitudinal direction test results. Elastic modulus of the tensile and compressive was almost similar at the compression test results in the longitudinal direction. Based on the GFRP fabric composite test results, GF91 was showed good performance at maximum compressive, maximum strain and elastic modulus.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.