Influence of Graphite Epoxy Composite Material on the Electrochemical Galvanic Corrosion of Metals (금속재료의 전기화학적 갈바닉 부식에 미치는 GECM의 영향)

  • Yoo, Y.R.;Son, Y.I.;Shim, G.T.;Kwon, Y.H.;Kim, Y.S.
    • Corrosion Science and Technology
    • /
    • v.8 no.1
    • /
    • pp.27-39
    • /
    • 2009
  • Non metallic composite materials, for example, GECM(graphite epoxy composite material) show high specific strength because of low density. These kinds of non metallic composite materials improved the structural effectiveness and operation economics. However, if these materials contacted several metals, corrosion can be arisen since non metallic composite materials have electrical conductivity. This paper dealt with galvanic corrosion between graphite epoxy composite material and several metals. Base on the electrochemical galvanic corrosion test between GECM and metals, corrosion current of carbon steel and aluminium increased with time but corrosion current of stainless steels and titanium decreased and galvanic potential increased. This behavior shows the galvanic corrosion depends upon the presence of passive film. Also, galvanic effect of GECM coupled with ferrous alloys and non-ferrous alloys was lower than that of 100% graphite, which is attributed to lower exposed area of graphite fiber in the GECM than apparent area of the GECM specimen used for the calculation of galvanic current in this work.

Galvanic Corrosion Behavior between Carbon Steel Bolted GECM(Graphite Epoxy Composite Material)/Al plates (탄소강 볼트 체결된 GECM(Graphite Epoxy Composite Material)/Al 판재 간의 갈바닉 부식 거동)

  • Kim, Youngsik;Park, Sujin;Yoo, Youngran
    • Corrosion Science and Technology
    • /
    • v.12 no.1
    • /
    • pp.12-26
    • /
    • 2013
  • This work focused on galvanic corrosion of carbon steel bolted GECM/Al plates by long-term test in tap water and NaCl solutions. Test product was carbon steel bolted between cross packed GECM and painted aluminium. Tests for the product and coupled parts determined corrosion rate in tap water and NaCl solutions. Also, using a potentiostat and salt water sprayer, galvanic test was done. In galvanic test on carbon steel bolted GECM/Al plates, corrosion of carbon steel bolt was faster in series of tap water>1% NaCl solution>3.5% NaCl solution. In galvanic couple between aluminium and carbon steel bolt, their corrosion rates were higher than those of single specimen. In galvanic couple between GECM, aluminium, and carbon steel bolt, corrosion behaviors of carbon steel bolt and aluminium were changed due to different corrosion mechanism in tap water and chloride solution.

Effect of Area Ratio on Galvanic Corrosion Between Metallic Materials and GECM in 3.5% NaCl Solution (3.5% NaCl 수용액 중에서의 금속과 GECM의 갈바닉 부식에 미치는 면적비의 영향)

  • Kim, Y.S.;Lim, H.K.;Sohn, Y.I.;Yoo, Y.R.;Chang, H.Y.
    • Corrosion Science and Technology
    • /
    • v.9 no.1
    • /
    • pp.39-47
    • /
    • 2010
  • Galvanic coupling between GECM(graphite epoxy composite material) and metallic materials can facilitate corrosion of metals and alloys because GECM is noble and electrically conductive. Galvanic corrosion is affected by many factors including metallic materials, area ratio, surface condition, and corrosivity. This work aims to evaluate the effect of area ratio on galvanic corrosion between GECM and several metals. In the case of glavanic coupling of carbon steel and Al to GECM, corrosion rate increased with increasing area ratio. Corrosion rate of sensitized STS 316S stainless steel decreased a little at an area ratio 1:1 but increased at an area ratio 30:1. It is considered to be due to that area ratio affects galvanic corrosion more in less corrosion resistant alloys. However, in case of STS 316 and Ti, galvanic coupling reduces corrosion rate by the formation of passive film.

Influences of Anodizing and Thermal Oxidation on the Galvanic Corrosion between Aluminium and Titanium and GECM (GECM과 Al 및 Ti 간의 갈바닉 부식에 미치는 양극산화 및 열산화의 영향)

  • Kim, Young-Sik;Lim, Hyun-Kwon;Sohn, Young-Il;Yoo, Young-Ran;Chang, Hyun-Young
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.6
    • /
    • pp.514-522
    • /
    • 2010
  • Graphite epoxy composite material (GECM) shows high specific strength and its application in the aerospace industry is gradually increasing. However, its application would induce galvanic corrosion between GECM and metallic materials. This work focused on the effects of anodizing and thermal oxidation on galvanic corrosion in a 3.5% NaCl solution between GECM and aluminium and titanium. In the case of anodized aluminium, galvanic corrosion resistance to the GECM was greatly improved by the anodizing treatment regardless of area ratio. In the case of anodized titanium, the anodizing by a formation voltage of 50V increased corrosion resistance of titanium in galvanic tests. Thermal oxidation of titanium also improved corrosion resistance of Ti to GECM.

Corrosion Behavior of the parts of Carbon Steel Bolted GECM(Graphite Epoxy Composite Material)/Al plates (탄소강 볼트 체결된 GECM(Graphite Epoxy Composite Material)/Al 판재의 구성 부재의 부식 거동)

  • Kim, Youngsik;Park, Sujin;Yoo, Youngran
    • Corrosion Science and Technology
    • /
    • v.11 no.6
    • /
    • pp.232-241
    • /
    • 2012
  • This work focused on corrosion of carbon steel bolted GECM/Al parts in tap water and NaCl solutions. In tap water and NaCl solutions, open circuit potential of GECM and its potentials in a series of carbon steel bolt>Ti>Al became active. Regardless of test materials, open circuit potentials in tap water were noble, and increasing NaCl concentration, its potentials became active. Immersion test of single specimen showed that no corrosion occur in Ti and GECM. In tap water, carbon steel bolt didn't show red corrosion product and in chloride solutions, corrosion rate in 1% NaCl solution was greater than its rate in 3.5% NaCl solution and red corrosion product in 1% NaCl solution was earlier observed than that in 3.5% NaCl solution. It seems that this behavior would be related to zinc-coatings on the surface of carbon stee l bolt. On the other hand, aluminium was corroded in tap water and chloride solutions. Corrosion of aluminium in tap water was due to the presence of chloride ion in tap water by sterilizing process.

Effects of NaCl Concentration and Solution Temperature on the Galvanic Corrosion between CFRP and AA7075T6

  • Hur, S.Y.;Kim, K.T.;Yoo, Y.R.;Kim, Y.S.
    • Corrosion Science and Technology
    • /
    • v.19 no.2
    • /
    • pp.75-81
    • /
    • 2020
  • To reduce structural weight, light metals, including aluminum and magnesium alloys, have been widely used in various industries such as aircraft, transportation and automobiles. Recently, composite materials such as Carbon Fiber Reinforced Plastics (CFRP) and Graphite Epoxy Composite Material (GECM) have also been applied. However, aluminum and its alloys suffer corrosion from various factors, which include aggressive ions, pH, solution temperature and galvanic contact by potential difference. Moreover, carbon fiber in CFRP and GECM is a very efficient cathode, and very noble in the galvanic series. Galvanic contact between carbon fiber composites and metals in electrolytes such as rain or seawater, is highly undesirable. Notwithstanding the potentially dangerous effects of chloride and temperature, there is little research on galvanic corrosion according to chloride concentration and temperature. This work focused on the effects of chloride concentration and solution temperature on AA7075T6. The increased galvanic corrosion between CRFP and AA7075T6 was evaluated by electrochemical experiments, and these effects were elucidated.