• 제목/요약/키워드: Friction Welded

검색결과 304건 처리시간 0.027초

인코넬 합금과 스테인레스 강의 마찰용접 특성 연구 (A Study on the friction weldability of inconel alloy-stainless steel)

  • 김의환;민택기
    • 한국공작기계학회논문집
    • /
    • 제10권2호
    • /
    • pp.73-78
    • /
    • 2001
  • In this study, the friction weldability and properties of inconel alloy(IN738LC) to stainless steel (STS304) was investigat-ed. Upset length increased according to increment of friction pressure and time. The tensile strength of the friction weld-ing reached 85% of the STS304 base metal strength under the conditions of 8 sec friction time, 50MPa friction pressure and 150 MPa upset pressure. From the result of fracture surface analysis, IN738LC section can be joined with STS 304 materials in shape of a convex lens. Also, the temperature of welded interface was measured with k-type thermocouple. Finally the plastic flow confirmed at the welded interface STS304 by micro test.

  • PDF

자동차 후진기어용 축재(SM 45C-SF 45)의 이종마찰용접 특성 (Mechanical Properties of Friction Welded SM 45C-SF 45 Joints for Automobile Reverse Idle Gear Shaft Applications)

  • 공유식;윤성필;김선진
    • 대한기계학회논문집A
    • /
    • 제34권1호
    • /
    • pp.85-90
    • /
    • 2010
  • 자동차 후진기어용 축재는 단조재로서 그 형상은 복잡하고 열처리 및 가공공정이 어려울 뿐 아니라, 제품수명 저하 등의 문제점으로 인한 경제적 손실이 크다. 따라서 종전의 일체형 단조품을 캠 형상 부분만을 기존의 단조품(SF 45)으로 사용하고, 나머지 축 부분은 일반 기계구조용 탄소강재(SM 45C)로 대체를 위한 이종마찰용접을 적용하였다. 마찰용접 변수인 회전수, 마찰압력, 업셋압력, 가열시간, 업셋시간 등의 상호작용에 의한 용접품질과의 상관관계를 고찰하였으며, 최적조건에서 마찰용접을 한 후 용접재(as-welded)와 고주파 열처리를 시행한 후열처리재(PWHT)의 접합부 특성을 비교 고찰하였다. 이는 종전의 일체형 단조품에 비해 단조비용 절감, 피로수명향상, 기계가공에 따른 공정수 및 재료절감 등의 경제적 파급효과가 클 것으로 기대된다.

고주파스핀들을 이용한 박판 알루미늄합금소재(Al5052-H32)의 마찰교반접합에 의한 용접성 평가 (The Weldability of a Thin Friction Stir Welded Plate of Al5052-H32 using High Frequency Spindle)

  • 주영환;박영찬;이용문;김광호;강명창
    • 한국기계가공학회지
    • /
    • 제16권1호
    • /
    • pp.90-95
    • /
    • 2017
  • Recently, smaller and lighter products have become of interest in industry applications that increasingly demand thin plate joints of thickness 1.0 mm or less using friction stir welding. In this study, high frequency spindles that run at 3,500-6,500 rpm are introduced for thin friction stir-welded plates. Weldability tests are performed for the butt-joint method of Al5052-H32 alloy of 1.0 mm thickness under 3,500-6,500 rpm spindle revolution with 250-400 mm/min feed speed. An optical microscope was used to analyze the bid structure of the welded zone and stir zone. The tensile-strength and hardness of the welded zone were then measured.

마찰교반접합된 니켈기 초합금의 기계적 특성 (Mechanical Properties of Friction Stir Welded Ni-Base Superalloy)

  • 송국현
    • 한국재료학회지
    • /
    • 제21권7호
    • /
    • pp.410-414
    • /
    • 2011
  • This study was carried out to evaluate the microstructures and mechanical properties of a friction stir welded Ni based alloy. Inconel 600 (single phase type) alloy was selected as an experimental material. For this material, friction stir welding (FSW) was performed at a constant tool rotation speed of 400 rpm and a welding speed of 150~200 mm/min by a FSW machine, and argon shielding gas was utilized to prevent surface oxidation of the weld material. At all conditions, sound friction stir welds without any weld defects were obtained. The electron back-scattered diffraction (EBSD) method was used to analyze the grain boundary character distributions (GBCDs) of the welds. As a result, dynamic recrystallization was observed at all conditions. In addition, grain refinement was achieved in the stir zone, gradually accelerating from 19 ${\mu}m$ in average grain size of the base material to 5.5 ${\mu}m$ (150 mm/min) and 4.1 ${\mu}m$ (200 mm/min) in the stir zone with increasing welding speed. Grain refinement also led to enhancement of the mechanical properties: the 200 mm/min friction stir welded zone showed 25% higher microhardness and 15% higher tensile strength relative to the base material.

육성용접된 Inconel 718 합금의 마찰교반을 이용한 개질처리 효과 (Effect of Surface Modification by Friction Stir Process on Overlap Welded Inconel 718 Alloy)

  • 송국현;홍도형;양병모
    • 한국재료학회지
    • /
    • 제23권9호
    • /
    • pp.501-509
    • /
    • 2013
  • To evaluate the development of the microstructure and mechanical properties on surface modified and post-heattreated Inconel 718 alloy, this study was carried out. A friction stir process as a surface modification method was employed, and overlap welded Inconel 718 alloy as an experimental material was selected. The friction stir process was carried out at a tool rotation speed of 200 rpm and tool down force of 19.6-39.2 kN; post-heat-treatment with two steps was carried out at $720^{\circ}C$ for 8 h and $620^{\circ}C$ for 6 h in vacuum. To prevent the surface oxidation of the specimen, the method of using argon gas as shielding was utilized during the friction stir process. As a result, applying the friction stir process was effective to develop the grain refinement accompanied by dynamic recrystallization, which resulted in enhanced mechanical properties as compared to the overlap welded material. Furthermore, the post-heat-treatment after the friction stir process accelerated the formation of precipitates, such as gamma prime (${\gamma}^{\prime}$) and MC carbides, which led to the significant improvement of mechanical properties. Consequently, the microhardness, yield, and tensile strengths of the post-heat-treated material were increased more than 110%, 124% and 85 %, respectively, relative to the overlap welded material. This study systematically examined the relationship between precipitates and mechanical properties.

선외기 샤프트용 재료의 마찰용접에 관한 연구 (Study on Friction Welding of SUS431 and SCM21 for External Shaft of Ship)

  • 오세규;이종환;배명주;오명석
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제17권4호
    • /
    • pp.38-48
    • /
    • 1993
  • A study on friction welding of stainless steel bar(SUS431) to chrome molybdenum steel bar(SCM21) was accomplished experimentally through analysis for relations among friction welding conditions, tension test, hardness test, microstructure test and acoustic emission test. The results obtained are summarized as follows ; 1. Through friction welding of SUS431 bar to SCM21 bar, the optimum welding condition by considering on strength and toughness was found to be the range of heating time of 3-5 sec when the number of rotating speed of 2000rpm, heating pressure of 10kg/$mm^2$, and upsetting time of 4 sec. 2. Quantitative ralationship was identified between heating time($T_1$, sec) and tensile strength (${\sigma},\;kgf/mm^2$) of the friction welded joint and the relation equation is $\sigma$=52.62$T_1{^{0.06}}$. 3. Through AE test, quantitative relationship was confirmed between heating time($T_1$, sec) and total AE(N, counts) during welding, and the relation is computed as follows ; N=30413.6$e^{0.06T1}$. 4. It was confirmed that the quantitative ralationship exists between the tensile strength of the welded joints and AE cumulative counts. And the relation is computed as the following ; ${\sigma}$=16.37(ln N)- 116.4. 5. When ONZ=36500-41500 counts by $OT_1Z$=3~5sec, it was identified by experiment that the range of welded joint tensile strength is 55.6-57.7kgf/$mm^2$/ whose joint efficiency is more than 100%, and it was experimentally confirmed that the real-time nondestructive quality(strength) evaluation for the friction welded joints could be possible by acoustic emission technique.

  • PDF

마찰접합 된 A6063 합금의 미세조직과 기계적 특성 평가 (Evaluation of the Microstructures and Mechanical Properties on Friction Welded A6063 Alloy)

  • 김은혜;조형환;송국현
    • 한국재료학회지
    • /
    • 제27권5호
    • /
    • pp.276-280
    • /
    • 2017
  • This study was carried out to evaluate the developed microstructures and mechanical properties of friction welded A6063 alloy. For this work, specimens were prepared at a size of 12 mm ${\O}{\times}80mm$, and friction welding was carried out at a rotation speed of 2,000 RPM, friction pressure of $12kgf/cm^2$ and upset pressure of $25kgf/cm^2$. To perform an analysis of the grain boundary characteristic distributions, such as the grain size, orientation and misorientation angle distributions, the electron back-scattering diffraction method was used. In addition, in order to identify the dispersed intermetallic compounds of the base and welded materials, transmission electron microscopy was used. The experimental results found that the application of friction welding on A6063 led to significant grain refinement of the welded zone relative to that of the base material. Besides this, intermetallic compounds such as AlMnSi and $Al_2Cu$ were found to be dispersed with more refined size relative to that of the base material. This formation retains the mechanical properties of the welds, which results in the fracture aspect at the base material zone. Therefore, based on the developed microstructures and mechanical properties, the application of friction welding on A6063 could be used to obtain a sound weld zone.

STS304 와 SM15C 이종마찰용접재의 변형 및파괴거동 (Behavior of Deformation and Fracture in Friction Welded Materials of STS304 and SM15C)

  • 오환섭
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 1996년도 추계학술대회 논문
    • /
    • pp.161-166
    • /
    • 1996
  • In this study behavior of deformation and fracture under static tensile load in friction welded dissimilar materials and necking 0phenomenon occuring at tensile yeilding point were shown. Fibrous zone with view of macroscope and dimple pattren with a view of microscope were observed at shear surface.

  • PDF

WCu-Cu 전기접점의 마찰용접 특성 연구 (A Study on Friction weldability of Copper-Tungsten Sinterd Alloy to Copper)

  • 안용호;윤기갑;민택기;한병성
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1934-1937
    • /
    • 1999
  • A copper-tungsten sintered alloy(Cu-W) has been friction-welded to a tough pitch copper (Cu) in order to investigate friction weldability. The tensile strength of the friction welded joint was increased up to 87% of the Cu base metal under the condition of friction time 1.0 see, friction pressure 40MPa and upset pressure 100MPa, upset time 5.0 sec. And it is related to upset pressure rather than friction time. Mixed layer was formed in the Cu adjacent weld interface and W particles which were included in mixed layer could induce fracture in the Cu adjacent to the weld interface. Thickness of mixed layer was reduced as upset pressure increase.

  • PDF

Mg Alloy(AZ61) 마찰교반용접 조건에 따른 용접부의 온도와 기계적 특성변화 (Temperature and Mechanical Properties of Welded Joints Under Friction Stir Welding Conditions of Mg Alloy (AZ61))

  • 이우근;김정석;선승주
    • 한국생산제조학회지
    • /
    • 제26권4호
    • /
    • pp.378-386
    • /
    • 2017
  • Friction stir welding was performed using six welding conditions to evaluate the mechanical properties and microstructure of the welded zone based on its temperature change in the extruded plate of magnesium alloy AZ61. The welded zone temperature was measured using a thermocouple, and the maximum temperature ranges for the advancing and retreating sides were approximately $210-315^{\circ}C$ and $254-339^{\circ}C$, respectively. Depending on the welding conditions, a temperature difference of more than $100^{\circ}C$ was observed. In addition, the maximum yield strength and maximum tensile strength of the welded component was 84.4% and 96.9%, respectively, of those of the base material. For the temperatures exceeding $300^{\circ}C$, oxidation defects occurred in the weld zone, which decreased the mechanical strength of the weld zone. The microstructure and texture confirmed that fracture occurred because of the grain size deviation of the welding tool and the severe anisotropy of the texture of the welded joints.